CN103643498A
CN103643498A CN201310629190.9A CN201310629190A CN103643498A CN 103643498 A CN103643498 A CN 103643498A CN 201310629190 A CN201310629190 A CN 201310629190A CN 103643498 A CN103643498 A CN 103643498A
Authority
CN
China
Prior art keywords
parts
mass
knitwear
treating agent
cashmere
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310629190.9A
Other languages
English (en)
Inventor
陈开恩
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU RABBONI CLOTHING Co Ltd
Original Assignee
SUZHOU RABBONI CLOTHING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU RABBONI CLOTHING Co Ltd filed Critical SUZHOU RABBONI CLOTHING Co Ltd
Priority to CN201310629190.9A priority Critical patent/CN103643498A/zh
Publication of CN103643498A publication Critical patent/CN103643498A/zh
Pending legal-status Critical Current

Links

Abstract

本发明公开了一种针织品绒料起毛处理剂的制备工艺,包括如下步骤:1)将1-2质量份羟丙基甲基纤维素、25-30质量份丙烯酸乙酯、7-8质量份六偏磷酸钠、25-30质量份聚氧乙烯辛基苯基醇、15-17质量份硬脂酸、2-3质量份羟甲基丙烯酰胺、4-5质量份过硫酸钾、185-190质量份水混合,搅拌均匀;2)再加入5-7质量份石蜡、10-15质量份聚丙二醇及6-8质量份1,4-丁二醇混合,加热至50-60℃,搅拌使其完全混合均匀,冷却至室温,既得成品。本发明制备的针织品绒料起毛处理剂具有良好的防起毛效果。

Description

针织品绒料起毛处理剂的制备工艺
技术领域
本发明涉及针织品绒料起毛处理剂的制备工艺。
背景技术
针织品在使用一段时间之后,其表面很容易发生起毛现象,这不仅严重影响了其外观和使用效果,同时也影响了其使用寿命,因此,需要对针织品进行防起毛处理。 
发明内容
本发明的目的在于提供一种针织品绒料起毛处理剂的制备工艺,其制备的针织品绒料起毛处理剂具有良好的防起毛效果。
为实现上述目的,本发明的技术方案是设计一种针织品绒料起毛处理剂的制备工艺,包括如下步骤:
1)将1-2质量份羟丙基甲基纤维素、25-30质量份丙烯酸乙酯、7-8质量份六偏磷酸钠、25-30质量份聚氧乙烯辛基苯基醇、15-17质量份硬脂酸、2-3质量份羟甲基丙烯酰胺、4-5质量份过硫酸钾、185-190质量份水混合,搅拌均匀;
2)再加入5-7质量份石蜡、10-15质量份聚丙二醇及6-8质量份1,4-丁二醇混合,加热至50-60℃,搅拌使其完全混合均匀,冷却至室温,既得成品。 
本发明的优点和有益效果在于:提供一种针织品绒料起毛处理剂的制备工艺,其制备的针织品绒料起毛处理剂具有良好的防起毛效果。
具体实施方式
下面结合实施例,对本发明的具体实施方式作进一步描述。以下实施例仅用于更加清楚地说明本发明的技术方案,而不能以此来限制本发明的保护范围。
本发明具体实施的技术方案是:
实施例1
一种针织品绒料起毛处理剂的制备工艺,包括如下步骤:
1)将1质量份羟丙基甲基纤维素、25质量份丙烯酸乙酯、7质量份六偏磷酸钠、25质量份聚氧乙烯辛基苯基醇、15质量份硬脂酸、2质量份羟甲基丙烯酰胺、4质量份过硫酸钾、185质量份水混合,搅拌均匀;
2)再加入5质量份石蜡、10质量份聚丙二醇及6质量份1,4-丁二醇混合,加热至50℃,搅拌使其完全混合均匀,冷却至室温,既得成品。
实施例2
一种针织品绒料起毛处理剂的制备工艺,包括如下步骤:
1)将2质量份羟丙基甲基纤维素、30质量份丙烯酸乙酯、8质量份六偏磷酸钠、30质量份聚氧乙烯辛基苯基醇、17质量份硬脂酸、3质量份羟甲基丙烯酰胺、5质量份过硫酸钾、190质量份水混合,搅拌均匀;
2)再加入7质量份石蜡、15质量份聚丙二醇及8质量份1,4-丁二醇混合,加热至60℃,搅拌使其完全混合均匀,冷却至室温,既得成品。
实施例3
一种针织品绒料起毛处理剂的制备工艺,包括如下步骤:
1)将1.2质量份羟丙基甲基纤维素、28质量份丙烯酸乙酯、7.8质量份六偏磷酸钠、29质量份聚氧乙烯辛基苯基醇、16质量份硬脂酸、2.3质量份羟甲基丙烯酰胺、4.5质量份过硫酸钾、188质量份水混合,搅拌均匀;
2)再加入5.7质量份石蜡、12质量份聚丙二醇及6.8质量份1,4-丁二醇混合,加热至55℃,搅拌使其完全混合均匀,冷却至室温,既得成品。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。

Claims (1)

1.针织品绒料起毛处理剂的制备工艺,其特征在于,包括如下步骤:
1)将1-2质量份羟丙基甲基纤维素、25-30质量份丙烯酸乙酯、7-8质量份六偏磷酸钠、25-30质量份聚氧乙烯辛基苯基醇、15-17质量份硬脂酸、2-3质量份羟甲基丙烯酰胺、4-5质量份过硫酸钾、185-190质量份水混合,搅拌均匀;
2)再加入5-7质量份石蜡、10-15质量份聚丙二醇及6-8质量份1,4-丁二醇混合,加热至50-60℃,搅拌使其完全混合均匀,冷却至室温,既得成品。
CN201310629190.9A 2013-12-02 2013-12-02 针织品绒料起毛处理剂的制备工艺 Pending CN103643498A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310629190.9A CN103643498A (zh) 2013-12-02 2013-12-02 针织品绒料起毛处理剂的制备工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310629190.9A CN103643498A (zh) 2013-12-02 2013-12-02 针织品绒料起毛处理剂的制备工艺

Publications (1)

Publication Number Publication Date
CN103643498A true CN103643498A (zh) 2014-03-19

Family

ID=50248776

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310629190.9A Pending CN103643498A (zh) 2013-12-02 2013-12-02 针织品绒料起毛处理剂的制备工艺

Country Status (1)

Country Link
CN (1) CN103643498A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104195817A (zh) * 2014-08-27 2014-12-10 无锡市奇盛针织手套厂 一种毛织物抗起球剂及其制备方法
CN104264460A (zh) * 2014-08-27 2015-01-07 无锡市奇盛针织手套厂 一种抗起球抗静电羊毛织品处理剂及其制备方法

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104195817A (zh) * 2014-08-27 2014-12-10 无锡市奇盛针织手套厂 一种毛织物抗起球剂及其制备方法
CN104264460A (zh) * 2014-08-27 2015-01-07 无锡市奇盛针织手套厂 一种抗起球抗静电羊毛织品处理剂及其制备方法

Similar Documents

Publication Publication Date Title
CN102978935A (zh) 一种针织品绒料起毛处理剂及其制备方法
CN103726297A (zh) 抗紫外线面料的生产工艺
CN104452290A (zh) 枕套面料的整理工艺
CN104452292A (zh) 仿丝面料的整理工艺
CN104532557A (zh) 服装面料的整理工艺
CN104480705A (zh) 弹性面料的整理工艺
CN105274834A (zh) 针织面料的后整理工艺
CN103466985A (zh) 一种石墨烯水泥增强剂
CN103290688B (zh) 一种棉纺织物精练剂
CN103643498A (zh) 针织品绒料起毛处理剂的制备工艺
CN105332280A (zh) 针织面料的整理工艺
CN103710986A (zh) 针织品绒料起毛处理剂的制备方法
CN103643501A (zh) 织物柔软整理剂的制备工艺
CN105064012A (zh) 一种服装面料的整理工艺
CN103696266A (zh) 织物的抗菌整理工艺
CN103643492A (zh) 织物用柔软整理剂的制备方法
CN103643511A (zh) 免烫衬衫的生产方法
CN105130311A (zh) 一种添加剑麻纤维的增强型轻质保温砂浆及其制备方法
CN103643517A (zh) 一种纤维织物抗静电整理剂及制备方法
CN103132322A (zh) 一种纺织经线浆料及其制备方法
CN103643505A (zh) 牛仔服装的加工工艺
CN103757895A (zh) 一种棉衣整理液及其制备方法
CN103979809A (zh) 利用锂云母提锂渣制备少熟料白色硅酸盐水泥的方法
CN103757934A (zh) 一种棉织物与聚酯纤维混纺织物印染方法
CN106634638A (zh) 一种高性能强力胶水

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20140319