CN103603252B - 一种水泥路路基防渗水方法 - Google Patents

一种水泥路路基防渗水方法 Download PDF

Info

Publication number
CN103603252B
CN103603252B CN201310517318.2A CN201310517318A CN103603252B CN 103603252 B CN103603252 B CN 103603252B CN 201310517318 A CN201310517318 A CN 201310517318A CN 103603252 B CN103603252 B CN 103603252B
Authority
CN
China
Prior art keywords
roadbed
road
waterproofing course
water spray
sealing substance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310517318.2A
Other languages
English (en)
Other versions
CN103603252A (zh
Inventor
尚诚德
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310517318.2A priority Critical patent/CN103603252B/zh
Publication of CN103603252A publication Critical patent/CN103603252A/zh
Application granted granted Critical
Publication of CN103603252B publication Critical patent/CN103603252B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种水泥路路基防渗水方法,涉及道路建设技术领域,首先在路面浇筑之前在路基上铺设一层具有耐腐蚀性能的防水层,将路基隔离起来,该防水层能够粘附在路基上;在铺设有防水层的路基上浇筑混凝土铺设路面,在路面铺设好5-8小时后,在接缝中填充密封物质,并将密封物质填充至与路面上表面齐平,并压实;在密封物质填充1-2小时之后,用喷水器往填充物质上进行第一次喷水,待有水流出即可;第一次喷水结束后12小时再进行第二次喷水,在第二次喷水的同时对路面进行适当洒水,待有水流出即可;检查接缝是否完全没有缝隙,如有缝隙在接缝中再灌入填充物质即可。本发明将传统的切缝,灌缝,嵌缝养护工作集中起来,一次完成,具有省工,省费用。

Description

一种水泥路路基防渗水方法
技术领域
本发明涉及道路建设技术领域,具体涉及一种水泥路路基防渗水方法。
背景技术
目前,国内在水泥路面缩缝的施工中,普遍使用的是沥青玛蹄脂灌缝法,它是在水泥路面铺筑完成后,采用切割,灌缝、嵌缝养护等工序实现的。由于沥青玛蹄脂的复原率只有30%左右,因此,水泥路面在遇热膨胀时,它被挤出;遇冷收缩时,它又无法复原,留下的缝隙往往为砂石灰渣所填充,失去了缩缝的作用。实践证明,沥青玛蹄脂灌缝在反复伸缩的做用下被不断挤出,很快(2—3年)缩缝就会失效,渗水现象不可避免,复灌工作也不可避免。而且,由于缩缝的失效,在高温季节路面的伸长董都会压向胀缝,容易造成胀缝的破坏。另外这种方法还存在有操作复杂,成本过高、工作环境恶劣等问题。
发明内容
本发明所要解决的技术问题在于提供一种工艺简单,成本低廉,实际效果好的水泥路路基防渗水方法。
本发明所要解决的技术问题采用以下技术方案来实现:
一种水泥路路基防渗水方法,包括如下工艺步骤,
1)首先在路面浇筑之前在路基上铺设一层具有耐腐蚀性能的防水层,将路基隔离起来,该防水层能够粘附在路基上;
2)在铺设有防水层的路基上浇筑混凝土铺设路面,在路面铺设好5-8小时后,在接缝中填充密封物质,并将密封物质填充至与路面上表面齐平,并压实;
3)在密封物质填充1-2小时之后,用喷水器往填充物质上进行第一次喷水,待有水流出即可;
4)第一次喷水结束后12小时再进行第二次喷水,在第二次喷水的同时对路面进行适当洒水,待有水流出即可;
5)检查接缝是否完全没有缝隙,如有缝隙在接缝中再灌入填充物质即可。
所述的防水层为具有弹性的软物质构成。
所述的软物质为熔融状态的橡胶。
所述的密封物质由以下重量百分比的组分构成,
本发明的有益效果是:本发明将传统的切缝,灌缝,嵌缝养护工作集中起来,一次完成,具有省工,省费用,不会出现渗水现象,提高路面质量,且接缝之间弹性和拉力强,耐腐蚀性能好。
具体实施方式
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体实施例,进一步阐述本发明。
实施例1
一种水泥路路基防渗水方法,包括如下工艺步骤,
1)首先在路面浇筑之前在路基上铺设一层具有耐腐蚀性能的防水层,将路基隔离起来,该防水层能够粘附在路基上;
2)在铺设有防水层的路基上浇筑混凝土铺设路面,在路面铺设好5-8小时后,在接缝中填充密封物质,并将密封物质填充至与路面上表面齐平,并压实;
3)在密封物质填充1-2小时之后,用喷水器往填充物质上进行第一次喷水,待有水流出即可;
4)第一次喷水结束后12小时再进行第二次喷水,在第二次喷水的同时对路面进行适当洒水,待有水流出即可;
5)检查接缝是否完全没有缝隙,如有缝隙在接缝中再灌入填充物质即可。
所述的防水层为具有弹性的软物质构成,该软物质为熔融状态的橡胶。
所述的密封物质由以下重量百分比的组分构成,
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。

Claims (1)

1.一种水泥路路基防渗水方法,其特征在于:包括如下工艺步骤,
1)首先在路面浇筑之前在路基上铺设一层具有耐腐蚀性能的防水层,将路基隔离起来,该防水层能够粘附在路基上;
所述的防水层为具有弹性的软物质构成,所述的软物质为熔融状态的橡胶;
2)在铺设有防水层的路基上浇筑混凝土铺设路面,在路面铺设好5-8小时后,在接缝中填充密封物质,并将密封物质填充至与路面上表面齐平,并压实;
所述的密封物质由以下重量百分比的组分构成,
3)在密封物质填充1-2小时之后,用喷水器往填充的密封物质上进行第一次喷水,待有水流出即可;
4)第一次喷水结束后12小时再进行第二次喷水,在第二次喷水的同时对路面进行适当洒水,待有水流出即可;
5)检查接缝是否完全没有缝隙,如有缝隙在接缝中再灌入密封物质即可。
CN201310517318.2A 2013-10-28 2013-10-28 一种水泥路路基防渗水方法 Active CN103603252B (zh)