CN103540247A - Hydrophilic anti-corrosion coating - Google Patents

Hydrophilic anti-corrosion coating Download PDF

Info

Publication number
CN103540247A
CN103540247A CN201310449139.XA CN201310449139A CN103540247A CN 103540247 A CN103540247 A CN 103540247A CN 201310449139 A CN201310449139 A CN 201310449139A CN 103540247 A CN103540247 A CN 103540247A
Authority
CN
China
Prior art keywords
parts
coating
resin
hydrophilic anti
epoxy resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310449139.XA
Other languages
Chinese (zh)
Inventor
孙梁博
王岐山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
QINGDAO BOYUTE RUBBER PLASTIC PRODUCT CO Ltd
Original Assignee
QINGDAO BOYUTE RUBBER PLASTIC PRODUCT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINGDAO BOYUTE RUBBER PLASTIC PRODUCT CO Ltd filed Critical QINGDAO BOYUTE RUBBER PLASTIC PRODUCT CO Ltd
Priority to CN201310449139.XA priority Critical patent/CN103540247A/en
Publication of CN103540247A publication Critical patent/CN103540247A/en
Pending legal-status Critical Current

Abstract

The invention discloses a hydrophilic anti-corrosion coating. The hydrophilic anti-corrosion coating comprises the following components in parts by weight: 30-50 parts of alkyd resin, 10-15 parts of epoxy resin, 10-15 parts of flame retardant, 5-10 parts of antimonous oxide, 10-15 parts of thickener, 5-10 parts of silicon dioxide particle, 3-5 parts of polyphosphoric acid aluminium and 10-20 parts of deionized water, wherein the alkyd resin has the characteristics of fast drying speed and good weather fastness, so that the prepared coating can quickly dry, and the coating efficiency is improved; the expoxy resin has very good adhesive force on multiple matrix media, so that the adhesive force of the coating on matrixes is improved due to the added epoxy resin; terpene resin is very stable for oxygen, light and heat and has excellent ageing-resistant performance, so that the coating has excellent weather fastness.

Description

A kind of wetting ability corrosion resistant coating
Technical field
The present invention relates to a kind of wetting ability corrosion resistant coating.
Background technology
After steel pipe rolls off the production line on Steel Plant's streamline, its surface corrosion resistance performance is poor, is easy to be corroded in storage and transport process, has a strong impact on its performance and used life.Once its surface is corroded, its subsequent processes is loaded down with trivial details, and workload is large.
Summary of the invention
The deficiency existing for prior art, technical problem to be solved by this invention is to provide a kind of applicable multiple form of construction work and energy seasoning, the wetting ability corrosion resistant coating strong and good to water pipe precaution performance with steel pipe bonding force.
For solving the problems of the technologies described above, the technical solution used in the present invention is: a kind of wetting ability corrosion resistant coating, is grouped into by the one-tenth of following weight part:
Synolac 30~50;
Epoxy resin 10~15;
Fire retardant 10~15;
Antimonous oxide 5~10;
Thickening material 10~15;
Silica dioxide granule 5~10;
Poly aluminium phosphate 3~5;
Deionized water 10~20.
The advantage of wetting ability corrosion resistant coating of the present invention is: the Synolac that the present invention adopts has rate of drying soon and the feature of good weatherability, and the coating making is dried rapidly, improves coating efficiency; The epoxy resin that the present invention adopts has good sticking power to multiple substrate medium, and adding of it improved the sticking power of coating to matrix; The terpine resin that the present invention adopts is all highly stable to oxygen, light and heat, and ageing-resistant performance is excellent, makes coating have good weather resistance; The rust-preventive agent that the present invention adopts can form in steel tube surface the protective layer of densification, strong adhesion, is stoped or is slowed down oxygen in environment and the infiltration of water, thereby hinder the generation of corrosion microbattery by buffer action, plays good anti-corrosion protection effect.
Embodiment
Below in conjunction with specific embodiment, the present invention is described in further details;
A corrosion resistant coating, is grouped into by the one-tenth of following weight part:
Synolac 30~50;
Epoxy resin 10~15;
Fire retardant 10~15;
Antimonous oxide 5~10;
Thickening material 10~15;
Silica dioxide granule 5~10;
Poly aluminium phosphate 3~5;
Deionized water 10~20.
Certainly, above-mentioned explanation is not limitation of the present invention, and the present invention is also not limited to above-mentioned giving an example; those skilled in the art; in essential scope of the present invention, the variation of making, remodeling, interpolation or replacement, all should belong to protection scope of the present invention.

Claims (1)

1. a wetting ability corrosion resistant coating, is characterized in that, by the one-tenth of following weight part, is grouped into:
Synolac 30~50;
Epoxy resin 10~15;
Fire retardant 10~15;
Antimonous oxide 5~10;
Thickening material 10~15;
Silica dioxide granule 5~10;
Poly aluminium phosphate 3~5;
Deionized water 10~20.
CN201310449139.XA 2013-09-29 2013-09-29 Hydrophilic anti-corrosion coating Pending CN103540247A (en)