CN103467867A - Anticorrosion plastic formula - Google Patents
Anticorrosion plastic formula Download PDFInfo
- Publication number
- CN103467867A CN103467867A CN2013104632468A CN201310463246A CN103467867A CN 103467867 A CN103467867 A CN 103467867A CN 2013104632468 A CN2013104632468 A CN 2013104632468A CN 201310463246 A CN201310463246 A CN 201310463246A CN 103467867 A CN103467867 A CN 103467867A
- Authority
- CN
- China
- Prior art keywords
- plastic formula
- agent
- corrosion resistant
- plastic
- polycarbonate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an anticorrosion plastic formula. The plastic formula relates to an anticorrosive agent, a modifying agent, an antioxidant and an antistatic agent. The anticorrosive agent is polymerized by ethylene-vinyl acetate and chlorinated polypropylene. The modifying agent is prepared by polycarbonate and polyphenyl ether. The antioxidant is prepared by polybutadiene and polyethylene. The antistatic agent is made of glass fibers. Multiple different substances are added to synthetic plastic, so that the synthetic plastic has the good wearproof and anticorrosion performance and can adapt to various environments, and a large amount of synthetic plastic can be grown.
Description
Technical field
The present invention relates to the engineering plastic field, particularly relate to a kind of corrosion resistant plastic formula that has.
Background technology
In recent years, Chinese plastic parts manufacturing capacity for technological innovation is further enhanced, and enterprise technology research and development centre quantity is on the increase; The industrial structure, the pattern of enterprises and product structure are constantly adjusted, and the industry intensity is progressively upgraded; The global advantage of industry is further promoted and is strengthened, with the gap of developed country in the world, dwindle gradually, some aspect reaches world-class levels, enter the critical period of the Sustainable development that power strides forward from big country to the advanced person, the ground plastic parts manufacturings such as Jiangsu, Zhejiang, Shanghai, Guangdong are flourish, no matter be number of the enterprise, or the production and marketing scale is all in national leading position, the set of regions moderate of industry is relatively high.
Be badly in need of in the market a kind of corrosion resistant plastic formula that has.
Summary of the invention
The technical problem that the present invention mainly solves is to provide a kind of corrosion resistant plastic formula that has.
For solving the problems of the technologies described above, the technical scheme that the present invention adopts is: a kind of corrosion resistant plastic formula that has is provided, comprise: corrosion-resistant agent, properties-correcting agent, antioxidant and static inhibitor, described corrosion-resistant agent is that ethylene-vinyl acetate and Chlorinated Polypropylene III are polymerized, described properties-correcting agent is that polycarbonate and polyphenylene oxide are prepared from, described antioxidant is that polyhutadiene and polyethylene are prepared from, and described static inhibitor is glass fibre.
In a preferred embodiment of the present invention, the weight proportion scope with corrosion resistant each composition of plastic formula is: ethylene-vinyl acetate 15-28%, Chlorinated Polypropylene III 20-30%, polycarbonate 8-13%, polyphenylene oxide prepares 5-8%, polyhutadiene 5-10%, polyethylene 3-6%, glass fibre 3-5%.
In a preferred embodiment of the present invention, the weight proportion with corrosion resistant each composition of plastic formula is: ethylene-vinyl acetate 23%, Chlorinated Polypropylene III 27%, polycarbonate 10%, polyphenylene oxide 5%, polyhutadiene 8%, polyethylene 4%, glass fibre 3%.
The invention has the beneficial effects as follows: the present invention has corrosion resistant plastic formula, after in synthetic rubber, adding multiple different material, make synthetic plastic there is better wear-resisting, corrosion resistant performance, make synthetic plastic can adapt to various environment, the synthetic plastic of can growing up in a large number.
Embodiment
Below will the technical scheme in the embodiment of the present invention be clearly and completely described, obviously, described embodiment is only a part of embodiment of the present invention, rather than whole embodiment.Embodiment based in the present invention, those of ordinary skills, not making all other embodiment that obtain under the creative work prerequisite, belong to the scope of protection of the invention.
The present invention has corrosion resistant plastic formula, comprise: corrosion-resistant agent, properties-correcting agent, antioxidant and static inhibitor, described corrosion-resistant agent is that ethylene-vinyl acetate and Chlorinated Polypropylene III are polymerized, described properties-correcting agent is that polycarbonate and polyphenylene oxide are prepared from, described antioxidant is that polyhutadiene and polyethylene are prepared from, and described static inhibitor is glass fibre.
In a preferred embodiment of the present invention, the weight proportion scope with corrosion resistant each composition of plastic formula is: ethylene-vinyl acetate 15-28%, Chlorinated Polypropylene III 20-30%, polycarbonate 8-13%, polyphenylene oxide 5-8%, polyhutadiene 5-10%, polyethylene 3-6%, glass fibre 3-5%.
In a preferred embodiment of the present invention, the weight proportion with corrosion resistant each composition of plastic formula is: ethylene-vinyl acetate 23%, Chlorinated Polypropylene III 27%, polycarbonate 10%, polyphenylene oxide 5%, polyhutadiene 8%, polyethylene 4%, glass fibre 3%.
In a preferred embodiment of the present invention, the impact resistance of ethylene-vinyl acetate is relatively good, and stretch capability is relatively good.
In a preferred embodiment of the present invention, the oil resistant of Chlorinated Polypropylene III, heat-resisting and light fastness is better.
In a preferred embodiment of the present invention, polycarbonate is wear-resisting anti-oxidant, and polyphenylene oxide has good water-fast, anti-steam performance, the tensile strength that the goods tool is higher and shock strength, and creep resistance might as well.
In a preferred embodiment of the present invention, polyethylene has good resistance to low temperature, and chemical stability is good, the erosion of the most of soda acids of ability.Be insoluble to common solvent under normal temperature, water-absorbent is little, and electrical insulation capability is good.
In a preferred embodiment of the present invention, glass fibre has the heat-resisting effect of insulation.
The present invention has corrosion resistant plastic formula, solved the defect in the technical scheme, after in synthetic rubber, adding multiple different material, made synthetic plastic there is better wear-resisting, corrosion resistant performance, make synthetic plastic can adapt to various environment, the synthetic plastic of can growing up in a large number.
The foregoing is only embodiments of the invention; not thereby limit the scope of the claims of the present invention; every equivalent structure or conversion of equivalent flow process that utilizes description of the present invention to do; or directly or indirectly be used in other relevant technical fields, all in like manner be included in scope of patent protection of the present invention.
Claims (3)
1. one kind has corrosion resistant plastic formula, it is characterized in that, comprise: corrosion-resistant agent, properties-correcting agent, antioxidant and static inhibitor, described corrosion-resistant agent is that ethylene-vinyl acetate and Chlorinated Polypropylene III are polymerized, described properties-correcting agent is that polycarbonate and polyphenylene oxide are prepared from, described antioxidant is that polyhutadiene and polyethylene are prepared from, and described static inhibitor is glass fibre.
2. according to claim 1 have a corrosion resistant plastic formula, it is characterized in that, weight proportion scope with corrosion resistant each composition of plastic formula is: ethylene-vinyl acetate 15-28%, Chlorinated Polypropylene III 20-30%, polycarbonate 8-13%, polyphenylene oxide 5-8%, polyhutadiene 5-10%, polyethylene 3-6%, glass fibre 3-5%.
3. according to claim 1 have a corrosion resistant plastic formula, it is characterized in that, the weight proportion with corrosion resistant each composition of plastic formula is: ethylene-vinyl acetate 23%, Chlorinated Polypropylene III 27%, polycarbonate 10%, polyphenylene oxide 5%, polyhutadiene 8%, polyethylene 4%, glass fibre 3%.