CN103421411A - Water-based paint formula - Google Patents
Water-based paint formula Download PDFInfo
- Publication number
- CN103421411A CN103421411A CN2013103695544A CN201310369554A CN103421411A CN 103421411 A CN103421411 A CN 103421411A CN 2013103695544 A CN2013103695544 A CN 2013103695544A CN 201310369554 A CN201310369554 A CN 201310369554A CN 103421411 A CN103421411 A CN 103421411A
- Authority
- CN
- China
- Prior art keywords
- water
- based paint
- parts
- formula
- paint formula
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a water-based paint formula. Water-based paint manufactured according to the water-based paint formula comprises, by mass, 20-25 parts of water-soluble epoxy resin, 0.1-0.2 part of 25% ammonium hydroxide, 0.2-0.5 part of additives, 0.1-0.3 part of sodium hexametaphosphate, 0.1-0.3 part of defoamers, 10-15 parts of light calcium carbonate and 5-10 parts of siloxane water repellent agents. The water-based paint formula has the advantages that the water-based paint is excellent in glossiness and heat resistance and high in hardness, abrasion resistance and adhesive force, and a water drop effect can be realized.
Description
Technical field
The present invention relates to a kind of formulation for coating material.
Background technology
Water-borne coatings in the market is generally to take the coating that polyvinyl alcohol is base-material, contains the hydroxy functional group that quantity is larger in the molecule of polyvinyl alcohol, its film forming exquisiteness, but ventilation property is poor, so the glossiness of coating is poor and resistance toheat is not high, work-ing life is short.
Summary of the invention
Goal of the invention: the present invention, in order to solve deficiency of the prior art, provides the water-borne coatings that a kind of glossiness is high, resistance toheat is good formula.
Technical scheme: a kind of water-borne coatings formula of the present invention, the formula that comprises following mass parts: water-soluble epoxy resin 20-25 part, 25% ammoniacal liquor 0.1-0.2 part, filler 0.2-0.5 part, Sodium hexametaphosphate 99 0.1-0.3 part, defoamer 0.1-0.3 part, light calcium carbonate 10-15 part, siloxanes hydrophobizing agent 5-10 part.
Beneficial effect: the present invention has advantages of that good glossiness and resistance toheat and hardness are good, wear resistance is good, adhesive power is good, and has water droplet effect.
Embodiment
Below in conjunction with specific embodiment, the invention will be further described:
Embodiment 1
A kind of water-borne coatings formula, comprise the formula of following mass parts: 20 parts of water-soluble epoxy resin, 25% 0.1 part of ammoniacal liquor, 0.2 part of filler, 0.1 part of Sodium hexametaphosphate 99,0.1 part of defoamer, 10 parts of light calcium carbonates, 5 parts of siloxanes hydrophobizing agents.
Claims (1)
1. a water-borne coatings formula, is characterized in that: the formula that comprises following mass parts: water-soluble epoxy resin 20-25 part, 25% ammoniacal liquor 0.1-0.2 part, filler 0.2-0.5 part, Sodium hexametaphosphate 99 0.1-0.3 part, defoamer 0.1-0.3 part, light calcium carbonate 10-15 part, siloxanes hydrophobizing agent 5-10 part.