CN103407233A - Cracking glass - Google Patents
Cracking glass Download PDFInfo
- Publication number
- CN103407233A CN103407233A CN2013103348642A CN201310334864A CN103407233A CN 103407233 A CN103407233 A CN 103407233A CN 2013103348642 A CN2013103348642 A CN 2013103348642A CN 201310334864 A CN201310334864 A CN 201310334864A CN 103407233 A CN103407233 A CN 103407233A
- Authority
- CN
- China
- Prior art keywords
- glass
- layer
- lamella
- crack
- glass sheet
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses cracking glass, which comprises a surface protective layer, a glass sheet layer and a resin plate layer, wherein the glass sheet layer is positioned between the surface protective layer and the resin plate layer; the surface protective layer is connected and fixed with the glass sheet layer through glue; the glass sheet layer is connected and fixed with the resin plate layer through glue; the surface protective layer is tempered flat glass; patterns pieced by a plurality of glass fragments are formed on the glass sheet layer. Through the mode, the cracking glass provided by the invention has the advantages that the pattern shapes of cracks can be set at will, the decorative effect is excellent, the firmness and scratch resistance of the surface are realized, the service life is long, the performance price ratio is high, the weight is relatively light, and the safety is high.
Description
Technical field
The present invention relates to the glass design field, particularly relate to a kind of crack glass.
Background technology
Safety glass has two large advantages, and the firstth, intensity improves several times than simple glass, and bending resistance, and the resistance to thermal shocks matter of safety glass has the raising of 3 ~ 5 times than simple glass; The secondth, use safety, its bearing capacity increases and has improved frangible character, also is the fractionlet without acute angle even safety glass destroys, and the injury of human body has greatly been reduced.
The general crack glass adopted is to adopt the compound steel glassy bond to form plate object, then broken formation crackle shakes on the angle, intermediate layer, but weight is relatively large, complex process, cost is high, and crack shape is uncontrollable, certainly also there is crack glass inferior to adopt ordinary plate glass to substitute outer field safety glass, in use, danger coefficient is higher.
Summary of the invention
The technical problem that the present invention mainly solves is to provide a kind of crack glass, and weight is relatively light, and the crackle moulding is random, good decorative property, and cost performance is high.
For solving the problems of the technologies described above, the technical scheme that the present invention adopts is: a kind of crack glass is provided, comprise: surface protecting layer, glass lamella and resin flaggy, described glass lamella is between surface protecting layer and resin flaggy, between described surface protecting layer and glass lamella, adopt glue to be connected and fixed, between described glass lamella and resin flaggy, adopt glue to be connected and fixed, described surface protecting layer is tempering plate glass, and described glass lamella is the pattern slapped together by a plurality of glass fragments.
In a preferred embodiment of the present invention, described glass fragment is the glass particle without acute angle.
In a preferred embodiment of the present invention, each thickness of described glass fragment is identical.
In a preferred embodiment of the present invention, described resin flaggy is transparent acrylic board.
The invention has the beneficial effects as follows: a kind of crack glass that the present invention points out, the intermediate glass lamella adopts the glass particle without acute angle to slap together, pattern modelling is random, positive safety glass provides firm protective capacities, and the acrylic board transparency at the back side is high, ageing-resistant, quality is relatively light, and shock-resistant, can provide good supplemental support effect to the safety glass damaged, overall security is high.
The accompanying drawing explanation
In order to be illustrated more clearly in the technical scheme in the embodiment of the present invention, in below describing embodiment, the accompanying drawing of required use is briefly described, apparently, accompanying drawing in the following describes is only some embodiments of the present invention, for those of ordinary skills, under the prerequisite of not paying creative work, can also according to these accompanying drawings, obtain other accompanying drawing, wherein:
Fig. 1 is the structural representation of crack glass one preferred embodiment of the present invention;
In accompanying drawing, the mark of each parts is as follows: 1, surface protecting layer, 2, the glass lamella, 3, the resin flaggy.
The specific embodiment
Below will the technical scheme in the embodiment of the present invention be clearly and completely described, obviously, described embodiment is only a part of embodiment of the present invention, rather than whole embodiment.Based on the embodiment in the present invention, those of ordinary skills, not making all other embodiment that obtain under the creative work prerequisite, belong to the scope of protection of the invention.
Refer to Fig. 1, the embodiment of the present invention comprises:
A kind of crack glass, comprise: surface protecting layer, glass lamella and resin flaggy, described glass lamella is between surface protecting layer and resin flaggy, between described surface protecting layer and glass lamella, adopt glue to be connected and fixed, between described glass lamella and resin flaggy, adopt glue to be connected and fixed, described surface protecting layer is tempering plate glass, and described glass lamella is the pattern slapped together by a plurality of glass fragments.
Further, described glass fragment is the glass particle without acute angle.
Further, each thickness of described glass fragment is identical.
Further, described resin flaggy is transparent acrylic board.
Acrylic board is polymerized by methyl olefin(e) acid methylmethacrylate monomer, is again lucite, and light transmission is good, can reach more than 92%, weather-proof and acid-proof alkaline good, can be because of not exposing to the sun and rain month after month throughout the year, and produce the phenomenon of yellowing and hydrolysis, anti-impact force is strong, be 16 times of simple glass, be applicable to being arranged on the safe area of special needs, from heavy and light, than simple glass light half, the load that building and support bear is little.
The most outstanding characteristics of crack glass of the present invention are the controllability of crackle, and the intermediate glass lamella adopts the glass particle without acute angle to slap together, twice laid, and pattern modelling is convenient, random, also can not cause large injury to human body after fragmentation, and security performance is outstanding.
In sum, a kind of crack glass that the present invention points out, the pattern modelling of crackle can arbitrarily be set, good decorative property, surperficial firm scratch resistance, the life-span is long, and cost performance is high, and quality is relatively light, safe.
The foregoing is only embodiments of the invention; not thereby limit the scope of the claims of the present invention; every equivalent structure or equivalent flow process conversion that utilizes description of the present invention to do; or directly or indirectly be used in other relevant technical field, all in like manner be included in scope of patent protection of the present invention.
Claims (4)
1. crack glass, it is characterized in that, comprise: surface protecting layer, glass lamella and resin flaggy, described glass lamella is between surface protecting layer and resin flaggy, between described surface protecting layer and glass lamella, adopt glue to be connected and fixed, between described glass lamella and resin flaggy, adopt glue to be connected and fixed, described surface protecting layer is tempering plate glass, and described glass lamella is the pattern slapped together by a plurality of glass fragments.
2. crack glass according to claim 1, is characterized in that, described glass fragment is the glass particle without acute angle.
3. crack glass according to claim 1, is characterized in that, each thickness of described glass fragment is identical.
4. crack glass according to claim 1, is characterized in that, described resin flaggy is transparent acrylic board.