CN103333391A - Compatible modifying agent for low-pressure polyethylene waste plate material and application method of compatible modifying agent - Google Patents
Compatible modifying agent for low-pressure polyethylene waste plate material and application method of compatible modifying agent Download PDFInfo
- Publication number
- CN103333391A CN103333391A CN2013102476272A CN201310247627A CN103333391A CN 103333391 A CN103333391 A CN 103333391A CN 2013102476272 A CN2013102476272 A CN 2013102476272A CN 201310247627 A CN201310247627 A CN 201310247627A CN 103333391 A CN103333391 A CN 103333391A
- Authority
- CN
- China
- Prior art keywords
- pressure polyethylene
- low pressure
- panel material
- useless panel
- modifying agent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a compatible modifying agent used for a low-pressure polyethylene waste plate material and an application method of the compatible modifying agent. The compatible modifying agent comprises the following component in parts by weight: 1.0 to 2.0 parts of chlorinated polyethylene. The application method comprises the following steps of: 1, processing the low-pressure polyethylene waste plate material; 2, detecting a melt index of the low-pressure polyethylene waste plate material; 3, preparing materials, namely, preparing materials according to the ratio of the low-pressure polyethylene waste plate material to chlorinated polyethylene of 100: (1.0-2.0); and 4, blanking and processing, namely, adding all the prepared components to a mixing machine, starting the mixing machine for 12 to 15 minutes at a normal temperature, stopping the mixing machine and discharging and packaging to obtain the finished product. The compatible modifying agent is reasonable in technology, simple to process, convenient to use, and capable of effectively improving the physical and chemical performance of the low-pressure polyethylene waste plate material as well as the quality of the product. The compatible modifying agent can be widely applied to the modification processing of the low-pressure polyethylene waste plate material.
Description
Technical field
The present invention relates to a kind of compatible modifier for plastics and using method, particularly relate to a kind of compatible modifier and using method thereof for the useless panel material of low pressure polyethylene.
Background technology
As everyone knows, the useless panel material processing means of existing low pressure polyethylene is outmoded, technology falls behind, and the product physical and chemical performance of producing is lower, second-rate, can not satisfy the demands of consumers, and also can not adapt to the demand of market development, thereby limits its range of application.
Summary of the invention
The objective of the invention is in order to overcome the deficiency of above-mentioned background technology, through the concentrating on studies and verifying repeatedly by production reality of contriver, provide a kind of compatible modifier and using method thereof for the useless panel material of low pressure polyethylene.
To achieve these goals, technical scheme of the present invention is such:
A kind of compatible modifier for the useless panel material of low pressure polyethylene provided by the invention, described compatible modifier comprises following component and weight part thereof: chlorinatedpolyethylene 1.0 ~ 2.0.
In technique scheme, described compatible modifier comprises following component and weight part thereof: chlorinatedpolyethylene 1.5.
The using method of a kind of compatible modifier for the useless panel material of low pressure polyethylene provided by the invention, may further comprise the steps: step 1, waste disposal, the useless panel material water of low pressure polyethylene is cleaned, remove foreign material and dust, to remove the useless panel material of clean low pressure polyethylene again and be broken into the close material of size, standby; Step 2, detection, the melt flow index of the useless panel material of detection low pressure polyethylene, setting melt flow index M1 is 0.5 ~ 3.0; Step 3, batching are got 100 parts of the useless panel materials of standby low pressure polyethylene, 1.0 ~ 2.0 parts of chlorinatedpolyethylenees by weight, and be standby; Step 4, processing feeds intake; the useless panel material of three described low pressure polyethylenes at first drops in the mixing machine for 100 parts set by step; with in 1.0 ~ 2.0 parts of input mixing machines of chlorinatedpolyethylene, started shooting at normal temperatures 12 ~ 15 minutes, shut down: step 5, the mixture discharging that will above-mentionedly process are packed and are got final product.
In technique scheme, when described melt flow index M1=0.5 ~ 0.8, useless panel material: the chlorinatedpolyethylene=100:1.0 of low pressure polyethylene then; When described melt flow index M1=0.8 ~ 1.5, useless panel material: the chlorinatedpolyethylene=100:1.3 of low pressure polyethylene then; When described melt flow index M1=1.5 ~ 2.0, useless panel material: the chlorinatedpolyethylene=100:1.5 of low pressure polyethylene then; When described melt flow index M1=2.0 ~ 3.0, useless panel material: the chlorinatedpolyethylene=100:2.0 of low pressure polyethylene then.
The compatible modifier and the using method thereof that are used for the useless panel material of low pressure polyethylene that the present invention is alleged have following beneficial effect: novel, technology rationally, processing is simple, easy to use, can realize requirement of industrialized batch production.The present invention can improve the physical and chemical performance of the useless panel material of low pressure polyethylene effectively, reduces melt flow index, makes material increase toughness and intensity, becomes the PP Pipe Compound with plate squeezing purposes.The present invention can be widely used for the modification processing of the useless panel material of low pressure polyethylene.
Embodiment
The present invention is described in further detail below in conjunction with embodiment, but this embodiment should not be construed as limitation of the present invention.
Embodiment 1
Compatible modifier of the present invention is prepared by following component and weight part: when melt flow index M1=0.5 ~ 0.8 of detecting the useless panel material of low pressure polyethylene, then get chlorinatedpolyethylene 1.0, and standby; Its using method is as follows:
The useless panel material water of low pressure polyethylene is cleaned, is broken into the close refuse material of size after removing foreign material and dust, get 100 parts standby;
Earlier the useless panel material of above-mentioned 100 parts of low pressure polyethylenes having handled is dropped in the mixing machine, more above-mentioned 1.0 parts of chlorinatedpolyethylenees are dropped in the mixing machine, start is 12 minutes under normal temperature condition, shuts down, and the discharging packing gets final product.
Embodiment 2
Present embodiment is substantially the same manner as Example 1, and difference is: when described melt flow index M1=0.8 ~ 1.5, then get 1.3 parts of chlorinatedpolyethylenees.
In the using method the useless panel material of above-mentioned 100 parts of low pressure polyethylenes having handled is dropped in the mixing machine, more above-mentioned 1.3 parts of chlorinatedpolyethylenees are dropped in the mixing machine, start is 13 minutes under normal temperature condition, shuts down, and the discharging packing gets final product.
Embodiment 3
Present embodiment is substantially the same manner as Example 1, and difference is: when described melt flow index M1=1.5 ~ 2.0, then get 1.5 parts of chlorinatedpolyethylenees.
In the using method the useless panel material of above-mentioned 100 parts of low pressure polyethylenes having handled is dropped in the mixing machine, more above-mentioned 1.5 parts of chlorinatedpolyethylenees are dropped in the mixing machine, start is 14 minutes under normal temperature condition, shuts down, and the discharging packing gets final product.
Embodiment 4
Present embodiment is substantially the same manner as Example 1, and difference is: when described melt flow index M1=2.0 ~ 3.0, then get 2.0 parts of chlorinatedpolyethylenees.
In the using method the useless panel material of above-mentioned 100 parts of low pressure polyethylenes having handled is dropped in the mixing machine, more above-mentioned 2.0 parts of chlorinatedpolyethylenees are dropped in the mixing machine, start is 15 minutes under normal temperature condition, shuts down, and the discharging packing gets final product.
Obviously, those skilled in the art can carry out various changes and modification to the present invention and not break away from the spirit and scope of the present invention.Like this, if of the present invention these are revised and modification belongs within the scope of claim of the present invention and equivalent technologies thereof, then the present invention also is intended to comprise these changes and modification interior.
The content that is not described in detail in this specification sheets belongs to this area professional and technical personnel's known prior art.
Claims (4)
1. compatible modifier that is used for the useless panel material of low pressure polyethylene, it is characterized in that: described compatible modifier comprises following component and weight part thereof: chlorinatedpolyethylene 1.0 ~ 2.0.
2. the compatible modifier for the useless panel material of low pressure polyethylene according to claim 1, it is characterized in that: described compatible modifier comprises following component and weight part thereof: chlorinatedpolyethylene 1.5.
3. using method that is used for the compatible modifier of the useless panel material of low pressure polyethylene is characterized in that: may further comprise the steps:
Step 1, waste disposal are cleaned the useless panel material water of low pressure polyethylene, remove foreign material and dust, will remove the useless panel material of clean low pressure polyethylene again and be broken into the close material of size, and be standby;
Step 2, detection, the melt flow index of the useless panel material of detection low pressure polyethylene, setting melt flow index M1 is 0.5 ~ 3.0;
Step 3, batching are got 100 parts of the useless panel materials of standby low pressure polyethylene, 1.0 ~ 2.0 parts of chlorinatedpolyethylenees by weight, and be standby;
Step 4, the processing that feeds intake, the useless panel material of three described low pressure polyethylenes at first drops in the mixing machine for 100 parts set by step, with in 1.0 ~ 2.0 parts of input mixing machines of chlorinatedpolyethylene, starts shooting at normal temperatures 12 ~ 15 minutes again, shuts down:
Step 5, the mixture discharging packing that processes above-mentioned get final product.
4. the using method of the compatible modifier for the useless panel material of low pressure polyethylene according to claim 3 is characterized in that:
When described melt flow index M1=0.5 ~ 0.8, useless panel material: the chlorinatedpolyethylene=100:1.0 of low pressure polyethylene then;
When described melt flow index M1=0.8 ~ 1.5, useless panel material: the chlorinatedpolyethylene=100:1.3 of low pressure polyethylene then;
When described melt flow index M1=1.5 ~ 2.0, useless panel material: the chlorinatedpolyethylene=100:1.5 of low pressure polyethylene then;
When described melt flow index M1=2.0 ~ 3.0, useless panel material: the chlorinatedpolyethylene=100:2.0 of low pressure polyethylene then.