CN103276399A - Cleaning fluid capable of reducing smog in scaffold spraying technology - Google Patents

Cleaning fluid capable of reducing smog in scaffold spraying technology Download PDF

Info

Publication number
CN103276399A
CN103276399A CN2013102328444A CN201310232844A CN103276399A CN 103276399 A CN103276399 A CN 103276399A CN 2013102328444 A CN2013102328444 A CN 2013102328444A CN 201310232844 A CN201310232844 A CN 201310232844A CN 103276399 A CN103276399 A CN 103276399A
Authority
CN
China
Prior art keywords
scavenging solution
cleaning fluid
smog
scaffolding
scaffold
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102328444A
Other languages
Chinese (zh)
Inventor
王斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JURONG HENGDA METAL PRODUCTS CO Ltd
Original Assignee
JURONG HENGDA METAL PRODUCTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JURONG HENGDA METAL PRODUCTS CO Ltd filed Critical JURONG HENGDA METAL PRODUCTS CO Ltd
Priority to CN2013102328444A priority Critical patent/CN103276399A/en
Publication of CN103276399A publication Critical patent/CN103276399A/en
Pending legal-status Critical Current

Abstract

The invention discloses a cleaning fluid capable of reducing smog in a scaffold spraying technology. The cleaning fluid comprises components in percentage by mass as follows: 30%-40% of an antirust agent and 70%-60% of hydrochloric acid with the concentration of 31%-35%. The cleaning fluid generates little smog during cleaning, cannot generate environmental pollution, and meets environmental requirements.

Description

A kind of scavenging solution that reduces smog in the scaffolding spraying coating process
Technical field
The present invention relates to a kind of scaffolding spraying coating process, specifically a kind of scavenging solution that reduces smog in the scaffolding spraying coating process.
Background technology
Scaffolding refers to the working-yard for workman's operation and solves various supports vertical and that the level transportation is set up, is used in the higher place that can't directly construct of exterior wall, inside fitting or floor height in the construction site.Mainly work up and down for the workmen or the maintenance of peripheral safety net and high-altitude installation component etc.It is steel pipe or synthetic materials etc. that the tradition scaffolding is made material, and scaffolding also extensively is used in departments such as advertising, municipal administration, traffic road and bridge, mines.But steel pipe gets rusty easily, and does not have erosion resistance, and life-time service does not have safety control, and work-ing life is short.
In order to improve the corrosion resistance nature of scaffolding, prolong the work-ing life of scaffolding, need carry out spraying coating process to scaffolding and handle, in traditional spraying coating process, the scavenging solution that adopts during cleaning is generally the rust-preventive agent of direct purchase,
Rust-preventive agent is a kind of synthetic permeate agent of super grade high efficiency, thereby it can powerfully infiltrate iron rust, corrode in thing, the greasy dirt and like a cork it is disposed.Have the infiltration rust cleaning, become flexible performances such as lubricating, resist burn into protection metal.This scavenging solution can produce a large amount of smog when cleaning, polluted environment, does not meet environmental requirement.
Summary of the invention
The generation of smog the purpose of this invention is to provide a kind of scavenging solution that reduces smog in the scaffolding spraying coating process when cleaning in order to reduce, and the smog that this scavenging solution produces when cleaning is few, compliance with environmental protection requirements.
The objective of the invention is to be achieved through the following technical solutions:
A kind of scavenging solution that reduces smog in the scaffolding spraying coating process is characterized in that: the quality composition of this scavenging solution is: rust-preventive agent 30-40%, concentration are the hydrochloric acid 70-60% of 31-35%.
Among the present invention, further, the quality of this scavenging solution composition is: rust-preventive agent 40%, concentration are 31% hydrochloric acid 60%.Perhaps, the quality of this scavenging solution composition is: rust-preventive agent 35%, concentration are 31% hydrochloric acid 65%.
Adopt the present invention that scaffolding is cleaned, can reduce the volatility hydrochloric acid acid mist of generation, can not produce environmental pollution, compliance with environmental protection requirements.
Embodiment
Embodiment 1
A kind of scavenging solution that reduces smog in the scaffolding spraying coating process, the quality of this scavenging solution are formed: rust-preventive agent 30-40%, concentration are the hydrochloric acid 70-60% of 31-35%.
Embodiment 2
A kind of scavenging solution that reduces smog in the scaffolding spraying coating process, the quality of this scavenging solution are formed: rust-preventive agent 40%, concentration are 31% hydrochloric acid 60%.
Embodiment 3
A kind of scavenging solution that reduces smog in the scaffolding spraying coating process, the quality of this scavenging solution are formed: rust-preventive agent 35%, concentration are 31% hydrochloric acid 65%.

Claims (3)

1. scavenging solution that reduces smog in the scaffolding spraying coating process is characterized in that: the quality of this scavenging solution is formed and is: rust-preventive agent 30-40%, concentration are the hydrochloric acid 70-60% of 31-35%.
2. the scavenging solution of smog in the minimizing scaffolding spraying coating process according to claim 1 is characterized in that: the quality of this scavenging solution is formed and is: rust-preventive agent 40%, concentration are 31% hydrochloric acid 60%.
3. the scavenging solution of smog in the minimizing scaffolding spraying coating process according to claim 1 is characterized in that: the quality of this scavenging solution is formed and is: rust-preventive agent 35%, concentration are 31% hydrochloric acid 65%.
CN2013102328444A 2013-06-13 2013-06-13 Cleaning fluid capable of reducing smog in scaffold spraying technology Pending CN103276399A (en)