CN103182786A - Manufacture technology of buttons - Google Patents

Manufacture technology of buttons Download PDF

Info

Publication number
CN103182786A
CN103182786A CN2012104293322A CN201210429332A CN103182786A CN 103182786 A CN103182786 A CN 103182786A CN 2012104293322 A CN2012104293322 A CN 2012104293322A CN 201210429332 A CN201210429332 A CN 201210429332A CN 103182786 A CN103182786 A CN 103182786A
Authority
CN
China
Prior art keywords
button
raw materials
plastic raw
wood grain
grain powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012104293322A
Other languages
Chinese (zh)
Inventor
林强
王永跃
王炜韬
韩鹏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Weixing Industrial Development Co Ltd
Original Assignee
Zhejiang Weixing Industrial Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Weixing Industrial Development Co Ltd filed Critical Zhejiang Weixing Industrial Development Co Ltd
Priority to CN2012104293322A priority Critical patent/CN103182786A/en
Publication of CN103182786A publication Critical patent/CN103182786A/en
Pending legal-status Critical Current

Abstract

The invention provides a manufacture technology of buttons. The manufacture technology comprises the following steps: preparing plastic material, adding 0.6 to 15 percent by weight of wood grain powder into the plastic material, heating and melting the plastic material with the wood grain powder added, ensuring that the plastic material at molten state is cooled to be molded so as to obtain button sectional material, and performing cutting and surface machining to the button sectional material so as to obtain finished buttons. The wood grain powder which can form wood texture is added into the plastic material, so that wood texture can be formed on the surface and at the interior of the button sectional material during the production process, and the wood texture formed by the wood grain powder is clearer, and more uniformly distributed on the plastic buttons and has better imitation wood effect because of the properties of the wood grain powder.

Description

A kind of button manufacturing process
Technical field
The present invention relates to button manufacturing technology field, more particularly, relate to a kind of button production technology.
Background technology
Button is the articles for daily use of generally using in people's daily life, and common button mostly is plastic button and wooden button greatly.
Wooden button has been subjected to people and has more favored because its native texture with timber makes it more attractive in appearance.But because the water imbibition of lumber fibre is very strong, one runs into wet weather or it is dropped in water, wooden button will very fast suction, expansion, might craze and transfiguration after drying again, and perhaps become coarse and can't bear, be easy to hook and pull garment fabric, clothing is impacted.
For fear of the generation of above-mentioned situation, the method that people expect is exactly to adopt in the imitated wood grain in the surface of plastic button, so namely can reach effect attractive in appearance, can not make button again because of wet environment or meet water deformation takes place.In the prior art, the manufacture method of the imitative wood grain of plastic button is on the surface of plastic button the AC blowing agent to be set, make the surface of plastic button form wood grain, but, the wood grain that this kind production technology forms only exists in the surface of plastic button, and texture is unintelligible, inhomogeneous, and imitative wood effect is relatively poor.
In sum, how providing a kind of button manufacturing process, to realize improving the imitative wood effect of plastic button, is present those skilled in the art's problem demanding prompt solution.
Summary of the invention
In view of this, the invention provides a kind of button manufacturing process, improved the imitative wood effect of plastic button.
In order to achieve the above object, the invention provides following technical scheme:
A kind of button manufacturing process, it may further comprise the steps:
11) allotment plastic raw materials;
12) adding part by weight in the described plastic raw materials is the wood grain powder of 0.6%-15%;
13) the described plastic raw materials that adds the wood grain powder is carried out heat fused;
14) make the described plastic raw materials cooling forming that is in molten state, obtain the button section bar;
15) to described button section bar shear, Surface Machining, obtain the finished product button.
Preferably, in the above-mentioned button manufacturing process, described wood grain powder joins in the described plastic raw materials in the color matching operation of described plastic raw materials.
Preferably, in the above-mentioned button manufacturing process, the concrete manufacturing process of described plastic raw materials heat fused and cooling forming may further comprise the steps:
31) the described plastic raw materials that will add described wood grain powder is put into the barrel of injection machine;
32) in described barrel, described plastic raw materials is heated, and by the screw rod of described injection machine described plastic raw materials is sheared;
33) by described screw rod, the melt of the described plastic raw materials after the plasticizing is pushed in the die casting system of described injection machine;
34) behind the described plastic raw materials cooling forming, it is taken out from described die casting system, obtain the button section bar.
Preferably, in the above-mentioned button manufacturing process, to described button section bar shear, Surface Machining, the concrete technology that obtains the finished product button may further comprise the steps:
41) surface of described button section bar is processed make it become the button semi-finished product;
42) described button semi-finished product are carried out polishing and then obtain the finished product button.
Preferably, in the above-mentioned button manufacturing process, also comprise and use the radium-shine processing step that described button semi-finished product are carved and/or cut.
In the button manufacturing process provided by the invention, may further comprise the steps: the allotment plastic raw materials; Adding part by weight in the plastic raw materials is the wood grain powder of 0.6%-15%; The plastic raw materials that adds the wood grain powder is carried out heat fused; Make the plastic raw materials cooling forming that is in molten state, obtain the button section bar; To the button section bar shear, Surface Machining, obtain the finished product button.Button manufacturing process provided by the invention, in plastic raw materials, add the wood grain powder that can form wood grain, no matter make the button section bar is on its surface in the process of producing or portion all can form wood grain within it, and because the characteristic of wood grain powder itself, make that the wood grain that is formed by the wood grain powder is more clear, plastic button distribute more even, imitative wood effect is better.
Description of drawings
In order to be illustrated more clearly in the embodiment of the invention or technical scheme of the prior art, to do to introduce simply to the accompanying drawing of required use in embodiment or the description of the Prior Art below, apparently, accompanying drawing in describing below only is some embodiments of the present invention, for those of ordinary skills, under the prerequisite of not paying creative work, can also obtain other accompanying drawing according to these accompanying drawings.
The flow chart of the button manufacturing process that Fig. 1 provides for the embodiment of the invention;
Fig. 2 is the concrete process chart in plastic raw materials heat fused and the cooling forming process;
Fig. 3 is for the button section bar is sheared, the concrete process chart of Surface Machining.
The specific embodiment
In order further to understand the present invention, be described below in conjunction with the preferred embodiment for the present invention of embodiment, but should be appreciated that these describe just in order to further specify the features and advantages of the present invention, rather than to the restriction of claim of the present invention.
The invention provides a kind of button manufacturing process, improved the imitative wood effect of plastic button.
Below in conjunction with the accompanying drawing in the embodiment of the invention, the technical scheme in the embodiment of the invention is clearly and completely described, obviously, described embodiment only is the present invention's part embodiment, rather than whole embodiment.Based on the embodiment among the present invention, those of ordinary skills belong to the scope of protection of the invention not making the every other embodiment that obtains under the creative work prerequisite.
As shown in Figure 1, the button manufacturing process that the embodiment of the invention provides, it may further comprise the steps:
S11, allotment plastic raw materials;
S12, to add part by weight in the plastic raw materials be the wood grain powder of 0.6%-15%;
S13, the plastic raw materials that adds the wood grain powder is carried out heat fused;
S14, make the plastic raw materials cooling forming that is in molten state, obtain the button section bar;
S15, to the button section bar shear, Surface Machining, obtain the finished product button.
The button manufacturing process that present embodiment provides, in plastic raw materials, add the wood grain powder that can form wood grain, no matter make the button section bar is on its surface in the process of producing or portion all can form wood grain within it, and because the characteristic of wood grain powder itself, make that the wood grain that is formed by the wood grain powder is more clear, plastic button distribute more even, imitative wood effect is better.The part by weight of wood grain powder is that the number range of 0.6%-15% is a preferable range.
In order further to optimize technique scheme, in the button manufacturing process that present embodiment provides, the wood grain powder joins in the plastic raw materials in the color matching operation of plastic raw materials.The color matching operation of plastic raw materials is the committed step that determines finished product button color and luster, the effect that the wood grain powder is incorporated in the plastic material is exactly to form wood grain in surface and the inside of finished product button, can farthest improve imitative wood effect so in this operation, add the wood grain powder, nor can follow-up operation be impacted.
Concrete, as shown in Figure 2, the concrete manufacturing process of plastic raw materials heat fused and cooling forming may further comprise the steps:
S31, the plastic raw materials that will add the wood grain powder are put into the barrel of injection machine;
S32, in barrel, plastic raw materials is heated, and by the screw rod of injection machine plastic raw materials is sheared;
S33, by screw rod, the melt of the plastic raw materials after the plasticizing is pushed in the die casting system of injection machine;
Behind S34, the plastic raw materials cooling forming, it is taken out from the die casting system, obtain the button section bar.
Wherein, when barrel heats plastic raw materials, use screw rod that plastic raw materials is sheared, make plastic raw materials convert viscous state to by the solid particle state, make mixing and the plasticizing of plastic raw materials expand to molecular level, adopt screw rod will plastify the end that good melt is pushed through screw rod then, its nozzle through injection machine is entered in the die casting system, and make plastic raw materials fill up the die cavity of die casting system, through cooling after a while, cooling can take place and shrink in the melt that is arranged in die cavity, use screw rod again the melt in the barrel to be pushed through in the die cavity this moment, and guarantee that screw rod is continuously applied extruding force, make the melt in the die cavity constantly obtain replenishing to keep die cavity to be in the state of being filled all the time, complete to guarantee the button profile shapes that obtains.After the plastic raw materials forming process is finished, remove the extruding force of screw rod, open die cavity, the button section bar is taken out from die cavity.
As shown in Figure 3, to the button section bar shear, Surface Machining, the concrete technology that obtains the finished product button may further comprise the steps:
S41, the surface of button section bar processed make it become the button semi-finished product;
S42, the button semi-finished product are carried out polishing and then obtain the finished product button.
Preferably, in the button manufacturing process that present embodiment provides, also comprise and use the radium-shine processing step that the button semi-finished product are carved and/or cut.Button can also utilize laser engraving pattern and character on finished product button surface according to client's actual needs in the engineering of producing, in addition, if desired, also can utilize and radium-shine the button semi-finished product be cut.
To the above-mentioned explanation of the disclosed embodiments, make this area professional and technical personnel can realize or use the present invention.Multiple modification to these embodiment will be apparent concerning those skilled in the art, and defined General Principle can realize under the situation that does not break away from the spirit or scope of the present invention in other embodiments herein.Therefore, the present invention will can not be restricted to these embodiment shown in this article, but will meet the wideest scope consistent with principle disclosed herein and features of novelty.

Claims (5)

1. a button manufacturing process is characterized in that, may further comprise the steps:
11) allotment plastic raw materials;
12) adding part by weight in the described plastic raw materials is the wood grain powder of 0.6%-15%;
13) the described plastic raw materials that adds the wood grain powder is carried out heat fused;
14) make the described plastic raw materials cooling forming that is in molten state, obtain the button section bar;
15) to described button section bar shear, Surface Machining, obtain the finished product button.
2. button manufacturing process according to claim 1 is characterized in that, described wood grain powder joins in the described plastic raw materials in the color matching operation of described plastic raw materials.
3. button manufacturing process according to claim 1 is characterized in that, the concrete manufacturing process of described plastic raw materials heat fused and cooling forming may further comprise the steps:
31) the described plastic raw materials that will add described wood grain powder is put into the barrel of injection machine;
32) in described barrel, described plastic raw materials is heated, and by the screw rod of described injection machine described plastic raw materials is sheared;
33) by described screw rod, the melt of the described plastic raw materials after the plasticizing is pushed in the die casting system of described injection machine;
34) behind the described plastic raw materials cooling forming, it is taken out from described die casting system, obtain the button section bar.
4. button manufacturing process according to claim 1 is characterized in that, to described button section bar shear, Surface Machining, the concrete technology that obtains the finished product button may further comprise the steps:
41) surface of described button section bar is processed make it become the button semi-finished product;
42) described button semi-finished product are carried out polishing and then obtain the finished product button.
5. button manufacturing process according to claim 4 is characterized in that, also comprises using the radium-shine processing step that described button semi-finished product are carved and/or cut.
CN2012104293322A 2012-10-31 2012-10-31 Manufacture technology of buttons Pending CN103182786A (en)