CN103129815A - Handling method for shelter corner - Google Patents

Handling method for shelter corner Download PDF

Info

Publication number
CN103129815A
CN103129815A CN2011103905986A CN201110390598A CN103129815A CN 103129815 A CN103129815 A CN 103129815A CN 2011103905986 A CN2011103905986 A CN 2011103905986A CN 201110390598 A CN201110390598 A CN 201110390598A CN 103129815 A CN103129815 A CN 103129815A
Authority
CN
China
Prior art keywords
shelter
corner
paint
processing method
solidify
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2011103905986A
Other languages
Chinese (zh)
Other versions
CN103129815B (en
Inventor
齐祥安
龙磊军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nuctech Co Ltd
Original Assignee
Nuctech Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nuctech Co Ltd filed Critical Nuctech Co Ltd
Priority to CN201110390598.6A priority Critical patent/CN103129815B/en
Publication of CN103129815A publication Critical patent/CN103129815A/en
Application granted granted Critical
Publication of CN103129815B publication Critical patent/CN103129815B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a handling method for a shelter corner. The method includes the steps: S1, first sealing materials are coated on a mask of an inner corner and a mask of an outer corner, and corner wrapping plates are fixed on the inner corner and the outer corner; S2, holes are drilled in the corner wrapping plates, blind rivets are put into the holes, wherein outer surfaces of the blind rivets are dipped in second sealing materials, and riveting and hole filling are carried out; S3, the first sealing materials and the second sealing materials are solidified, and exposed parts of the blind rivets are polished, coated with third sealing materials and solidified; S4, primer is spray coated and solidified, filling materials are blade coated on the primer, and floating coat is spray coated on the primer after solidification and polish; and S5, the floating coat is solidified, polished, finish paint is spray coated on the floating coat, and the finish coat is solidified. By utilization of the method, the shelter corner is handled, so that the fisheye phenomenon of the shelter corner can be avoided, and image and quality of appearance of a shelter are improved.

Description

Shelter corner processing method
Technical field
The present invention relates to shelter manufacturing technology field, relate in particular to a kind of shelter corner processing method.
Background technology
Along with the development of civilian and military facility demand, the demand of shelter (contain military cabin body, below all use " shelter " word) is significantly increased.In traditional manufacture method, generally use the method (also claiming " bright rivetting method ") that pulling rivet exposes that the corner of shelter is processed, the effect after processing as shown in Figure 1.These class methods affect the image appearance of shelter because the staking ailhead exposes in a large number.
More attractive in appearance for the corner (seamed edge is mainly external corner) that makes shelter, a lot of manufacturing enterprises use sinks to then carrying out the process of application with the staking ailhead, and the staking ailhead is covered under the application coating, is called as " dark rivetting method ".This kind method is decorated the corner (rib) of shelter fine, has improved the presentation quality of product, and has formed a production technology of generally using, and flow scheme sees Fig. 2 for details.But there is a problem that is difficult to overcome in this technique: after the shelter cornerite is coated (after application coating drying or after several hours) soon, there is the part of pulling rivet the vestige of staking ailhead will occur, the spitting image of the eyes of fish, so this defects of coatings (defective) is called as " flake ".As time goes on, this defects of coatings (" flake ") forms tiny crackle gradually, and corrosive medium crackle thus constantly penetrates into cornerite inside, causes the corrosion of parent metal, and corrosion product makes again the position of staking ailhead form larger crackle.The formation vicious circle that goes round and begins again of this phenomenon can cause just in 2-3 that application coating Local Cracking peels off, parent metal and staking ailhead be corroded, and had a strong impact on image appearance and the product design of shelter.In order to repair this type of cornerite disadvantage of shelter, expend a large amount of expenses and delay the use of shelter.
Summary of the invention
The technical matters that (one) will solve
The technical problem to be solved in the present invention is: how a kind of shelter corner processing method is provided, can avoids " flake " phenomenon of shelter corner, improve image appearance and the quality of shelter.
(2) technical scheme
For addressing the above problem, the invention provides a kind of shelter corner processing method, the method comprising the steps of:
S1. smear the first leakproofing material on the illiteracy plate at the interior angle of pending shelter corner and exterior angle, the cornerite plate is fixed on interior angle and exterior angle;
S2. hole on described cornerite plate, outside face is dipped in the pulling rivet of the second leakproofing material and put into described hole, and carry out staking and filling perforation operation;
S3. solidify described the first leakproofing material and the second leakproofing material, the part that described pulling rivet exposes is polished and smeared the 3rd leakproofing material, and solidify;
S4. spray priming paint and solidify, blade coating is filled and led up material on priming paint, and to its be cured and grinding process after, be coated with in the spraying thereon;
S5. solidify and be coated with and polish in described, spray paint, solidify described finish paint thereon.
Wherein, described the first leakproofing material is two component sealing gum or unsaturated polyester resin or epoxy resin.
Wherein, in step S2, described the second leakproofing material is the former paint of two component epoxy priming paint or unsaturated polyester resin or epoxy resin.
Wherein, in step S2, carry out the filling perforation operation with aluminium wire, and the interface use former paint of two component epoxy priming paint or unsaturated polyester resin or the epoxy sealing of taking out heart hole of described aluminium wire and described pulling rivet.
Wherein, in step S3, be the former paint of two component epoxy priming paint or unsaturated polyester resin or epoxy resin at described the 3rd leakproofing material.
Wherein, the former paint of described two component epoxy priming paint does not add solvent or diluent.
Wherein, described unsaturated polyester resin or epoxy resin do not add glass fibre.
Wherein, be unsaturated polyester resin or epoxy resin at described the 3rd leakproofing material, and wherein add glass fibre formation glass-felt plastic.
(3) beneficial effect
The shelter corner of using method of the present invention to process the flake phenomenon can not occur, and the image appearance of shelter is good, and the product design that improves, the use and maintenance cost of having saved shelter.
Description of drawings
Fig. 1 is that traditional use staking method staking ailhead exposes schematic diagram;
Fig. 2 is traditional dark rivetting method flow scheme;
Fig. 3 is the shelter corner processing method flow diagram according to one embodiment of the present invention;
The cornerite local structure schematic diagram of the shelter that Fig. 4 processes for the shelter corner processing method of using one embodiment of the present invention;
Fig. 5 is the partial enlarged drawing of II in Fig. 4;
Wherein, 1, side plate exterior skin; 2, base plate exterior skin; 3, side plate inside panel; 4, base plate inside panel; 5, cap head is taken out heart pulling rivet; 6, cornerite plate; 7, cover plate; 8, square tube.
The specific embodiment
The present invention proposes shelter corner processing method reaches by reference to the accompanying drawings embodiment and is described in detail as follows.
Before using method of the present invention that the shelter corner is processed, need the strict surface of clearing up each interface, cleanliness level arrives 1 grade (before GB/T 18570.3-2005 coating coating, qualification test the 3rd part of steel surface treatment surface cleanliness level applies the dust evaluation (pressure-sensitive adhesive tape method) of the front steel surface of coating).
As shown in Figure 3, the shelter corner processing method according to one embodiment of the present invention comprises step:
S1. smear two component sealing gum on the illiteracy plate at the interior angle of pending shelter corner and exterior angle, the cornerite plate is fixed on interior angle and exterior angle, wherein, also scribble same two component sealing gum on the square tube of shelter corner and this illiteracy plate, its assembling schematic diagram and partial enlarged drawing are respectively as shown in Fig. 4-5;
S2. hole on the cornerite plate, outside face is dipped in the pulling rivet of the former paint of two component epoxy priming paint (not adding solvent or diluent) and put into this hole, and carry out staking and filling perforation operation, wherein the former paint of bi-component epoxy priming paint (not adding solvent or diluent) sealing is used at the interface of taking out between heart hole and packing aluminium wire of pulling rivet;
S3. solidify (drying) aforementioned leakproofing material, the part that pulling rivet exposes is smeared the former paint of bi-component epoxy priming paint (not adding solvent or diluent), solidify (drying), polishing, spraying priming paint;
S4. solidify (drying) priming paint, and blade coating epoxy resin coating or epoxy resin etc. are filled and led up material on dried priming paint, solidify (drying), polishing is coated with in the spraying thereon;
S5. be coated with in curing (drying), coat the finish paint that sprays the materials such as aliphatic category polyurethane in dried, solidify (drying) finish paint.
Continue as shown in Figure 3, the shelter corner processing method according to another embodiment of the present invention comprises step:
D1. smear unsaturated polyester resin (not adding glass fibre) on the illiteracy plate at the interior angle of pending shelter corner and exterior angle, the cornerite plate is fixed on interior angle and exterior angle, wherein, also scribble same unsaturated polyester resin on the square tube of shelter corner and this illiteracy plate, its assembling schematic diagram and partial enlarged drawing are also respectively as shown in Fig. 4-5;
D2. hole on the cornerite plate, outside face is dipped in the pulling rivet of unsaturated polyester resin (not adding glass fibre) and put into this hole, and carry out staking and filling perforation operation, wherein unsaturated polyester resin (not adding glass fibre) sealing is used at the interface of taking out between heart hole and packing aluminium wire of pulling rivet;
D3. solidify (drying) aforementioned leakproofing material, the part that pulling rivet exposes is smeared unsaturated polyester resin (add glass fibre and form glass-felt plastic), solidify (drying) polishing, spraying priming paint;
D4. solidify (drying) priming paint, and on dried priming paint the material such as blade coating epoxy resin coating or epoxy resin fill and lead up material, solidify (drying), polishing is coated with in the spraying thereon;
D5. solidify in (drying) and be coated with, polishing, in coat the finish paint of the material such as spraying aliphatic category polyurethane, and solidify (drying) finish paint.
Continue as shown in Figure 3, the shelter corner processing method according to another embodiment of the present invention comprises step:
P1. smear epoxy resin on the illiteracy plate at the interior angle of pending shelter corner and exterior angle, the cornerite plate is fixed on interior angle and exterior angle, wherein, also scribble same epoxy resin on the square tube of shelter corner and this illiteracy plate, its assembling schematic diagram and partial enlarged drawing are also respectively as shown in Fig. 4-5;
P2. hole on the cornerite plate, outside face is dipped in the pulling rivet of epoxy resin and put into this hole, and carry out staking and filling perforation operation, wherein epoxy sealing is used at the interface of taking out between heart hole and packing aluminium wire of pulling rivet;
P3. solidify (drying) aforementioned leakproofing material, the part that pulling rivet exposes is smeared epoxy resin (add glass fibre and form glass-felt plastic), solidify (drying) polishing, spraying priming paint;
P4. solidify (drying) priming paint, and on priming paint the material such as blade coating epoxy resin coating or epoxy resin fill and lead up material, solidify (drying), polishing is coated with in the spraying thereon;
P5. be coated with polishing, (drying) finish paint of spray paint, and curing thereon in curing (drying).
To sum up, with respect to the One component Sealant that uses in orthodox method, due to it in solidification process, there is the moisture absorption to solidify the contraction or expansion that causes or the shortcoming that can not solidify for a long time because sealed environment lacks steam, become one of key factor of the generation that has caused flake, the present invention's new material used has fundamentally been avoided the formation of flake.
In addition, in traditional handicraft, a large amount of putty (atomized ash) that use are filled and led up local surfaces, cause local easily suction, expansion, localized cracks and corrosion, and method of the present invention has solved problems effectively by the material of filling and leading up that adopts non-putty material;
Moreover, in the tradition manufacturing process, the problem that has sealant, putty (atomized ash), priming paint three to contact and but can not combine closely in the part of pulling rivet, poor adhesive force, thereby caused the generation of flake, by in the pulling rivet hole and the processing of the leakproofing material of exposed parts etc., avoided the generation of problems in method of the present invention.
Above embodiment only is used for explanation the present invention; and be not limitation of the present invention; the those of ordinary skill in relevant technologies field; without departing from the spirit and scope of the present invention; can also make a variety of changes and modification; therefore all technical schemes that are equal to also belong to category of the present invention, and scope of patent protection of the present invention should be defined by the claims.

Claims (8)

1. a shelter corner processing method, is characterized in that, the method comprising the steps of:
S1. smear the first leakproofing material on the illiteracy plate at the interior angle of pending shelter corner and exterior angle, the cornerite plate is fixed on interior angle and exterior angle;
S2. hole on described cornerite plate, outside face is dipped in the pulling rivet of the second leakproofing material and put into described hole, and carry out staking and filling perforation operation;
S3. solidify described the first leakproofing material and the second leakproofing material, the part that described pulling rivet exposes is polished and smeared the 3rd leakproofing material, and solidify;
S4. spray priming paint and solidify, blade coating is filled and led up material on priming paint, and to its be cured and grinding process after, be coated with in the spraying thereon;
S5. solidify and be coated with and polish in described, spray paint, solidify described finish paint thereon.
2. shelter as claimed in claim 1 corner processing method, is characterized in that, described the first leakproofing material is two component sealing gum or unsaturated polyester resin or epoxy resin.
3. shelter as claimed in claim 2 corner processing method, is characterized in that, in step S2, described the second leakproofing material is the former paint of two component epoxy priming paint or unsaturated polyester resin or epoxy resin.
4. shelter as claimed in claim 2 corner processing method, it is characterized in that, in step S2, carry out the filling perforation operation with aluminium wire, and the interface use former paint of two component epoxy priming paint or unsaturated polyester resin or the epoxy sealing of taking out heart hole of described aluminium wire and described pulling rivet.
5. shelter as claimed in claim 2 corner processing method, is characterized in that, in step S3, is the former paint of two component epoxy priming paint or unsaturated polyester resin or epoxy resin at described the 3rd leakproofing material.
6. as the described shelter of claim 2-5 any one corner processing method, it is characterized in that, the former paint of described two component epoxy priming paint does not add solvent or diluent.
7. as the described shelter of claim 2-4 any one corner processing method, it is characterized in that, described unsaturated polyester resin or epoxy resin do not add glass fibre.
8. shelter as claimed in claim 5 corner processing method, is characterized in that, is unsaturated polyester resin or epoxy resin at described the 3rd leakproofing material, and wherein add glass fibre and form glass-felt plastic.
CN201110390598.6A 2011-11-30 2011-11-30 Handling method for shelter corner Active CN103129815B (en)