CN103056167A - Control method of oppositely cutting material board shape quality - Google Patents

Control method of oppositely cutting material board shape quality Download PDF

Info

Publication number
CN103056167A
CN103056167A CN2010105839414A CN201010583941A CN103056167A CN 103056167 A CN103056167 A CN 103056167A CN 2010105839414 A CN2010105839414 A CN 2010105839414A CN 201010583941 A CN201010583941 A CN 201010583941A CN 103056167 A CN103056167 A CN 103056167A
Authority
CN
China
Prior art keywords
cutting
stretching
break down
board shape
bending correction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2010105839414A
Other languages
Chinese (zh)
Other versions
CN103056167B (en
Inventor
周建波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Southwest Aluminum Group Co Ltd
Original Assignee
Southwest Aluminum Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Southwest Aluminum Group Co Ltd filed Critical Southwest Aluminum Group Co Ltd
Priority to CN201010583941.4A priority Critical patent/CN103056167B/en
Publication of CN103056167A publication Critical patent/CN103056167A/en
Application granted granted Critical
Publication of CN103056167B publication Critical patent/CN103056167B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a control method of oppositely cutting material board shape quality. The control method of the oppositely cutting material board shape quality comprises rip cutting and oppositely cutting, stretching-bending correction, and packaging. According to the control method of the oppositely cutting material board shape quality, more specific requirements are raised to rip cutting and stretching-bending correction, and an oppositely cutting finished product is finally produced in a stretching-bending correction line. Although the thickness of stretching-bending correction is not changed, the width of stretching-bending correction is 50 millimeters narrower than half of an original strip. When a narrow material finished product is produced, the capacity of a stretching-bending correction device can fully satisfy. Finally, strip board shape is obviously improved, wave height is controlled within 1 millimeter, and user requirements are fully satisfied. When an oppositely cutting semi-finished product is produced, the influences, caused by limitation of the capacity of the stretching-bending correction device, from the material width and the material thickness are eliminated. Finally, cutting material board shape quality is improved.

Description

A kind of to break down template method of quality control
Technical field
The present invention relates to cold-rolling process, more particularly, relate to a kind of to break down template method of quality control.
Background technology
Thickness 〉=0.7mm is mainly used in decorating to break down, and is therefore very high to the quality requirement of aluminium base, especially the strip shape quality of base material.Finishing procedure stretch bending line is: stretch-bending straightening-rip cutting is to cuing open-packing.When rectifying the thick material semi-finished product of production by this technique stretch bending (thickness 〉=0.7mm), because the stretch bending straightening equipment is limited in one's ability, the motor load of each roller system has reached maximum, but extend and still can not reach setting value, and machine occurs sometimes and be listed as unusual jitter conditions, finally finding expression in plate shape does not smooth, through rip cutting to Strip Shape wave height after cuing open be: 3~5mm, the capacity of equipment that can not meet consumers' demand is inadequate, when producing semi-finished product, can not effectively smooth band, cause rip cutting still not reach user's request to cuing open rear plate shape, affect the user and use.
Summary of the invention
In view of this, the invention provides a kind of to break down template method of quality control, to improve break down template quality.
For achieving the above object, the invention provides following technical scheme:
A kind of to break down template method of quality control, comprising:
Rip cutting is to cuing open;
Stretch bending is rectified;
And packing.
Preferably, above-mentioned to break down template method of quality control in, described rip cutting is specially cuing open: two volume semi-finished product are twisted on the same sleeve, when stub bar when sleeve is rolled up 3~5m, depressing the upper cutter shaft of cutting edge.
Preferably, above-mentioned to break down template method of quality control in, described stub bar is not cut edge, and is bonded on the described sleeve by the fiber adhesive tape.
Preferably, above-mentioned to break down template method of quality control in, described step rip cutting is to also comprising after cuing open: a volume in described two volumes is along the circumferential direction made a call to a steel band.
Preferably, above-mentioned to break down template method of quality control in, described stretch bending is rectified and to be specially: after processing a volume of not beating steel band in described two volumes, a volume of steel band is beaten in processing.
Can find out from technique scheme, method is rectified to produce to rip cutting, stretch bending and has been done the more requirement of detail in the embodiment of the invention, the break down finished product is finally rectified the line output at stretch bending, although thickness does not become, stretch bending is rectified 1/2 also about narrow 50mm of band before the Width, and production is when expecting finished product in a narrow margin, stretch bending straightening equipment ability can satisfy fully, final Strip Shape has obvious improvement, and wave height is controlled within the 1mm, satisfies user's demand fully.Eliminated because the stretch bending straightening equipment is limited in one's ability, when producing the break down semi-finished product, be subjected to the impact of supplied materials width and thickness.Finally improved the quality of break down template.
The specific embodiment
Thickness 〉=0.7mm is mainly used in decorating to break down, and is therefore very high to the quality requirement of aluminium base, especially the strip shape quality of base material.Finishing procedure stretch bending line is: stretch-bending straightening-rip cutting is to cuing open-packing.When rectifying the thick material semi-finished product of production by this technique stretch bending (thickness 〉=0.7mm), because the stretch bending straightening equipment is limited in one's ability, the motor load of each roller system has reached maximum, but extend and still can not reach setting value, and machine occurs sometimes and be listed as unusual jitter conditions, finally finding expression in plate shape does not smooth, through rip cutting to Strip Shape wave height after cuing open be: 3~5mm, the capacity of equipment that can not meet consumers' demand is inadequate, when producing semi-finished product, can not effectively smooth band, cause rip cutting still not reach user's request to cuing open rear plate shape, affect the user and use.The embodiment of the invention is to the optimization of the production process route of break down.
The below is clearly and completely described the technical scheme in the embodiment of the invention, and obviously, described embodiment only is the present invention's part embodiment, rather than whole embodiment.Based on the embodiment among the present invention, those of ordinary skills belong to the scope of protection of the invention not making the every other embodiment that obtains under the creative work prerequisite.
A kind of to break down template method of quality control, comprising: rip cutting is to cuing open; Stretch bending is rectified; And packing.
Above-mentioned to break down template method of quality control in, rip cutting is specially cuing open: two volume semi-finished product are twisted on the same sleeve, when stub bar when sleeve is rolled up 3~5m, depressing the upper cutter shaft of cutting edge.Its objective is 1.: guarantee to help the volume quality, prevent that inner ring from not helping tight generation to take out a phenomenon; 2.: cutting edge rear two, to list tight conditions at machine consistent, guarantees to batch the end face quality.
Stub bar is not cut edge, and is bonded on the described sleeve by the fiber adhesive tape.
Rip cutting also comprises after cuing open: a volume in described two volumes is along the circumferential direction made a call to a steel band.Purpose is to prevent that rectifying the other aluminium volume of not producing when producing at stretch bending is got rid of pine;
Stretch bending is rectified and is specially: after processing a volume of not beating steel band in described two volumes, a volume of steel band is beaten in processing.
Method is rectified to produce to rip cutting, stretch bending and has been done the more requirement of detail in the embodiment of the invention, the break down finished product is finally rectified the line output at stretch bending, although thickness does not become, but 1/2 of band also about narrow 50mm before the strong Width of stretch bending, and produce when expecting finished product in a narrow margin, stretch bending straightening equipment ability can satisfy fully, and final Strip Shape has obvious improvement, wave height is controlled within the 1mm, satisfies user's demand fully.Eliminated because the stretch bending straightening equipment is limited in one's ability, when producing the break down semi-finished product, be subjected to the impact of supplied materials width and thickness.Finally improved the quality of break down template.
To the above-mentioned explanation of the disclosed embodiments, make this area professional and technical personnel can realize or use the present invention.Multiple modification to these embodiment will be apparent concerning those skilled in the art, and General Principle as defined herein can in the situation that does not break away from the spirit or scope of the present invention, realize in other embodiments.Therefore, the present invention will can not be restricted to these embodiment shown in this article, but will meet the widest scope consistent with principle disclosed herein and features of novelty.

Claims (5)

1. one kind to break down template method of quality control, it is characterized in that, comprising:
Rip cutting is to cuing open;
Stretch bending is rectified;
And packing.
2. according to claim 1ly break down template method of quality control be is characterized in that described rip cutting is specially cuing open: two volume semi-finished product are twisted on the same sleeve, when stub bar when sleeve is rolled up 3~5m, depressing the upper cutter shaft of cutting edge.
3. according to claim 2ly break down template method of quality control be is characterized in that described stub bar is not cut edge, be bonded on the described sleeve by the fiber adhesive tape.
4. according to claim 2 break down template method of quality control be is characterized in that described step rip cutting also comprises after cuing open: a volume in described two volumes is along the circumferential direction made a call to a steel band.
5. according to claim 4 break down template method of quality control be is characterized in that described stretch bending is rectified and is specially: after processing a volume of not beating steel band in described two volumes, a volume of steel band is beaten in processing.
CN201010583941.4A 2010-12-10 2010-12-10 A kind of to break down method for controlling shape Active CN103056167B (en)