CN103047852A - Drying cylinder for dyeing machine - Google Patents

Drying cylinder for dyeing machine Download PDF

Info

Publication number
CN103047852A
CN103047852A CN2012105461414A CN201210546141A CN103047852A CN 103047852 A CN103047852 A CN 103047852A CN 2012105461414 A CN2012105461414 A CN 2012105461414A CN 201210546141 A CN201210546141 A CN 201210546141A CN 103047852 A CN103047852 A CN 103047852A
Authority
CN
China
Prior art keywords
drying cylinder
materials
drying
dyeing machine
bonding layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012105461414A
Other languages
Chinese (zh)
Inventor
平华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUJIANG JINPINGHUA TEXTILE CO Ltd
Original Assignee
WUJIANG JINPINGHUA TEXTILE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUJIANG JINPINGHUA TEXTILE CO Ltd filed Critical WUJIANG JINPINGHUA TEXTILE CO Ltd
Priority to CN2012105461414A priority Critical patent/CN103047852A/en
Publication of CN103047852A publication Critical patent/CN103047852A/en
Pending legal-status Critical Current

Abstract

The invention relates to a drying cylinder for a dyeing machine. The drying cylinder comprises a drying cylinder body, a NiCrAlY bonding layer is arranged outside the drying cylinder body, a ZrO2-8%Y2O3 ceramic working layer prepared by the aid of plasma spraying technology is arranged outside the NiCrAlY bonding layer, the thickness of the NiCrAlY bonding layer is 20-400 micrometers, and the thickness of the ZrO2-8%Y2O3 ceramic working layer is 300-900 micrometers. The drying cylinder has the advantages that traditional stainless steel materials are replaced by low-carbon steel, the bonding layer and a composite ceramic coating are arranged outside base materials, the materials can be effectively protected from corrosion by preventing surface corrosion as the materials are corroded from surfaces of the materials, corrosion resistance of the materials is ensured, and manufacturing cost is effectively saved.

Description

A kind of dyeing machine Drying
Technical field
The present invention relates to a kind of Drying, relate in particular to the Drying that a kind of dyeing is used.
Background technology
In dyeing, Drying is one of the most basic accessory, often be subject to the dip-dye corrosion of the various raw materials such as fuel in the environment that Drying is used, in order to improve the Drying corrosion resistance, each manufacturer takes into thought, and the most frequently used method is to adopt the good stainless steel material of corrosion resistance to make Drying, but this method manufacturing cost is high, in case a Drying part is corroded, will integral replacing, caused huge waste of material and the wasting of resources.
Summary of the invention
Technical problem to be solved by this invention is that a kind of manufacturing cost of effective reduction Drying, the dyeing machine Drying that economizes on resources are provided.
In order to solve the problems of the technologies described above, the present invention is achieved by the following technical solutions: this dyeing machine Drying, comprise the Drying body, described Drying body exterior arranges layer of Ni CrAlY tack coat, and the outside of described NiCrAlY tack coat also is provided with the ZrO that one deck is prepared from by plasma spraying technology 2-8%Y 2O 3The pottery working lining.
Further, the thickness of described NiCrAlY tack coat is 20 ~ 400 μ m.
Further, described ZrO 2-8%Y 2O 3Pottery work layer thickness is 300 ~ 900 μ m.
Compared with prior art, usefulness of the present invention is: this dyeing machine changes traditional stainless steel material into mild steel with Drying, and at base material outer setting tack coat and composite ceramic coat, because corrosion occurs from the surface of material, stop the effectively corrosion of protective materials of surface corrosion own, so not only guaranteed the material corrosion resistance but also effectively saved manufacturing cost.
Description of drawings:
Accompanying drawing 1 is the structural representation of dyeing machine of the present invention with Drying.
Among the figure: 1, Drying body; 2, NiCrAlY tack coat; 3, ZrO 2-8%Y 2O 3The pottery working lining.
The specific embodiment:
Describe the present invention below in conjunction with the drawings and specific embodiments.
A kind of dyeing machine Drying as shown in Figure 1 comprises Drying body 1, described Drying body 1 outer setting layer of Ni CrAlY tack coat 2, and the outside of described NiCrAlY tack coat 2 also is provided with the ZrO that one deck is prepared from by plasma spraying technology 2-8%Y 2O 3Pottery working lining 3.
The thickness of described NiCrAlY tack coat 2 is 20 ~ 400 μ m.
Described ZrO 2-8%Y 2O 3Pottery working lining 3 thickness are 300 ~ 900 μ m.
This dyeing machine changes traditional stainless steel material into mild steel with Drying, and at base material outer setting tack coat and composite ceramic coat, because corrosion occurs from the surface of material, stop the effectively corrosion of protective materials of surface corrosion own, so not only guaranteed the material corrosion resistance but also effectively saved manufacturing cost.
It is emphasized that: above only is preferred embodiment of the present invention, be not that the present invention is done any pro forma restriction, every foundation technical spirit of the present invention all still belongs in the scope of technical solution of the present invention any simple modification, equivalent variations and modification that above embodiment does.

Claims (3)

1. dyeing machine Drying, comprise Drying body (1), it is characterized in that: described Drying body (1) outer setting layer of Ni CrAlY tack coat (2), the outside of described NiCrAlY tack coat (2) also is provided with the ZrO that one deck is prepared from by plasma spraying technology 2-8%Y 2O 3Pottery working lining (3).
2. dyeing machine Drying according to claim 1, it is characterized in that: the thickness of described NiCrAlY tack coat (2) is 20 ~ 400 μ m.
3. dyeing machine Drying according to claim 1 is characterized in that: described ZrO 2-8%Y 2O 3Pottery working lining (3) thickness is 300 ~ 900 μ m.
CN2012105461414A 2012-12-17 2012-12-17 Drying cylinder for dyeing machine Pending CN103047852A (en)