CN103046386A - 一种镇静安神羽绒的生产工艺 - Google Patents
一种镇静安神羽绒的生产工艺 Download PDFInfo
- Publication number
- CN103046386A CN103046386A CN2013100033744A CN201310003374A CN103046386A CN 103046386 A CN103046386 A CN 103046386A CN 2013100033744 A CN2013100033744 A CN 2013100033744A CN 201310003374 A CN201310003374 A CN 201310003374A CN 103046386 A CN103046386 A CN 103046386A
- Authority
- CN
- China
- Prior art keywords
- eider down
- finished product
- raw material
- semi
- down semi
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种镇静安神羽绒的生产工艺,依次按照以下步骤进行:预分;除灰;精分;初洗;清洗;漂洗:将清洗后的羽绒半成品放入沸水中煮10-15分钟,取出后再用10-15%双氧水浸泡5-10分钟,再用清水漂洗干净;一次脱水;浸泡:将脱水处理后的1/4-1/5羽绒半成品放入中药液中浸泡4-6小时,中药液的温度为30-40℃;二次脱水;烘干,得到羽绒成品。中药液中,各原料组分的重量配比为:钩藤8-12、菊花13-17、天麻13-17、大风草6-10、柏子仁8-12、万寿菊6-10、丁香13-17,放入清水煮沸20-30分钟,得到滤液。本发明使用的中药液采用镇静安神的中药,通过将脱水处理后的羽绒半成品浸泡在这样中药液中,中药精华浸入到羽绒本体内,使得羽绒同时具备保暖和镇静安神的功效。
Description
技术领域:
本发明主要涉及羽绒加工技术领域,尤其涉及一种镇静安神羽绒的生产工艺。
背景技术:
羽绒是长在鹅、鸭的腹部,成芦花朵状的绒毛,成片状的叫羽毛。由于羽绒是一种动物性蛋白质纤维,比棉花(植物性纤维素)保温性高,且羽绒球状纤维上密布千万个三角形的细小气孔,能随气温变化而收缩膨胀,产生调温功能,可吸收人体散发流动的热气,隔绝外界冷空气的入侵。因此,羽绒被大量用于羽绒被、羽绒衣等。
目前的羽绒也有与中药包配合使用,使其不仅具备保暖的功效,还具有保健的功效,但是,中药包增加了羽绒的重量而且容易移位掉落,使用不方便。
发明内容:
本发明目的就是为了弥补已有技术的缺陷,提供一种镇静安神羽绒的生产工艺,它将羽绒半成品浸泡在中药液中,使得中药精华浸入到羽绒本体内,使得羽绒本体同时具备保暖和镇静安神的功效。
本发明是通过以下技术方案实现的:
一种镇静安神羽绒的生产工艺,其特征在于:依次按照以下步骤进行:
一、预分:将原料毛中的翅梗、杂质、灰沙与羽绒分离,得到羽绒原料。
二、除灰:将预分得到的羽绒原料进行清理,进一步除去羽绒原料中的灰渣、杂质和皮屑,使羽绒原料中杂质含量低于10%。
三、精分:将除灰得到的羽绒原料进行提绒加工及拼堆,得到羽绒半成品。
四、初洗:将羽绒半成品用清水清洗3-7分钟,清除灰沙杂质。
五、清洗:将初洗后的羽绒半成品放入混有洗涤剂的水溶液中清洗20分钟。
六、漂洗:将清洗后的羽绒半成品放入沸水中煮10-15分钟,取出后再用10-15%双氧水浸泡5-10分钟,再用清水漂洗干净。
七、一次脱水:对漂洗后的羽绒半成品进行脱水处理,使羽绒半成品的含水量为28-32%。
八、浸泡:将脱水处理后的1/4-1/5羽绒半成品放入中药液中浸泡4-6小时,中药液的温度为30-40℃。
九、二次脱水:对浸泡后的羽绒半成品再次进行脱水处理,使羽绒半成品的含水量为28-32%。
十、烘干:对一次脱水后的羽绒半成品与二次脱水的羽绒半成品混合均匀,进行烘干处理,得到羽绒成品。
所述中药液中,各原料组分的重量配比为:钩藤8-12、菊花13-17、天麻13-17、大风草6-10、柏子仁8-12、万寿菊6-10、丁香13-17、清水1000-1200,煮沸20-30分钟,得到滤液。
一种镇静安神羽绒的生产工艺,其特征在于:依次按照以下步骤进行:
一、预分:将原料毛中的翅梗、杂质、灰沙与羽绒分离,得到羽绒原料。
二、除灰:将预分得到的羽绒原料进行清理,进一步除去羽绒原料中的灰渣、杂质和皮屑,使羽绒原料中杂质含量低于10%。
三、精分:将除灰得到的羽绒原料进行提绒加工及拼堆,得到羽绒半成品。
四、初洗:将羽绒半成品用清水清洗5分钟,清除灰沙杂质。
五、清洗:将初洗后的羽绒半成品放入混有洗涤剂的水溶液中清洗20分钟。
六、漂洗:将清洗后的羽绒半成品放入沸水中煮12分钟,取出后再用12%双氧水浸泡8分钟,再用清水漂洗干净。
七、一次脱水:对漂洗后的羽绒半成品进行脱水处理,使羽绒半成品的含水量为30%。
八、浸泡:将脱水处理后的1/4-1/5羽绒半成品放入中药液中浸泡5小时,中药液的温度为35℃。
九、二次脱水:对浸泡后的羽绒半成品再次进行脱水处理,使羽绒半成品的含水量为30%。
十、烘干:对一次脱水后的羽绒半成品与二次脱水的羽绒半成品混合均匀,进行烘干处理,得到羽绒成品。
所述中药液中,各原料组分的重量配比为:钩藤10、菊花15、天麻15、大风草8、柏子仁10、万寿菊8、丁香15、清水1100,煮沸25分钟,得到滤液。
在步骤六中,将羽绒半成品采用沸水煮沸后用双氧水浸泡,一方面可以起到漂白作用,另一方面可以取出羽绒半成品中的异味。
把这些羽绒应用到羽绒被或羽绒衣后,人体吸入中药散发的气味起到一定的安神作用。
本发明的优点是:
本发明使用的中药液采用镇静安神的中药,通过将脱水处理后的羽绒半成品浸泡在这样中药液中,中药精华浸入到羽绒本体内,使得羽绒同时具备保暖和镇静安神的功效。
具体实施方式:
一种镇静安神羽绒的生产工艺,依次按照以下步骤进行:
一、预分:将原料毛中的翅梗、杂质、灰沙与羽绒分离,得到羽绒原料。
二、除灰:将预分得到的羽绒原料进行清理,进一步除去羽绒原料中的灰渣、杂质和皮屑,使羽绒原料中杂质含量低于10%。
三、精分:将除灰得到的羽绒原料进行提绒加工及拼堆,得到羽绒半成品。
四、初洗:将羽绒半成品用清水清洗5分钟,清除灰沙杂质。
五、清洗:将初洗后的羽绒半成品放入混有洗涤剂的水溶液中清洗20分钟。
六、漂洗:将清洗后的羽绒半成品放入沸水中煮12分钟,取出后再用12%双氧水浸泡8分钟,再用清水漂洗干净。
七、一次脱水:对漂洗后的羽绒半成品进行脱水处理,使羽绒半成品的含水量为30%。
八、浸泡:将脱水处理后的1/4-1/5羽绒半成品放入中药液中浸泡5小时,中药液的温度为35℃。
九、二次脱水:对浸泡后的羽绒半成品再次进行脱水处理,使羽绒半成品的含水量为30%。
十、烘干:对一次脱水后的羽绒半成品与二次脱水的羽绒半成品混合均匀,进行烘干处理,得到羽绒成品。
所述中药液中,各原料组分的重量(g)为:钩藤10、菊花15、天麻15、大风草8、柏子仁10、万寿菊8、丁香15、清水1100,煮沸25分钟,得到滤液。
Claims (2)
1.一种镇静安神羽绒的生产工艺,其特征在于:依次按照以下步骤进行:
一、预分:将原料毛中的翅梗、杂质、灰沙与羽绒分离,得到羽绒原料;
二、除灰:将预分得到的羽绒原料进行清理,进一步除去羽绒原料中的灰渣、杂质和皮屑,使羽绒原料中杂质含量低于10%;
三、精分:将除灰得到的羽绒原料进行提绒加工及拼堆,得到羽绒半成品;
四、初洗:将羽绒半成品用清水清洗3-7分钟,清除灰沙杂质;
五、清洗:将初洗后的羽绒半成品放入混有洗涤剂的水溶液中清洗20分钟;
六、漂洗:将清洗后的羽绒半成品放入沸水中煮10-15分钟,取出后再用10-15%双氧水浸泡5-10分钟,再用清水漂洗干净;
七、一次脱水:对漂洗后的羽绒半成品进行脱水处理,使羽绒半成品的含水量为28-32%;
八、浸泡:将脱水处理后的1/4-1/5羽绒半成品放入中药液中浸泡4-6小时,中药液的温度为30-40℃;
九、二次脱水:对浸泡后的羽绒半成品再次进行脱水处理,使羽绒半成品的含水量为28-32%;
十、烘干:对一次脱水后的羽绒半成品与二次脱水的羽绒半成品混合均匀,进行烘干处理,得到羽绒成品;
所述中药液中,各原料组分的重量配比为:钩藤8-12、菊花13-17、天麻13-17、大风草6-10、柏子仁8-12、万寿菊6-10、丁香13-17、清水1000-1200,煮沸20-30分钟,得到滤液。
2.根据权利要求1所述的一种镇静安神羽绒的生产工艺,其特征在于:依次按照以下步骤进行:
一、预分:将原料毛中的翅梗、杂质、灰沙与羽绒分离,得到羽绒原料;
二、除灰:将预分得到的羽绒原料进行清理,进一步除去羽绒原料中的灰渣、杂质和皮屑,使羽绒原料中杂质含量低于10%;
三、精分:将除灰得到的羽绒原料进行提绒加工及拼堆,得到羽绒半成品;
四、初洗:将羽绒半成品用清水清洗5分钟,清除灰沙杂质;
五、清洗:将初洗后的羽绒半成品放入混有洗涤剂的水溶液中清洗20分钟;
六、漂洗:将清洗后的羽绒半成品放入沸水中煮12分钟,取出后再用12%双氧水浸泡8分钟,再用清水漂洗干净;
七、一次脱水:对漂洗后的羽绒半成品进行脱水处理,使羽绒半成品的含水量为30%;
八、浸泡:将脱水处理后的1/4-1/5羽绒半成品放入中药液中浸泡5小时,中药液的温度为35℃;
九、二次脱水:对浸泡后的羽绒半成品再次进行脱水处理,使羽绒半成品的含水量为30%;
十、烘干:对一次脱水后的羽绒半成品与二次脱水的羽绒半成品混合均匀,进行烘干处理,得到羽绒成品;
所述中药液中,各原料组分的重量配比为:钩藤10、菊花15、天麻15、大风草8、柏子仁10、万寿菊8、丁香15、清水1100,煮沸25分钟,得到滤液。