CN103042839B - A kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment - Google Patents
A kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment Download PDFInfo
- Publication number
- CN103042839B CN103042839B CN201310029350.6A CN201310029350A CN103042839B CN 103042839 B CN103042839 B CN 103042839B CN 201310029350 A CN201310029350 A CN 201310029350A CN 103042839 B CN103042839 B CN 103042839B
- Authority
- CN
- China
- Prior art keywords
- scuff
- support
- xian district
- guo xian
- container cup
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The present invention discloses a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment, and comprise support and the container cup be arranged on this support and Guo Xian district from top to bottom, described container cup and bottom, Guo Xian district are provided with switch valve, and described Guo Xian district is provided with liquid-leaking nozzle.Because the present invention adopts technique scheme, both wire rod cost had been reduced, the lettering scuff meeting client requires (450G bear a heavy burden get wet on felt-cloth 10 letterings back and forth do not come off), to solve in prior art because coding lettering not scuff and the various negative consequences that cause, be formulated to intra-company's standard simultaneously and get the nod in colleague; In addition, can according to extruder size before and after Row sum-equal matrix height; Simple to operation, easily carry and deposit, and having environmental protection feature.
Description
Technical field
The invention belongs to cable typing equipment field, be specifically related to a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment.
Background technology
Modern due to environmental pollution serious, people focus on environmental protection to surrounding environment, and cable industry also slowly turns to bittern-free flame-proof material from PVC material.But there are a kind of special circumstances in industry, thermoplastic halogen-free flame retarding material is if use type wheel lettering, that prints off word of coming and numeral is unusual scuff, but use ink jet numbering machine lettering, that word gushed out and numeral are not scuff, this just causes domestic enterprise of much doing foreign trade because coding lettering not scuff and resulting in a loss, and even goes bankrupt.
Summary of the invention
Technical problem to be solved by this invention is for above-mentioned the deficiencies in the prior art, a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment is provided, it makes the coding lettering more scuff on thermoplastic halogen-free flame retarding material, meet the lettering scuff requirement of client, this equipment has the advantages such as simple to operation, easy carrying is deposited, environmental protection simultaneously.
The technical solution adopted in the present invention is: a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment, comprise support and the container cup be arranged on this support and Guo Xian district from top to bottom, described container cup and bottom, Guo Xian district are provided with switch valve, and described Guo Xian district is provided with liquid-leaking nozzle.
As preferably, described support, container cup and Guo Xian district are the stainless steel material of corrosion-resistant and high-temperature resistant.
As preferably, described container cup is by can the quill of running fix on the bracket be connected with support.
As preferably, described Guo Xian district is by can the quill of running fix on the bracket be connected with support.
As preferably, described quill is connected with described container cup Huo Guoxian district by telescopic strut.
As preferably, liquid collecting place in described Guo Xian district has watch window.
As preferably, in described Guo Xian district, be provided with sponge.
As preferably, described frame bottom is provided with base.
As preferably, described base is provided with retracting device.
Beneficial effect of the present invention is: because the present invention adopts technique scheme, both wire rod cost had been reduced, the lettering scuff meeting client requires (450G bear a heavy burden get wet on felt-cloth 10 letterings back and forth do not come off), to solve in prior art because coding lettering not scuff and the various negative consequences that cause, be formulated to intra-company's standard simultaneously and get the nod in colleague; In addition, can according to extruder size before and after Row sum-equal matrix height; Simple to operation, easily carry and deposit, and having environmental protection feature.
Accompanying drawing explanation
Fig. 1 is structural representation of the present invention;
Fig. 2 is structural representation of the present invention.
In figure: 1, support; 2, container cup; 3, Guo Xian district; 4, switch valve; 5, liquid-leaking nozzle; 6, quill; 7, telescopic strut; 8, watch window; 9, base; 10, retracting device.
Detailed description of the invention
Below in conjunction with the accompanying drawings and the specific embodiments the present invention is described in further detail.
As depicted in figs. 1 and 2, a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment, the container cup 2 comprising support 1 and be arranged on this support 1 from top to bottom and Guo Xian district 3, described container cup 2 and bottom, Guo Xian district 3 are provided with switch valve 4, described container cup 2 and Guo Xian district 3 are all by can the quill 6 of running fix on described support 1 be connected with support 1, described quill 6 is connected with described container cup 2 Huo Guoxian district 3 by telescopic strut 7 simultaneously, and described Guo Xian district 3 is provided with liquid-leaking nozzle 5.
In order to make thermoplastic halogen-free flame retarding material coding lettering scuff, thermoplastic halogen-free flame retarding material coding lettering scuff equipment of the present invention, is equipped with high-quality diluent, and is placed on operation between extruder first paragraph hot water storgae and ink jet numbering machine in described container cup 2; Put one piece of sponge in described Guo Xian district 3, can not allow liquid splashes, allow simultaneously wire rod by time fully absorb diluent, to improve scuff ability.
Use procedure of the present invention is as follows:
When wire rod is extruded out from head, cool through first paragraph tank, at this moment wire rod is through the Guo Xian district 3 of this equipment, allow wire surface be stained with diluent, diluent just carries out wire surface to corrode (having no effect to wire rod), and the wire surface corroded is no longer smooth, can be gone into be invisible to the naked eye concavo-convex on surface, allow ink jet numbering machine spray numeral or word again, then dry up surface through air jet pipe, such lettering is very scuff.
In order to reduce costs, thermoplastic halogen-free flame retarding material coding lettering scuff equipment of the present invention, described material has all easily been bought, and support 1 of the present invention, container cup 2 and Guo Xian district 3 are the stainless steel material of corrosion-resistant and high-temperature resistant.
Preferably, base 9 is provided with bottom described support 1, base 9 is provided with retracting device 10, have watch window 8 in liquid collecting place in described Guo Xian district 3, in the present embodiment, watch window 8 one has four, lays respectively on four sides in described Guo Xian district 3, its objective is the dosage observing diluent in Guo Xian district 3, when diluent starts to overflow, can open in the retracting device 10 that switch valve 4 is recycled on base 9, reach secondary and utilize.
Because the present invention adopts technique scheme, both wire rod cost had been reduced, the lettering scuff meeting client requires (450G bear a heavy burden get wet on felt-cloth 10 letterings back and forth do not come off), to solve in prior art because coding lettering not scuff and the various negative consequences that cause, be formulated to intra-company's standard simultaneously and get the nod in colleague; In addition, can according to extruder size before and after Row sum-equal matrix height; Simple to operation, easily carry and deposit, and having environmental protection feature.
The above, be only present pre-ferred embodiments, therefore can not limit scope of the invention process with this, and the equivalence namely done according to the present patent application the scope of the claims and description changes and modifies, and all should still remain within the scope of the patent.
Claims (3)
1. a thermoplastic halogen-free flame retarding material coding lettering scuff equipment, it is characterized in that: comprise support (1) and the container cup (2) that is arranged on this support (1) and Guo Xian district (3) from top to bottom, described container cup (2) and Guo Xian district (3) bottom are provided with switch valve (4), be equipped with for corroding wire surface and making its surface form the concavo-convex diluent be invisible to the naked eye in described container cup (2), described Guo Xian district (3) is provided with liquid-leaking nozzle (5), sponge is provided with in described Guo Xian district (3), described support (1) bottom is provided with base (9), base (9) is provided with retracting device (10),
Described container cup (2) is by being connected with support (1) at the quill (6) of the upper running fix of described support (1), described Guo Xian district (3) is by being connected with support (1) at the quill (6) of the upper running fix of described support (1), and described quill (6) is connected with described container cup (2) Huo Guoxian district (3) by telescopic strut (7).
2. a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment according to claim 1, is characterized in that: described support (1), container cup (2) and Guo Xian district (3) are the stainless steel material of corrosion-resistant and high-temperature resistant.
3. a kind of thermoplastic halogen-free flame retarding material coding lettering scuff equipment according to claim 1, is characterized in that: liquid collecting place of described Guo Xian district (3) has watch window (8).