CN103005795B - Small diamond matching and inlaying process and auxiliary tools thereof - Google Patents
Small diamond matching and inlaying process and auxiliary tools thereof Download PDFInfo
- Publication number
- CN103005795B CN103005795B CN201210566778.XA CN201210566778A CN103005795B CN 103005795 B CN103005795 B CN 103005795B CN 201210566778 A CN201210566778 A CN 201210566778A CN 103005795 B CN103005795 B CN 103005795B
- Authority
- CN
- China
- Prior art keywords
- wax
- parison
- pattern
- broken
- adhered layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a small diamond matching and inlaying process and auxiliary tools of the small diamond matching and inlaying process. The matching and inlaying process comprises 7 steps of wax pattern manufacturing, matching and inlaying of small diamonds on the wax pattern, small diamond stripping, parison manufacturing, formation of metal jewelry with diamond hole sites, polishing as well as hole site cleaning treatment and small diamond fixation; and the auxiliary tools of the matching and inlaying process comprise a wax pattern, a parison formation chamber, a parison and a bonding layer, wherein the wax pattern is a jewelry mould without small diamonds being matched and inlaid yet; the wax pattern is accommodated in the parison formation chamber; the parison is manufactured by the parison formation chamber accommodating the wax pattern; and the bonding layer covers the surface of the wax pattern fixed with small diamonds, and is provided with viscous force with the small diamonds. According to the small diamond matching and inlaying process and auxiliary tools thereof disclosed by the invention, the matching and inlaying effect of the small diamonds is very conveniently ensured via using the wax pattern and the parison; and at the same time, the production efficiency is improved greatly.
Description
Technical field
The present invention relates to a kind of mosaic technology and aid thereof, relate in particular to a kind of broken brill and spell edge technique and aid thereof.
Background technology
Since ancient times, diamond is considered as power, prestige, status and rich and honour symbol by the mankind always.Its indestructible, all-conquering, faithful eternal and firm and persistent manly quality is the target that the mankind pursue forever.It has potential, huge cultureal value.Glittering and translucent, the very beautiful noble quality of bitellos in diamond, however bitellos is often also expensive, is not that ordinary people can bear.And meanwhile, broken brill is mostly the leftover pieces of diamond, the market price is very cheap; These are broken be drilled in after designer's design, not only can set off out the color and gorgeous color of the fire of other jewel and style is more, visually very dazzling, give luxurious sense, therefore now on market this broken brill to spell the product of inlaying gradually popular.Yet the technology of at present spelling edge about broken brill exists problems, such as because broken brill is not of uniform size, how efficiently the broken row that creeps into is spelled to edge, realized broken brill spell the smooth of whole surface after edge when guaranteeing brightness.
Summary of the invention
The object of the invention is to spell for existing broken brill the deficiency of edge technique, provide a kind of efficient broken brill to spell edge technique.
In order to achieve the above object, the present invention has adopted following technical scheme:
Broken brill is spelled an edge technique, comprises following 7 steps:
S1, making and the wax-pattern that inlaid diamond jewellery are not identical;
S2, broken the pressure of the drill is entered to wax-pattern surface and make wax-pattern surface keep smooth, the broken the pressure of the drill of difference is entered to wax-pattern surface and keep afterwards whole broken the smooth of surface that bore;
S3, be pressed into after all broken brills, being fixed with wax-pattern surface coverage one adhered layer of broken brill, by the stickup of adhered layer and diamond bizet, all broken brills peeled off to wax-pattern surface;
S4, utilize the wax-pattern that diamond has been stripped from after S3 step process to make parison;
S5, utilize parison to carry out the metal jewelry that pressure injection obtains position, existing diamond hole;
S6, the metal jewelry of the position, existing diamond hole being obtained by described S5 step is carried out to polishing and position, hole cleaning;
S7, will be bonded at broken brill on described adhered layer and embed position, corresponding diamond hole the fixing corresponding broken brill of described metal jewelry.
Adopting above-mentioned 7 steps to carry out broken brill spells while inlaying, although broken brill is not of uniform size, but first on wax-pattern, carrying out ranking fixes, only need be by boring and simple instrument is modified and can be completed the arranging and obtain the wax-pattern with position, diamond hole of broken brill by crushing, guaranteed that very simply and easily broken brill spells edge effect; Adopt adhered layer that all broken brills are directly peeled away from wax-pattern, not only convenient and swift but also can not upset the broken brill position of having arranged; Polishing and the cleaning of position, diamond hole has been guaranteed to treat the quality of the metal jewelry of diamond setting stone; By making parison, complete once the making of waiting to inlay broken brill metal jewelry with position, all diamonds hole, improved production efficiency.
Particularly, the adhered layer of S3 step adopts an adhesive band; S7 step embeds the broken brill on adhered layer and is fixed in the position, corresponding diamond hole of metal jewelry one by one.
Preferably, the adhered layer of S3 step is hard adhered layer; S7 step directly overlays the adhered layer that is stained with all broken brills on the metal jewelry being obtained by S6 step and embeds position, corresponding diamond hole, then carries out diamond and fixes.
Particularly, S6 step adopt at edge, position, hole, shovel out that ailhead pushes again or directly extruded hole position edge metal fix broken brill.That is, follow closely the mode fixed diamonds of edge and micro-edge by employing, this fixed form does not show metal, more can give full play to the gloss of whole diamond.
Particularly, S4 step is inserted parison formation chamber by mould, pours into gypsum, then wax-pattern is melted, thereby make parison in parison formation chamber.
Meanwhile, the present invention also discloses the aid that a kind of broken brill is spelled edge technique simultaneously, comprises a wax-pattern, a parison formation chamber, a parison and an adhered layer; Wax-pattern is the jewellery die of not spelling the broken brill of edge; The indoor accommodating wax-pattern of parison formation, and be provided with at least one conduit, conduit contact wax-pattern; Parison is made by the parison formation chamber that is equipped with wax-pattern; Adhered layer covers the wax-pattern surface be fixed with broken brill, and with the broken viscous force that is drilled with.
Particularly, parison is gypsum parison.
Particularly, adhered layer adopts an adhesive band, is preferably hard adhered layer.
The invention discloses a kind of broken brill and spell edge technique and aid thereof.This kind spells edge technique and aid has guaranteed the spelling edge effect of broken brill very easily by the use of wax-pattern, parison, also greatly improved production efficiency simultaneously.
Accompanying drawing explanation
Fig. 1 is that broken brill is spelled edge technique aid schematic diagram;
Fig. 2 is that broken brill is spelled the schematic diagram after edge technique S3 step process;
Fig. 3 is the schematic cross-section that wax-pattern is inserted parison formation chamber;
The parison sectional view of Fig. 4 for producing according to S4 step;
Number in the figure: wax-pattern 1, is fixed with the wax-pattern 1` of broken brill, the wax-pattern 1`` that diamond has been stripped from, adhesive band 2, parison formation chamber 3, parison 4, conduit 5.
The specific embodiment
Below in conjunction with specific embodiment, technical scheme of the present invention is made further clear and complete instructions.
Embodiment
Embodiment discloses a kind of broken brill and has spelled edge technique, and it is example that the present embodiment be take broken brill spelling edge to bracelet, and this spelling edge technique comprises following 7 steps:
S1, making and the wax-pattern 1 that inlaid diamond jewellery are not identical;
S2, broken the pressure of the drill is entered to wax-pattern 1 surface and makes wax-pattern surface keep smooth, keep whole broken the smooth of surface that bore after the broken the pressure of the drill of difference is entered to wax-pattern 1 surface;
S3, be pressed into after all broken brills, be fixed with wax-pattern 1` surface coverage one deck adhesive band 2 of broken brill, by adhesive band 2 and the stickup of diamond bizet, all broken brills are peeled off to wax-pattern surface;
S4, utilize the wax-pattern 1`` that diamond has been stripped from after S3 step process to make parison 4; Be about to mould and insert parison formation chamber 3, in parison formation chamber 3, pour into gypsum, more above-mentioned wax-pattern 1`` is melted, and its conduit that passes through parison formation chamber 35 is flowed out, thereby make parison 4;
S5, to pressure injection metal liquid in parison 4, after metal liquid solidifies, parison 4 is broken, thereby is obtained the metal jewelry of position, existing diamond hole;
S6, this metal jewelry is carried out to polishing and position, hole cleaning;
S7, will be bonded at broken brill on adhesive band 2 and embed one by one and be fixed in the position, corresponding diamond hole of metal jewelry, (also can adopt hard adhered layer in other embodiments, the adhered layer that is stained with all broken brills directly overlayed on the metal jewelry being obtained by S6 step and embed behind position, corresponding diamond hole, carrying out diamond fixes again), fixed form adopts and at edge, position, hole, shovels out ailhead, the mode of extruded hole position edge metal fixes corresponding broken brill (also directly extruded hole position edge metal fixes broken brill in other embodiments) again.
Adopting above-mentioned 7 steps to carry out broken brill spells while inlaying, although broken brill is not of uniform size, but first on wax-pattern, carrying out ranking fixes, only need be by boring and simple instrument is modified and can be completed the arranging and obtain the wax-pattern with position, diamond hole of broken brill by crushing, guaranteed that very simply and easily broken brill spells edge effect; Adopt adhesive band that all broken brills are directly peeled away from wax-pattern, not only convenient and swift but also can not upset the broken brill position of having arranged; Polishing and the cleaning of position, diamond hole has been guaranteed to treat the quality of the metal jewelry of diamond setting stone; By making parison, complete once the making of waiting to inlay broken brill metal jewelry with position, all diamonds hole, improved production efficiency.
At broken brill, spell in edge technique and related to the aid of spelling edge technique, comprise a wax-pattern 1, a parison formation chamber 3, a parison 4 and an adhesive band 2; Wax-pattern 1 is the jewellery die of not spelling the broken brill of edge; The interior accommodating wax-pattern 1 in parison formation chamber 3, and be provided with a conduit 5, these conduit 5 contact wax-patterns 1; Parison 4 is made by the parison formation chamber 3 that is equipped with wax-pattern 1, adopts gypsum material; Adhesive band 2 covers wax-pattern 1 surface that is fixed with broken brill, and with the broken viscous force that is drilled with.
From above-described embodiment, the invention discloses a kind of broken brill and spell edge technique and aid thereof.This kind spells edge technique and aid has guaranteed the spelling edge effect of broken brill very easily by the use of wax-pattern, parison, also greatly improved production efficiency simultaneously.
It should be noted that; above-described embodiment is only illustrating technical scheme of the present invention; and this is practical to be not used in restriction; it is that numerous broken brills are spelled an example in frosting product that broken brill is spelled edge bracelet; everyly the present invention is done to being equal to of same design replaces or conversion, all belong to protection scope of the present invention.
Claims (9)
1. broken brill is spelled an edge technique, and described spelling edge technique comprises:
S1, making and the wax-pattern (1) that inlaid diamond jewellery are not identical;
S2, broken the pressure of the drill is entered to wax-pattern (1) surface and make wax-pattern surface keep smooth, keep whole broken the smooth of surface that bore after the broken the pressure of the drill of difference is entered to wax-pattern (1) surface;
It is characterized in that, also comprise:
S3, be pressed into after all broken brills, being fixed with the wax-pattern of broken brill (1`) surface coverage one adhered layer, by the stickup of adhered layer and diamond bizet, all broken brills peeled off to wax-pattern surface;
S4, utilize wax-pattern (1``) and parison formation chamber (3) that diamond has been stripped from after described S3 step process to make parison (4);
S5, utilize parison (4) to carry out the metal jewelry that pressure injection obtains position, existing diamond hole;
S6, the metal jewelry of the position, existing diamond hole being obtained by described S5 step is carried out to polishing and position, hole cleaning;
S7, will be bonded at broken brill on described adhered layer and embed position, corresponding diamond hole the fixing corresponding broken brill of described metal jewelry.
2. spelling edge technique according to claim 1, is characterized in that: the adhered layer of described S3 step adopts an adhesive band (2); Described S7 step embeds the broken brill on adhered layer and is fixed in the position, corresponding diamond hole of described metal jewelry one by one.
3. spelling edge technique according to claim 1, is characterized in that: the adhered layer of described S3 step is hard adhered layer; Described S7 step directly overlays the adhered layer that is stained with all broken brills by the metal jewelry described in S6 step and embed position, corresponding diamond hole, then carries out diamond and fixes.
4. according to the arbitrary described spelling edge technique of claim 1-3, it is characterized in that: described S7 step employing shovels out ailhead and pushes or directly push position, described hole edge metal and fix described broken brill at edge, position, described hole.
5. spelling edge technique according to claim 1, is characterized in that: described S4 step is inserted parison formation chamber (3) by mould, the middle perfusion gypsum to described parison formation chamber (3), more described wax-pattern (1``) is melted, thereby make described parison (4).
6. broken brill is spelled an aid for edge technique, comprises a wax-pattern (1), a parison formation chamber (3) and a parison (4), and described wax-pattern (1) is the jewellery die of not spelling the broken brill of edge; Accommodating described wax-pattern (1) in described parison formation chamber (3), and be provided with at least one conduit (5), described conduit (5) contacts described wax-pattern (1); Described parison (4) is made by the described parison formation chamber (3) that is equipped with described wax-pattern (1), it is characterized in that: also include an adhered layer; Described adhered layer covers described wax-pattern (1) surface that is fixed with broken brill, and with the broken viscous force that is drilled with.
7. aid according to claim 6, is characterized in that: described parison (4) is gypsum parison.
8. aid according to claim 6, is characterized in that: described adhered layer adopts an adhesive band (2).
9. aid according to claim 6, is characterized in that: described adhered layer adopts hard adhered layer.