CN102912399B - One changes into production line Cathode plate structure - Google Patents
One changes into production line Cathode plate structure Download PDFInfo
- Publication number
- CN102912399B CN102912399B CN201210452660.4A CN201210452660A CN102912399B CN 102912399 B CN102912399 B CN 102912399B CN 201210452660 A CN201210452660 A CN 201210452660A CN 102912399 B CN102912399 B CN 102912399B
- Authority
- CN
- China
- Prior art keywords
- cathode plate
- plate body
- changing
- plate structure
- liquid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a kind of Cathode plate structure, especially relate to one and change into production line Cathode plate structure, belong to the production unit technical field of the sub-product of Japanese TV play.Thering is provided a kind of is changing in raw process, can make in electrolyzer change into that liquid carries out even convective change into production line Cathode plate structure.Described Cathode plate structure comprises cathode plate body, described cathode plate body plane is furnished with at least three changing into of being parallel to each other uniformly and produces liquid convective tank.
Description
Technical field
The present invention relates to a kind of Cathode plate structure, especially relate to one and change into production line Cathode plate structure, belong to the production unit technical field of electronic product.
Background technology
Electrical condenser is one of primary clustering in electronic circuit, has the function of filtering, rectification, coupling and high speed discharge and recharge, and have volume little, store the large characteristic of electricity.And electrode aluminium foil is the critical material manufacturing aluminium electrolutic capacitor.The quality of electrode aluminium foil quality directly determines the quality of aluminium electrolutic capacitor.This just changes into the production process of producing aluminium foil to high pressure and proposes high requirement, particularly requires higher to the magnitude of voltage of the production voltage changing into production line.And described change into production magnitude of voltage, be again produce after applying positive voltage and negative voltage respectively to the electrode aluminium foil changed in production process and cathode plate.In prior art, because described cathode plate is made up of one block of overall stainless steel, and in order to make the surface of electrode aluminium foil both sides changing in electrolyzer produce in liquid and can well change into, so the both sides entering the electrode aluminium foil of electrolyzer at each section arrange the described cathode plate be made up of one block of overall stainless steel respectively.Like this, changing in production process, just convection current can only can be carried out by the space of groove inner cathode pole plate both end sides owing to changing into production liquid, and cause change into produce liquor strength uneven, change into production fluid temperature uneven, even occur that local liquid level thermal value is comparatively large, groove temperature is difficult to control, and occurs the phenomenon of quick-fried temperature time serious.Owing to changing into the ununiformity of producing liquor strength, temperature, the instability of the electrical property the causing formed aluminum foil horizontal and vertical such as performance such as withstand voltage, specific volume.
Summary of the invention
Technical problem to be solved by this invention is: provide a kind of and changing in raw process, can make in electrolyzer change into that liquid carries out even convective change into production line Cathode plate structure.
: one changes into production line Cathode plate structure, comprises cathode plate body in described cathode plate body plane, be furnished with at least three changing into of being parallel to each other uniformly produce liquid convective tank for solving the problems of the technologies described above adopted technical scheme.
Further, described cathode plate body is made up of installing frame and the grizzly bar be arranged on uniformly on described installing frame, and the described production liquid convective tank that respectively changes into is made up of the gap between two pieces grizzly bar of leading mutually be arranged on installing frame.
Further, described each grizzly bar is arranged in shutter on installing frame.
Further, it is horizontally disposed on described cathode plate that described each bar changes into production liquid convective tank, and arrange whole cathode plate body plane from top to bottom.
The invention has the beneficial effects as follows: arrange that many changing into of being parallel to each other produce liquid convective tank by uniform in the plane of cathode plate body, and then the cathode plate body of described structure is installed to the both sides that each section enters the electrode aluminium foil in electrolyzer, the electrification one-tenth production that works of going forward side by side.Liquid convective tank is produced owing to being furnished with on the surface in cathode plate body to change into, like this, when there is concentration and temperature variation changing into production liquid and being subject to galvanic action, not only can carry out convection current by the both end sides of electrode aluminium foil, liquid convective tank can also be produced by described changing into fast and carry out convection current, thus effectively ensure that in production process, changing in electrolyzer produces the even, stable of the concentration of liquid and temperature, there will not be local liquid level thermal value larger, difficult control of temperature in groove, the phenomenon of even quick-fried temperature.And then effectively solve the difficult problem changing into horizontal, longitudinal electrical property inequality of producing the finished electrode aluminium foil brought in aluminium foil process.
Accompanying drawing explanation
Fig. 1 is a kind of front view changing into production line Cathode plate structure of the present invention;
Fig. 2 is sectional view;
Fig. 3 is the layout schematic diagram in electrolyzer of Cathode plate structure of the present invention.
Be labeled as in figure: cathode plate body 1, change into and produce liquid convective tank 2, installing frame 3, grizzly bar 4, electrolyzer 5, electrode aluminium foil 6, change into and produce liquid 7.
Embodiment
As shown in Figure 1, Figure 2 and be that one provided by the invention is changing in raw process shown in figure, can make in electrolyzer change into that liquid carries out even convective change into production line Cathode plate structure.Described cathode plate comprises cathode plate body 1, described cathode plate body 1 plane is furnished with at least three changing into of being parallel to each other uniformly and produces liquid convective tank 2.Arrange that many changing into of being parallel to each other produce liquid convective tank 2 above by uniform in the plane of cathode plate body 1, and then the cathode plate body 1 of described structure is installed to the both sides that each section enters the electrode aluminium foil 6 in electrolyzer 5, the electrification one-tenth production that works of going forward side by side.Liquid convective tank 2 is produced owing to being furnished with on the surface in cathode plate body 1 to change into, like this, when there is concentration and temperature variation changing into production liquid 7 and being subject to galvanic action, not only can carry out convection current by the both end sides of electrode aluminium foil 6, liquid convective tank 2 can also be produced by described changing into fast and carry out convection current, thus effectively ensure that in production process, changing in electrolyzer produces the even, stable of the concentration of liquid 7 and temperature, there will not be local liquid level thermal value larger, difficult control of temperature in groove, the phenomenon of even quick-fried temperature.And then effectively solve the difficult problem changing into horizontal, longitudinal electrical property inequality of producing the finished electrode aluminium foil 6 brought in aluminium foil process.
Changing in the cathode plate body 1 in above-mentioned embodiment produces liquid convective tank 2, can adopt existing cathode plate carry out jet-bedding be transformed into have described in change into the cathode plate body 1 of producing liquid convective tank 2; Also structure disclosed in the present application can be adopted, namely described cathode plate body 1 is made up of installing frame 3 and the grizzly bar 4 be arranged on uniformly on described installing frame 3, described in change into and produce liquid convective tank 2 and be made up of the gap between two pieces grizzly bar 4 of leading mutually be arranged on installing frame 3.But no matter be which kind of structure, vertical uplift after all heating up owing to changing into production liquid 7, and the thickness of cathode plate body 1 is too thin, and be unfavorable for the formation changing into the convection current of producing liquid 7.In order to make cathode plate body 1 produce promoter action to the formation changing into the convection current of producing liquid 7 after heating up, improving to change into and producing the convection effects of liquid 7, the invention become by described each grizzly bar 4 being arranged on installing frame 3 in shutter.Like this, the convection effects changing into and produce liquid 7 can just effectively be improved.Meanwhile, make described each bar change into production liquid convective tank 2 horizontally disposed in described cathode plate body 1, and arrange full whole cathode plate body 1 plane from top to bottom.Like this, just can make to greatest extent to change into and produce after liquid 7 heats up in electrolyzer 6, carry out effective convection current, ensure the homogeneity and the stability that change into production liquid 7 concentration and temperature, and then ensure to change into horizontal, the longitudinal electrical property producing the finished electrode aluminium foil that aluminium foil is produced.
Claims (2)
1. one kind changes into production line Cathode plate structure, comprise cathode plate body (1), described cathode plate body (1) plane is furnished with at least three changing into of being parallel to each other uniformly and produces liquid convective tank (2), it is characterized in that: described cathode plate body (1) is made up of installing frame (3) and the grizzly bar (4) be arranged on uniformly on described installing frame (3), described change into produce liquid convective tank (2) be made up of the gap between the adjacent two pieces grizzly bar (4) be arranged on installing frame (3), described each grizzly bar (4) is upper at installing frame (3) is that shutter is arranged.
2. one according to claim 1 changes into production line Cathode plate structure, it is characterized in that: it is upper horizontally disposed in described cathode plate body (1) that described each bar changes into production liquid convective tank (2), and arrange full whole cathode plate body (1) plane from top to bottom.