CN102911651A - Oil field compound type anti-scale corrosion inhibitor and preparation method thereof - Google Patents
Oil field compound type anti-scale corrosion inhibitor and preparation method thereof Download PDFInfo
- Publication number
- CN102911651A CN102911651A CN2012104457229A CN201210445722A CN102911651A CN 102911651 A CN102911651 A CN 102911651A CN 2012104457229 A CN2012104457229 A CN 2012104457229A CN 201210445722 A CN201210445722 A CN 201210445722A CN 102911651 A CN102911651 A CN 102911651A
- Authority
- CN
- China
- Prior art keywords
- corrosion inhibitor
- oil field
- type anti
- preparation
- compositional type
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to an oil field compound type anti-scale corrosion inhibitor and a preparation method thereof, belonging to the technical field of corrosion inhibitor. The oil field compound type anti-scale corrosion inhibitor is characterized by comprising the components by mass percent: 5-10% of sodium molybdate, 10-20% of sodium phosphate, 0.5-1% of acrylic acid-2-acrylamido-2-methyl propane sulfonic acid (AA-AMPS) copolymer, 1-2% of amino trimethylene phosphonic acid and 1-2% of hydroxyl ethylidene diphosphonic acid (HEDP). The preparation method comprises the steps of: firstly, completely dissolving sodium molybdate and sodium phosphate by using water; then, adding the AA-AMPS copolymer under the condition of stirring until the copolymer is completely dissolved; subsequently, adding ATMP and the HEDP, and further stirring for dissolving; and finally, adding water until the concentration of the mixed solution is in accordance with the requirement, so as to obtain the oil field compound type anti-scale corrosion inhibitor. The inhibitor disclosed by the invention has the advantages of simple components, available raw materials, simple technology, high efficiency, low cost, low dosage, good scale inhibition, descaling and corrosion inhibition effects and the like, and is convenient to prepare, rapid.
Description
Technical field
The invention belongs to the inhibiter technical field, particularly relate to a kind of oil field Compositional type anti-incrustation corrosion inhibitor and preparation method thereof.
Background technology
At present, corrosion refers to destruction or the denaturalization phenomenon that material causes under the effect of its surrounding environment medium.Industrial gas oil is subjected to corrosion harmfulness the most serious.Oil-gas field is distributed in saline and alkaline marshy terrain and ocean mostly, in having, strong, even strong especially corrodibility, very serious to various pipes, corrosion buried, maritime facilities, add most oil-gas fields and entered middle and high Water-cut Period, the water ratio of Produced Liquid is generally more than 70%~90%, and very serious to the corrosion of all kinds of facilities, erosion rate is up to 1.5~3mm/a.According to the Zhongyuan Oil Field report analysis, the annual Direct Loss that cause to the Zhongyuan Oil Field of corrosion are very large, and wherein replacing and the aboveground facility maintenance cost of the down-hole facilities such as oil pipe, sucker rod, pump are very high, in addition, also have loss and the technical problems such as stopping production and loss of life and personal injury.
Summary of the invention
The present invention provides a kind of oil field Compositional type anti-incrustation corrosion inhibitor and preparation method thereof for solving the technical problem that exists in the known technology.
The oil field Compositional type anti-incrustation corrosion inhibitor of the characteristics such as one of purpose of the present invention provides that a kind of to have a component simple, and raw material is easy to get, and preparation is convenient, with low cost, and scale inhibition, scale removal, corrosion mitigating effect are good.
Oil field of the present invention is to solve the technical scheme that the technical problem that exists in the known technology takes to be with the Compositional type anti-incrustation corrosion inhibitor:
A kind of oil field Compositional type anti-incrustation corrosion inhibitor is characterized in: the oil field with the composition of Compositional type anti-incrustation corrosion inhibitor is, the mass percent that the aqueous solution contains each component is,
Following technical scheme can also be adopted with the Compositional type anti-incrustation corrosion inhibitor in oil field of the present invention:
Described oil field Compositional type anti-incrustation corrosion inhibitor is characterized in: AAAMPS is the multipolymer of vinylformic acid-2-acrylamide-2-methylpro panesulfonic acid, and molecular formula is as follows:
The oil field of the characteristics such as two of purpose of the present invention provides that a kind of to have technique simple, and preparation is convenient, and is rapidly and efficiently with low cost, and production efficiency is high, and scale inhibition, scale removal, corrosion mitigating effect the are good preparation method of Compositional type anti-incrustation corrosion inhibitor.
Oil field of the present invention is to solve the technical scheme that the technical problem that exists in the known technology takes to be with the preparation method of Compositional type anti-incrustation corrosion inhibitor:
A kind of oil field preparation method of Compositional type anti-incrustation corrosion inhibitor, it is characterized in that: at first, water dissolves Sodium orthomolybdate and sodium phosphate fully, then, under agitation condition, add the AA-AMPS multipolymer, after dissolving fully, add again ATMP and HEDP, continue stirring and dissolving, add water to desired concn, obtain oil field Compositional type anti-incrustation corrosion inhibitor.
Following technical scheme can also be adopted with the preparation method of Compositional type anti-incrustation corrosion inhibitor in oil field of the present invention:
Described oil field is characterized in Compositional type anti-incrustation corrosion inhibitor and preparation method thereof: when water dissolves Sodium orthomolybdate and sodium phosphate fully, adopt 25-85 ℃ hot water.
Advantage and positively effect that the present invention has are:
The oil field owing to adopted the brand-new technical scheme of the present invention, compared with prior art, has following characteristics with Compositional type anti-incrustation corrosion inhibitor and preparation method thereof:
1, the scope of application is extensive, and pH value scope is 5.1~9.2, and temperature range is 25~85 ℃, and each component has good synergy, has good scale inhibitor effect, and slowly-releasing efficient reaches 97.56%.
2, the used inhibiter consumption of the present invention is few, and cost is low, and prescription is simple, and raw material is easy to get.
Embodiment
For further understanding summary of the invention of the present invention, Characteristic, hereby exemplify following examples and be described in detail as follows:
Present embodiment is that the simulation oil field mining liquid is to the corrosion of pipeline in experiment, and the main component that corrosion simulation liquid is joined by institute is sodium ion, magnesium ion, bicarbonate radical, calcium ion and micro-iron ion, and autoclave passes into the pH value of carbonic acid gas adjusting corrosive fluid.Adopt the static etch rate measuring method to carry out the corrosion mitigating effect evaluation.
Embodiment 1
The oil field is as follows with the quality proportioning of Compositional type anti-incrustation corrosion inhibitor each component:
The oil field is with Compositional type anti-incrustation corrosion inhibitor preparation process: at first with hot water Sodium orthomolybdate and sodium phosphate are dissolved fully, then vigorous stirring, in whipping process, add the AA-AMPS multipolymer, to adding ATMP and HEDP after the dissolving fully, continue stirring and dissolving, add water to 1000g, obtain oil field Compositional type anti-incrustation corrosion inhibitor.
Experimental temperature is 70 ℃, and inhibiting solution soaks lacing film 72h, corrosion mitigating effect such as following table:
The different adding consistency slowly-releasing of table 1 efficient
Embodiment 2
The oil field is as follows with the quality proportioning of Compositional type anti-incrustation corrosion inhibitor each component:
The oil field is with the preparation process of Compositional type anti-incrustation corrosion inhibitor, with embodiment 1.
Experimental temperature is 70 ℃, and inhibiting solution soaks lacing film 72h, corrosion mitigating effect such as following table:
The different adding consistency slowly-releasing of table 2 efficient
Embodiment 3:
The oil field is as follows with the quality proportioning of Compositional type anti-incrustation corrosion inhibitor each component:
The oil field is with the preparation process of Compositional type anti-incrustation corrosion inhibitor, with embodiment 1.
Experimental temperature is 70 ℃, and inhibiting solution soaks lacing film 72h, corrosion mitigating effect such as following table:
The different adding consistency slowly-releasing of table 3 efficient
Embodiment 4
The oil field is as follows with the quality proportioning of Compositional type anti-incrustation corrosion inhibitor each component:
The oil field is with the preparation process of Compositional type anti-incrustation corrosion inhibitor, with embodiment 1.
Experimental temperature is 70 ℃, and inhibiting solution soaks lacing film 72h, corrosion mitigating effect such as following table:
The different adding consistency slowly-releasing of table 4 efficient
Claims (4)
3. oil field claimed in claim 1 is with the preparation method of Compositional type anti-incrustation corrosion inhibitor, it is characterized in that: at first, water dissolves Sodium orthomolybdate and sodium phosphate fully, then, under agitation condition, add the AAAMPS multipolymer, after dissolving fully, add again ATMP and HEDP, continue stirring and dissolving, add water to desired concn, obtain oil field Compositional type anti-incrustation corrosion inhibitor.
4. according to the preparation method of a kind of oil field claimed in claim 3 with the Compositional type anti-incrustation corrosion inhibitor, it is characterized in that: when water dissolves Sodium orthomolybdate and sodium phosphate fully, adopt 25-85 ℃ hot water.