CN102745973B - 一种用于超氯盐渍土中的耐腐蚀混凝土桩及其制作和施工 - Google Patents
一种用于超氯盐渍土中的耐腐蚀混凝土桩及其制作和施工 Download PDFInfo
- Publication number
- CN102745973B CN102745973B CN201210220830.6A CN201210220830A CN102745973B CN 102745973 B CN102745973 B CN 102745973B CN 201210220830 A CN201210220830 A CN 201210220830A CN 102745973 B CN102745973 B CN 102745973B
- Authority
- CN
- China
- Prior art keywords
- concrete
- pile
- saline soil
- corrosion resistant
- parts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
时间 | 3天 | 7天 | 28天 | 90天 | 180天 | 360天 |
清水中强度(MPa) | 49.5 | 37.7 | 28.7 | 21.2 | 15.6 | 13.1 |
卤水中强度(MPa) | 68.3 | 75.4 | 81.4 | 91.7 | 93.5 | 95.5 |
时间 | 28天 | 90天 | 180天 | 360天 | 540天 | 720天 |
普通混凝土桩在盐渍土中强度(MPa) | 29.2 | 29.0 | 27.3 | 25.2 | 22.1 | 18.3 |
本发明混凝土桩在盐渍土中度(MPa) | 28.6 | 29.0 | 29.3 | 29.8 | 30.1 | 30.3 |
Claims (9)