CN102637483A - Softening enamelling device of copper enamelled wires - Google Patents

Softening enamelling device of copper enamelled wires Download PDF

Info

Publication number
CN102637483A
CN102637483A CN2012100656435A CN201210065643A CN102637483A CN 102637483 A CN102637483 A CN 102637483A CN 2012100656435 A CN2012100656435 A CN 2012100656435A CN 201210065643 A CN201210065643 A CN 201210065643A CN 102637483 A CN102637483 A CN 102637483A
Authority
CN
China
Prior art keywords
wire
copper
tank
tube
conduit
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012100656435A
Other languages
Chinese (zh)
Inventor
鲍征
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI LEESOV INDUSTRY Co Ltd
Original Assignee
ANHUI LEESOV INDUSTRY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI LEESOV INDUSTRY Co Ltd filed Critical ANHUI LEESOV INDUSTRY Co Ltd
Priority to CN2012100656435A priority Critical patent/CN102637483A/en
Publication of CN102637483A publication Critical patent/CN102637483A/en
Pending legal-status Critical Current

Abstract

The invention discloses a softening enamelling device of copper enamelled wires. The device comprises annealing chambers, wherein wire inlet holes are arranged at the wire inlet ends of the annealing chambers and copper wires enter the annealing chambers from the wire inlet holes. The device is characterized in that a plurality of parallel wire conduits are arranged at the wire outlet ends of the annealing chambers; the copper wires pass out of the wire conduits; the wire conduits incline downwards; a water tank is arranged in front of the wire conduits; a steam pipe is arranged above one end of the water tank; the lower ends of the wire conduits extend into the water tank; steam enters the annealing chambers; the bare copper wires passing out of the wire conduits enter wire outlet pipes via wire wheels in the water tank; enamelling and drying devices are arranged behind the annealing chambers; and the copper wires enter the enamelling and drying devices via the wire outlet pipes. The device has the following advantages that the structure is improved ingeniously and simply, the high temperature steam is utilized to heat the passing bare copper wires and the temperature is uniform, so that the copper wires are softened uniformly and bubbles are greatly reduced after the copper wire surfaces are enamelled, thus ensuring the quality of the copper enamelled wires.

Description

The copper enamelled wire softens painting installation
Technical field
The present invention relates to paint charter bare copper on the processing device is primarily a copper enameled wire paint softening devices.
Background technology
Enameled copper production need to be annealed bare copper is mainly to eliminate after drawing cold hardening, annealing annealing temperature on the indoor heated conduit, the existing technology is in the room with electric heating annealing annealing furnace body because each position temperature differences can cause uneven softening bare copper wire, copper wire coated back surface blistering more, resulting in the annealing effect is reduced; and art from the annealing furnace conduit extending directly into the cooling tank cooling, so that no bare copper softening uniform was immediately cooled, undermining the overall performance of bare copper wire.
Summary of the invention
The present invention is to solve the technical problem of providing a softening enameled copper paint apparatus of simple structure improvement clever use of high temperature steam heating through the bare copper, the average temperature, such softening evenly, so that a desired bare copper softness, surface blistering after painting greatly reduced, to meet the requirements, which can guarantee the quality of enameled copper.
For solving the problems of the technologies described above, the technical scheme that the present invention adopts is:
A copper enameled wire paint softening apparatus comprising annealing chamber, the annealing chamber has a line side of the holes, to the line wire hole into the annealing chamber, characterized in that: the outlet end of the annealing chamber has a plurality of parallel wire tube, copper tube from the wire piercing, obliquely downward of the conduit, the conduit provided in front of the tank, one end of the tank above the steam tube, said steam tube communicates a plurality of branch pipes, each branch pipe and the end portions of the respective conduit Unicom, the wire at the lower end extending into the water tank; said tank with the other end bracket, a plurality of lines on a rotatably mounted wheel, said plurality of lines corresponding to the wheel and a plurality of conduits set; other side of the water tank has a support frame, the support bracket fixed to a plurality of outlet tubes, and a plurality of outlet pipes to correspond to a plurality of line wheels; the described the piercing tube from the wire through the bare copper wire wheel inside the tank into the outlet tube, annealing chamber behind a painting, drying device, from the outlet of the copper tube into the painting, drying device .
Conduit top in the said tank is provided with depression bar, and depression bar is pressed in the lower end of conduit.
In the present invention, bare copper wire from the wire through the tube, the steam enters the steam pipe to the branch tube, seal the tank role in making the steam from the branch pipe into the annealing chamber, thus making each segment of bare copper through have been The average high temperature steam to soften; piercing from the wire bare copper tube into the water bath cooling, and the line from the tank into the outlet on the wheel through the tube.From going out copper cash entering japanning, the oven dry flow process that spool comes out.
Advantage of the present invention is:
Ingeniously simple structural improvement of the invention, the use of high-temperature steam heating through the bare copper wire, temperature average, making soften uniform, painted rear surface blistering greatly reduced, to meet the requirements, which can guarantee the quality of the copper enameled wire.
Description of drawings
Fig. 1 is a structural representation of the present invention.
Embodiment
Referring to Figure 1, A copper enameled wire paint softening devices, including annealing chamber 1, the annealing chamber inlet terminal has tapped cable, copper wire into the line from the hole into the annealing chamber 1, annealing chamber outlet end with multi- a conductor tube 2, wire 3 from the wire piercing the tube, said conduit sloped down in front of the wire tube 2 has a water tank 4, the top of the tank 4, a steam pipe 5, said vapor tube 5 is in communication with a plurality of branch pipes 6, each end of the branch pipe 6 is connected with a casing 7, each of said conduit 2, respectively, in front of the respective branch pipe casing 7 Unicom, the wire into the lower end of the tube 2 to a water tank 4, the seal play role in making the steam into the annealing chamber 1; wherein the other end of the tank 4 is provided with a bracket 9, rotatably mounted on the housing 9 a plurality of wire wheels 10, said plurality of lines wheel 10 and the tube 2 corresponding to the set plurality of conductors; on the other side of the tank 4 has a support frame 11, a bracket 11 is fixed to a plurality of outlet tubes 12, a plurality of outlet tube 12 and the wheel 10 to correspond to a plurality of line ; wherein the piercing tube from the wire bare copper wire 3 tank 4 through the wire ring 10 into the outlet pipe 12, the annealing chamber behind a painting, drying device, from the outlet of said copper pipe into to painting, drying apparatus.
Conduit top in the said tank 4 is provided with depression bar 13, and depression bar 13 is pressed in the lower end of conduit 2.

Claims (2)

1 An enameled copper paint softening apparatus comprising annealing chamber, the annealing chamber has a feed line into the line side holes into the hole to the line wire annealing chamber, characterized in that: the outlet end of the annealing chamber has a plurality of parallel wire tube, copper tube from the wire piercing, obliquely downward of said conduit, said conduit in front of a tank, one end of the tank above the steam pipe, the steam pipes communicating on a plurality of branch pipes, each branch pipe and the end portions of the respective conduit Unicom, the wire at the lower end extending into the water tank; said tank with the other end bracket, rotatably mounted on a plurality of lines wheel, pulley and said plurality of tubes corresponding to the set plurality of conductors; other side of the water tank has a support frame, the support bracket fixed to a plurality of outlet tubes, a plurality of outlet tube and provided corresponding to a plurality of line wheels ; wherein the piercing tube from the wire through the bare copper wire wheel inside the tank into the outlet tube, annealing chamber behind a painting, drying device, from the outlet of the copper tube into the painting, drying Dry devices.
2. the softening painting installation of a kind of copper enamelled wire according to claim 1 is characterized in that: the conduit top in the said tank is provided with depression bar, and depression bar is pressed in the lower end of conduit.
CN2012100656435A 2012-03-13 2012-03-13 Softening enamelling device of copper enamelled wires Pending CN102637483A (en)