A kind of processing method of stone material pit hair side
Technical field
The present invention relates to the processing of stone technical field, be meant a kind of processing method of stone material pit surface specifically.
Background technology
Stone material is as a kind of construction material; The Along with people's growth in the living standard; People are also increasingly high for the requirement of stone material pattern; The stone material of simple cutting back polishing moulding can't satisfy people's aesthstic desire demand, and therefore having occurred some in the market has the combination with decorative surfaces of nature pit, the stone material with high aesthetic values.
Existing processing method with pit hair side stone material generally has following several method: one, thermal-flame torch firing, often be subject to the thickness of stone material, and its baked wheaten cake speed is fast; Surface sense naturally is strong; But this method is hardening cracked stone material because its application technology is not mature enough easily, and waste product is many; Waste stone material raw material has increased production cost; Two, water under high pressure dashes, and this method need be wasted great amount of water resources and electric energy, and its production cost is higher; Three, wheel load, this method production efficiency is not high, and stone material thickness is also had certain requirement, and its product aesthetic feeling of producing is not good, and waste product is more; Four, manual pounding cut, and production efficiency is extremely low, poor product quality, and waste product is many etc.
To sum up, to the defective that existing stone material pit hair side processing method exists, the processing method of the measured stone material pit of the matter hair side of a kind of production efficiency height and product is provided at present.
Summary of the invention
The present invention provides a kind of processing method of stone material pit hair side, and its main purpose is to overcome the shortcoming that there is above-mentioned deficiency in existing stone material pit hair side processing method.
The present invention adopts following technical scheme:
A kind of processing method of stone material pit hair side, process according to following steps:
A, on the processing of stone face, spray with an amount of conducting liquid;
B, treat that conducting liquid penetrates into processing of stone face appropriate depth after, rapidly its machined surface is carried out discharge process with the high-tension electricity that has spray point, burst apart in its machined surface part, form a plurality of pit hair sides;
C, the base mud on above-mentioned pit hair side flushing removed promptly form semi-finished product stone material face brick;
D, semi-finished product stone material face brick is repaired in various degree got product at last.
Above-mentioned high-tension electricity voltage is between 1KV~10KV.
Said spray point is two, and wherein one connects the high-tension electricity positive pole, and another root connects negative pole.
As a kind of preferred embodiment, any one of said spray point is fixed on the processing of stone face, and another root is located at the top of processing of stone face upper surface.
As another kind of preferred embodiment, said two spray point in the vertical directions become " V " shape, leave the gap between the termination, lower end of these two spray points.
Above-mentioned stone material to be processed is fixed on the work top; Spray point and the stone material of above-mentioned processing of stone face top do relative motion according to required processing graphic pattern shape, the distance of above-mentioned spray point through adjusting voltage and spray point and processing of stone face to processing of stone face discharge process to form the pit hair side of required size.
Further, the relative distance of the minimum of when discharge of the spray point on the above-mentioned processing of stone face and said processing of stone face is between 0.1mm~3mm.
Again further, above-mentioned spray point can be provided with one or more groups, and spray point can discharge as required continuously or intermittently.
Can know by the above-mentioned description of this invention, the invention has the advantages that: the processing method of this stone material pit hair side, adopt electrion to make the local hair side formation pit that bursts apart fast; Energy utilization rate is high, when having improved production efficiency, has reduced production cost; Spray point can be selected voltage swing, intermittence or continuity discharge as required, can arbitrarily process the arbitrary graphic pattern shape, because of this method need not stone material is exerted pressure; So the stone material pit hair side that this law is produced does not receive thickness limits; Quality is high, and percent defective is low, can produce good economic benefit.
The specific embodiment
The specific embodiment of the present invention is described with reference to the accompanying drawings.
A kind of processing method of stone material pit surface, process according to following steps:
(1) on the processing of stone face, sprays with an amount of conducting liquid;
(2) treat that conducting liquid penetrates into processing of stone face appropriate depth after, rapidly its machined surface is carried out discharge process with the high-tension electricity that has spray point, burst apart in its machined surface part, form a plurality of pit hair sides;
(3) flushing of the base mud on above-mentioned pit hair side removing is promptly formed semi-finished product stone material face brick;
(4) semi-finished product stone material face brick is repaired in various degree got product at last.
Above-mentioned high-tension electricity voltage is between 1KV~100KV; Above-mentioned spray point is two; Above-mentioned spray point can be provided with one or more groups; Spray point can be as required continuously or intermittently discharge, during the spray point discharge of processing of stone face top and the relative distance of the minimum of said processing of stone face upper surface be between 0.1mm~3mm.
Embodiment one
In the above-mentioned steps (2); As a kind of preferred version; Any one of said spray point is fixed on the processing of stone face, and another root is located at the top of processing of stone face upper surface, and stone material to be processed is fixed on the work top; Spray point and the processing of stone face of above-mentioned processing of stone face top do relative motion according to required processing graphic pattern shape, the distance of spray point through adjusting voltage and spray point and processing of stone face to processing of stone face discharge process to form the pit hair side of required size.
Embodiment two
In the above-mentioned steps (2); As another kind of preferred version; Above-mentioned two spray point in the vertical directions become " V " shape; Leave suitable gap (the discharge of stone material face brick being formed the pit hair side for suitable) between the termination, lower end of these two spray points; The spray point and the processing of stone face of two one-tenth " V " font do relative motion according to required processing graphic pattern shape, the distance of spray point through adjustment voltage and spray point and processing of stone face to stone material face brick machined surface discharge process to form the pit hair side of required size.
The processing method of this stone material pit hair side adopts electrion to make the partial operation face formation pit that bursts apart fast, and energy utilization rate is high; When having improved production efficiency, reduced production cost, spray point can be selected voltage swing, intermittence or continuity discharge as required; Can arbitrarily process the arbitrary graphic pattern shape, because of this method need not stone material is exerted pressure, so the stone material pit hair side that this law is produced does not receive thickness limits; Quality is high, and percent defective is low, can produce good economic benefit.
Above-mentionedly be merely the specific embodiment of the present invention, but design concept of the present invention is not limited thereto, allly utilizes this design that the present invention is carried out the change of unsubstantiality, all should belong to the behavior of invading protection domain of the present invention.