CN102418029A - 高强度气缸套材料及铸造工艺 - Google Patents

高强度气缸套材料及铸造工艺 Download PDF

Info

Publication number
CN102418029A
CN102418029A CN2010102946147A CN201010294614A CN102418029A CN 102418029 A CN102418029 A CN 102418029A CN 2010102946147 A CN2010102946147 A CN 2010102946147A CN 201010294614 A CN201010294614 A CN 201010294614A CN 102418029 A CN102418029 A CN 102418029A
Authority
CN
China
Prior art keywords
cylinder sleeve
casting process
sleeve material
strength cylinder
casting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010102946147A
Other languages
English (en)
Inventor
贾维珍
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010102946147A priority Critical patent/CN102418029A/zh
Publication of CN102418029A publication Critical patent/CN102418029A/zh
Pending legal-status Critical Current

Abstract

高强度气缸套材料及铸造工艺所采用的技术方案是,通过对气缸套化学成分中Cu含量的增加至1.7%,以Cu代替部分的Ni和Mo合金高温熔炼,实现铸态贝氏体的形成,满足气缸套较高机械性能的要求。

Description

高强度气缸套材料及铸造工艺
所属技术领域
本发明涉及高强度气缸套铸造成形生产工艺。
背景技术
随着整个社会对环境保护的重视,发动机向大功率小体积发展,对汽车发动机的重要零部件气缸套要求越来越高,普通的低合金气缸套金相和理化指标都不能满足使用要求,而贝氏体组织的气缸套的金相组织和机械性能均能满足高强度的要求,但是为了在铸造过程中获得贝氏体组织,在熔炼过程中需要加入Ni、Mo等贵重合金元素,原材料的成本很大。
发明内容
为了提高汽车气缸套的机械性能和减低铸造成本,本发明提供一种高强度气缸套铸造成形。
本发明解决其技术问题所采用的技术方案是,通过对气缸套化学成分中Cu的含量的增加至1.7%,以Cu代替部分的Ni和Mo,同时以一合理的浇铸工艺,实现高强度气缸套铸造成形。
本发明的有益效果是,在铸造过程中能产生贝氏体基体组织,石墨形态好,满足了气缸套机械性能的提升需求,减少了原材料的成本,缩短了气缸套的生产周期,减少了热处理获得贝氏体造成的环境二次污染。
附图说明
无附图。
具体实施方式
用中频电炉按如下的化学成分配料(%):C:2.8-3.0,Si:1.8-2.2,Mn:0.4-0.6,P<0.1,S<0.1,Cu:1.7,Mo:0.7,Ni:0.2,其余为Fe。将缓慢升温至1400℃左右,取样化验,化学成分调整合格后,将电炉内铁水的温度迅速升温至1570-1600℃,开始常规孕育,孕育结束后,保证在浇铸坩埚内的温度在1440-1460℃的范围内进行浇铸,在浇铸模具的温度冷却至1150℃左右,实施水冷却,至浇铸毛坯的温度在700℃停止冷却,毛坯出模。

Claims (1)

1.高强度气缸套材料及铸造工艺其特征是:在熔炼过程中,C:2.8-3.0,Si:1.8-2.2,Mn:0.4-0.6,P<0.1,S<0.1,Cu:1.7,Mo:0.7,Ni:0.2,其余为Fe。Cu的含量的增加至1.7%。
CN2010102946147A 2010-09-27 2010-09-27 高强度气缸套材料及铸造工艺 Pending CN102418029A (zh)