CN102371729A - 仿铝复合膜 - Google Patents
仿铝复合膜 Download PDFInfo
- Publication number
- CN102371729A CN102371729A CN2011103657878A CN201110365787A CN102371729A CN 102371729 A CN102371729 A CN 102371729A CN 2011103657878 A CN2011103657878 A CN 2011103657878A CN 201110365787 A CN201110365787 A CN 201110365787A CN 102371729 A CN102371729 A CN 102371729A
- Authority
- CN
- China
- Prior art keywords
- layer
- pet
- composite membrane
- membrane
- aluminum composite
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种仿铝复合膜,包括PET膜层、粘合剂层、铝箔层、PVC膜层;其特征在于:所述的PET膜层和PVC膜层通过粘合剂层(4)粘结于铝箔层的两侧;本发明另外一种方案,用PET膜层,取代PVC膜层。本发明仿铝复合膜,完整的保留了铝金属材料的金属光泽和质感,同时由于铝箔层位于PET膜层和PVC/PET膜层之间,因此,能够完全隔绝氧气,防止氧化,达到长久保持铝箔原有金属光泽的效果;并可进一步复合于冷轧薄板、铝板、镀锌板、建筑材料表面,起装饰保护和美观的作用,工艺简单、操作简便、成本低。
Description
技术领域
本发明涉及一种复合膜,尤其涉及一种仿铝复合膜。
背景技术
目前技术中,金属板特别是钢板、铝材在工业和生活中的应用越来越广泛,汽车、冰箱、洗衣机、厨房设备、工业和民用建筑都需要使用。一般的钢板在使用过程中,金属板容易氧化、易腐蚀,因此 ,需要先进行防腐防锈处理,比如喷涂油漆,但是防锈防腐能力不强,且油漆容易刮伤和脱落,致使金属板的寿命降低,而且还严重影响了金属板的外观。
近年来在家电行业中逐渐兴起了在金属板的表面设有覆膜,起到防护作用,然而遗憾的是在获得更多色彩和图案的同时也遮盖了金属光泽,失去了金属原有的质感。
发明内容
本发明所要解决的技术问题是:提供一种由PET、真空镀铝膜层和PVC组成的仿铝复合膜,能够完全保留铝箔金属材料特有的光泽和质感,还可以在PET内表面制作多种色彩和图案,使产品的装饰效果更加丰富。
为解决上述技术问题,本发明的技术方案是:仿铝复合膜,包括PET膜层、粘合剂层、铝箔层和PVC膜层;其特征在于:所述的PET膜层和PVC膜层通过粘合剂层粘结于铝箔层的两侧。
作为优先方案,所述PET膜层内侧还设有印花层,印花层的增设可以根据客户需求进行各种图案或防伪商标的印刷,使产品更具色彩层次感和装饰效果。
所述PET膜层外表面还设有UV保护膜层,对内部结构起到保护作用的同时,还有一定的防指纹效果,可以有效减少使用后的养护。
另一种技术方案:仿铝复合膜,包括两层PET膜层,粘合剂层和铝箔层,其特征在于:所述的两层PET膜层通过粘合剂层粘结于铝箔层的两侧。
作为优先方案,所述其中一层PET膜层内侧还设有印花层,印花层的增设可以根据客户需求进行各种图案或防伪商标的印刷,使产品更具色彩层次感和装饰效果。
所述内侧设有印花层的PET膜层外表面还设有UV保护膜层,对内部结构起到保护作用的同时,还有一定的防指纹效果,可以有效减少使用后的养护。
用PET膜层取代PVC膜层,可以提高仿铝复合膜的表面强度和硬度。
其中,仿铝复合膜中各层的厚度可以根据客户的不同需求进行随意组合。
采用了上述技术方案后,本发明的效果是:
1)本发明仿铝复合膜,由于铝箔层位于PET膜和PVC膜之间,完整的保留了铝箔金属材料的光泽和质感的同时,PET和PVC/PET膜层能够隔绝氧气,防止氧化,防腐蚀,达到长久保持铝箔原有金属光泽的效果;
2)本发明的仿铝复合膜,可进一步复合于冷轧薄板、铝板、镀锌板、建筑材料表面,起装饰保护和美观的作用,工艺简单、操作简便、成本低。
3)由于PET内表面设有印花层,因此,该复合膜可以根据客户需求设计各种图案和色彩,使产品种类增多,产品档次提高。
附图说明
下面结合附图和实施例对本发明进一步说明。
图1,本发明实施例的局部结构剖视图;
附图中,1.UV保护膜层,2. PET膜层,3. 印花层,4. 粘合剂层,5. 铝箔层, 6.PVC膜层。
具体实施方式
下面通过具体实施例对本发明作进一步的详细描述。
一种仿铝复合膜,如图1所示,包括UV保护膜层1, PET膜层2, 印花层3,粘合剂层4,铝箔层5, PVC膜层6;
具体而言,仿铝复合膜,所述PET膜层2和PVC膜层6通过粘合剂层4粘结于铝箔层5的两侧。为增加装饰效果,在PET膜层2内表面设有印花层3(印花层3图案为透明或镂空);所述PET膜层2外表面还设有UV保护膜层1。
本发明可广泛应用于汽车、冰箱、洗衣机、厨房设备、工业和民用建筑等领域,保留铝金属光泽和质感的同时,贴附物起到很好的防锈、防腐、保护和装饰美观作用;同时由于印花层的加入,大大增加了产品的观赏装饰性。
以上所述实施例仅是对本发明的优选实施方式的描述,不作为对本发明范围的限定,在不脱离本发明设计精神的基础上,对本发明技术方案作出的各种变形和改造,均应落入本发明的权利要求书确定的保护范围内。
Claims (6)
1.仿铝复合膜,包括PET膜层(2)、粘合剂层(4)、铝箔层(5)和PVC膜层(6);其特征在于:所述的PET膜层(2)和PVC膜层(6)通过粘合剂层(4)粘结于铝箔层(5)的两侧。
2.如权利要求1所述的仿铝复合膜,其特征在于:所述PET膜层(2)内侧还设有印花层(3)。
3.如权利要求1或2所述的仿铝复合膜,其特征在于,所述PET膜层(2)外表面还设有UV保护膜层(1)。
4.仿铝复合膜,包括两层PET膜层(2),粘合剂层(4)和铝箔层(5),其特征在于:所述的两层PET膜层(2)通过粘合剂层(4)粘结于铝箔层(5)的两侧。
5.如权利要求4所述的仿铝复合膜,其特征在于:所述其中一层PET膜层(2)内侧还设有印花层(3)。
6.如权利要求4或5所述的仿铝复合膜,其特征在于:所述内侧设有印花层(3)的PET膜层(2)外侧还设有UV保护膜层(1)。