CN102294805A - Anti-wiredrawing and quick-break-proof device for die dispensing points - Google Patents
Anti-wiredrawing and quick-break-proof device for die dispensing points Download PDFInfo
- Publication number
- CN102294805A CN102294805A CN 201110229989 CN201110229989A CN102294805A CN 102294805 A CN102294805 A CN 102294805A CN 201110229989 CN201110229989 CN 201110229989 CN 201110229989 A CN201110229989 A CN 201110229989A CN 102294805 A CN102294805 A CN 102294805A
- Authority
- CN
- China
- Prior art keywords
- air blowing
- cooling
- mould
- die
- blowing piece
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention belongs to the technical field of plastic die, and especially relates to an anti-wiredrawing and quick-break-proof device for die dispensing points. The device provided by the invention comprises a cooling insert block 3 near a heat spout 2, wherein the cooling insert block 3 is provided with two anti-wiredrawing and quick-break-proof technical schemes: the first one is characterized in that the cooling insert block 3 is equipped with an air blowing block 1or is connected with the air blowing block 1, one end of which communicates with an air inlet pipe 5 inside the die, and the air blowing direction of a blow hole 8 is corresponding to an outlet of the heat spout 2; the second one is characterized in that a water conveying pipe 7 is disposed inside the cooling insert block 3, one end of the water conveying pipe 7 communicates with an inlet pipe 6 inside the die, the other end of the water conveying pipe 7 communicates with an outlet pipe 4 inside the die, and the water conveying pipe 7 is arranged near the outlet of the heat spout 2. The two technical schemes are preferably combined. According to the invention, cooling water flows inside the water conveying pipe to rapidly lower the temperature of the heat spout, and compressed air again blows air to cool a cast gate and breaks wire drawing in initial stage. Therefore, the wiredrawing phenomenon can be completely avoided by the dual functions.
Description
Technical field
The invention belongs to the plastic moulds technology field, relate to a kind of in injection moulding is produced because of the insufficient solution that the wire drawing phenomenon occurs of cast gate place cooling, particularly a kind of mould advances glue point and prevents the wire drawing quick-break device.
Background technology
In hot flow path was produced, higher because of near the temperature the hot mouth, Ru Rezui can not get sufficient cooling.The stock coagulation time at hot mouth place is longer, and when mould was opened, the sizing material at hot mouth place did not also solidify fully, will produce the phenomenon of plastic cement wire drawing, was exactly after hot flow path is pulled out die cavity, also had fine collodion silk and cast gate and connected together.If this collodion silk is bonded on the mould, precision and mould itself that will mold damage when the mould matched moulds; As be bonded at again on a collection of product, will influence the outward appearance of product, particularly for the plastic member product of high precision, if glued collodion silk on the plastic, this a collection of product just will be as waste disposal, therefore, resolve the phenomenon of wire drawing, not only can improve the quality and the service life of mould, also can improve the quality and the production efficiency of product, reduce percent defective, thereby reach energy-saving and cost-reducing.Prior art can only go to remove to the generation of this phenomenon or the control injection temperature by hand, and the former obviously can influence production efficiency of products, and there is certain limitation in the latter to the injection mo(u)lding of product.
Summary of the invention
At problems of the prior art, the object of the present invention is to provide a kind ofly increases cooling Yun Shui and logical compressed air is accelerated the cooling of hot mouth and blown disconnected initial stage wire drawing near hot mouth, thereby prevents that effectively mould that the phenomenon of wire drawing takes place from advancing glue point and preventing the wire drawing quick-break device.
The present invention is achieved in that it is included near the cooling that is provided with the hot mouth and inserts, and cooling is inserted and is provided with two kinds of anti-wire drawing quick-break technical schemes:
First kind is: described cooling is inserted and is provided with the air blowing piece, or is connected with the air blowing piece, and the air inlet pipe in an end of air blowing piece and the mould is communicated with, and the air blowing direction of the gas hole of air blowing piece is corresponding with the position of the outlet of hot mouth;
Second kind is: be provided with the fortune water pipe in described cooling is inserted, fortune water pipe one end is communicated with water inlet pipe in the mould, and the interior outlet pipe of the other end and mould is communicated with, and transports water pipe and is arranged near hot mouth exports.
The combination of preferably above-mentioned two kinds of technical schemes is provided with the fortune water pipe in described cooling is inserted, and described cooling is inserted and is provided with the air blowing piece, or is connected with the air blowing piece.
The gas hole of described air blowing piece cooling insert below, the air blowing direction of gas hole faces the gate portions of the product after the die sinking, the bottom face that cooling is inserted and the die face level of this mould, and another mould is provided with groove, during matched moulds, the gas hole of air blowing piece falls in the described groove.
Described cooling is inserted and is arranged on the below of hot mouth outlet, the internal drilling that the fortune water pipe is inserted for cooling, and the fortune water pipe is located near the gate portions of product.
The present invention is used for logical cooling water and cooling and inserts and increase the air blowing piece again on the limit in the cooling internal drilling of inserting, after sizing material injects mold cavity, at once to the cooling logical cooling water of inserting; Can take away a large amount of heats when cooling water flows in the fortune water pipe, thereby the temperature at hot mouth place is lowered fast, just can not form wire drawing after the die sinking.When mould was just opened, compressed air blowed to cast gate fast by the gas hole in the air blowing piece then, thereby cast gate was cooled off and blows disconnected initial stage wire drawing once more, can avoid the generation of wire drawing phenomenon fully by this double action.
Description of drawings
Fig. 1, the local main schematic diagram of looking of the embodiment of the invention 1 mould.
Fig. 2, the local schematic side view of the embodiment of the invention 1 mould.
Fig. 3, the air blowing schematic diagram when has just opened the embodiment of the invention 1 mould part.
Among the figure: air blowing piece 1, hot mouth 2, cooling inserts 3, outlet pipe 4, air inlet pipe 5, water inlet pipe 6, fortune water pipe 7, gas hole 8.
The specific embodiment
The present invention can specifically implement by the technology that illustrates in the summary of the invention, can further describe the present invention by the following examples, yet scope of the present invention is not limited to following embodiment.
Embodiment 1:
It is included near the cooling that is provided with the hot mouth 2 and inserts 3, and described cooling is inserted and is provided with fortune water pipe 7 in 3, and fortune water pipe 7 one ends are communicated with water inlet pipe 6 in the mould, and the interior outlet pipe 4 of the other end and mould is communicated with, and transports water pipe 7 and is arranged near hot mouth 2 exports.
Described cooling is inserted and 3 is provided with air blowing piece 1, or is connected with air blowing piece 1, and an end of air blowing piece 1 is communicated with air inlet pipe 5 in the mould, and the air blowing direction of the gas hole 8 of air blowing piece 1 and the outlet of hot the mouth 2 just position of product gate part are corresponding;
The gas hole 8 of described air blowing piece 1 cooling insert 3 below, the air blowing direction of gas hole 8 faces the gate portions of the product after the die sinking, cooling insert 3 the bottom face and the die face level of this mould, and another mould is provided with groove, during matched moulds, the gas hole 8 of air blowing piece 1 falls in the described groove.
Described cooling 3 belows that are arranged on 2 outlets of hot mouth of inserting, fortune water pipe 7 is insert 3 internal drilling of cooling, fortune water pipe 7 is located near the gate portions of product in the die cavity.
The quick cooling of cast gate realizes by the following method.Increase by a cooling at hot mouth 2 places and insert 3, better in order to make cooling effect, cooling insert 3 used heat-transfer effect preferably beryllium copper make.Increase cooling water hole, logical cooling water in cooling water hole at the cooling 3 upper edges hot mouth periphery of inserting.When plastic cement just injected mold cavity, at once to the cooling 3 logical cooling waters of inserting, cooling water was inserted mobile fast in 3 in cooling, thereby takes away the heat at hot mouth place, and hot mouth place sizing material is cooled off fast; When mould is just opened, give air blowing piece 1 logical pressure fast air, press fast air to blow to cast gate fast by the hole in the air blowing piece 1.Thereby once more cast gate is cooled off and, solidify fully because of cooling the glue position at cast gate place, this just can be avoided the generation of wire drawing phenomenon to solidify the back, presses fast air can blow the wire drawing of the weak point of disconnected initial stage formation again simultaneously, thereby has avoided the generation of wire drawing phenomenon fully.
Claims (4)
1. a mould advances the anti-wire drawing quick-break device of glue point, and it is included near the cooling that is provided with the hot mouth (2) and inserts (3), it is characterized in that:
Described cooling insert (3) be provided with air blowing piece (1), or be connected with air blowing piece (1), air inlet pipe (5) in one end of air blowing piece (1) and the mould is communicated with, and the air blowing direction of the gas hole (8) of air blowing piece (1) is corresponding with the position of the outlet of Re Zui (2);
Or described cooling inserts and is provided with fortune water pipe (7) in (3), and fortune water pipe (7) one ends are communicated with water inlet pipe (6) in the mould, and the interior outlet pipe (4) of the other end and mould is communicated with, and transports water pipe (7) and is arranged near hot mouth (2) exports.
2. mould according to claim 1 advances the anti-wire drawing quick-break device of glue point, it is characterized in that described cooling is inserted to be provided with fortune water pipe (7) in (3), described cooling insert (3) be provided with air blowing piece (1), or be connected with air blowing piece (1).
3. mould according to claim 2 advances the anti-wire drawing quick-break device of glue point, insert in the cooling below of (3) of the gas hole (8) that it is characterized in that described air blowing piece (1), the air blowing direction of gas hole (8) faces the gate portions of the product after the die sinking, cool off the die face level of bottom face and this mould of insert (3), another mould is provided with groove, during matched moulds, the gas hole (8) of air blowing piece (1) falls in the described groove.
4. mould according to claim 2 advances the anti-wire drawing quick-break device of glue point, it is characterized in that described cooling insert (3) be arranged on the below of hot mouth (2) outlet, fortune water pipe (7) is for cooling off the internal drilling of insert (3), and fortune water pipe (7) is located near the gate portions of product.