CN102290275A - 用于高压断路器的闸刀片及其镀银工艺 - Google Patents
用于高压断路器的闸刀片及其镀银工艺 Download PDFInfo
- Publication number
- CN102290275A CN102290275A CN201110222711XA CN201110222711A CN102290275A CN 102290275 A CN102290275 A CN 102290275A CN 201110222711X A CN201110222711X A CN 201110222711XA CN 201110222711 A CN201110222711 A CN 201110222711A CN 102290275 A CN102290275 A CN 102290275A
- Authority
- CN
- China
- Prior art keywords
- silver
- blade
- knife switch
- matrix
- plating process
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明公开了一种用于高压断路器的闸刀片,包括:基体,所述基体包括固定连接端和活动连接端,所述固定连接端和活动连接端表面有一层镀银层。本发明还公开了一种用于高压断路器的闸刀片的镀银工艺,所述镀银工艺的具体步骤包括:表面处理→镀银→剥离→抛光。本发明的用于高压断路器的闸刀片性能好、成本低,本发明的镀银工艺简单可行,镀银层与基体结合牢固,有足够的附着强度;在镀层有效范围内无漏镀现象,均镀能力好;产品镀层表面无腐蚀、无划伤、碰撞损伤、发黄、黑点等缺陷存在。
Description
技术领域
本发明涉及电力装置领域,特别是涉及一种用于高压断路器或高压隔离开关的闸刀片及其镀银工艺。
背景技术
高压断路器和隔离开关是电力系统中最重要的组件。断路器担负着控制和保护电力系统安全稳定运行的作用,所谓控制,就是对电网中的部分电力设施、线路在运行过程中发生故障或电网调度时,通过断路器等的分合将故障部分快速分离,保证部分电网正常运行。断路器在高压及有负载的条件下操作,操作过程中会产生强电弧,因而断路器经常按灭弧原理分为油断路器、压缩空气断路器、六氟化硫断路器、真空断路器、磁吹断路器和空气断路器等。也有按使用环境的电压等级来划分:如35 kV以下称为中压断路器;110 kV、220 kV称为高压断路器;330 kV及以上电压等级的称为超高压断路器。
闸刀片是断路器等高压开关的关键部件,应具有以下性能:1)大的分断电流的能力;2)高的耐压值;3)优良的抗熔焊性能;4)高的导电和导热能力;5)耐电弧烧损;6)低的截流值。
由于这些性能的相互矛盾性,对闸刀片要求也就高。目前高压真空断路器所采用的基体材料为CuW、CuBi、CuCr合金,同时会对闸刀片进行银镀膜增加导电性。
但是银作为一种贵金属材料,要对用于高压断路器的闸刀片特别是用于高压隔离开关的大型闸刀片进行整体镀银膜,成本较高。
发明内容
本发明主要解决的技术问题是提供一种用于高压断路器的闸刀片及其镀银工艺,能够兼顾闸刀片的性能和成本。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种用于高压断路器的闸刀片,包括:基体,所述基体包括固定连接端和活动连接端,所述固定连接端和活动连接端表面有一层镀银层。
在本发明一个较佳实施例中,所述镀银层厚度大于等于25.4 um。
在本发明一个较佳实施例中,所述基体为铜或铜合金材料制成。
为解决上述技术问题,本发明采用的另一个技术方案是:提供一种用于高压断路器的闸刀片的镀银工艺,所述镀银工艺的具体步骤包括:
(100)、表面处理:将所述闸刀片的基体整体浸入绝缘漆中,在基体表面形成一层绝缘膜;自干24小时后,将固定连接端和活动连接端要镀银部位进行定位剥漆,使需镀银部位的基体裸露;
(200)、镀银:对所述闸刀片的裸露部位进行镀银;
(300)、剥离:将剩余的绝缘膜剥离;
(400)、抛光:将镀银层水磨、抛光,形成光滑光亮表面。
在本发明一个较佳实施例中,所述镀银步骤中,所述电源为脉冲电源,电源频率为900~1000 Hz,通断比为10~20%,波形为方形,时间为20~40分钟。
本发明的有益效果是:本发明的用于高压断路器的闸刀片性能好、成本低,本发明的镀银工艺简单可行,镀银层与基体结合牢固,有足够的附着强度;在镀层有效范围内无漏镀现象,均镀能力好;产品镀层表面无腐蚀、无划伤、碰撞损伤、发黄、黑点等缺陷存在。
附图说明
图1是本发明用于高压断路器的闸刀片一较佳实施例的结构示意图;
图2是本发明用于高压断路器的闸刀片镀银工艺的流程示意图;
附图中各部件的标记如下:1为基体,2为固定连接端,3为活动连接端。
具体实施方式
下面结合附图对本发明的较佳实施例进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
请参阅图1,本发明实施例包括:
一种用于高压断路器的闸刀片,包括:基体1,基体1呈长条形,包括固定连接端2和活动连接端3,固定连接端和活动连接端表面有一层镀银层,为保证其最佳性能,镀银层厚度大于等于25.4 um,本实施例中,固定连接端2的镀银层长度D1要大于29 mm,活动连接端3长度D2要大于26 mm;基体1为铜或铜合金材料制成。
请参阅图2,用于高压断路器的闸刀片的镀银工艺,所述镀银工艺的具体步骤包括:
(100)、表面处理:将所述闸刀片的基体整体浸入绝缘漆中,在基体表面形成一层绝缘膜;自干24小时后,将固定连接端和活动连接端要镀银部位进行定位剥漆,使需镀银部位的基体裸露;
(200)、镀银:对所述闸刀片的裸露部位进行镀银;优选采用脉冲镀银法,电源频率为900~1000 Hz,通断比为10~20%,波形为方形,时间为20~40分钟;
(300)、剥离:将剩余的绝缘膜剥离;
(400)、抛光:将镀银层水磨、抛光,形成光滑光亮表面。
本发明的用于高压断路器的闸刀片性能好、成本低,本发明的镀银工艺简单可行,镀银层与基体结合牢固,有足够的附着强度;在镀层有效范围内无漏镀现象,均镀能力好;产品镀层表面无腐蚀、无划伤、碰撞损伤、发黄、黑点等缺陷存在。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书及附图内容所作的等效结构或等效流程变换,或直接或间接运用在其他相关的技术领域,均同理包括在本发明的专利保护范围内。
Claims (5)
1.一种用于高压断路器的闸刀片,其特征在于,包括:基体,所述基体包括固定连接端和活动连接端,所述固定连接端和活动连接端表面有一层镀银层。
2.根据权利要求1所述的用于高压断路器的闸刀片,其特征在于,所述镀银层厚度大于等于25.4um。
3.根据权利要求1所述的用于高压断路器的闸刀片,其特征在于,所述基体为铜或铜合金材料制成。
4.一种权利要求1所述的用于高压断路器的闸刀片的镀银工艺,其特征在于,所述镀银工艺的具体步骤包括:
(100)、表面处理:将所述闸刀片的基体整体浸入绝缘漆中,在基体表面形成一层绝缘膜;自干24小时后,将固定连接端和活动连接端要镀银部位进行定位剥漆,使需镀银部位的基体裸露;
(200)、镀银:对所述闸刀片的裸露部位进行镀银;
(300)、剥离:将剩余的绝缘膜剥离;
(400)、抛光:将镀银层水磨、抛光,形成光滑光亮表面。
5.根据权利要求4所述的用于高压断路器的闸刀片的镀银工艺中,其特征在于,所述镀银步骤中,所述电源为脉冲电源,电源频率为900~1000Hz,通断比为10~20%,波形为方形,时间为20~40分钟。