CN102189070A - Surface treatment method for shell - Google Patents
Surface treatment method for shell Download PDFInfo
- Publication number
- CN102189070A CN102189070A CN2010101198736A CN201010119873A CN102189070A CN 102189070 A CN102189070 A CN 102189070A CN 2010101198736 A CN2010101198736 A CN 2010101198736A CN 201010119873 A CN201010119873 A CN 201010119873A CN 102189070 A CN102189070 A CN 102189070A
- Authority
- CN
- China
- Prior art keywords
- spraying
- oil
- surface treatment
- treatment method
- oil spout
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a surface treatment method for a plastic/metal product, which is characterized by comprising the following steps of: spraying base oil on the whole external surface of the product; spraying the oil on the local external surface of the product from any side, wherein the thicknesses of oil spraying coatings are shallower, the particles of the oil spraying coatings are sparser and the oil spraying speed is higher from the beginning to the end of oil spraying, so that a two-color gradual change effect can be achieved; and spraying the oil from a position, which is needed to be subjected to three-color gradual change, of the external surface of the product, wherein the thicknesses of oil spraying coatings are shallower, the particles of the oil spraying coatings are sparser and the oil spraying speed is higher from the beginning to the end of oil spraying, and a multi-color gradual change effect can be achieved by the oil spraying method with the same step as the step 3.
Description
Technical field
The present invention relates to a kind of surface treatment method, the surface treatment method of particularly a kind of plastic cement, metallic article.
Technical background:
At present, the surface treatment of plastic shell, metal shell, all be to be coated with the last layer gloss oil at product surface, electroplating or carry out film increases smooth degree, pattern and the color and luster of product surface, and can not realize that any one color of product surface is to the effect of another kind of color transition.
The present invention is directed to the above-mentioned defective of prior art, a kind of surface treatment method is provided, so that the product surface coating has had new breakthrough technically.This method running cost is low, and is practical.
Summary of the invention:
A kind of surface treatment method, it is characterized in that, this method may further comprise the steps: feeling secure in article outer surface, (oil that do not feel secure is also passable in oil processing, effect do not feel secure oil effect good), the entire portion of current oil spout spray product outer surface, carry out the oil spout second time again, from any one side, carry out the oil spout second time, the local part of a current oil spout spray product outer surface, from commencement of fuel injection to the end oil spout, the thickness of oil spout coating by thick to shallow, to rare, the speed of oil spout from slow to fast by close for the particle of oil spout coating.Can reach the effect of dichromatism gradual change, oil spout is for the third time carried out in three look gradual changes in this way, and current oil spout needs the position commencement of fuel injection of the 3rd section gradual change to the end oil spout from spray product outer surface, the thickness of oil spout coating by thick to shallow, to rare, oil spout speed from slow to fast by close for the oil spout coating granule.The same third step of more colors gradual changed method fuel injecting method.
As can be seen from the above technical solutions, institute of the present invention injector layer is to the transition gradually of another kind of color by a kind of color, perhaps by multiple color to the transition gradually of multiple color, not only increased the brightness of article outer surface, aesthetics and wearability, and make article coatings have innervation, increased its vigor.
The present invention to the surface treatment procedure of computer camera shell is: the ABS or the PC material shell of injection mo(u)lding are carried out whole oil spout processing, carry out the gradual change oil spout by the number of colors of product needed gradual change then and handle.To finishing oil spout, to shallow, to rare, oil spout speed from slow to fast by close for the oil spout coating granule by thick for the thickness of oil spout coating from commencement of fuel injection in the gradual change processing.The present invention is adapted to plastic cement, the surface treatment of metal and other goods.
The specific embodiment:
Be further described with the present invention below in conjunction with example.
Example one: do spray end oil processing on the plastic cement surface, on the surperficial primary colours of the plastic cement that sprayed end oil, carry out locally sprayed another kind of color then.The multiple color gradient of needs is arranged, adopt repeatedly locally sprayed method.
Example two: directly carry out locally sprayed another kind of color on the plastic cement surface.The multiple color gradient of needs is arranged, adopt repeatedly locally sprayed method.
The above example only shows several embodiment of the present invention, but is not the outer surface processing that patent of the present invention only is adapted to these two kinds of materials, so the protection domain of patent of the present invention just is as the criterion with claims.
Claims (3)
1. a surface treatment method is characterized in that, this surface treatment method change may further comprise the steps: gradually look spraying of background color spraying--spraying of gradual change look---repeatedly.
2. by the described a kind of surface treatment method of claim 1, it is characterized in that: described primary colours spraying is that whole article outer surface is sprayed comprehensively.Or be primary colours with the color of material itself.
3. by the described a kind of surface treatment method of claim 1, it is characterized in that: the spraying of described gradual change look, ground carries out locally sprayed to article outer surface, and the thickness of oil spout coating by thick to shallow, to rare, the speed of oil spout from slow to fast by close for the particle of oil spout coating.