CN102180806A - Preparation method of cobalt glycinate - Google Patents

Preparation method of cobalt glycinate Download PDF

Info

Publication number
CN102180806A
CN102180806A CN2011100780194A CN201110078019A CN102180806A CN 102180806 A CN102180806 A CN 102180806A CN 2011100780194 A CN2011100780194 A CN 2011100780194A CN 201110078019 A CN201110078019 A CN 201110078019A CN 102180806 A CN102180806 A CN 102180806A
Authority
CN
China
Prior art keywords
cobalt
glycine
preparation
cobalt glycinate
glycinate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011100780194A
Other languages
Chinese (zh)
Inventor
仲伟静
邹书通
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHENJIANG OUKE BIOLOGICAL TECHNOLOGY Co Ltd
Original Assignee
ZHENJIANG OUKE BIOLOGICAL TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHENJIANG OUKE BIOLOGICAL TECHNOLOGY Co Ltd filed Critical ZHENJIANG OUKE BIOLOGICAL TECHNOLOGY Co Ltd
Priority to CN2011100780194A priority Critical patent/CN102180806A/en
Publication of CN102180806A publication Critical patent/CN102180806A/en
Pending legal-status Critical Current

Abstract

The invention belongs to the field of organic compound synthesis and relates to a preparation method of cobalt glycinate. The method comprises the following steps of: (1) performing chelation to form salt, namely adding glycine, basic cobaltous carbonate and water into a reaction kettle, stirring, heating the materials to 60 to 80 DEG C, preserving heat and continuously stirring for 30 minutes, so that carbon dioxide can be overflowed completely and the cobalt glycinate is generated; and (2) drying, namely performing centrifugal dehydration on the cobalt glycinate, transferring to a fluidized bed and drying at the temperature of between 100 and 120 DEG C to obtain the cobalt glycinate product. The preparation method has the advantages that: (1) the cobalt glycinate prepared by the method has uniform particles, is easy to dry, contributes to improving production efficiency and reduces production cost; (2) the solution obtained through centrifugation in the preparation method can be recycled in the next production process of the products, without waste water; and (3) the cobalt glycinate product prepared by the method has high flowing property, is difficult to cake, and can be widely and safely applied to livestock production.

Description

The preparation method of glycine cobalt
Technical field
The invention belongs to the synthetic field of organic compound, relate to a kind of preparation method of glycine cobalt.
Technical background
The glycine cobalt is as a kind of organic cobalt, and, price low, discharging low, environmental pollution few etc. low, effective owing to its consumption had a few, and is increasingly extensive with using in livestock industry, has broad application prospects.The common production method of glycine cobalt is to make with glycine, soda ash, rose vitriol reaction, and its shortcoming is: (1) gained glycine cobalt thickness, and not easily separated, be difficult for dry; (2) gained glycine cobalt product free-running property is poor, and easy caking uses inconveniently on producing, and contains that the cobalt amount is high to cause animal to poison even dead thereby easily make the feeds product part; (3) reaction can produce the sodium sulfate byproduct, forms the contaminated wastewater environment.
Summary of the invention
The object of the invention is, overcomes the deficiency of existing production technology, and a kind of preparation method of new glycine cobalt is provided.Feasible even by the obtained glycine cobalt granule of this preparation method, be easy to drying, help enhancing productivity, reduce production costs; Centrifugal gained solution can be re-used in next products production, and no waste water produces; Glycine cobalt product free-running property is good, prevented from caking, can be in herding be produced extensively, Secure Application.
The preparation method of glycine cobalt of the present invention comprises the steps:
(1) chelating salify step: glycine, cobaltous dihydroxycarbonate, water are dropped in the reactor, stir, be heated to 60 ℃~80 ℃, keep temperature to continue to stir, carbonic acid gas is fully overflowed, generate the glycine cobalt;
(2) drying step: the centrifuge dehydration of gained glycine cobalt, to transfer in the fluidized-bed, 100 ℃~120 ℃ oven dry obtain glycine cobalt product.
In the above-mentioned steps (1), the glycine of input and the mol ratio of cobaltous dihydroxycarbonate are 10:0.9-1.1.
Advantage of the present invention and positively effect are:
(1) even by the obtained glycine cobalt granule of this preparation method, be easy to drying, help enhancing productivity, reduce production costs;
(2) can be re-used in next products production by the centrifugal gained solution of this preparation method, no waste water produces;
(3) good by the obtained glycine cobalt of this preparation method product free-running property, prevented from caking, can be in herding be produced extensively, Secure Application.
Embodiment
Below by specific embodiment the present invention is described in further detail.
Embodiment 1:
A kind of preparation method of glycine cobalt may further comprise the steps:
(1) chelating salify step: in 500 liters of reactors that have heating unit, whipping appts and a thermometer, add 250 premium on currency, 1000 moles of glycine, 100 moles of cobaltous dihydroxycarbonates successively, stir, be heated to 60 ℃~80 ℃, keep temperature to continue to stir 30 minutes, generate the glycine cobalt;
(2) drying step: the centrifuge dehydration of gained glycine cobalt, transfer in the fluidized-bed, dried 30 minutes for 100 ℃~120 ℃, obtain glycine cobalt product, this glycine cobalt product cobalt contents is greater than 25%.
Embodiment 2:
(1) chelating salify step: in 2000 liters of reactors that have heating unit, whipping appts and a thermometer, add 1000 premium on currency, 4000 moles of glycine, 400 moles of cobaltous dihydroxycarbonates successively, stir, be heated to 60 ℃~80 ℃, keep temperature to continue to stir 30 minutes, generate the glycine cobalt;
(2) drying step: the centrifuge dehydration of gained glycine cobalt, transfer in the fluidized-bed, dried 30 minutes for 100 ℃~120 ℃, obtain glycine cobalt product, this glycine cobalt product cobalt contents is greater than 25%.
Embodiment 3:
(1) chelating salify step: in 2000 liters of reactors that have heating unit, whipping appts and a thermometer, add centrifugal gained solution among 800 liters of embodiment 2,200 premium on currency, 3800 moles of glycine, 380 moles of cobaltous dihydroxycarbonates successively, stir, be heated to 60 ℃~80 ℃, keep temperature to continue to stir 30 minutes, generate the glycine cobalt;
(2) drying step: the centrifuge dehydration of gained glycine cobalt, transfer in the fluidized-bed, dried 30 minutes for 100 ℃~120 ℃, obtain glycine cobalt product, this glycine cobalt product cobalt contents is greater than 25%.

Claims (2)

1. the preparation method of a glycine cobalt is characterized in that: comprises the steps,
(1) chelating salify step: glycine, cobaltous dihydroxycarbonate, water are dropped in the reactor, stir, be heated to 60 ℃~80 ℃, keep temperature to continue to stir, carbonic acid gas is fully overflowed, generate the glycine cobalt;
(2) drying step: the centrifuge dehydration of gained glycine cobalt, to transfer in the fluidized-bed, 100 ℃~120 ℃ oven dry obtain glycine cobalt product.
2. the preparation method of glycine cobalt according to claim 1 is characterized in that: in the step (1), the glycine of input and the mol ratio of cobaltous dihydroxycarbonate are 10:0.9-1.1.
CN2011100780194A 2011-03-30 2011-03-30 Preparation method of cobalt glycinate Pending CN102180806A (en)