CN102128753A - Water solubility test method for household paper - Google Patents

Water solubility test method for household paper Download PDF

Info

Publication number
CN102128753A
CN102128753A CN201110020031XA CN201110020031A CN102128753A CN 102128753 A CN102128753 A CN 102128753A CN 201110020031X A CN201110020031X A CN 201110020031XA CN 201110020031 A CN201110020031 A CN 201110020031A CN 102128753 A CN102128753 A CN 102128753A
Authority
CN
China
Prior art keywords
paper
water
beaker
vortex
pattern
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201110020031XA
Other languages
Chinese (zh)
Other versions
CN102128753B (en
Inventor
郭淳
帕特里克帕特.陈
亚历克斯
于洁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hainan Jinhongye Paper Co ltd
Gold HongYe Paper Group Co Ltd
Original Assignee
Gold HongYe Paper Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Gold HongYe Paper Group Co Ltd filed Critical Gold HongYe Paper Group Co Ltd
Priority to CN 201110020031 priority Critical patent/CN102128753B/en
Publication of CN102128753A publication Critical patent/CN102128753A/en
Application granted granted Critical
Publication of CN102128753B publication Critical patent/CN102128753B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A water solubility test method for household paper, comprising the steps of: cutting the thin paper into a square paper pattern; placing the paper pattern in a drying oven with the temperature of 105 +/-2 ℃ and curing for 15 minutes; placing the paper sample in an environment with the temperature of 23 +/-2 ℃ and the relative humidity of 40 +/-2% to balance moisture; putting the magnetic stirrer into a beaker, adding water into the beaker, and forming a vortex in the beaker under the stirring of the magnetic stirrer; pinching four corners of the paper pattern, placing the bottom of the paper pattern at the moment of the vortex, and starting to record the duration; after the paper is completely dispersed, the duration recording is ended, thereby obtaining a duration value. The method is simple and practical to operate, convenient and fast, and high in accuracy.

Description

A kind of water-soluble method of testing that is used to life paper
Technical field
The present invention relates to a kind of water-soluble method of testing, be specifically related to a kind of water-soluble method of testing that is used to life paper.
Background technology
Paper using amount per capita along with China constantly promoted in recent years, and the industry development of the slim life paper of China also is with rapid changepl. never-ending changes and improvements.No matter be also is constantly soaring in output or on product category.But the test for slim paper is not perfect, especially slim life paper water-soluble still do not have corresponding test method, and water-soluble performance is very important performance for slim life paper, this point often fails to cause slim life paper manufacturer, such as the toilet paper in the paper for daily use,, can stop up toilet for various reasons though can directly throw into toilet, this is exactly the water-soluble too poor of toilet paper, still has nothing to do at home in the water miscible method of testing of slim life paper according to investigations.
Summary of the invention
The object of the invention provides a kind of water-soluble method of testing that is used to life paper, this method practicality simple to operate, convenient and swift and accuracy is higher.
For achieving the above object, the technical solution used in the present invention is:
A kind of water-soluble method of testing that is used to life paper may further comprise the steps:
Step 1. described slim paper is cut into foursquare pattern;
Step 2. described pattern is positioned in 105 ± 2 ° the baking oven slaking 15 minutes;
Step 3. described pattern is positioned over equilibrium moisture under the environment that temperature is 23 ± 2 ℃ and relative humidity 40 ± 2%;
Step 4. the magnetic stirrer is put into beaker, add water in beaker, this burns water in the cup and form whirlpool under the stirring of magnetic stirrer;
Step 5. pinch four angles of described pattern, the bottom of pattern is positioned over moment of described whirlpool, opening entry duration with this moment;
Step 6. treat that described pattern is decomposed into some paper scraps, and area is less than 1cm 2Paper scrap quantity surpass 90%, finish the duration record, thereby obtain the dissolution time value.
Related content in the technique scheme is explained as follows:
1, in the such scheme, amount of water is 300ml in the described beaker, and described whirlpool bottom level is no more than 2/3 of whirlpool height.
2, in the such scheme, between described step 4 and step 5, need the described whirlpool of wait to stablize 10 second time.
Because the technique scheme utilization, the present invention compared with prior art has following advantage and effect:
The present invention provides the quick and higher water-soluble method of testing of accuracy simple to operate, practical and convenient for life paper, and this method can provide reliable data for production.Secondly, form eddy current by the magnetic stirrer, the shearing force of eddy current is disperseed fibrous bundle, thereby the hydrogen bond rupture between will life paper fiber, fibrous bundle becomes and is easy to separate, dissolution time is short more under certain shearing force shows that then the bond strength of paper in water is more little, and toilet paper dissolves in toilet will be fast more.Once more, method of testing is accurately simulated the toilet inside environment that draws water, and demonstrates fully the dissolving situation of paper in toilet, can guarantee that through test the paper produced can dissolving fast in water fully, to reach the situation of not stopping up toilet.
Embodiment
Below in conjunction with embodiment the present invention is further described:
Embodiment: a kind of water-soluble method of testing that is used for slim paper may further comprise the steps:
Step 1. described slim paper is cut into foursquare pattern;
Step 2. described pattern is positioned in 105 ± 2 ° the baking oven slaking 15 minutes;
Step 3. described pattern is positioned over equilibrium moisture under the environment that temperature is 23 ± 2 ℃ and relative humidity 40 ± 2%;
Step 4. the magnetic stirrer is put into beaker, add water in beaker, this burns water in the cup and form whirlpool under the stirring of magnetic stirrer;
Step 5. pinch four angles of described pattern, the bottom of pattern is positioned over moment of described whirlpool, opening entry duration with this moment;
Step 6. treat that described pattern is decomposed into some paper scraps, and area is less than 1cm 2Paper scrap quantity surpass 90%, finish the duration record, thereby obtain the dissolution time value.
Amount of water is 300ml in the above-mentioned beaker, and described whirlpool bottom level is no more than 2/3 of whirlpool height.
Between the above step 4 and the step 5, need the described whirlpool of wait to stablize 10 second time.
The foregoing description only is explanation technical conceive of the present invention and characteristics, and its purpose is to allow the personage who is familiar with this technology can understand content of the present invention and enforcement according to this, can not limit protection scope of the present invention with this.All equivalences that spirit is done according to the present invention change or modify, and all should be encompassed within protection scope of the present invention.

Claims (3)

1.一种用于生活纸的水溶性测试方法,其特征在于:包括以下步骤:1. a water-soluble test method for household paper, characterized in that: comprises the following steps: 步骤一.将所述薄型纸裁剪成正方形的纸样;step one. The thin paper is cut into a square pattern; 步骤二.将所述纸样放置于105±2°的烘箱中,熟化15分钟;Step two. Place the paper pattern in an oven at 105±2°, and cure it for 15 minutes; 步骤三.将所述纸样放置于温度为23±2℃ 和相对湿度 40±2% 的环境下平衡水分;Step three. Place the paper sample in an environment with a temperature of 23±2°C and a relative humidity of 40±2% to balance moisture; 步骤四.将磁性搅拌子放入烧杯中,在烧杯中加水,此烧杯中水在磁性搅拌子的搅拌下形成漩涡;Step four. Put the magnetic stirring bar into the beaker, add water in the beaker, and the water in the beaker forms a vortex under the stirring of the magnetic stirring bar; 步骤五.捏住所述纸样四个角,将此时纸样的底部放置于所述漩涡的时刻,开始记录持续时间; Step five. Pinch the four corners of the paper pattern, place the bottom of the paper pattern at the moment of the vortex, and start recording the duration; 步骤六.待所述纸样分解为若干纸屑,且面积小于1cm2的纸屑数量超过90%,结束持续时间记录,从而获得溶解时间值。Step six. After the paper sample is decomposed into several pieces of paper, and the number of pieces of paper with an area of less than 1 cm exceeds 90%, the recording of the duration is ended, so as to obtain the value of the dissolution time. 2.根据权利要求1所述的水溶性测试方法,其特征在于:所述烧杯中加水量为300ml,所述漩涡底部高度不超过漩涡高度的2/3。2. The water solubility testing method according to claim 1, characterized in that: the amount of water added to the beaker is 300ml, and the height of the bottom of the vortex is no more than 2/3 of the height of the vortex. 3.根据权利要求1所述的水溶性测试方法,其特征在于:在所述步骤四与步骤五之间,需等待所述漩涡稳定10秒时间。3. The water solubility testing method according to claim 1, characterized in that: between the fourth step and the fifth step, it is necessary to wait for the vortex to stabilize for 10 seconds.
CN 201110020031 2011-01-18 2011-01-18 Water solubility test method for household paper Active CN102128753B (en)