CN102115993A - Mould for forging wire rope - Google Patents

Mould for forging wire rope Download PDF

Info

Publication number
CN102115993A
CN102115993A CN 201010596247 CN201010596247A CN102115993A CN 102115993 A CN102115993 A CN 102115993A CN 201010596247 CN201010596247 CN 201010596247 CN 201010596247 A CN201010596247 A CN 201010596247A CN 102115993 A CN102115993 A CN 102115993A
Authority
CN
China
Prior art keywords
wire rope
mould
forging
straight trough
encircling manner
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010596247
Other languages
Chinese (zh)
Inventor
张正强
李长春
徐春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
STABLE STEEL PRODUCTS CO Ltd
Original Assignee
STABLE STEEL PRODUCTS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by STABLE STEEL PRODUCTS CO Ltd filed Critical STABLE STEEL PRODUCTS CO Ltd
Priority to CN 201010596247 priority Critical patent/CN102115993A/en
Publication of CN102115993A publication Critical patent/CN102115993A/en
Pending legal-status Critical Current

Abstract

The invention discloses a mould for forging a wire rope, which does not form forging marks on the wire rope and prevents a steel wire at the external layer of the wire rope from being broken during forging. The mould consists of a plurality of mould bodies arranged in an encircling manner, wherein each mould body is provided with a straight groove and trumpet-shaped grooves arranged at both sides of the straight groove and respectively connected with the straight groove; and when the plurality of mould bodies form an integral body in the encircling manner, a deforming zone is formed by the straight grooves arranged in the encircling manner, and the trumpet-shaped grooves are also arranged in the encircling manner so as to respectively form an inlet cone and an outlet cone. The advantages are as follows: the mould endowed with the structure and used for forging the wire rope divides the wire rope forging process into forging, sizing and guiding so as to effectively solve the variation of sizing reduction during instant forging, which is caused due to the vibration of an in service rope closer and the nonuniform diameter of a core of the wire rope, and to avoid the influence generated by the characteristic of post-forging pringback of the wire rope, thus increasing the production efficiency.

Description

The mould that is used for forge wire rope
Technical field
The present invention relates to a kind of mould that is used for forge wire rope.
Background technology
Forge wire rope has the density metal height, structure is tight, stable, and structural stretch is little, and whole rope rupture pull force is big; Anti-wear performance is good, and shock resistance and the good characteristics of anti-extrusion performance extensively apply to hoisting and conveying machinery and equipments such as vertical shaft hoisting, power shovel elevator, rotary drilling rig, harbour handling.As shown in Figure 1 and Figure 2, the mould that is used for forge wire rope commonly used around forming, is respectively arranged with flared channels 2 by several die bodys 1 on the die body 1, and when some die bodys 1 are looped around a time-out, flared channels 2 is looped around and just is formed into prostomum 3 together.The operation principle of above-mentioned mould is: die body 1 can be done separately, closed motion under the effect of external force, goes round and begins again, and has just realized the purpose that the steel wire ropes 4 in the die entrance awl 3 are forged.Closed that the operating vibration of rope equipment, wire rope core diameter inhomogeneities cause that moment forges that sizing reduction changes and the influence of the characteristic that steel wire rope can resilience after forging, and die body 1 can periodically separate, closure, the steel wire rope at mould A place is easy to be blocked by die body among Fig. 1, gently then can on steel wire rope, stay and significantly forge trace, heavy then cover wire steel wire rope can be interrupted, and steel wire rope is forced to interrupt, can not be by producing length requirement production, cause the waste of resource, reduce production efficiency.If when above-mentioned situation occurring, in time do not stop steel wire rope being forged, even can cause mould to damage.
Summary of the invention
Technical problem to be solved by this invention is: provides can not produce on a kind of steel wire rope to forge trace, and the steel wire rope cover wire mould that is used for forge wire rope that can not be interrupted.
For solving the problems of the technologies described above, the technical solution used in the present invention is: a kind of mould that is used for forge wire rope, this mould by several die bodys around forming, the flared channels that is respectively arranged with straight trough on the described die body and is arranged on the straight trough both sides and links to each other with straight trough respectively, some die bodys are looped around a time-out, straight trough is looped around and forms the deformed area together, and flared channels is looped around and is formed into prostomum together respectively and goes out prostomum.
Described straight trough and the flared channels that is arranged on the straight trough both sides connect by circular arc respectively.
The invention has the beneficial effects as follows: the mould that is used for forge wire rope of said structure the process of forging of steel wire rope is divided into forge, sizing, guiding, efficiently solve and close that the operating vibration of rope equipment, wire rope core diameter inhomogeneities cause that moment forges that sizing reduction changes and influence that characteristic that steel wire rope can resilience after forging is brought, thereby enhance productivity.
Description of drawings
Fig. 1 is the front view that is used for the mould of forge wire rope in the background technology;
Fig. 2 is the right view of Fig. 1;
Fig. 3 is the front view that the present invention is used for the mould of forge wire rope;
Fig. 4 is the structural representation of die body among the present invention;
Fig. 5 is the vertical view of Fig. 4;
Fig. 6 is the structure chart of Fig. 3 when forge wire rope.
Among Fig. 1, Fig. 2: 1, die body, 2, flared channels, 3, approach cone, 4, steel wire rope.
Among Fig. 3 to Fig. 6: 1, die body, 2, flared channels, 3, approach cone, 4, steel wire rope, 5, straight trough, 6, the inlet flared channels, 7, the outlet flared channels, 8, approach cone, 9, go out prostomum, 10, the deformed area.
The specific embodiment
Below in conjunction with accompanying drawing, describe specific embodiments of the present invention in detail.
As Fig. 3, Fig. 4, Fig. 5, shown in Figure 6, the mould that is used for forge wire rope of the present invention, around forming, the quantity of die body 1 can set up on their own according to needs of production this mould by several die bodys 1.The flared channels that is respectively arranged with straight trough 5 on the described die body 1 and is arranged on straight trough 5 both sides and links to each other with straight trough 5 respectively---inlet flared channels 6 and outlet flared channels 7, when die body 1 is looped around a time-out, straight trough 5 is looped around and forms deformed area 10 together, inlet flared channels 6 is looped around and is formed into prostomum 8 together, outlet flared channels 7 is looped around and forms prostomum 9 together, and straight trough and the flared channels that is arranged on the straight trough both sides connect by circular arc respectively.
Operation principle of the present invention is: after steel wire rope enters approach cone 8, B place at Fig. 6 forges, because the steel wire rope after forging has the characteristic of resilience, deformed area 10 is just to steel wire rope sizing by force, and deformed area 10 has also been eliminated and has been closed the operating vibration of rope equipment, wire rope core diameter inhomogeneities and cause that moment forges sizing reduction and change influence to steel wire rope, has reduced the possibility that steel wire rope blocks at the B place simultaneously.At last, steel wire rope is derived going out prostomum place 9, also is arranged to bell mouth shape owing to go out prostomum 9 places, has further reduced the jammed possibility of wire.Thereby improve the shaping efficiency of steel wire rope, guaranteed the continuity of Wire Rope Production line, improved production efficiency.

Claims (2)

1. the mould that is used for forge wire rope, this mould by several die bodys around forming, it is characterized in that: the flared channels that is respectively arranged with straight trough on the described die body and is arranged on the straight trough both sides and links to each other with straight trough respectively, some die bodys are looped around a time-out, straight trough is looped around and forms the deformed area together, and flared channels is looped around and is formed into prostomum together respectively and goes out prostomum.
2. the mould that is used for forge wire rope according to claim 1 is characterized in that: described straight trough and the flared channels that is arranged on the straight trough both sides connect by circular arc respectively.
CN 201010596247 2010-12-20 2010-12-20 Mould for forging wire rope Pending CN102115993A (en)