CN102092200A - Double-sided code spraying method for material - Google Patents
Double-sided code spraying method for material Download PDFInfo
- Publication number
- CN102092200A CN102092200A CN2009102011476A CN200910201147A CN102092200A CN 102092200 A CN102092200 A CN 102092200A CN 2009102011476 A CN2009102011476 A CN 2009102011476A CN 200910201147 A CN200910201147 A CN 200910201147A CN 102092200 A CN102092200 A CN 102092200A
- Authority
- CN
- China
- Prior art keywords
- adhesive material
- plane materiel
- coding
- release liners
- passed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a double-sided code spraying method for a material, and relates to a code spraying method. The method comprises the following steps that: 1, the material passes through a feed roll, and is unfolded and straightened; 2, the material passes through a peeling roll, an adhesive sticker material surface material of the material is peeled from release paper, the adhesive sticker material surface material passes through one positioning roll and the release paper passes through the other positioning roll; 3, a code spraying machine is arranged on the adhesive side of the adhesive sticker material surface material, and sprays codes onto the adhesive side; 4, the adhesive sticker material surface material of which the adhesive side is subjected to code spraying and the release paper simultaneously pass through a doubling roller for lamination; and 5, a code spraying machine is arranged on the adhesive sticker material surface material surface of the laminated material, and sprays codes onto the surface. The method has the advantages that: multiple sides of the material can be subjected to code spraying, the code spraying time is saved, production efficiency is improved, the label anti-counterfeiting function is realized and the production cost is reduced.
Description
Technical field
The present invention relates to a kind of coding method, particularly relate to a kind of two-sided coding method of adhesive material label.
Background technology
Along with the raising day by day of development and national economy and living standards of the people, China's cosmetics and the development of health care medical industry are flourishing.People crave for and pay attention to healthy and beautiful, allow the market demand of medicine, the skin care products that keeps healthy grow with each passing day.Under the intense market competition environment, the external packing of product except keep basic product introduction and design more meet the consumer aesthetic, also need meet the requirement and the false proof requirement of rules.Perfect along with rules allows medicine or this class of health care skin care products contact with human body or edible product must provide clear and definite date of manufacture of consumer and shelf-life and effective antifalse effect, and these require just to have brought technical barrier in the printing of label.Sometimes in order to stamp anti-fake mark, need be in the glue face and the positive coding simultaneously of label, the method of the now general two-sided coding of label is earlier that a spray printing is good, again it is sprayed other one side conversely, the time that this method not only spends is long, but also needs operation manually is badly in need of having a kind of method of automatic double-sided coding to solve above problem.
Summary of the invention
At the defective that exists in the two-sided code spraying technology in the prior art, the present invention proposes a kind of two-sided coding method of material to address the deficiencies of the prior art.
To achieve these goals, technical scheme of the present invention is as follows, a kind of two-sided coding method of material, and it is characterized in that: described material is an adhesive material, steps of the method are:
One, adhesive material is passed through feed roller, with adhesive material expansion, stretching;
Two, adhesive material is peeled off the adhesive material plane materiel and the release liners of adhesive material by stripper roll, then the adhesive material plane materiel is passed through a registration roller, and release liners is passed through another registration roller;
Three, at the adhesive material plane materiel by after the registration roller, in glue face one side of adhesive material plane materiel an ink jet numbering machine is set, and it is carried out the coding of glue face;
Four, will fit by doubling roller simultaneously through adhesive material plane materiel after the coding of glue face and release liners.
Five, surface one side at the adhesive material plane materiel of the adhesive material that posts is provided with an ink jet numbering machine, and surperficial coding is carried out on its surface.
A kind of two-sided coding method of material, it is characterized in that: described material is an adhesive material, steps of the method are:
One, adhesive material is passed through feed roller, with adhesive material expansion, stretching;
Two, adhesive material is peeled off the adhesive material plane materiel and the release liners of adhesive material by stripper roll, then the adhesive material plane materiel is passed through a registration roller, and release liners is passed through another registration roller;
Three, at the adhesive material plane materiel by after the registration roller, in glue face one side of adhesive material plane materiel an ink jet numbering machine is set, and it is carried out the coding of glue face;
Four, will fit by doubling roller simultaneously through adhesive material plane materiel after the coding of glue face and release liners.
Five, surface one side in the release liners of the adhesive material that posts is provided with an ink jet numbering machine, and surperficial coding is carried out on its surface.
A kind of two-sided coding method of material, it is characterized in that: described material is an adhesive material, steps of the method are:
One, adhesive material is passed through feed roller, with adhesive material expansion, stretching;
Two, adhesive material is peeled off the adhesive material plane materiel and the release liners of adhesive material by stripper roll, then the adhesive material plane materiel is passed through a registration roller, and release liners is passed through another registration roller;
Three, after the adhesive material plane materiel passed through registration roller, one side was provided with an ink jet numbering machine on the surface of adhesive material plane materiel, and it is carried out the coding of glue face;
Four, will fit by doubling roller simultaneously through adhesive material plane materiel after the coding of glue face and release liners.
Five, surface one side in the release liners of the adhesive material that posts is provided with an ink jet numbering machine, and surperficial coding is carried out on its surface.
A kind of two-sided coding method of material is characterized in that: steps of the method are:
One, material is passed through feed roller, with material expansion, stretching;
Two, material passes through a registration roller by stripper roll again with material;
Three, after material passed through registration roller, one side was provided with an ink jet numbering machine on the surface of material, and it is carried out surperficial coding;
Four, will pass through doubling roller through the material after the surperficial coding.
Five, material is by after the doubling roller, and one side is provided with an ink jet numbering machine at the back side of material, and back side coding is carried out at its back side.
The invention has the beneficial effects as follows: can to glue face and the release liners back side or the front of adhesive label and the coding of the release liners back side of the front of adhesive label and glue face or adhesive label or the obverse and reverse of general material carries out coding simultaneously, not only saved the coding time, improved production efficiency, reach the function of label anti-counterfeit simultaneously, and reduced production cost.
Description of drawings
Describe the present invention in detail below in conjunction with the drawings and specific embodiments:
Fig. 1 is the reference diagram of embodiment 1.
Fig. 2 is the reference diagram of embodiment 2.
Fig. 3 is the reference diagram of embodiment 3.
Fig. 4 is the reference diagram of embodiment 4.
The specific embodiment
For technological means, creation characteristic that the present invention is realized, reach purpose and effect is easy to understand, below in conjunction with concrete diagram, further set forth the present invention.
Embodiment 1:
Referring to Fig. 1, a kind of two-sided coding method of adhesive material the steps include:
One, adhesive material 8 is passed through feed roller 1, the effect of feed roller 1 is to make adhesive material can satisfy the condition that next step operation is implemented adhesive material 8 expansion, stretching;
Two, after expansion and stretching through feed roller 1, adhesive material 8 is by stripper roll 2, in the charging first time by manually adhesive material plane materiel 81 and release liners 82 being peeled off, make after adhesive material plane materiel 81 and release liners 82 peel off, the glue face of adhesive material plane materiel 81 just comes out, and makes things convenient for next step glue face to adhesive material plane materiel 81 to carry out the coding of glue face.Simultaneously because after adhesive material plane materiel 81 peels off with release liners 82, the glue face of adhesive material plane materiel 81 is exposed in the air, be easy to be stained with dust in air on the glue face, influence later bonding, so when using the method that the glue face is carried out coding, preferably in aseptic dustless environment, carry out;
A registration roller 3 and a registration roller 4 are set after stripper roll 2, need at intervals between registration roller 3 and the registration roller 4, adhesive material plane materiel 81 is passed through registration roller 3, release liners 82 is passed through registration roller 4, again because have certain distance between registration roller 3 and the registration roller 4, so that the interval that also produces certain distance between adhesive material plane materiel 81 and the release liners 82;
Three, at adhesive material plane materiel 81 by after the registration roller 3, in glue face one side of adhesive material plane materiel 81 ink jet numbering machine 6 is set, and it is carried out the coding of glue face, so just make also to have stamped literal or pattern on the glue face of adhesive material plane materiel 81;
Four, will fit by doubling roller 5 together simultaneously through adhesive material plane materiel 81 after the coding of glue face and release liners 82, and make adhesive material plane materiel 81 and release liners 82 fit to together, the adhesive material 8 of this moment restores to the original state.
Five, surface one side at the adhesive material plane materiel 81 of the adhesive material 8 that posts is provided with an ink jet numbering machine 7, and surperficial coding is carried out on its surface, and so far, the surface of whole adhesive sticker and glue face have all carried out coding.
Embodiment 2:
Referring to Fig. 2, a kind of two-sided coding method of adhesive material the steps include:
One, adhesive material 8 is passed through feed roller 1, the effect of feed roller 1 is to make adhesive material can satisfy the condition that next step operation is implemented adhesive material 8 expansion, stretching;
Two, after expansion and stretching through feed roller 1, adhesive material 8 is by stripper roll 2, in the charging first time by manually adhesive material plane materiel 81 and release liners 82 being peeled off, make after adhesive material plane materiel 81 and release liners 82 peel off, the glue face of adhesive material plane materiel 81 just comes out, and makes things convenient for next step glue face to adhesive material plane materiel 81 to carry out the coding of glue face.Simultaneously because after adhesive material plane materiel 81 peels off with release liners 82, the glue face of adhesive material plane materiel 81 is exposed in the air, be easy to be stained with dust in air on the glue face, influence later bonding, so when using the method that the glue face is carried out coding, preferably in aseptic dustless environment, carry out;
A registration roller 3 and a registration roller 4 are set after stripper roll 2, need at intervals between registration roller 3 and the registration roller 4, adhesive material plane materiel 81 is passed through registration roller 3, release liners 82 is passed through registration roller 4, again because have certain distance between registration roller 3 and the registration roller 4, so that the interval that also produces certain distance between adhesive material plane materiel 81 and the release liners 82;
Three, at adhesive material plane materiel 81 by after the registration roller 3, in glue face one side of adhesive material plane materiel 81 ink jet numbering machine 6 is set, and it is carried out the coding of glue face, so just make also to have stamped literal or pattern on the glue face of adhesive material plane materiel 81;
Four, will fit by doubling roller 5 together simultaneously through adhesive material plane materiel 81 after the coding of glue face and release liners 82, and make adhesive material plane materiel 81 and release liners 82 fit to together, the adhesive material 8 of this moment restores to the original state.
Five, surface one side in the release liners 82 of the adhesive material 8 that posts is provided with an ink jet numbering machine 7, and surperficial coding is carried out on its surface, and so far, the surface of whole adhesive sticker and glue face have all carried out coding.
Embodiment 3:
Referring to Fig. 3, a kind of two-sided coding method of adhesive material the steps include:
One, adhesive material 8 is passed through feed roller 1, the effect of feed roller 1 is to make adhesive material can satisfy the condition that next step operation is implemented adhesive material 8 expansion, stretching;
Two, after expansion and stretching through feed roller 1, adhesive material 8 is by stripper roll 2, in the charging first time by manually adhesive material plane materiel 81 and release liners 82 being peeled off, make after adhesive material plane materiel 81 and release liners 82 peel off, the glue face of adhesive material plane materiel 81 just comes out.Simultaneously because after adhesive material plane materiel 81 peels off with release liners 82, the glue face of adhesive material plane materiel 81 is exposed in the air, be easy to be stained with dust in air on the glue face, influence later bonding, so when using the method that the glue face is carried out coding, preferably in aseptic dustless environment, carry out;
A registration roller 3 and a registration roller 4 are set after stripper roll 2, need at intervals between registration roller 3 and the registration roller 4, adhesive material plane materiel 81 is passed through registration roller 3, release liners 82 is passed through registration roller 4, again because have certain distance between registration roller 3 and the registration roller 4, so that the interval that also produces certain distance between adhesive material plane materiel 81 and the release liners 82;
Three, at adhesive material plane materiel 81 by after the registration roller 3, a side is provided with an ink jet numbering machine 6 on the surface of adhesive material plane materiel 81, and it is carried out surperficial coding, so just makes also to have stamped literal or pattern on the surface of adhesive material plane materiel 81;
Four, will fit by doubling roller 5 together simultaneously through adhesive material plane materiel 81 after the coding of glue face and release liners 82, and make adhesive material plane materiel 81 and release liners 82 fit to together, the adhesive material 8 of this moment restores to the original state.
Five, surface one side in the release liners 82 of the adhesive material 8 that posts is provided with an ink jet numbering machine 7, and surperficial coding is carried out on its surface, and so far, the surface of whole adhesive sticker and glue face have all carried out coding.
Embodiment 4:
Referring to Fig. 4, a kind of two-sided coding method of material, material is the monolayer material of non-adhesive sticker, the steps include:
One, material 8 is passed through feed roller 1, the effect of feed roller 1 is to make material can satisfy the condition that next step operation is implemented material 8 expansion, stretching;
Two, after expansion and stretching through feed roller 1, material 8 is provided with a registration roller 3 by stripper roll 2 after stripper roll 2, and material 8 is passed through registration roller 3;
Three, at material 8 by after the registration roller 3, a side is provided with an ink jet numbering machine 6 on the surface of material 8, and it is carried out surperficial coding, so just makes to have stamped literal or pattern on the surface of material 8;
Four, will be through material plane materiel after the surperficial coding 8 by doubling roller 5.
Five, material 8 is by after the doubling roller 5, and a side is provided with an ink jet numbering machine 7 at the back side of material 8, and back side coding is carried out at its back side.
More than show and described basic principle of the present invention, principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; that describes in the foregoing description and the specification just illustrates principle of the present invention; the present invention also has various changes and modifications without departing from the spirit and scope of the present invention, and these changes and improvements all fall in the claimed scope of the invention.The claimed scope of the present invention is defined by appending claims and equivalent thereof.
Claims (4)
1. the two-sided coding method of a material, it is characterized in that: described material is an adhesive material, steps of the method are:
One, adhesive material is passed through feed roller, with adhesive material expansion, stretching;
Two, adhesive material is peeled off the adhesive material plane materiel and the release liners of adhesive material by stripper roll, then the adhesive material plane materiel is passed through a registration roller, and release liners is passed through another registration roller;
Three, at the adhesive material plane materiel by after the registration roller, in glue face one side of adhesive material plane materiel an ink jet numbering machine is set, and it is carried out the coding of glue face;
Four, will fit by doubling roller simultaneously through adhesive material plane materiel after the coding of glue face and release liners.
Five, surface one side at the adhesive material plane materiel of the adhesive material that posts is provided with an ink jet numbering machine, and surperficial coding is carried out on its surface.
2. the two-sided coding method of a material, it is characterized in that: described material is an adhesive material, steps of the method are:
One, adhesive material is passed through feed roller, with adhesive material expansion, stretching;
Two, adhesive material is peeled off the adhesive material plane materiel and the release liners of adhesive material by stripper roll, then the adhesive material plane materiel is passed through a registration roller, and release liners is passed through another registration roller;
Three, at the adhesive material plane materiel by after the registration roller, in glue face one side of adhesive material plane materiel an ink jet numbering machine is set, and it is carried out the coding of glue face;
Four, will fit by doubling roller simultaneously through adhesive material plane materiel after the coding of glue face and release liners.
Five, surface one side in the release liners of the adhesive material that posts is provided with an ink jet numbering machine, and surperficial coding is carried out on its surface.
3. the two-sided coding method of a material, it is characterized in that: described material is an adhesive material, steps of the method are:
One, adhesive material is passed through feed roller, with adhesive material expansion, stretching;
Two, adhesive material is peeled off the adhesive material plane materiel and the release liners of adhesive material by stripper roll, then the adhesive material plane materiel is passed through a registration roller, and release liners is passed through another registration roller;
Three, after the adhesive material plane materiel passed through registration roller, one side was provided with an ink jet numbering machine on the surface of adhesive material plane materiel, and it is carried out the coding of glue face;
Four, will fit by doubling roller simultaneously through adhesive material plane materiel after the coding of glue face and release liners.
Five, surface one side in the release liners of the adhesive material that posts is provided with an ink jet numbering machine, and surperficial coding is carried out on its surface.
4. the two-sided coding method of a material is characterized in that: steps of the method are:
One, material is passed through feed roller, with material expansion, stretching;
Two, material passes through a registration roller by stripper roll again with material;
Three, after material passed through registration roller, one side was provided with an ink jet numbering machine on the surface of material, and it is carried out surperficial coding;
Four, will pass through doubling roller through the material after the surperficial coding.
Five, material is by after the doubling roller, and one side is provided with an ink jet numbering machine at the back side of material, and back side coding is carried out at its back side.