CN102041494A - 镀锌层钝化剂 - Google Patents

镀锌层钝化剂 Download PDF

Info

Publication number
CN102041494A
CN102041494A CN2009102341669A CN200910234166A CN102041494A CN 102041494 A CN102041494 A CN 102041494A CN 2009102341669 A CN2009102341669 A CN 2009102341669A CN 200910234166 A CN200910234166 A CN 200910234166A CN 102041494 A CN102041494 A CN 102041494A
Authority
CN
China
Prior art keywords
zinc coating
passivating agent
coating passivating
acid
percentage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2009102341669A
Other languages
English (en)
Inventor
张艳华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009102341669A priority Critical patent/CN102041494A/zh
Publication of CN102041494A publication Critical patent/CN102041494A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种镀锌层钝化剂,由铬酸、硫酸、醋酸、柠檬酸、水组成。本发明配方合理,使用效果好,生产成本低。

Description

镀锌层钝化剂
技术领域:
本发明涉及一种金属镀锌层钝化剂。
背景技术:
现有的金属镀锌层钝化剂,效果不理想,生产成本高。
发明内容:
本发明的目的在于提供一种使用效果好的镀锌层钝化剂。
本发明的技术解决方案是:
一种镀锌层钝化剂,其特征是:由下列重量百分比的成分组成:
所述的镀锌层钝化剂,由下列重量百分比的成分组成:
Figure B2009102341669D0000012
所述的镀锌层钝化剂,由下列重量百分比的成分组成:
Figure B2009102341669D0000021
本发明配方合理,使用效果好,生产成本低。
下面结合实施例对本发明作进一步说明。
具体实施方式:
实施例1:
一种镀锌层钝化剂,由下列重量百分比的成分组成:
Figure B2009102341669D0000022
实施例2:一种镀锌层钝化剂,由下列重量百分比的成分组成:
Figure B2009102341669D0000023

Claims (3)

1.一种镀锌层钝化剂,其特征是:由下列重量百分比的成分组成:
Figure F2009102341669C0000011
2.根据权利要求1所述的镀锌层钝化剂,其特征是:由下列重量百分比的成分组成:
Figure F2009102341669C0000012
3.根据权利要求1所述的镀锌层钝化剂,其特征是:由下列重量百分比的成分组成:
CN2009102341669A 2009-10-15 2009-10-15 镀锌层钝化剂 Pending CN102041494A (zh)