CN101781690A - 一种矿渣粉磨助磨剂 - Google Patents

一种矿渣粉磨助磨剂 Download PDF

Info

Publication number
CN101781690A
CN101781690A CN201010104529A CN201010104529A CN101781690A CN 101781690 A CN101781690 A CN 101781690A CN 201010104529 A CN201010104529 A CN 201010104529A CN 201010104529 A CN201010104529 A CN 201010104529A CN 101781690 A CN101781690 A CN 101781690A
Authority
CN
China
Prior art keywords
grinding aid
slag powder
slag
powder grinding
water glass
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010104529A
Other languages
English (en)
Inventor
徐福明
张平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201010104529A priority Critical patent/CN101781690A/zh
Publication of CN101781690A publication Critical patent/CN101781690A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种矿渣粉磨助磨剂,其特征在于,以重量计,包括:三乙醇胺15~20%,木钙10~15%,水玻璃15~20%,水45~55%。本发明在选择三乙醇胺和木钙的合理配比的同时,引入了以前没有作为矿渣助磨剂使用的水玻璃,经实验验证,采用本发明的矿渣粉磨助磨剂,可以提高矿渣粉磨产量30%左右,大大降低了能耗;同时,通过限定水玻璃的模数,产生了意想不到的效果,可以有效保证混合物不发生凝结,从而方便助磨剂的配制、储存、运输和使用。

Description

一种矿渣粉磨助磨剂
技术领域
本发明涉及一种对矿渣进行粉磨时使用的添加剂,具体涉及一种用于提高粉磨效率的矿渣粉磨助磨剂。
背景技术
矿渣是钢铁工业的高炉大量产生的一种副产品,为了有效利用资源,通常将其磨成细粉后作为水泥混合材使用。由于矿渣非常硬,细磨过程中需要消耗大量的能量和生产时间。通常,采用乙二醇或者含有乙二醇的混合物作为助磨剂,可以提高矿渣磨机产量,实现节能减排。
然而,目前采用这类助磨剂,通常只能提高产量10%左右。因此,寻求新的矿渣助磨剂,以进一步提高矿渣粉磨产量,减小能量消耗,受到本领域技术人员所的关注。
发明内容
本发明目的是提供一种矿渣粉磨助磨剂,以有效提高矿渣粉磨的产量,进一步实现节能减排。
为达到上述目的,本发明采用的技术方案是:一种矿渣粉磨助磨剂,以重量计,包括:
三乙醇胺    15~20%,
木钙        10~15%,
水玻璃      15~20%,
水          45~55%。
优选的技术方案,所述水玻璃的模数为1.75~2.1。
水玻璃通常被用作水泥增强剂或激发剂,未有在矿渣粉磨中作助磨剂的报道;另一方面,水玻璃中加入其它成份时,通常会发生凝结,形成类似棉花球状的析出物,导致无法使用。
本申请的发明人发现,常用水玻璃的模数为2.6~3.0,而当降低水玻璃的模数到1.75~2.1之间时,产生了意外的结果,即,可以在加入本申请技术方案中的其它成份后,保持水玻璃的液体状态,而不发生凝结。
使用时,在矿渣中,掺入重量百分比0.1%左右的上述助磨剂,即可以有效提高矿渣粉磨的产量。
由于上述技术方案运用,本发明与现有技术相比具有下列优点:
1.本发明在选择三乙醇胺和木钙的合理配比的同时,引入了以前没有作为矿渣助磨剂使用的水玻璃,经实验验证,采用本发明的矿渣粉磨助磨剂,可以提高矿渣粉磨产量30%左右,大大降低了能耗。
2.本发明通过限定水玻璃的模数,产生了意想不到的效果,可以有效保证混合物不发生凝结,从而方便助磨剂的配制、储存、运输和使用。
具体实施方式
下面结合实施例对本发明作进一步描述:
实施例一:一种矿渣粉磨助磨剂,以重量计,包括:
三乙醇胺    200千克,
木钙        150千克,
水玻璃      150千克,
水          500千克,
将上述组份混合均匀,获得1吨的助磨剂,其中,所述水玻璃的模数为1.75~2.1。
实施例二:采用实施例一的矿渣粉磨助磨剂分别在4台不同的矿渣粉磨机上进行试验,助磨剂添加量为总重量的0.1%,同时,采用市售助磨剂进行对比试验,试验情况如下表所示:
Figure GSA00000019366300031
从表中数据可以看出,在保证粉磨比表面积的前提下,市售助磨剂可以使产量提高5~10%,而本申请的助磨剂可以提高产量26~33%,具有显著的效果。

Claims (2)

1.一种矿渣粉磨助磨剂,其特征在于,以重量计,包括:
三乙醇胺    15~20%,
木钙        10~15%,
水玻璃      15~20%,
水          45~55%。
2.根据权利要求1所述的矿渣粉磨助磨剂,其特征在于:所述水玻璃的模数为1.75~2.1。
CN201010104529A 2010-02-03 2010-02-03 一种矿渣粉磨助磨剂 Pending CN101781690A (zh)