CN101699548A - Preparation method of removable adhesive label - Google Patents
Preparation method of removable adhesive label Download PDFInfo
- Publication number
- CN101699548A CN101699548A CN200910184997A CN200910184997A CN101699548A CN 101699548 A CN101699548 A CN 101699548A CN 200910184997 A CN200910184997 A CN 200910184997A CN 200910184997 A CN200910184997 A CN 200910184997A CN 101699548 A CN101699548 A CN 101699548A
- Authority
- CN
- China
- Prior art keywords
- layer
- oil
- facestock layer
- adhesive label
- printing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a preparation method of a removable adhesive label, comprising a plane materiel layer, a binding agent layer and a bottom complex binding layer. A bidirectional stretched polypropylene film layer is coated between the plane materiel layer and the binding agent layer. The method comprises the steps of printing a complex label, coating with water-based UV base oil and UV gloss oil, cutting film at one time; and discharging. The method has the advantages of low cost, environment protection, being capable of preparing adhesive label with out residue when being removed, and convenience, etc.
Description
Technical field
The present invention field that designs a package specifically is a kind of method for making of removable adhesive label.
Background technology
Along with the raising of rapid development of economy and people's level of consumption, commodity packaging has become indispensable part in its production link.The pleasing visual impact of people is not only given in a feast for the eyes commodity packaging, meanwhile the Reclaim of package waste that grows with each passing day is handled and has been brought a huge difficult problem to people again.Therefore, " green package " theory is arisen at the historic moment." green package " must contain two layers of meaning: (1), whole packaging process can not pollute and damage ecologic environment and health; (2), the wrappage of Shi Yonging must be the sustainable development materials of reproducible utilization.According to two conditions, wrappage must be to take from nature can constitute real green circulation by back to nature again, make the mankind in the beautiful impression that the commodity packaging of enjoying modern fineness brings, can have good living environment and lasting resource provision again.
And any commodity all need labeling " to identify the card body ".More than 50 hundred million populations are arranged in the world, and its daily consumer goods are considerable.So can imagine, how huge the demand of labeling and the output value are.The basic composition synoptic diagram of labeling as shown in Figure 1.Relevant data has shown that the packaging industry of China, especially labeling industry are since coming into effect monitoring system, and annual rate of growth all reaches 20%.In quantity, the labeling total amount reaches more than 1,000,000,000 square metre.From the growth of labeling consumption, to 2006, global labeling consumption will rise 6.2%, compare with 20,400,000,000 square metres of calendar year 2001, will rise to 33,000,000,000 square metres.The labeling market of developing will increase with double-digit ratio, and the market growth speed of having developed is 3%-5%.But growth rate is unevenness, wherein, China's year growth by 15%, U.S.'s year increases by 5%, and Eastern Europe year increases by 12%, and Latin American's year increases by 10%, and Europe can reach 3%-5% with the growth rate of Japan.The growth rate in China, Latin American, labeling market, Europe (east) is the fastest.The film labeling of rotary press printing and in-mold label, cut and pile up labeling and also will grow steadily.As the organic component of commodity packaging, the huge labeling of output needs, also must implement the theory of green package, is applied to take from nature and returns in nature.In the near future, the enterprise of not production environmental protection labeling will inevitably be eliminated by market.The environmental protection of labeling is mainly reflected in following three aspect contents: the first, the material therefor of labeling itself is environment-friendly materials; The second, the used adhesive of labeling will meet environmental protection standard; What three, labeling was wanted to finish clears up from the commodity external packing, do not have residual, the recycling of convenience goods external packing.
Summary of the invention
The invention provides a kind of method for making of removable adhesive label, have the cost material environment friendly, and the noresidue when removing of the adhesive label of made, the simple advantage of method for making.
Technical scheme of the present invention is:
A kind of method for making of removable adhesive label is characterized in that: may further comprise the steps:
(1), on the one side of facestock layer, apply one deck bidirectional stretching polypropylene film, coating layer of adhesive layer on the bidirectional stretching polypropylene film layer then, bonding agent is selected Acrylic Pressure Sensitive Adhesive for use, facestock layer is undertaken bonding compound by adhesive phase and bottom
(2), on the one side of the uncoated bonding agent of facestock layer, carry out water color ink 4 look printings, oil at the bottom of applying one deck water-based UV on the one side facestock layer after the printing then, adopt the UV lustring machine to applying the UV oil polish on the printing facestock layer that applied end oil, strengthen the light fastness of printing ink;
(3), adopt computer photograph cross cutting knife plate by specification requirement, with the last labeling of crossing UV oil on automatic die cutter once property finish the cross cutting waste discharge, product.
The method for making of described removable adhesive label is characterized in that: described facestock layer is selected 80-120g/m for use
2Art paper; Described bottom is selected 80-100g/m for use
2Ox-hide body paper or art paper; The thickness of described bidirectional stretching polypropylene film layer is the 1-1.4 silk.
The present invention applies one deck bidirectional stretching polypropylene film layer between facestock layer and adhesive phase, rapid wear is not broken for facestock layer when removing; Described facestock layer after the printing, on apply one deck water-based UV before the UV oil polish at the bottom of oil, help the flatness and the smooth finish of printing surface; Described employing computer photograph cross cutting knife plate, with the last labeling of crossing UV oil on automatic die cutter once property finish the degree of accuracy that the cross cutting waste discharge helps controlling the size of adhesive label.
Embodiment
A kind of method for making of removable adhesive label is characterized in that: may further comprise the steps:
(1), at 80-120g/m
2The one side of art paper on to apply a layer thickness be 1.2 Acrylic Pressure Sensitive Adhesive, coating one deck Acrylic Pressure Sensitive Adhesive layer on the Acrylic Pressure Sensitive Adhesive layer then is with 80-100g/m
2The ox-hide body paper or art paper by Acrylic Pressure Sensitive Adhesive layer and 80-120g/m
2Art paper carry out bonding compound;
(2), on the one side of the uncoated bonding agent of facestock layer, carry out water color ink 4 look printings, oil at the bottom of applying one deck water-based UV on the one side facestock layer after the printing then, adopt the UV lustring machine to applying the UV oil polish on the printing facestock layer that applied end oil, strengthen the light fastness of printing ink;
(3), adopt computer photograph cross cutting knife plate by specification requirement, with the last labeling of crossing UV oil on automatic die cutter once property finish the cross cutting waste discharge, product.
Claims (2)
1. the method for making of a removable adhesive label is characterized in that: may further comprise the steps:
(1), on the one side of facestock layer, applies one deck bidirectional stretching polypropylene film, on the bidirectional stretching polypropylene film layer, be coated with the layer of adhesive layer then, bonding agent is selected Acrylic Pressure Sensitive Adhesive for use, and facestock layer is undertaken bonding compound by adhesive phase and bottom;
(2), on the one side of the uncoated bonding agent of facestock layer, carry out water color ink 4 look printings, oil at the bottom of applying one deck water-based UV on the one side facestock layer after the printing then, adopt the UV lustring machine to applying the UV oil polish on the printing facestock layer that applied end oil, strengthen the light fastness of printing ink;
(3), adopt computer photograph cross cutting knife plate by specification requirement, with the last labeling of crossing UV oil on automatic die cutter once property finish the cross cutting waste discharge, product.
2. the method for making of removable adhesive label according to claim 1, it is characterized in that: described facestock layer is selected 80-120g/m for use
2Art paper; Described bottom is selected 80-100g/m for use
2Ox-hide body paper or art paper; The thickness of described bidirectional stretching polypropylene film layer is the 1-1.4 silk.