CN101676747B - 一种适用于铀资源勘查的低本底地气勘查方法 - Google Patents

一种适用于铀资源勘查的低本底地气勘查方法 Download PDF

Info

Publication number
CN101676747B
CN101676747B CN 200810211220 CN200810211220A CN101676747B CN 101676747 B CN101676747 B CN 101676747B CN 200810211220 CN200810211220 CN 200810211220 CN 200810211220 A CN200810211220 A CN 200810211220A CN 101676747 B CN101676747 B CN 101676747B
Authority
CN
China
Prior art keywords
polyester film
uranium
ground vapour
explorers
earth atmosphere
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN 200810211220
Other languages
English (en)
Other versions
CN101676747A (zh
Inventor
韩绍阳
谈成龙
田华
柯丹
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beijing Research Institute of Uranium Geology
Original Assignee
Beijing Research Institute of Uranium Geology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beijing Research Institute of Uranium Geology filed Critical Beijing Research Institute of Uranium Geology
Priority to CN 200810211220 priority Critical patent/CN101676747B/zh
Publication of CN101676747A publication Critical patent/CN101676747A/zh
Application granted granted Critical
Publication of CN101676747B publication Critical patent/CN101676747B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明属于铀资源勘查领域,具体公开一种适用于铀资源勘查的低本底地气勘查方法:将聚酯膜地气探测器浸泡于超声波清洗器中的去离子水中,用超声波、去离子水清洗至少90分钟;将聚酯膜地气探测器晾干后制成地气探测器;设置等间距的测线,每条测线上多个点;在每一个测点下方挖深坑,将悬有细线的聚酯膜地气探测器放置在坑底;聚酯膜地气探测器的埋藏时间至少为30天,到期后,取出各个测点对应的聚酯膜地气探测器;聚酯膜地气探测器经灰化、酸溶预处理后,再用等离子体质谱仪实施样品中的铀测量、并进行聚酯膜地气探测器重量归一化处理后,获得纳米级铀含量。本发明的方法在铀资源勘查中获得隐伏铀矿化引起的高信噪比纳米级铀微粒信息。

Description

一种适用于铀资源勘查的低本底地气勘查方法
技术领域
本发明属于铀资源勘查领域,具体涉及一种适用于铀资源勘查的低本底地气勘查方法。
背景技术
在隐伏铀资源勘查中,地气测量方法是一种定位深部铀矿体的有效方法。地气找铀方法测量的采样对象是:流经矿体的地气所携带至土壤层中的纳米级铀微粒,地气(铀)测量所使用的探测器是聚酯膜,测量的是天然附着在聚酯膜上的微量铀。从市场购置回来的聚脂膜,由于生产厂家的不同而其所含的杂质、污垢含量也不一样,如果直接用作地气探测器,那么其所含的杂质、污垢等就会成为地气测量的一种干扰;聚酯膜作为找矿专用的地气探测器,在使用前必须经净化处理(去杂质),降低其本底铀含量;地气探测器上的本底铀含量越低,则在铀矿体上测得的微量铀信噪比将越大。国内有关部门多以常态清水漂洗用做地气探测器的聚酯膜,在降低杂质方面取得了一定效果,但仍然洗不干净;在铀资源勘查中,地气探测器的野外埋藏方法和最佳的地气探测器埋藏时间,也未见报道;国内外的地气测量方法仍以剖面测量为主,难以消除体积效应的影响。
发明内容
本发明目的在于提供一种适用于铀资源勘查的低本底地气勘查方法,该勘查方法在铀资源勘查中可获得隐伏铀矿化引起的高信噪比纳米级铀微粒信息。
实现本发明目的的技术方案:一种适用于铀资源勘查的低本底地气勘查方法,它包括以下步骤:
(1)把拟用做聚酯膜地气探测器的聚酯膜裁减成坯料;
(2)将超声波清洗器置于净化工作台里,在超声波清洗器中加入去离子水;
(3)将聚酯膜地气探测器浸泡于超声波清洗器中的去离子水中,在常温、常压条件下,应用超声波、去离子水清洗时间至少90分钟;
(4)将去离子水中的聚酯膜地气探测器晾干且称重后,封装在保鲜袋中,便制成了用于铀矿勘查的低本底聚酯膜地气探测器;
(5)在铀资源勘查区,设置等间距的测线,每条测线上取点距和线距相等的多个点;在每一个测点下方挖50cm~60cm深的深坑,将坑底部整平,并在现场将悬有细线的聚酯膜地气探测器,通过细线固定在半球形塑料容器的内侧顶部,将半球形容器开口向下,放置在坑底;在深坑的上面用塑料布遮封,最后在其上面用浮土覆盖;
(6)应用地气方法寻找隐伏铀矿时,将聚酯膜地气探测器的埋藏时间至少为30天,埋藏时间到期后,取出各个测点对应的聚酯膜地气探测器,且封装在塑料保鲜袋中;
(7)对聚酯膜地气探测器经灰化、酸溶预处理后,再用等离子体质谱仪实施样品中的铀测量、并进行聚酯膜地气探测器重量归一化处理后,可获得聚酯膜地气探测器中的纳米级铀含量。
本发明的有益技术效果在于:本发明综合应用超声波、去离子水清洗的聚酯膜地气探测器,可极大地减低探测器本身引起的各种干扰噪声;提出的野外地气采集和分析测试方法容易操作,有利于获得高信噪比的纳米级铀异常信息;提出的点距和线距相等的面积测量方法,相对于“剖面测量”方法而言,有利于消除体积效应的影响;采用多重分形空间插值方法,在保持和增强局部异常信息方面具有良好的应用效果。
具体实施方式
下面结合实施例对本发明所提供的一种适用于铀资源勘查的低本底地气勘查方法作进一步详细说明。
实施例1
一种适用于铀资源勘查的低本底地气勘查方法,它包括以下步骤:
(1)在室内把拟用做聚酯膜地气探测器的聚酯膜裁减成4cm×4cm的坯料。
(2)在室内,将公知的超声波清洗器置于净化工作台里,在超声波清洗器中加入一半容积的去离子水。
(3)将聚酯膜地气探测器浸泡于超声波清洗器中的去离子水中,在常温、常压条件下,应用超声波、去离子水清洗时间达90分钟。
(4)将去离子水中的聚酯膜地气探测器晾干且称重后,封装在保鲜袋中,编号后,便制成了用于铀矿勘查的低本底聚酯膜地气探测器。
(5)在铀资源勘查区,设置20条等间距的测线,每条测线上取点距和线距相等的多个点;在每一个测点下方挖50cm深的深坑,将坑底部整平,并在现场将悬有细线的聚酯膜地气探测器,通过细线固定在半球形塑料容器的内侧顶部,将半球形容器开口向下,放置在坑底;在深坑的上面用塑料布遮封(防漏气、挡雨水),最后在其上面用浮土覆盖。
(6)应用地气方法寻找隐伏铀矿时,将聚酯膜地气探测器的埋藏时间设为30天,时间到后,取出各个测点对应的聚酯膜地气探测器(避免探测器受人为污染),且封装在塑料保鲜袋中,编号封存。
(7)在实验室里,对聚酯膜地气探测器经公知的灰化、酸溶预处理后,再用公知的等离子体质谱仪实施样品中的铀测量、并进行聚酯膜地气探测器重量归一化处理后,可获得聚酯膜地气探测器中的纳米级铀含量。
(8)采用公知的多重分形插值方法绘制出研究区地气中铀含量等值图;然后应用公知的统计分析方法圈定铀异常下限,对铀矿化的空间位置进行推断。
实施例2
一种适用于铀资源勘查的低本底地气勘查方法,它包括以下步骤:
(1)在室内把拟用做聚酯膜地气探测器的聚酯膜裁减成6cm×6cm的坯料。
(2)在室内,将公知的超声波清洗器置于净化工作台里,在超声波清洗器中加入三分之二容积的去离子水。
(3)将聚酯膜地气探测器浸泡于超声波清洗器中的去离子水中,在常温、常压条件下,应用超声波、去离子水清洗时间达150分钟。
(4)将去离子水中的聚酯膜地气探测器晾干且称重后,封装在保鲜袋中,编号后,便制成了用于铀矿勘查的低本底聚酯膜地气探测器。
(5)在铀资源勘查区,设置30条等间距的测线,每条测线上取点距和线距相等的多个点;在每一个测点下方挖55cm深的深坑,将坑底部整平,并在现场将悬有细线的聚酯膜地气探测器,通过细线固定在半球形塑料容器的内侧顶部,将半球形容器开口向下,放置在坑底;在深坑的上面用塑料布遮封(防漏气、挡雨水),最后在其上面用浮土覆盖。
(6)应用地气方法寻找隐伏铀矿时,将聚酯膜地气探测器的埋藏时间设为40天,时间到后,取出各个测点对应的聚酯膜地气探测器(避免探测器受人为污染),且封装在塑料保鲜袋中,编号封存。
(7)在实验室里,对聚酯膜地气探测器经公知的灰化、酸溶预处理后,再用公知的等离子体质谱仪实施样品中的铀测量、并进行聚酯膜地气探测器重量归一化处理后,可获得聚酯膜地气探测器中的纳米级铀含量。
(8)采用公知的多重分形插值方法绘制出研究区地气中铀含量等值图;然后公知的应用统计分析方法圈定铀异常下限,对铀矿化的空间位置进行推断。
实施例3
一种适用于铀资源勘查的低本底地气勘查方法,它包括以下步骤:
(1)在室内把拟用做聚酯膜地气探测器的聚酯膜裁减成8cm×8cm的坯料。
(2)在室内,将公知的超声波清洗器置于净化工作台里,在超声波清洗器中加入五分之四容积的去离子水。
(3)将聚酯膜地气探测器浸泡于超声波清洗器中的去离子水中,在常温、常压条件下,应用超声波、去离子水清洗时间达180分钟。
(4)将去离子水中的聚酯膜地气探测器晾干且称重后,封装在保鲜袋中,编号后,便制成了用于铀矿勘查的低本底聚酯膜地气探测器。
(5)在铀资源勘查区,设置40条等间距的测线,每条测线上取点距和线距相等的多个点;在每一个测点下方挖60cm深的深坑,将坑底部整平,并在现场将悬有细线的聚酯膜地气探测器,通过细线固定在半球形塑料容器的内侧顶部,将半球形容器开口向下,放置在坑底;在深坑的上面用塑料布遮封(防漏气、挡雨水),最后在其上面用浮土覆盖。
(6)应用地气方法寻找隐伏铀矿时,将聚酯膜地气探测器的埋藏时间设为50天,时间到后,取出各个测点对应的聚酯膜地气探测器(避免探测器受人为污染),且封装在塑料保鲜袋中,编号封存。
(7)在实验室里,对聚酯膜地气探测器经公知的灰化、酸溶预处理后,再用公知的等离子体质谱仪实施样品中的铀测量、并进行聚酯膜地气探测器重量归一化处理后,可获得聚酯膜地气探测器中的纳米级铀含量。
(8)采用公知的多重分形插值方法绘制出研究区地气中铀含量等值图;然后公知的应用统计分析方法圈定铀异常下限,对铀矿化的空间位置进行推断。

Claims (1)

1.一种适用于铀资源勘查的低本底地气勘查方法,其特征在于:它包括以下步骤:
(1)把拟用做聚酯膜地气探测器的聚酯膜裁减成坯料;
(2)将超声波清洗器置于净化工作台里,在超声波清洗器中加入去离子水;
(3)将聚酯膜地气探测器浸泡于超声波清洗器中的去离子水中,在常温、常压条件下,应用超声波、去离子水清洗时间至少90分钟;
(4)将去离子水中的聚酯膜地气探测器晾干且称重后,封装在保鲜袋中,便制成了用于铀矿勘查的低本底聚酯膜地气探测器;
(5)在铀资源勘查区,设置等间距的测线,每条测线上取点距和线距相等的多个点;在每一个测点下方挖50cm~60cm深的深坑,将坑底部整平,并在现场将悬有细线的聚酯膜地气探测器,通过细线固定在半球形塑料容器的内侧顶部,将半球形容器开口向下,放置在坑底;在深坑的上面用塑料布遮封,最后在其上面用浮土覆盖;
(6)应用地气方法寻找隐伏铀矿时,将聚酯膜地气探测器的埋藏时间至少为30天,埋藏时间到期后,取出各个测点对应的聚酯膜地气探测器,且封装在塑料保鲜袋中;
(7)对聚酯膜地气探测器经灰化、酸溶预处理后,再用等离子体质谱仪实施样品中的铀测量、并进行聚酯膜地气探测器重量归一化处理后,可获得聚酯膜地气探测器中的纳米级铀含量。
CN 200810211220 2008-09-18 2008-09-18 一种适用于铀资源勘查的低本底地气勘查方法 Active CN101676747B (zh)