Summary of the invention
Primary technical problem to be solved by this invention is to provide a kind of toy for children wax rope at the situation of prior art, this wax rope can be bonded on the paper, on the wall, perhaps on the desktop, can make various plane patterns and space pattern, can be used as children, teen-age toy and educational aid, edify children's creation of art thinking, the article that also Pasting is lighter certainly such as the little scraps of paper.
Another technical problem to be solved by this invention is the situation at prior art, and a kind of production method of toy for children wax rope is provided, and method is simple and practical.
Another technical problem to be solved by this invention is the situation at prior art, and a kind of process units of toy for children wax rope is provided, and is simple and practical.
The present invention solves the technical scheme that above-mentioned primary technical problem adopts: a kind of toy for children wax rope, it is characterized in that including cotton rope, and the cotton rope surface impregnation has wax.
Used wax comprises: paraffin and synthetic wax (microwax, Tissuemat E etc.), and these waxes use separately, or mixing by a certain percentage, preferably add the tackifying resin of proper proportion, vaseline or liquid polyisobutene when adopting synthetic wax, it is colourless making formed wax, or white.Having certain viscosity tack-free, is solid-state at normal temperatures.
What is called is not touched with one's hand, and when being meant under the normal temperature with hand kneading wax rope, the constituent of wax rope can obviously not stick on hand.So-called toughness is meant with the wax rope to stick on the materials such as clean glass, plank, the scraps of paper, cardboard that when these materials were vertically placed, the wax rope can not fall down voluntarily.
As recommended formula, the set of dispense of prescription 1 is such as following:
40~70 parts in paraffin
30~50 parts of albolene
0~40 part of synthetic wax
0~20 part of tackifying resin;
Another proportioning is as follows:
30~90 parts of microwaxes
10~70 parts of polyisobutene;
Have proportioning as follows again:
30~90 parts of Tissuemat Es
10~70 parts of polyisobutene;
Described umber is a mass fraction.
Selected wax comprises paraffin, microwax, and Tissuemat Es etc. also can be other wax, perhaps they mix mutually by a usual practice.But melting range is 50~120 ℃ in principle.Tackifying resin can be ester gum or oil resin etc., in order to obtain suitable viscosity.Albolene and polyisobutene etc., be softening agent be again binding agent.It makes wax body softness, can adhere to cotton rope well again.
Used cotton rope can be a sub-thread, and two strands, three strands until five strands.Thickness gets final product according to requirement of client, and material is polyacrylonitrile preferably, natural wool, terylene, spandex or their blending thing.But heat-resisting will be above 150 ℃.
Described wax can include appropriate amount of auxiliary materials, and auxiliary material is pigment or/and essence, makes the wax rope have certain color and fragrance.
At last, described wax surface process polishing.
The present invention solves the technical scheme that above-mentioned another technical problem adopts: a kind of production method of toy for children wax rope is characterized in that step is:
(1). join wax: make wax want toughness at normal temperatures, do not touch with one's hand;
(2). route selection: select sub-thread, the line yarn more than two strands or three strands is as cotton rope;
(3). waxdip: cotton rope is by heating container, and the thawing of the wax of heating container inside is liquid, thereby makes the cotton rope dipping go up wax;
(4). cooling: cooling just come out the wax rope, make the wax liquid solid that congeals into;
Further, production method also includes
(5). cut off;
(6). packing.
Be convenient to actual production manufacturing and use.
Described waxdip is to carry out in a waxdip pond, so-called waxdip pond is exactly a heater, heating-up temperature is 80~150 ℃, there is one or several transfer roller its inside, can guarantee that cotton rope fully soaks in wax liquid and extension wax, hole, one to 12 road, opposing parallel are in twos respectively opened in the vertical both sides of transfer roller, the turnover in hole becomes horn-like, makes the discrepancy of cotton rope smooth and easy.
Described cooling can be adopted air-conditioning, water-cooled, and air cooling, temperature is lower than 70 ℃, gets final product.
The present invention solves the technical scheme that above-mentioned another technical problem adopts: a kind of process units of toy for children wax rope, it is characterized in that being used to contain the heating container of wax as the waxdip pond, be furnished with a plurality of transfer rollers in the heating container, thereby make cotton rope walk around the transfer roller dipping successively and go up the wax that melts, one end of cotton rope extends the heating container outside and is connected with the barrel of line material, the other end of cotton rope extends the heating container outside, carries through haulage drum to be connected to cutting mechanism.
Be furnished with the cooling device that is used for the cooling of wax rope between described haulage drum and the heating container.
Compared with prior art, the invention has the advantages that: this wax rope toughness but do not touch with one's hand can be bonded on the paper, on the wall, perhaps on the desktop, can make various plane patterns and space pattern, can be used as children, teen-age toy and educational aid, edify children's creation of art thinking, certainly the article that also Pasting is lighter such as little scraps of paper or the like, and simple and practical production method, the efficient height, with low cost, process units is simple and practical.
The specific embodiment
Embodiment describes in further detail the present invention below in conjunction with accompanying drawing.
Process units is such: a kind of process units of toy for children wax rope, it adopts the heating container 2 that contains wax as the waxdip pond, be furnished with a plurality of transfer rollers 3 in the heating container 2, thereby make cotton rope walk around the transfer roller dipping successively and go up the wax that melts, one end of cotton rope extends the heating container outside and is connected with the barrel 1 of line material, the other end of cotton rope extends the heating container outside, carries through haulage drum 4 to be connected to cutting mechanism 5.Be furnished with the cooling device 6 that is used for the cooling of wax rope between haulage drum 4 and the heating container 2.
The cotton rope that at first will hang wax twines on the roller of barrel 1 of online material, and this roller is on line yarn roller.One end of cotton rope is passed the import that the waxdip pond is a heating container 2, and the bottom by transfer roller 3 in the waxdip pond is pulled through the cooling zone by outlet again, under cooling device 6 coolings, is entangled in then on another thicker roller (wax wire roller), as haulage drum 4.Add wax and softening agent by proportioning in the waxdip pond, be heated to 100~120 ℃, treat that wax melts after, the roller at two (line yarn roller and wax wire roller) rotates, waxdip cooling successively, be wound on another roller after, carry to be connected to cutting mechanism 5, cut off through cutting machine, packing obtains product of the present invention.
Embodiment 1.
Select three strands of acrylic fibers lines for use, green white four kinds of color reddish yellow, construction skill strictly according to the facts is described, pass the waxdip pond, the cooling zone is entangled on the wax wire roller, pressed 45: 25: 5 in the waxdip pond: 30 mass ratio adds paraffin, Tissuemat E, ester gum and albolene, be heated to 120 ℃, after treating its whole thawing, with fast rotational line yarn roller, wax rope roller, cut off packing then.
Embodiment 2.
Select 5 strands of acrylic fibers lines for use, green white four kinds of color reddish yellow, construction skill strictly according to the facts is described, pass the waxdip pond, the cooling zone is entangled on the wax wire roller, and the mass ratio by 80: 20 in the waxdip pond adds Tissuemat E and liquid polyisobutene, be heated to 120 ℃, after treating its whole thawing, with fast rotational line yarn roller, wax rope roller, cut off packing then.
Embodiment 3.
Select three strands of acrylic fibers spandex union twist yarns for use, green white black five kinds of color reddish yellow, construction skill strictly according to the facts is described, pass the waxdip pond, the cooling zone is entangled on the wax wire roller, and the mass ratio by 90: 10 in the waxdip pond adds microwax and liquid polyisobutene, be heated to 120 ℃, after treating its whole thawing, with fast rotational line yarn roller, wax rope roller, cut off packing then.
Embodiment 4.
Select two strands of wool blended lines for use, green white black purple six kinds of color reddish yellow, construction skill strictly according to the facts is described, pass the waxdip pond, the cooling zone is entangled on the wax wire roller, pressed 40: 22: 8 in the waxdip pond: 30 mass ratio adds paraffin, microwax, ester gum and albolene, be heated to 120 ℃, after treating its whole thawing, with fast rotational line yarn roller, wax rope roller, cut off packing then.
Embodiment 5.
Select two strands of wool blended lines for use, green white black purple six kinds of color reddish yellow, construction skill strictly according to the facts is described, passes the waxdip pond, the cooling zone, be entangled on the wax wire roller, pressed 60: 30: 8 in the waxdip pond: 2 mass ratio adds paraffin, albolene, microwax and ester gum, is heated to 120 ℃, after treating its whole thawing, rotational line yarn roller and wax rope roller cut off then, packing.
Embodiment 6.
Select three strands of wool blended lines for use, color is white, and construction skill strictly according to the facts is described, pass the waxdip pond, the cooling zone is entangled on the wax wire roller, presses 40: 34: 20 in the waxdip pond: 5: 1 mass ratio adds paraffin, albolene, Tissuemat E and ester gum and essence, be heated to 120 ℃, after treating its whole thawing, with fast rotational line yarn roller, wax rope roller, cut off packing then.