CN101468908A - 一种环保健康电气石陶制品 - Google Patents
一种环保健康电气石陶制品 Download PDFInfo
- Publication number
- CN101468908A CN101468908A CNA2007101145648A CN200710114564A CN101468908A CN 101468908 A CN101468908 A CN 101468908A CN A2007101145648 A CNA2007101145648 A CN A2007101145648A CN 200710114564 A CN200710114564 A CN 200710114564A CN 101468908 A CN101468908 A CN 101468908A
- Authority
- CN
- China
- Prior art keywords
- tourmaline
- fictile
- environment protection
- human body
- far infrared
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供了一种环保健康电气石陶制品,由电气石、陶土按如下重量比配料组成:主料电气石的掺入量为5-80份,辅料陶土的掺入量为20-95份。有以下特点:1.可以发射接近身体4-18微米的远红外波线;2.可以产生负离子;3.具有杀菌作用。可以广泛适用于装饰、建筑、城市绿化、器皿、保健理疗、水处理等。本发明可有效补充人体负电位能量,使细胞保持极化电位,恢复人体弱碱性体液;远红外辐射产生温热效应,使血管扩张,血液循环和微循环,大大改善睡眠质量。
Description
技术领域
本发明属于电气石应用领域,具体涉及一种环保健康电气石陶制品。
背景技术
研究证实,电气石是地球上存在的矿物质中,唯一带永久电极的晶体。在不需任何附加条件和任何人工助力的情况下,只要吸收太阳的光能,,其表面就能够产生电荷。电气石集“远红外线发射仪”、“空气维生素”、“细胞活化剂”、“生物电平衡仪”等诸多美誉于一身,成为世界上所有矿物材料中罕见的保健资源。电气石所产生的负离子、微电流和远红外线对改善人体健康和生存环境十分有益,使用含有电气石的产品,其流动的0.06mA微电流,可补充和平衡人体的生物电;其散发的负离子可平衡人体体液,使酸性体液碱性化;其释放的远红外线可起到扩张毛细血管、促进血液循环、活化细胞、促进新陈代谢等作用,同时可阻断各种有害电磁辐射对人体的伤害。因此,含有电气石的产品能从生命的本质角度改善人体的健康状况,增强人体的免疫功能,从而达到祛病强身之功效。
因此对电气石的应用技术应运而生,如中国专利200410079022,提出了一种含有电气石的陶瓷砖的生产方法,但它在制备过程中的温度过高,破坏了电气石的功效。
发明内容
本发明针对上述问题,提出了一种环保健康电气石陶制品,真正发挥电气石独有功效,可有效补充人体负电位能量,使细胞保持极化电位,恢复人体弱碱性体液;远红外辐射产生温热效应,使血管扩张,血液循环和微循环,大大改善睡眠质量。
本发明的技术方案如下:
本发明提供了一种环保健康电气石陶制品,由电气石、陶土按如下重量比配料组成:主料电气石的掺入量为5—80份,辅料陶土的掺入量为20—95份。
本发明提供一种环保健康电气石陶制品,主辅料的颗粒细度为200目以上,越细越好。
本发明提供一种环保健康电气石陶制品按正常陶制品工艺生产,在600---950℃温度下,4---8小时烧成。
具体实施方式
淄博神邦科技新材料科技公司依据以上方案制成的环保健康电气石陶制品,有以下特点:1、可以发射接近身体4---18微米的远红外波线;2、可以产生负离子;3、具有杀菌作用。可以广泛适用于装饰、建筑、城市绿化、器皿、保健理疗、水处理等。
电气石、陶土按如下重量比配料
本发明的制作工艺同正常的陶制品制作工艺:物料选配→将电气石磨成200目以上→与陶土进入球磨机混料均匀→成型→烧成处理→制成品。
Claims (3)
1、一种环保健康电气石陶制品,由电气石、陶土组成,其特征在于:主料电气石的掺入量为15—80%,辅料陶土的掺入量为20—85%。
2、根据权利要求1所述的一种环保健康电气石陶制品,其特征在于:主辅料的颗粒细度为200目以上。
3、根据权利要求1或2所述的一种环保健康电气石陶制品,其特征在于:在600---950℃温度下,4---8小时烧成。