CN101342093A - 修复不锈钢牙冠口腔内焊接工艺 - Google Patents

修复不锈钢牙冠口腔内焊接工艺 Download PDF

Info

Publication number
CN101342093A
CN101342093A CNA2008101392086A CN200810139208A CN101342093A CN 101342093 A CN101342093 A CN 101342093A CN A2008101392086 A CNA2008101392086 A CN A2008101392086A CN 200810139208 A CN200810139208 A CN 200810139208A CN 101342093 A CN101342093 A CN 101342093A
Authority
CN
China
Prior art keywords
stainless steel
oral cavity
dentis
corona dentis
welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2008101392086A
Other languages
English (en)
Inventor
周百政
周培莒
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA2008101392086A priority Critical patent/CN101342093A/zh
Publication of CN101342093A publication Critical patent/CN101342093A/zh
Pending legal-status Critical Current

Abstract

本发明提供了一种修复不锈钢牙冠口腔内焊接工艺,在修复不锈钢牙冠与相邻牙齿(或牙冠)的缝隙时,牙冠不需要拆换,而是用电容储能脉冲焊接机在口腔内直接焊接,通过在牙缝两边或单边修磨坡口,预制T型或L型不锈钢镶嵌件,多点焊接,上下牙齿咬合修磨几个步骤后,即可完成修复。该法修复的牙齿缝隙质量高,效果好,费用低,安全可靠,患者无痛苦,而且能彻底解决进食塞牙的问题。

Description

修复不锈钢牙冠口腔内焊接工艺
技术领域
本发明属于口腔卫生领域,具体地说涉及一种修复不锈钢牙冠口腔内焊接工艺。
背景技术
牙科医院常对一些损坏的牙齿加套不锈钢牙冠进行修复。在经过一段时间的使用后,不锈钢牙冠和相邻牙齿(或不锈钢牙冠)之间的缝隙会逐渐扩大,导致食物易塞入其中。而患者在每次饭后都要剔牙缝,更加剧了牙齿的破坏。牙科医院目前对这种情况的修复办法是:把原不锈钢牙冠切割去掉,重新加工新的不锈钢牙冠。这种方法不但医疗费用高,并且由于需要经过拆牙冠、做牙模、制作不锈钢牙冠、以及安装磨合等步骤,需要很长的周期,增加了患者的痛苦。
发明内容
本发明提供了一种修复不锈钢牙冠口腔内焊接工艺,解决了传统的修复方法医疗费用高、修复周期长的缺点。
本发明的技术方案是这样实现的:修复不锈钢牙冠口腔内焊接工艺,利用电容储能焊接机,其正负极分别连接不锈钢牙冠和焊笔,其工艺步骤如下:
①修磨不锈钢牙冠和相邻牙齿或不锈钢牙冠,在缝隙之间开坡口;
②制备“T”型或“L“型不锈钢镶嵌件;
③焊笔压住不锈钢镶嵌件,接通牙科专用焊接机脚踏开关;
所述的焊笔的笔尖用银及银合金材料制作;
所述的不锈钢T型镶嵌件用于双边开坡口,不锈钢L型镶嵌件用于单边开坡口;
焊笔尖接触处的接触面积控制在0.8-1.2mm2之间;
焊接参数为:焊接时间:<ms级,脉冲电流:>103A。
本发明的有益效果是:在修复不锈钢牙冠与相邻牙齿(或不锈钢牙冠)的缝隙时,不锈钢牙冠不需要拆换,而是用电容储能焊接机在口腔内直接焊接,通过在牙缝两边或单边修磨坡口,预制T型或L型不锈钢镶嵌件,多点焊接,上下牙齿咬合修磨几个步骤后,即可完成修复。该法修复的牙齿缝隙质量高,效果好,费用低,安全可靠,患者无痛苦,而且能彻底解决进食塞牙的问题。
说明书附图
图1为本发明的待修复的不锈钢牙冠示意图;
图2为本发明的不锈钢牙冠的修磨坡口示意图;
图3为本发明的T型不锈钢镶嵌件或L型不锈钢镶嵌件示意图;
图4为本发明的焊接工艺示意图。
零件说明:1、不锈钢牙冠,2、相邻牙齿(或不锈钢牙冠),3、T型不锈钢镶嵌件或L型不锈钢镶嵌件,4、电容储能焊接机,5、电源负极,6、焊笔,7、焊机脚踏开关。
具体实施方式
下面结合附图对本发明作进一步描述:不锈钢牙冠(1)和相邻牙齿(或不锈钢牙冠)(2)之间产生缝隙δ,如图1所示。在缝隙两边的不锈钢牙冠(1)和相邻牙齿(或不锈钢牙冠)(2)上修磨坡口。根据情况可以修磨双边坡口,也可以修磨单边坡口,如图2所示。制备尺寸合适的不锈钢T型不锈钢镶嵌件(3),用于双边开坡口,或L型不锈钢镶嵌件(3),用于单边开坡口,如图3所示。电容储能焊接机(4)的焊接电源负极(5)以较大接触面积夹紧在不锈钢牙冠(1)上,正极端接焊笔(6),笔尖用银及银合金材料制作,笔尖压住不锈钢镶嵌件(3),与不锈钢牙冠(1)之间产生一定压力,踩下焊机脚踏开关(7),焊机的脉冲电流使焊笔尖接触处(接触面积控制在1mm2左右)的不锈钢镶嵌件(3)与不锈钢牙冠(1)之间产生电阻热,接点处瞬间产生冶金熔接,形成一个1mm2左右的焊点,由于作用时间短(<ms级),脉冲电流大(>103A),热作用区极少,热量尚来不及扩散,焊接过程结束,如图4所示。根据实际情况可以多焊几个焊点,形成较大焊接面以增加强度。为防止连续焊接带来温升过高,点焊间隔要适当长些。实践证明,焊接过程对口腔器官无损伤,安全可靠,无不适感觉。

Claims (5)

1、修复不锈钢牙冠口腔内焊接工艺,利用电容储能焊接机(4),其正负极分别连接不锈钢牙冠(1)和焊笔(6),其工艺步骤如下:
①修磨不锈钢牙冠(1)和相邻牙齿或不锈钢牙冠(2),缝隙两边开坡口;
②制备“T”型或“L“型不锈钢镶嵌件(3);
③焊笔(6)压住不锈钢镶嵌件(3),接通电容储能焊接机(4)的脚踏开关(7)。
2、根据权利要求1所述的修复不锈钢牙冠口腔内焊接工艺,其特征是所述的焊笔(6)的笔尖用银及银合金材料制作。
3、根据权利要求1所述的修复不锈钢牙冠口腔内焊接工艺,其特征是所述的不锈钢T型镶嵌件(3)用于双边开坡口,不锈钢L型镶嵌件(3)用于单边开坡口。
4、根据权利要求1或2所述的修复不锈钢牙冠口腔内焊接工艺,其特征是所述的焊笔(6)笔尖接触处的接触面积控制在0.8-1.2mm2之间。
5、根据权利要求1或2或3所述的修复不锈钢牙冠口腔内焊接工艺,焊接参数为:焊接时间:<ms级,脉冲电流:>103A。
CNA2008101392086A 2008-08-16 2008-08-16 修复不锈钢牙冠口腔内焊接工艺 Pending CN101342093A (zh)