CN101307647A - 一种注塑杯状混凝土模板和应用方法 - Google Patents
一种注塑杯状混凝土模板和应用方法 Download PDFInfo
- Publication number
- CN101307647A CN101307647A CNA2008100387146A CN200810038714A CN101307647A CN 101307647 A CN101307647 A CN 101307647A CN A2008100387146 A CNA2008100387146 A CN A2008100387146A CN 200810038714 A CN200810038714 A CN 200810038714A CN 101307647 A CN101307647 A CN 101307647A
- Authority
- CN
- China
- Prior art keywords
- injection moulding
- cup
- concrete
- shaped
- terrace
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种注塑杯状混凝土模板和应用方法,是在建筑的地下工程底板上,满铺本发明产品,再整浇地坪混凝土,最后形成由砼支点抗压的中空地坪,可以排渗漏水、隔潮。本发明包括产品发明和应用发明,产品的边缘既能互相叠合,又能互相搭接,杯状支点高度在20mm~80mm,能承受施工荷载,在板面上绑扎钢筋,使地坪一次整浇完成,提高了工程质量,使地下工程从单一堵水,发展为堵排组合构造。
Description
一、技术领域
本发明是在建筑地下工程的结构底板上满铺一种注塑杯状砼模板,然后再浇混凝土,在室内形成砼中空地坪。在这一个总发明构思中有一种具体的塑料模板产品发明和应用方法发明,本发明有二项独立权利要求。
二、背景技术
国家标准《地下工程防水技术规范》GB50108-2001,在明挖法地下工程防水设防中,只有将结构自防水与柔性防水组合的做法,没有在室内采用中空夹层排水的做法。在本人的一系列发明中,是采用塑料片材再吸塑成为整卷的带支点板材,然后边铺边浇一层砼垫层,养护10天后再可以绑钢筋浇地坪砼,主要原因是原先的产品不能满足施工时人员走动绑钢筋的施工荷载,所以采用二次浇砼的施工方法,在砼中形成了施工缝,又降低了工效。
三、发明内容
A、产品发明
原先是整卷的吸塑产品,不能达到较高的抗压强度,所以就改为注塑生产出方块的杯状塑料模板,模板的边口有搭接设计,设计原则是边口重叠使砼不产生漏浆,边口又要拉接,施工时不会互相脱开。可以设计为凹槽搭扣,或者上下平板加搭钮的做法。平板上有空心杯状支点,浇入砼后就成为砼支点;支点之间的平板上有加劲肋,可以提高模板的抗压强度。模板平面可以是正方形、矩形、六角形,每平方米可以由2~16块互相拼接组成,支点高度可以在20~80mm。本产品可以用废旧塑料生产,达到节约资源环保的目的。
B、应用方法发明
1、地下工程底板的面积较大,无法做出整体找坡,但又要使渗漏水有序地排入集水井,所以采用局部小面积找坡,既可以降低找坡高度,又可以将水引导到集水井。
2、用水平仪对结构面检查,无积水洼地后,再满铺杯状塑料模板,到墙边可以切割。
3、绑扎钢筋后,可以一次浇捣砼,最后形成砼支点抗压的耐久性中空地坪。
C、有益效果
当支点高度在20mm以上到80mm之间时,采用本发明注塑生产的方块杯状模板才能满足施工荷载,使砼面层一次施工,消除了中间的施工缝,提高了砼地坪的质量,使地下工程从单一“堵”水,发展为“堵排”组合构造。
四、附图说明
图1是杯状塑料模板的平面图;
图2是杯状塑料模板A-A剖面图;
图3是模板之间的联接构造A;
图4是模板之间的联接构造B;
图5是中空砼地坪完成剖面。
五、具体实施方式
图1是本发明产品的局部平面图,1是锥形杯状支点,2是平板和加劲肋,3是边缘凹槽,4是边缘扣条;
图2是该平面的A-A剖面;
图3是本发明产品的边缘凹槽3与边缘扣条4互相联接的剖面图;
图4是本发明产品的边缘是上、下平板互搭,在上平板5的下面有个别塑料支点,可以插下下平板6的孔眼中,使平板互相拉接。
图5是在地下工程结构底板上先浇局部找坡7,再铺本发明产品,最后再整浇钢筋砼8,成为中空地坪。
Claims (5)
1、一种注塑杯状混凝土模板,是注塑生产的块状塑料板,其特征是:有平面和杯状支点,板的边缘有联接边口,联接边口既能叠合不漏浆,又能拉接不脱开。
2、如权利要求1所述的一种注塑杯状混凝土模板,其特征是:平面上有加劲肋。
3、如权利要求1所述的一种注塑杯状混凝土模板,其特征是:板的边缘可以做成凹槽和扣条的联接状态,也可以做成上、下平板加搭钮的做法。
4、如权利要求1所述的一种注塑杯状混凝土模板,其特征是:每平方米可以由2~16块互相拼接组成,支点高度可以在20mm~80mm。
5、一种注塑杯状混凝土模板和应用方法,是在塑料模板上浇砼,其特征是:模板满铺后,墙边可以切割,在模板上绑扎钢筋,最后一次浇捣地坪混凝土。