CN101240162A - 抗盐抗高温降失水剂 - Google Patents
抗盐抗高温降失水剂 Download PDFInfo
- Publication number
- CN101240162A CN101240162A CNA2007100567106A CN200710056710A CN101240162A CN 101240162 A CN101240162 A CN 101240162A CN A2007100567106 A CNA2007100567106 A CN A2007100567106A CN 200710056710 A CN200710056710 A CN 200710056710A CN 101240162 A CN101240162 A CN 101240162A
- Authority
- CN
- China
- Prior art keywords
- water loss
- grout
- resisting
- temperature
- salt
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种抗盐抗高温降失水剂,由下列原料按照如下重量份合成的:丙烯酰胺4-7份、丙烯0.5-0.7份、AMPS 10-40份、引发剂(过硫化钾)0.2-0.5份。本发明具有如下的优点和积极效果:1.本降失水剂可有效地通过提高水相粘度和降低滤饼渗透率来降低水泥浆失水,具有较宽温度使用范围,较强适应能力。2.可有效控制水泥浆的失水,配制出符合固井要求的具有低失水量的水泥浆,保护油气层和施工安全。3.如与相配套的分散剂、中温缓凝剂、高温缓凝剂等一起配合使用,可配制出满足不同固井施工要求的低失水水泥浆。4.适用于API各级油井水泥。
Description
技术领域:
本发明涉及一种油田固井作业中所应用的外加剂,特别涉及一种油田固井作业中所用的抗盐抗高温降失水剂。
背景技术:
在油田作业中每一口井钻完以后都要进行固井作业,固井是将一层钢管下入到井内预定深度,再在钢管和井壁之间注入水泥浆,以达到封隔地下油、气、水层,支撑保护套管的目的。在固井时,水泥浆经过渗透性地层后,由于渗透性地层对水泥浆的滤失作用,会危害固井的安全施工和影响固井质量。因此为了保证施工安全和提高固井质量,就必须加入固井用降失水剂以提高水泥浆的抗渗能力,减少渗透层对水泥浆的滤失作用。目前,国内外普遍使用的固井水泥降失水剂纤维素衍生物类和聚乙烯醇类降失水剂等,这几类降失水剂虽然价格低廉、降失水能力强,但是其具有增稠作用,泵送性能差、耐高温耐盐能力差等缺陷,当温度超过100℃时,有的降失水能力则明显下降,有的降失水剂能力全部失去;当在饱和或半饱和盐水环境下,这些浆失水剂就没有功效了。
发明内容:
本发明的目的就在于克服上述现有技术中存在的不足,而提供一种抗盐抗高温降失水剂,该降失水剂具有较宽的温度使用范围,并且在饱和或半饱和盐水环境中不影响水泥浆正常性能。
本发明的技术方案是:一种抗盐抗高温降失水剂,其特征在于:由下列原料按照如下重量份合成的:丙烯酰胺4-7份、丙烯0.5-0.7份、AMPS 10-40份、引发剂(过硫化钾)0.2-0.5份。
本发明具有如下的优点和积极效果:
1、本降失水剂是一种针对油井水泥而合成的新型的水溶性聚合物,通过吸附和聚集的双重作用,在溶液中形成弱胶结的胶体聚集体,可稳定的嵌入泥滤饼,并能够吸附在水泥颗粒表面,减小孔隙尺寸,有效地通过提高水相粘度和降低滤饼渗透率来降低水泥浆失水,是一种具有较宽温度使用范围,较强适应能力,耐温、抗盐的新型有效一种通用型液体降失水剂。
2、可有效控制水泥浆的失水,配制出符合固井要求的具有低失水量的水泥浆,保护油气层和施工安全。
3、如与相配套的分散剂、中温缓凝剂、高温缓凝剂等一起配合使用,可配制出满足不同固井施工要求的低失水水泥浆。
4、适用于API各级油井水泥。
具体实施方式:
实施例1:将丙烯酰胺4千克、丙烯0.5千克、AMPS 10千克、引发剂(过硫化钾)3克进行水溶液聚合,将得到的降失水剂60克,水340克,水泥800克配成水泥浆,该水泥浆就具有低失水抗盐抗高温性能。
实施例2:丙烯酰胺7千克、丙烯0.7千克、AMPS 40千克、引发剂(过硫化钾)6克,水300克进行水溶液聚合,将得到降失水剂60克用半饱和盐水配制成水泥浆,其120℃的API失水只有60ml,稠化时间大于300min,水泥石强度26MPa。
Claims (1)
1. 一种抗盐抗高温降失水剂,其特征在于:由下列原料按照如下重量份合成的:丙烯酰胺4-7份、丙烯0.5-0.7份、AMPS 10-40份、引发剂(过硫化钾)0.2-0.5份。