CN101063063B - Jewellery, jadeware and gold-silver ornaments cleaning powder and preparation method thereof - Google Patents
Jewellery, jadeware and gold-silver ornaments cleaning powder and preparation method thereof Download PDFInfo
- Publication number
- CN101063063B CN101063063B CN2006100795536A CN200610079553A CN101063063B CN 101063063 B CN101063063 B CN 101063063B CN 2006100795536 A CN2006100795536 A CN 2006100795536A CN 200610079553 A CN200610079553 A CN 200610079553A CN 101063063 B CN101063063 B CN 101063063B
- Authority
- CN
- China
- Prior art keywords
- zinc oxide
- powder
- kaolin
- gold
- lime carbonate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The invention discloses a cleaning powder of jewelry, jade ware and gold or silver ornament and preparing method, which comprises the following steps: allocating amidon, caoline and zinc oxide at 1 : (0. 5-4) : (0. 125-0. 25) : (0. 125-0. 25); mixing and stirring evenly; grinding into fine powder; split-charging; getting the product. This invention possesses simple craft, which can be used repeatedly.
Description
The application is an application number: 200410020891.3, and the applying date: on July 2nd, 2004, title: the dividing an application of jewelry, jadeware, gold-silver ornaments cleaning powder and preparation method thereof.
Affiliated technical field
The present invention relates to a kind of jewelry, jadeware, gold-silver ornaments cleaning powder and preparation method thereof, relate in particular to a kind of not only environmental protection but also, be used to remove jewelry, jadeware, gold-silver ornaments oxide on surface the ornaments not damaged and the cleaning product that can reuse.Belong to technical field of chemical products.
Background technology
Jewelry, jadeware, gold-silver ornaments, duration of service of a specified duration its surface not only can produce dirt and also can form oxide on surface, ornaments are tarnished, general cleaning supplies all have certain damage to ornaments, and not environmental protection, can not reuse again.Therefore it is a kind of to jewelry, jadeware, gold-silver ornaments not damaged, environmental protection, the cleaning powder that can reuse to be badly in need of exploitation.
Summary of the invention
The object of the present invention is to provide a kind of jewelry, jadeware, gold-silver ornaments cleaning powder and preparation method thereof, this cleaning powder does not have any damage to ornaments such as jewelry, jadeware, gold and silver, and easy to use, belongs to environmentally friendly machine.
Technical scheme of the present invention is as follows:
The present invention is made of by weight following raw material:
Talcum powder: kaolin: lime carbonate: zinc oxide=(0.5-0.25): (0.5-4): (0.25-0.5): (0.125-0.3).
Above-mentioned talcum powder raw material can be replaced by starch material, i.e. the present invention can be made of by weight following raw material:
Starch: kaolin: lime carbonate: zinc oxide=1: (0.5-4): (0.125-0.25): (0.125-0.25).
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: (0.5-2.5): (0.5-4): (0.05-0.25): (0.125-0.25).
Optimum feed stock weight ratio of the present invention is:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 2.5: 0.5: 0.5: 0.15, right amount of auxiliary materials.
The present invention can comprise following auxiliary material:
Zinc stearate, lime carbonate, zinc oxide, pigment and essence;
The present invention includes auxiliary material optimum feed stock weight ratio is:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide: pigment: essence=1: 2.5: 0.5: 0.25: 0.25: 0.025: 0.025
Preparation method of the present invention is as follows:
Get each raw material by above-mentioned weight ratio, mixing and stirring grinds to form fine powder, and packing gets final product.
The present invention can use magnesiumcarbonate, and Magnesium Carbonate Light 41-45 substitutes lime carbonate.
The present invention can use zinc stearate, octadecyl ester zinc, hard magnesium, zinc oxide, stearic acid polyoxyethylene fat to substitute zinc oxide.
The invention has the beneficial effects as follows that this cleaning powder to jewelry, jadeware, gold-silver ornaments not damaged, is the ring-like product of a kind of environmental protection, its production technique is simple, be fit to produce in batches, and easy to use can the recycling.
Embodiment 1
The present invention is made of by weight following raw material:
Talcum powder: kaolin: lime carbonate: zinc oxide=0.5: 0.5: 0.25: 0.125
The preparation method of jewelry of the present invention, jadeware, gold-silver ornaments cleaning powder is as follows:
Get talcum powder 50g by above-mentioned weight ratio, kaolin 50g, lime carbonate 5g, zinc oxide 12.5g, mixing and stirring grinds to form fine powder, and packing gets final product.
Embodiment 2
The present invention is made of by weight following raw material:
Talcum powder: kaolin: lime carbonate: zinc oxide=2.5: 4: 0.5: 0.3
Get talcum powder 25g by above-mentioned weight ratio, kaolin 40g, lime carbonate 5g, zinc oxide 3g, mixing and stirring grinds to form fine powder, and packing gets final product.
Embodiment 3
The present invention is made of by weight following raw material:
Talcum powder: kaolin: lime carbonate: zinc oxide=1: 2: 0.25: 0.125
Get talcum powder 100g by above-mentioned weight ratio, kaolin 200g, lime carbonate 25g, zinc oxide 12.5g, mixing and stirring grinds to form fine powder, and packing gets final product.
Embodiment 4
Above-mentioned talcum powder raw material can be replaced by starch material, i.e. the present invention can be made of by weight following raw material:
Starch: kaolin: lime carbonate: zinc oxide=1: 0.5: 0.125: 0.125
Get starch 100g by above-mentioned weight ratio, kaolin 50g, lime carbonate 12.5g, zinc oxide 12.5g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 5
The present invention can be made of by weight following raw material:
Starch: kaolin: lime carbonate: zinc oxide=1: 2: 0.15: 0.15
Get starch 100g by above-mentioned weight ratio, kaolin 200g, lime carbonate 15g, zinc oxide 15g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 6
The present invention can be made of by weight following raw material:
Starch: kaolin: lime carbonate: zinc oxide=1: 4: 0.25: 0.25
Get starch 100g by above-mentioned weight ratio, kaolin 400g, lime carbonate 25g, zinc oxide 25g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 7
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 0.5: 0.5: 0.05: 0.125
Get starch 100g by above-mentioned weight ratio, talcum powder 50g, kaolin 50g, lime carbonate 25g, zinc oxide 12.5g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 8
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 1.5: 2: 0.25: 0.2
Get starch 100g by above-mentioned weight ratio, talcum powder 150g, kaolin 200g, lime carbonate 25g, zinc oxide 20g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 9
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 2.5: 4: 0.25: 0.25
Get starch 100g by above-mentioned weight ratio, talcum powder 250g, kaolin 400g, lime carbonate 25g, zinc oxide 25g mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 10
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 0.5: 0.5: 0.05: 0.125
Get starch 100g by above-mentioned weight ratio, talcum powder 50g, kaolin 50g, lime carbonate 5g, zinc oxide 12.5g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 11
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 1.5: 2: 0.25: 0.2
Get starch 100g by above-mentioned weight ratio, talcum powder 150g, kaolin 200g, lime carbonate 25g, zinc oxide 20g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 12
The present invention can also be made of by weight following raw material:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 2.5: 4: 0.25: 0.25
Get starch 100g by above-mentioned weight ratio, talcum powder 250g, kaolin 400g, lime carbonate 25g, zinc oxide 25g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 13
Optimum feed stock weight ratio of the present invention is:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide=1: 2.5: 0.5: 0.5: 0.4, right amount of auxiliary materials.Get starch 100g by above-mentioned weight ratio, talcum powder 250g, kaolin 50g, lime carbonate 50g, zinc oxide 40g, mixing and stirring grinds to form fine powder, and packing is finished product.
Embodiment 14
The raw material weight ratio that the present invention includes auxiliary material is:
Starch: talcum powder: kaolin: lime carbonate: zinc oxide: pigment: essence=1: 2.5: 0.5: 0.25: 0.25: 0.025: 0.025
Get starch 100g by above-mentioned weight ratio, talcum powder 250g, kaolin 50g, lime carbonate 25g, zinc oxide 25g, pigment 2.5g, essence 2.5g, mixing and stirring grinds to form fine powder, and packing is finished product.
Using method of the present invention is:
Jewelry, jadeware, gold and silver trinket are imbedded in the cleaning powder of the present invention, the time of inserting can be 12-48 hour, take out the back and dip in soft cloth and get cleaning powder wiping ornaments of the present invention and remove powder on the ornaments, can remove ornaments surface contaminants and surface oxide layer.
Jewelry, jadeware, big ornaments of gold and silver are directly dipped in soft cloth get cleaning powder wiping of the present invention and can remove surface contaminants and surface oxide layer.
Embodiment 15
Get 16 of pearl necklaces making surperficial clean, randomly draw and be divided into two groups.
8 pearl necklaces of first group are inserted respectively in the cleaning powder of the present invention, the time of inserting is 48 hours, (also can insert the longer time) taken out 8 pearl necklaces respectively the back then and dipped in soft cloth and get cleaning powder wiping ornaments of the present invention and remove powder on the ornaments.8 pearl necklace surface dirts of first group are removed recovery gloss fully.And with the 2nd group of mattness of conventional purging method (promptly adding water with soap makes the soap solution mode and clean), and clean not thorough.
Embodiment 16
Get the jade that to make surperficial clean and weigh down 16, randomly draw and be divided into two groups.
First group 8 beautiful bobs are inserted respectively in the cleaning powder of the present invention, and the time of inserting is 12 hours, then 8 pearl necklaces are taken out the back respectively and dip in soft cloth and get cleaning powder wiping ornaments of the present invention and remove powder on the ornaments.8 beautiful clean and recovery gloss of surperficial dirt full scale clearance that weigh down each of first group.And 8 beautiful necklace cleaning surfaces that weigh down of second group of conventional cleaning (promptly cleaning with common washings) are not thorough, and matt.
Embodiment 17
Getting 10 of gold ring need making surperficial clean inserts respectively in the cleaning powder of the present invention, the time of inserting is 48 hours, then 10 gold are guarded against son and taken out the back respectively and dip in soft cloth and get cleaning powder wiping ornaments of the present invention and remove powder on the ornaments, can remove surface contaminants and surface oxide layer.
The conventional cleaning of gold-silver ornaments adopted the pickling mode, although cleaning performance is pretty good, not only gold-silver ornaments had certain damage, simultaneously there is unsafe hidden danger in the operator.
Embodiment 18
Get 8 in silverware making surperficial clean, directly dip in and get cleaning powder wiping of the present invention and can remove silverware surface contaminants and surface oxide layer with soft cloth.
The present invention's cleaning performance easy to use is good, ornaments and human body are not had injury, general purging method such as with sulfuric acid cleaned by having certain danger, and can not reuse, and other clean-out system can not reach better cleaning effect, so advantage of the present invention is more obvious.
Claims (2)
1. jewelry, jadeware, gold-silver ornaments cleaning powder is characterized in that being made up of by weight following raw material: starch: kaolin: lime carbonate: zinc oxide=1: (0.5-4): (0.125-0.25): (0.125-0.25).
2. the preparation method of jewelry, jadeware, gold-silver ornaments cleaning powder is characterized in that by following raw material by weight forming:
Starch: kaolin: lime carbonate: zinc oxide=1: (0.5-4): (0.125-0.25): (0.125-0.25);
Its preparation method is as follows:
Get each raw material by above-mentioned weight ratio, mixing and stirring grinds to form fine powder, and packing gets final product.