CA2170769C - Bags and method of making bags - Google Patents
Bags and method of making bags Download PDFInfo
- Publication number
- CA2170769C CA2170769C CA002170769A CA2170769A CA2170769C CA 2170769 C CA2170769 C CA 2170769C CA 002170769 A CA002170769 A CA 002170769A CA 2170769 A CA2170769 A CA 2170769A CA 2170769 C CA2170769 C CA 2170769C
- Authority
- CA
- Canada
- Prior art keywords
- web
- webs
- bags
- bag
- weakness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
Methods of making a container strip in the form of a chain of interconnected preopened bags with openings preferably having longitudinal dimensions of at least about 1/64 inch is disclosed. The container strip provides greatly enhanced facility for bag registration and opening during packaging operations utilizing the improved container strip. Processes of forming a chain of preopened bags are also disclosed. Face (14) and back (5) plastic webs are fed along individual paths of travel to a common path (28). In one embodiments the webs are differentially tensioned while in their independent paths by stretching the face web, by rollers (18) more than the back web by rollers (20) such that the face web will retract longitudinally more than the back web upon release of the web tension. While so tensioned edge seals are formed between the webs to convert the webs into a tube and longitudinally spaced transverse seals are formed between the webs to delineate bottoms of bags. Transverse lines of weakness are formed in said back web to facilitate separation of bags from the remainder of the web during a subsequent use. Tension in individual bag sections of the face web is released by forming longitudinally spaced transverse separations of the sections and thereby producing a space between each contiguous pair of sections. In other embodiments, pairs of transverse lines of severance are formed in a front section of the webs and parts between the lines of severance are removed to form the novel bags without the need for differential stretching.
Description
BAGS AND METHOD OF MAKING BAGS
Field of Invention This invention relates to chains of interconnected, pre-opened bags used in packaging and more particularly relates to a novel and improved method of making chains of bags.
Backs~round of the Invention U.S. Patent 3,254,828, issued June 7, 1966, to Hershey Lerner under the title Flexible Container Strips is directed to so called bags on a roll (here the AutoBag patent). This patent discloses a web of bags interconnected by lines of weakness, preferably in the form of perforations, with each of the bags being open on one face. In use the bags are sequentially fed to a loading station. When at the loading station, each bag is blown open, a product is inserted and thereafter separated from the web and, if desired, the bag is then sealed to form a package.
These container strips in the form of chains of pre-opened bags are supplied either on a roll as taught in the AutoBag patent or festooned in a carton in the manner taught in Patent 4,201,029, issued May 6, 1980, to Bernard Lerner et al. under the title Method and Apparatus for Packaging, (here the Wig-Wag patent). Such container strips have been sold by Automated Packaging Systems, Inc. of Streetsboro, Ohio, the assignee of the present case, under the trademark AutoBag and have enjoyed great commercial success.
Both AutoBag and competitive products have usually been made by feeding a tube through a converting machine. Such a machine forms transverse seals to delineate the bottoms of the bags and transverse lines of weakness by perforating both layers of the tube to delineate contiguous ends of adjacent bags. After the perforations are formed, a "zinging" operation is performed on each bag to open the front of the bag while leaving the perforations of the back intact.
WO 95/09727 ~ ~ ~~ PCT/US94/11346
Field of Invention This invention relates to chains of interconnected, pre-opened bags used in packaging and more particularly relates to a novel and improved method of making chains of bags.
Backs~round of the Invention U.S. Patent 3,254,828, issued June 7, 1966, to Hershey Lerner under the title Flexible Container Strips is directed to so called bags on a roll (here the AutoBag patent). This patent discloses a web of bags interconnected by lines of weakness, preferably in the form of perforations, with each of the bags being open on one face. In use the bags are sequentially fed to a loading station. When at the loading station, each bag is blown open, a product is inserted and thereafter separated from the web and, if desired, the bag is then sealed to form a package.
These container strips in the form of chains of pre-opened bags are supplied either on a roll as taught in the AutoBag patent or festooned in a carton in the manner taught in Patent 4,201,029, issued May 6, 1980, to Bernard Lerner et al. under the title Method and Apparatus for Packaging, (here the Wig-Wag patent). Such container strips have been sold by Automated Packaging Systems, Inc. of Streetsboro, Ohio, the assignee of the present case, under the trademark AutoBag and have enjoyed great commercial success.
Both AutoBag and competitive products have usually been made by feeding a tube through a converting machine. Such a machine forms transverse seals to delineate the bottoms of the bags and transverse lines of weakness by perforating both layers of the tube to delineate contiguous ends of adjacent bags. After the perforations are formed, a "zinging" operation is performed on each bag to open the front of the bag while leaving the perforations of the back intact.
WO 95/09727 ~ ~ ~~ PCT/US94/11346
2 Relatively recently a market has developed for these chains of bags made from two layers of plastic, so that the plastic of the front of the bag is different from that of the back of the bag. For example, some customers for such bags may wish the back of the bag to be white to enhance the legibility of information imprinted on it such as instructions on how to use a product packaged in the bag.
The front of the bag is clear, so that the contents of a package are readily visible.
To accomplish this two single layer webs of plastic are fed from respective supplies in a manner similar to that taught in U.S. patent 4,337,058 issued June 29, 1982 to Bernard Lerner under the title Method of Making a Container Strip Having Inserts. Marginal edges of the two webs are then fused together to form a tube and remainder of the container strip manufacture is identical to that when the supplied work piece is a flattened tube.
So called "multiple up" production has also become quite customary. With multiple up, the work piece may be either a relatively wide flattened tube or two relatively wide single ply sheets fed together and fused. In either event hot knives are used to sever the work piece into two or more elongate tubes and thereafter each new tube is made into a chain of pre-opened bags.
When bags are made from two single ply webs, every effort has been made to provide identical tension on the two webs, so that once made into a tube the only difference of the tube from one provided as a tubular work piece is that the front and back are not identical, such as the back may be pigmented while the front is clear. With the two single ply approach, if the bag making machine was not adjusted properly, once opened the bags would not lie flat with the separated edges which delineate the openings lying in closely juxtaposed positions. The resultant product was often scrap. If the edges were not juxtaposed but rather there was a gap between them, these "gap" bags were rejected because they were perceived to be unacceptable to customers as unsightly and bags which would produce packages with malaligned top edges. If the top edge of an opened bag overlapped the bottom of the adjacent bag, they were not subject to a policy of universal rejection as were the gap bags but all too often the spark gap detector WO 95/09727 2 ~ ~ ~ ~ ~ ~ PCT/US94/11346
The front of the bag is clear, so that the contents of a package are readily visible.
To accomplish this two single layer webs of plastic are fed from respective supplies in a manner similar to that taught in U.S. patent 4,337,058 issued June 29, 1982 to Bernard Lerner under the title Method of Making a Container Strip Having Inserts. Marginal edges of the two webs are then fused together to form a tube and remainder of the container strip manufacture is identical to that when the supplied work piece is a flattened tube.
So called "multiple up" production has also become quite customary. With multiple up, the work piece may be either a relatively wide flattened tube or two relatively wide single ply sheets fed together and fused. In either event hot knives are used to sever the work piece into two or more elongate tubes and thereafter each new tube is made into a chain of pre-opened bags.
When bags are made from two single ply webs, every effort has been made to provide identical tension on the two webs, so that once made into a tube the only difference of the tube from one provided as a tubular work piece is that the front and back are not identical, such as the back may be pigmented while the front is clear. With the two single ply approach, if the bag making machine was not adjusted properly, once opened the bags would not lie flat with the separated edges which delineate the openings lying in closely juxtaposed positions. The resultant product was often scrap. If the edges were not juxtaposed but rather there was a gap between them, these "gap" bags were rejected because they were perceived to be unacceptable to customers as unsightly and bags which would produce packages with malaligned top edges. If the top edge of an opened bag overlapped the bottom of the adjacent bag, they were not subject to a policy of universal rejection as were the gap bags but all too often the spark gap detector WO 95/09727 2 ~ ~ ~ ~ ~ ~ PCT/US94/11346
3 used for bag registration in a bagging machine would not function properly.
Such a bagging machine is disclosed in Patent 4,014,154, issued March 29, 1977, to Bernard Lerner and related patents identified therein (here the H-100 patents).
SummarEr of the Invention As taught in the Parent Case, it has now been recognized for the first time that if chains of bags are made from single ply webs that are differentially tensioned an improved and superior product can be produced.
The improved product is a flexible container strip formed of an elongated flexible tube of plastic material capable of bonding to itself at a predetermined temperature on application of pressure but being otherwise non-adherent to material of identical composition. The tube is longitudinally collapsed with face and back plies joined together along their longitudinal side edges. A
plurality of spaced, transversely disposed bottom seals each secure the plies together and delineate ends of fillable bag spaces. Each seal extends transversely from one side edge of the tube to another such that the tube is separated into a chain of connected bags. The face ply of each bag has a transverse end opening extending substantially from one side edge of the bag to the other and extending longitudinally a distance sufficient to facilitate bag opening and loading and to provide detection access to aligned lines of weakness in the back ply. Each opening is adjacent the end of the bag remote from its bottom seal forming the filling space end of that bag such that the bags of the chain are all oriented in the same direction.
The openings all formed in the face ply and are at longitudinally spaced intervals equal to the spacing of the bottom seals. The back ply of each bag has a transversely weakened tearable portion extending substantially from one side edge to another to permit facile separation of the bags while maintaining the integrity of the back ply and the tube. Each tearable portion is aligned with and accessible through the end opening of its bag. Thus, the improved strip is a chain of collapsed bags which may be fed serially along a path from a supply to bag ~ 17 C~~ b9
Such a bagging machine is disclosed in Patent 4,014,154, issued March 29, 1977, to Bernard Lerner and related patents identified therein (here the H-100 patents).
SummarEr of the Invention As taught in the Parent Case, it has now been recognized for the first time that if chains of bags are made from single ply webs that are differentially tensioned an improved and superior product can be produced.
The improved product is a flexible container strip formed of an elongated flexible tube of plastic material capable of bonding to itself at a predetermined temperature on application of pressure but being otherwise non-adherent to material of identical composition. The tube is longitudinally collapsed with face and back plies joined together along their longitudinal side edges. A
plurality of spaced, transversely disposed bottom seals each secure the plies together and delineate ends of fillable bag spaces. Each seal extends transversely from one side edge of the tube to another such that the tube is separated into a chain of connected bags. The face ply of each bag has a transverse end opening extending substantially from one side edge of the bag to the other and extending longitudinally a distance sufficient to facilitate bag opening and loading and to provide detection access to aligned lines of weakness in the back ply. Each opening is adjacent the end of the bag remote from its bottom seal forming the filling space end of that bag such that the bags of the chain are all oriented in the same direction.
The openings all formed in the face ply and are at longitudinally spaced intervals equal to the spacing of the bottom seals. The back ply of each bag has a transversely weakened tearable portion extending substantially from one side edge to another to permit facile separation of the bags while maintaining the integrity of the back ply and the tube. Each tearable portion is aligned with and accessible through the end opening of its bag. Thus, the improved strip is a chain of collapsed bags which may be fed serially along a path from a supply to bag ~ 17 C~~ b9
4 opening and load stations, may be readily and accurately registered at a load station through spark detector location of the tearable portions and may be opened by a blast of air directed longitudinally of the path and then loaded and separated from the chain sequentially and one at a time.
In the preferred method of manufacture of the Parent Case the tension on the web which will become the face of the bags is carefully differentially tensioned to stretch it, without exceeding its elastic limit, more than the web which will become the back of the bags. Alternatively the back web is tensioned more than the front and the back to exceed its elastic limit. While the differential tensioning is maintained, side seams are formed to produce a tube. Preferably the balance of the container strip formation operation is that which has been employed in the past, so that existing manufacturing equipment can be used without modification.
With the preferred process of the Parent Case, the improved product results when the face of a bag is "zung" to form a transverse opening delineating the top of the bag. The formation of the opening releases the tension in the face of the bag, so that the face of the bag will shrink relative to the back with the result that the top edge of the just opened bag will be at least about 1J~
(one sixty fourth) of an inch from the bottom edge of the following adjacent bag.
The resultant product not only facilitates bag opening at a load station, but also assists in reliably producing appropriate bag registration at a load station.
Registration is enhanced because the perforations in the back face, being aligned with and accessible through the elongated opening, are readily, precisely and reliably detected by a spark detector.
In an alternate system for making the improved chain of bags, bottom seals and perforations are formed and the web is "zung" to separate perforations of the face web. Thereafter side seals are formed while the back web is maintained under controlled tension to produce bags having top openings of consistent and desired longitudinal extent.
The process of this invention includes feeding face and back plastic web sections along respective paths of travel and as they are fed forming transversely WO 95/097:27 2 t 7 ~ 7 6 9 s extending lines of weakness in the back section. Spaced pairs of transversely extending lines of severance are formed in the front section at longitudinally spaced intervals corresponding to the spacing of the lines of weakness. The sections are superposed with the lines of severance positioned with an associated one of the lines of weakness longitudinally located between the lines of severance of the associated pair. Transverse seals are formed between the sections at least some of which delineate bag bottoms each near a line of weakness and its associated pair of lines of severance. A side edge seal is formed between the sections which is spaced from a second side edge delineated by a selected one of a longitudinally extending fold or a second side edge seal. Bag openings are formed by removing portions of the face section between the lines of severance of each pair.
The spacing of the lines of severance of each pair is sufficient to assure that the associated line of weakness may be readily detected as by a spark gap detector when the lines of weakness are perforations. Preferably the spacing of the lines of s~° rv erance is at least about 1/64 inch.
~~.s suggested previously the sections may be either independent, separate webs or alternately formed by a single wide web folded to produce the two sections. Optionally, the face section may be in the form of a series of independently precut portions which are secured to the back section with each portion forming the front of an individual bag of the chain of bags being formed.
With all of the options, although the sections may be folded from a single web, it is considered that prior to juxtaposing the sections together the face and back sections traverse respective paths of travel and following juxtaposition the sections traverse a common path of travel.
Accordingly, the objects of the invention are to provide a novel and improved methods of making chains of interconnected but pre-opened bags.
217 ~~ ~9 In the Drawings Figure 1 is a fragmentary plan view of a section of a chain of interconnected bags made in accordance with invention;
Figure 2 is a sectional view of the chain of Figure 1 as seen from the plane indicated by the line 2-2 of Figure 1;
Figure 3 is an enlarged sectional view of a section of the chain indicated by the circle 3 of Figure 2;
Figure 4 is a side elevational, schematic view of a process of making a chain;
Figure 5 is a schematic plan view of the machine of Figure 4;
Figure 6 is a schematic perspective view of a method of forming a chain of bags from a single web in which the web sections are joined by a fold;
Figure 7 is a schematic perspective view of a method of forming a chain of interconnected bags from independent sections; and, Figure 8 is a schematic perspective view of a method of forming bags from independent web sections wherein the face section is severed into independent portions prior to securement to the back section.
Description of the Preferred Embodiments Referring now to the drawings and to Figures 4 and 5 in particular where the process of The Parent Case is shown. With this process, a pair of single ply individual web supplies 10, 12 are provided which are face and back webs respectively. Webs from the supplies 10, 12 are respectively fed along individual paths of travel 14, 15 to a juncture at juncture nip rolls 17. Tension control nip roll sets 18, 20 are provided. The set 18 is positioned along the path 14 to tension the face web 10 while the set 20 is along the path 15 to tension the back web 12.
When in operation the nip roll set 18 will be set to tension the face web to a higher level than the back web, in that the web from the supply 10 will form the , face of fronts of bags being produced.
21 ~~~~~
The webs are fed from the juncture nip rolls 17 along a common path of travel 28. Hot knives 22, 23 are positioned downstream from the juncture nips to form bead seals along side edges of the webs and convert the webs into a tube.
Trim strips 25, 26 formed by the hot knives are removed for collection and recycling.
Once formed into a tube the combined webs pass through a sealer 30 which forms transverse seals to become the bottoms of the bags being produced. Next a perforator 32 forms transverse lines of weakness in the tube to delineate, in each case, a bag bottom adjacent a transverse seal and the top of an adjoining bag.
A rotating finger known as a "zinger" 34 is provided. The zinger has a surface speed slightly greater than the speed of the web so that as the zinger strikes a section of the web that will be the front of a bag, acting against the resistance of an anvil roll 35, it separates the perforations of the front web to form a bag opening. Thereafter the web, now formed into a container strip of intercon-nected but open bags, is collected at a take up 38. Apart from the adjustment of the tension control nips 18, 20 to provide differential tensioning, the machine and the process thus far described are now conventional and well known to those in the art.
Deferring now to Figures 1 through 3, the novel container strip of The Parent Case is shown generally at 40. The strip includes a plurality of intercon-nected bags 42 joined together in a back ply 43 by lines of weakness 44 in the form of ~rforations. Transverse seals 46 delineate the bottoms of bags.
The face ply formed by the web from the supply 10 is separated into individual bag face sections 48. A transversely extending bag opening 50 is adjacent the top of each bag face section 48. Each opening 50 extends completely across tine web from one side edge 52 to the other 53, while the perforations in the back 43 remain intact. Each bag opening extends longitudinally of the web preferably at least 1/64 (one sixty fourth) of an inch.
The importance of the longitudinal extent of these openings is besE
understood by reference to Figure 3. A conventional spark detector is shown 2'1 ~ 0~ ~° g .
schematically at 55. Assuming the web is moving from right to left in Figure 3 so that the bags are being fed closed end first in a bagging machine, as is conven-tional, it will be seen that the detector 55 will readily be able to locate the per- , forations 44 once the spark path indicated schematically at 58 is aligned with the perforations.
Referring now to Figure 6, a web 60 is fed along a path of travel indicated by an arrow 61. Transverse lines of weakness in the form of perforations 62 and spaced pairs lines of severance 64 are shown as concurrently formed in the web.
The lines of weakness and severance are formed by coacting cutting and anvil rolls 65, 66.
As the web 60 proceeds along its path of travel a fold 68 is formed in a known manner as by a well known V board. Through the folding process a face section 69 of the web 60 is superposed over a back section 70.
The parts of the base section 69 between each of the pairs of lines of severance 64 is removed as by a vacuum head shown schematically at 72 to produce a bag opening aligned with and superposed over an associated line of weakness 62.
Transverse seals 74 are formed by a heat sealer shown schematically at 75.
Each of the seals shown in Figure 6, delineates a bottom of one of the chain of bags being formed. A hot knife 77 forms a bead seal 78 along the web side edge opposite the fold 68 to complete the chain of bags. Optionally a second hot knife 80 may form an opposed bead seal 81 to assure that the openings delineated by the lines of severance 64 extend fully from one side edge to the other of each bag, if that is desired. Alternatively, the lines of severance may extend to the fold and use of the second hot knife 80 is not required.
Referring now to Figure 7, face and back webs 10, 12, as in the embodiment of Figures 4 and 5, are fed along individual paths. Lines of weakness 62 and lines of severance 64 are respectively formed in a manner similar to the embodiment of Figure 6 but with separate cutter and anvil rolls (not shown) rather than the dual cutter and anvil rolls 65, 66 of Figure 6. Thereafter, they are juxtaposed and the transverse seals 74 and the bead seal 78, 81 are formed in a manner corresponding to the embodiment of Figure 6.
With the embodiment of Figure 8, the upper face section 10 is severed into individual parts 83 by cutter and anvil rolls 84, 85 which form lines of severance 64 extending across the full width of web. Thereafter the individual parts 83 are suitably fed by a conventional mechanism, not shown, into juxtaposition with the back web 12. Transverse lines of weakness 62 are formed in the back web by coacting cutter and anvil rolls 87, 88, shown at a location prior to wet juxtaposition but they may be located at down stream locations along the path of travel. Once the parts 83 are juxtaposed with the back web 12, the transverse seals 24 and the bead seals 78, 81 are formed in the manner described in connection with Figure 6.
Operation hi operation as depicted in Figures 4 and 5, coils of single ply plastic are mounted to provide the front and back supplies 10, 12. The materials of the webs may be other than identical so long as they are capable of being sealed together.
For example, one web may be pigmented such that it is translucent or opaque while the other web is clear. Typically the plastic will be polyethylene, although other thermal softenable plastics capable of adherence together on application of heat and pressure are sometimes employed.
Webs from the supplies 10, 12 are fed along their respective independent paths of travel through the tension control nip rolls 18, 20 to the juncture nips 17.
They are then fed along the path 28 past the hot knives 22, 23, the transverse sealer 30, the perforator 32, the zinger 34 and thence to the take up 38.
Once the machine is set up and operation commences and the nips 18, 20 are adjusted to provide differential tension along the paths 14, 15. The appropriate tension is a function of the material, its thickness and its width.
Once appropriate tension has been at least provisionally established and temperatures of the hot knives and transverse sealer are adjusted to appropriate to levels, production commences. Tension is further adjusted as the machine operates until desired finished products are consistently produced. During production the two plies are fed past the hot knives to create a tube with a front face stretched more than the back. This differential stretching is maintained as the now formed tube passes the transverse sealer and the perforator. Once the face web is opened by the zinging operation, the tension in the just opened web face section is released and it will shrink longitudinally of the web relative to the back preferably to produce the desired opening of at least 1/64 (one sixty fourth) of an inch measured longitudinally of the web.
With the embodiments of Figures 6 - 8, relative tension of the web sections is not critical in that bag openings of sufficient width are formed by producing the pairs of lines of severance 74 in each of those embodiments in the manner described. In the three embodiments shown once the lines of severance 64 and the lines of weakness 62 are formed, the front and back sections are juxtaposed.
Thereafter, the bead seals 78 and the transverse seal 74 are formed. While in each embodiment the schematic drawings depict the formation of the transverse seals before the bead seals, the sequence can obviously be reversed.
Similarly, removal of web parts between lines of severance is shown in Figure 6 to occur as the webs are juxtaposed, but this operation may also be performed at other locations along the path of travel. After juxtaposition of the front and back sections, the bead seal 81 is formed in the embodiments of Figures 7 and 8 and may be formed in the embodiment of Figure 6 if desired. With all three embodiments, a chain of bags is produced in which each bag opening, as in the embodiment depicted in Figures 4 and 5, has sufficient longitudinal extent to assure facile detection of the associated line of weakness.
Although the invention has been described in its preferred form with a certain degree of particularity, it is understood that the present disclosure of the preferred form has been made only by way of example and that numerous changes in the details of construction, operation and the combination and arrangement of WO 95/09727 ~ ~ PCTlUS94111346 parts may be resorted to without departing from the spirit and the scope of the invention as hereinafter claimed.
In the preferred method of manufacture of the Parent Case the tension on the web which will become the face of the bags is carefully differentially tensioned to stretch it, without exceeding its elastic limit, more than the web which will become the back of the bags. Alternatively the back web is tensioned more than the front and the back to exceed its elastic limit. While the differential tensioning is maintained, side seams are formed to produce a tube. Preferably the balance of the container strip formation operation is that which has been employed in the past, so that existing manufacturing equipment can be used without modification.
With the preferred process of the Parent Case, the improved product results when the face of a bag is "zung" to form a transverse opening delineating the top of the bag. The formation of the opening releases the tension in the face of the bag, so that the face of the bag will shrink relative to the back with the result that the top edge of the just opened bag will be at least about 1J~
(one sixty fourth) of an inch from the bottom edge of the following adjacent bag.
The resultant product not only facilitates bag opening at a load station, but also assists in reliably producing appropriate bag registration at a load station.
Registration is enhanced because the perforations in the back face, being aligned with and accessible through the elongated opening, are readily, precisely and reliably detected by a spark detector.
In an alternate system for making the improved chain of bags, bottom seals and perforations are formed and the web is "zung" to separate perforations of the face web. Thereafter side seals are formed while the back web is maintained under controlled tension to produce bags having top openings of consistent and desired longitudinal extent.
The process of this invention includes feeding face and back plastic web sections along respective paths of travel and as they are fed forming transversely WO 95/097:27 2 t 7 ~ 7 6 9 s extending lines of weakness in the back section. Spaced pairs of transversely extending lines of severance are formed in the front section at longitudinally spaced intervals corresponding to the spacing of the lines of weakness. The sections are superposed with the lines of severance positioned with an associated one of the lines of weakness longitudinally located between the lines of severance of the associated pair. Transverse seals are formed between the sections at least some of which delineate bag bottoms each near a line of weakness and its associated pair of lines of severance. A side edge seal is formed between the sections which is spaced from a second side edge delineated by a selected one of a longitudinally extending fold or a second side edge seal. Bag openings are formed by removing portions of the face section between the lines of severance of each pair.
The spacing of the lines of severance of each pair is sufficient to assure that the associated line of weakness may be readily detected as by a spark gap detector when the lines of weakness are perforations. Preferably the spacing of the lines of s~° rv erance is at least about 1/64 inch.
~~.s suggested previously the sections may be either independent, separate webs or alternately formed by a single wide web folded to produce the two sections. Optionally, the face section may be in the form of a series of independently precut portions which are secured to the back section with each portion forming the front of an individual bag of the chain of bags being formed.
With all of the options, although the sections may be folded from a single web, it is considered that prior to juxtaposing the sections together the face and back sections traverse respective paths of travel and following juxtaposition the sections traverse a common path of travel.
Accordingly, the objects of the invention are to provide a novel and improved methods of making chains of interconnected but pre-opened bags.
217 ~~ ~9 In the Drawings Figure 1 is a fragmentary plan view of a section of a chain of interconnected bags made in accordance with invention;
Figure 2 is a sectional view of the chain of Figure 1 as seen from the plane indicated by the line 2-2 of Figure 1;
Figure 3 is an enlarged sectional view of a section of the chain indicated by the circle 3 of Figure 2;
Figure 4 is a side elevational, schematic view of a process of making a chain;
Figure 5 is a schematic plan view of the machine of Figure 4;
Figure 6 is a schematic perspective view of a method of forming a chain of bags from a single web in which the web sections are joined by a fold;
Figure 7 is a schematic perspective view of a method of forming a chain of interconnected bags from independent sections; and, Figure 8 is a schematic perspective view of a method of forming bags from independent web sections wherein the face section is severed into independent portions prior to securement to the back section.
Description of the Preferred Embodiments Referring now to the drawings and to Figures 4 and 5 in particular where the process of The Parent Case is shown. With this process, a pair of single ply individual web supplies 10, 12 are provided which are face and back webs respectively. Webs from the supplies 10, 12 are respectively fed along individual paths of travel 14, 15 to a juncture at juncture nip rolls 17. Tension control nip roll sets 18, 20 are provided. The set 18 is positioned along the path 14 to tension the face web 10 while the set 20 is along the path 15 to tension the back web 12.
When in operation the nip roll set 18 will be set to tension the face web to a higher level than the back web, in that the web from the supply 10 will form the , face of fronts of bags being produced.
21 ~~~~~
The webs are fed from the juncture nip rolls 17 along a common path of travel 28. Hot knives 22, 23 are positioned downstream from the juncture nips to form bead seals along side edges of the webs and convert the webs into a tube.
Trim strips 25, 26 formed by the hot knives are removed for collection and recycling.
Once formed into a tube the combined webs pass through a sealer 30 which forms transverse seals to become the bottoms of the bags being produced. Next a perforator 32 forms transverse lines of weakness in the tube to delineate, in each case, a bag bottom adjacent a transverse seal and the top of an adjoining bag.
A rotating finger known as a "zinger" 34 is provided. The zinger has a surface speed slightly greater than the speed of the web so that as the zinger strikes a section of the web that will be the front of a bag, acting against the resistance of an anvil roll 35, it separates the perforations of the front web to form a bag opening. Thereafter the web, now formed into a container strip of intercon-nected but open bags, is collected at a take up 38. Apart from the adjustment of the tension control nips 18, 20 to provide differential tensioning, the machine and the process thus far described are now conventional and well known to those in the art.
Deferring now to Figures 1 through 3, the novel container strip of The Parent Case is shown generally at 40. The strip includes a plurality of intercon-nected bags 42 joined together in a back ply 43 by lines of weakness 44 in the form of ~rforations. Transverse seals 46 delineate the bottoms of bags.
The face ply formed by the web from the supply 10 is separated into individual bag face sections 48. A transversely extending bag opening 50 is adjacent the top of each bag face section 48. Each opening 50 extends completely across tine web from one side edge 52 to the other 53, while the perforations in the back 43 remain intact. Each bag opening extends longitudinally of the web preferably at least 1/64 (one sixty fourth) of an inch.
The importance of the longitudinal extent of these openings is besE
understood by reference to Figure 3. A conventional spark detector is shown 2'1 ~ 0~ ~° g .
schematically at 55. Assuming the web is moving from right to left in Figure 3 so that the bags are being fed closed end first in a bagging machine, as is conven-tional, it will be seen that the detector 55 will readily be able to locate the per- , forations 44 once the spark path indicated schematically at 58 is aligned with the perforations.
Referring now to Figure 6, a web 60 is fed along a path of travel indicated by an arrow 61. Transverse lines of weakness in the form of perforations 62 and spaced pairs lines of severance 64 are shown as concurrently formed in the web.
The lines of weakness and severance are formed by coacting cutting and anvil rolls 65, 66.
As the web 60 proceeds along its path of travel a fold 68 is formed in a known manner as by a well known V board. Through the folding process a face section 69 of the web 60 is superposed over a back section 70.
The parts of the base section 69 between each of the pairs of lines of severance 64 is removed as by a vacuum head shown schematically at 72 to produce a bag opening aligned with and superposed over an associated line of weakness 62.
Transverse seals 74 are formed by a heat sealer shown schematically at 75.
Each of the seals shown in Figure 6, delineates a bottom of one of the chain of bags being formed. A hot knife 77 forms a bead seal 78 along the web side edge opposite the fold 68 to complete the chain of bags. Optionally a second hot knife 80 may form an opposed bead seal 81 to assure that the openings delineated by the lines of severance 64 extend fully from one side edge to the other of each bag, if that is desired. Alternatively, the lines of severance may extend to the fold and use of the second hot knife 80 is not required.
Referring now to Figure 7, face and back webs 10, 12, as in the embodiment of Figures 4 and 5, are fed along individual paths. Lines of weakness 62 and lines of severance 64 are respectively formed in a manner similar to the embodiment of Figure 6 but with separate cutter and anvil rolls (not shown) rather than the dual cutter and anvil rolls 65, 66 of Figure 6. Thereafter, they are juxtaposed and the transverse seals 74 and the bead seal 78, 81 are formed in a manner corresponding to the embodiment of Figure 6.
With the embodiment of Figure 8, the upper face section 10 is severed into individual parts 83 by cutter and anvil rolls 84, 85 which form lines of severance 64 extending across the full width of web. Thereafter the individual parts 83 are suitably fed by a conventional mechanism, not shown, into juxtaposition with the back web 12. Transverse lines of weakness 62 are formed in the back web by coacting cutter and anvil rolls 87, 88, shown at a location prior to wet juxtaposition but they may be located at down stream locations along the path of travel. Once the parts 83 are juxtaposed with the back web 12, the transverse seals 24 and the bead seals 78, 81 are formed in the manner described in connection with Figure 6.
Operation hi operation as depicted in Figures 4 and 5, coils of single ply plastic are mounted to provide the front and back supplies 10, 12. The materials of the webs may be other than identical so long as they are capable of being sealed together.
For example, one web may be pigmented such that it is translucent or opaque while the other web is clear. Typically the plastic will be polyethylene, although other thermal softenable plastics capable of adherence together on application of heat and pressure are sometimes employed.
Webs from the supplies 10, 12 are fed along their respective independent paths of travel through the tension control nip rolls 18, 20 to the juncture nips 17.
They are then fed along the path 28 past the hot knives 22, 23, the transverse sealer 30, the perforator 32, the zinger 34 and thence to the take up 38.
Once the machine is set up and operation commences and the nips 18, 20 are adjusted to provide differential tension along the paths 14, 15. The appropriate tension is a function of the material, its thickness and its width.
Once appropriate tension has been at least provisionally established and temperatures of the hot knives and transverse sealer are adjusted to appropriate to levels, production commences. Tension is further adjusted as the machine operates until desired finished products are consistently produced. During production the two plies are fed past the hot knives to create a tube with a front face stretched more than the back. This differential stretching is maintained as the now formed tube passes the transverse sealer and the perforator. Once the face web is opened by the zinging operation, the tension in the just opened web face section is released and it will shrink longitudinally of the web relative to the back preferably to produce the desired opening of at least 1/64 (one sixty fourth) of an inch measured longitudinally of the web.
With the embodiments of Figures 6 - 8, relative tension of the web sections is not critical in that bag openings of sufficient width are formed by producing the pairs of lines of severance 74 in each of those embodiments in the manner described. In the three embodiments shown once the lines of severance 64 and the lines of weakness 62 are formed, the front and back sections are juxtaposed.
Thereafter, the bead seals 78 and the transverse seal 74 are formed. While in each embodiment the schematic drawings depict the formation of the transverse seals before the bead seals, the sequence can obviously be reversed.
Similarly, removal of web parts between lines of severance is shown in Figure 6 to occur as the webs are juxtaposed, but this operation may also be performed at other locations along the path of travel. After juxtaposition of the front and back sections, the bead seal 81 is formed in the embodiments of Figures 7 and 8 and may be formed in the embodiment of Figure 6 if desired. With all three embodiments, a chain of bags is produced in which each bag opening, as in the embodiment depicted in Figures 4 and 5, has sufficient longitudinal extent to assure facile detection of the associated line of weakness.
Although the invention has been described in its preferred form with a certain degree of particularity, it is understood that the present disclosure of the preferred form has been made only by way of example and that numerous changes in the details of construction, operation and the combination and arrangement of WO 95/09727 ~ ~ PCTlUS94111346 parts may be resorted to without departing from the spirit and the scope of the invention as hereinafter claimed.
Claims (13)
1. A process of forming a chain of pre-opened bags comprising:
a) independently feeding first and second plastic webs along individual paths of travel to a common path;
b) differentially tensioning the webs while in their independent paths by stretching the first web more than the second such that the first web which will form bag faces will retract longitudinally more than the second web upon release of the web tension;
c) while so differentially tensioned forming edge seals between the webs to convert the webs into a tube;
d) forming longitudinally spaced transverse seals between the webs to delineate bottoms of bags being formed;
e) forming transverse lines of weakness in said second web to facilitate separation of bags from the remainder of the web during a subsequent use; and f) releasing the tension in individual bag sections of said first web by forming longitudinally spaced transverse separations of the sections and thereby producing a space between each contiguous pair of said sections.
a) independently feeding first and second plastic webs along individual paths of travel to a common path;
b) differentially tensioning the webs while in their independent paths by stretching the first web more than the second such that the first web which will form bag faces will retract longitudinally more than the second web upon release of the web tension;
c) while so differentially tensioned forming edge seals between the webs to convert the webs into a tube;
d) forming longitudinally spaced transverse seals between the webs to delineate bottoms of bags being formed;
e) forming transverse lines of weakness in said second web to facilitate separation of bags from the remainder of the web during a subsequent use; and f) releasing the tension in individual bag sections of said first web by forming longitudinally spaced transverse separations of the sections and thereby producing a space between each contiguous pair of said sections.
2. The process of claim 1 wherein transverse lines of weakness are concurrently formed in both webs and thereafter the lines of weakness in the first web are broken to form the transverse separations and thereby release the tension in the sections of the first web.
3. The process of claim 2 wherein the lines of weakness are perforations.
4. The process of claim 1 wherein the lines of weakness are perforations.
5. The process of claim 1 wherein the differential stretching is achieved while the webs are in their independent paths.
6. The process of claim 5 wherein each such space is at least 1/32 inch in dimension longitudinally of the web.
7. The process of claim 6 wherein the differential tensioning is maintained in those portions of the webs being joined by side seals.
8. The process of claim 5 wherein the differential stretching is accomplished by differential tensioning the webs while in their independent paths.
9. A process of forming a chain of interconnected and pre-opened bags comprising:
a) feeding a bag face web along an independent path of travel to a joint path of travel;
b) feeding a bag back web along a different independent path of travel to the joint path;
c) tensioning the webs as they are fed along their respective independent paths to differentially stretch the webs with the face web being stretched more than the back web;
d) forming side seals between the webs while so differentially stretched to form a tube;
e) delineating bag bottoms by forming transverse, longitudinally spaced seals between the webs;
f) forming face and back web pairs of transverse lines of weakness at longitudinally spaced locations with each pair of lines delineating a bag top;
g) zinging sections of the face web forming bag faces to tear the face web perforations and thereby open each bag; and h) releasing the web tension to allow the inherent resiliency of each web to achieve an unstretched condition and thereby produce a space between each bag face and its adjacent bag end whereby to provide a chain of easy open bags with easily detectable lines of weakness.
a) feeding a bag face web along an independent path of travel to a joint path of travel;
b) feeding a bag back web along a different independent path of travel to the joint path;
c) tensioning the webs as they are fed along their respective independent paths to differentially stretch the webs with the face web being stretched more than the back web;
d) forming side seals between the webs while so differentially stretched to form a tube;
e) delineating bag bottoms by forming transverse, longitudinally spaced seals between the webs;
f) forming face and back web pairs of transverse lines of weakness at longitudinally spaced locations with each pair of lines delineating a bag top;
g) zinging sections of the face web forming bag faces to tear the face web perforations and thereby open each bag; and h) releasing the web tension to allow the inherent resiliency of each web to achieve an unstretched condition and thereby produce a space between each bag face and its adjacent bag end whereby to provide a chain of easy open bags with easily detectable lines of weakness.
10. A process for forming an elongate chain of interconnected, preopened, plastic bags comprising:
a) forming an elongate flattened tube having juxtaposed face and back plies;
b) forming a series of spaced, bag bottom delineating, transverse seals between the plies;
c) forming transverse lines of weakness in the back ply spaced from one another at intervals corresponding to the spacing between the seals, each of the lines of weakness being near one of the seals to delineate ends of two contiguous bags being formed;
d) forming bag openings in the front ply, each bag opening being aligned with an associated one of the lines of weakness with each opening extending longitudinally of the web in both directions from its associated line of weakness a distance sufficient to assure detector access to the associated line of weakness; and, e) collecting a quantity of the formed interconnected bags into a dispensing arrangement comprised of a selected one of a coil and a festooned array.
a) forming an elongate flattened tube having juxtaposed face and back plies;
b) forming a series of spaced, bag bottom delineating, transverse seals between the plies;
c) forming transverse lines of weakness in the back ply spaced from one another at intervals corresponding to the spacing between the seals, each of the lines of weakness being near one of the seals to delineate ends of two contiguous bags being formed;
d) forming bag openings in the front ply, each bag opening being aligned with an associated one of the lines of weakness with each opening extending longitudinally of the web in both directions from its associated line of weakness a distance sufficient to assure detector access to the associated line of weakness; and, e) collecting a quantity of the formed interconnected bags into a dispensing arrangement comprised of a selected one of a coil and a festooned array.
11. The process of claim 10 wherein the longitudinal dimension of each opening is at least about 1/32 inch.
12. The process of claim 11 wherein each opening is substantially longitudinally symmetrical of its associated line of weakness.
13. The process of claim 10 wherein each opening is substantially longitudinally symmetrical of its associated line of weakness.