Prior art keywords
oil
composition
soluble
alkyl
substituted
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Abandoned
Application number
CA 2070131
Other languages
French (fr)
Inventor
John V. Hanlon
Charles H. Kolich
John G. Bostick
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Afton Chemical Corp
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Publication of CA2070131A1 publication Critical patent/CA2070131A1/en
Abandoned legal-status Critical Current

Links

Abstract

Case EI-6349+

ORGANIC PHOSPHATES AND THEIR USE AS WEAR INHIBITORS
Abstract of the Disclosure Compositions comprising a combination of (i) at least one hydrocarbon-soluble aryl phosphate of the formula (RO)3PO
wherein each R is, independently, phenyl or an alkyl-substituted phenyl group; and (ii) at least one hydrocarbon-soluble aryl polyphosphate of the formula

Description

Case EI-6349+
2~7~131 ORGANIC PHOSPHATES AND THEIR USE_AS WEAR INHIBITORS

This inven~ion relates to novel organic phosphate ester combinations and their preparation, combinations which are particularly useful as wear inhibitors in fuels, lubricants and functional fluids.
A need exists for ashless (i.e., metal-free) wear inhi-bitors for use in lubricating oils and oil-based functional fluids subjected to high temperatures during actual service conditions.
This need is particularly acute in the case of syn-thetic diester-based lubricants for use as gas turbine lubricants. A need also exists for ashless wear inhibitors for use in middle distillate fuels such as diesel fuels, jet fuels and turbine fuels.
This invention provides, in one of its embodiments, a combination of aryl phosphates deemed suitable for use in fulfilling the aforesaid needs. The combination is composed of (i) at least one fuel- and/or oil-soluble aryl phosphate of the formula (RO)3P~
wherein each R is, independently, phenyl or an alkyl-substi-tuted phenyl group; and (ii) at least one fuel- and/or oil-soluble aryl polyphosphate of the formula O O
ll ll RO-[-P-O-Ar-~-] n P ( OR; z OR
wherein each R is, independently, phenyl or an alkyl-substituted phenyl group, Ar is m-phenylene or an alkyl-substituted m-phenylene group, and n is a wh~le or number from 1 to 4; said combination containing from 2 to 30% by weight of component (i). When the above formula represents a mixture of the depicted polyphosphates, n is a whole or fractional number from 1 to 4, as n represents the average composition of the mixture.
Among the advantages of these combinations is the ease with which they can be formed pursuant to another em-bodiment of this invention. In particular, the foregoing Case EI-6349~
2~7~13~

combinations can be formed by a process which comprises (a) reacting from about 1.9 to about 2.1 equlvalents of phenol and/or alkyl-substituted phenol with one equivalent of phos-phoryl trihalide in the presence of a Lewis acid catalyst, and (b) reacting the intermediate product formed in (a) with from about 0.9 to about 1.1 equivalents of resorcinol and/or alkyl-substituted resorcinol per equivalent of phosphoryl trihalide employed in (a) again in the presence of a Lewis acid catalyst. Although other modes of addition can be used, it is preferable in (a) to add the phenol and/or al-kyl-substituted phenol to the phosphoryl trihalide, and in (b) to add the resorcinol and/or alkyl-substituted resorci-nol to the intermediate product formed in (a). Non-limiting examples of suitable Lewis acid catalysts include AlCl3, AlBr3, FeCl3, FeBr3, BCl3, PCls, and MgCl2. In an alternate process, the Lewis acid catalyst is replaced by a stoichio-metric amount of a hydrogen halide acceptor and a solvent is used. In step (a) a solution of phenol and/or an alkyl-sub-stituted phenol and hydrogen halide acceptor is added to a solution of the phosphoryl trihalide, and in step (b) a so-lution of resorcinol and/or an alkyl-substituted resorcinol and hydrogen halide acceptor is added to the intermediate product formed in step (a).
In still another embodiment, the foregoing combina-tions are ~oxmed by a process which comprises (a) reacting from about 0.9 to about l.1 equivalents of resorcinol and/or alkyl-substituted res~rcinol with one equivalent of phospho-ryl trihalide in the presence of a Lewis acid catalyst, and (b) reacting the intermediate product formed in (a) with from about 1.9 to about 2.1 equivalents of phenol and/or alkyl-substituted phenol per equivalent of phosphoryl tri-halide employed in (a) again in the presence of a Lewis acid catalyst. Although other modes of addition can be used, it is preferable in (a) and in (b) to add the resorcinolic and the phenolic reactants to the phosphoryl trihalide and to the reaction mixture formed in (a), respectively. In an alternate process, the Lewis acid catalyst is replaced by a stoichiometric amount of a hydrogen halide acceptor and a Case EI-6349+
~ 3 ~ 2~70131 solvent is used. In step (a) a solution of resorcinol and/
or an alkyl-substituted resorcinol and hydrogen halide ac-ceptor is added to a solution of the phosphoryl trihalide, and in step (b) a solution of phenol and/or an alkyl-substi-tuted phenol and hydrogen halide acceptor is added to theintermediate product for~ed in step (a).
In each of the above processes, it is preferred to employ the reactants in proportions such that there are at least 3.1 equivalents of ar-hydroxy groups (phenolic reac-tant plus resorcinolic reactant) per equivalent of phosphor-yl trihalide used.
Lubricant compositions which comprisa a major pro-portion of oil of lubricating viscosity -- preferably a diester-based lubricating oil, i.e., a lubricating oil composed predominantly or entirely of one or more diester lubricating oils -- containing and a minor wear-inhibiting amount of a combination of phosphate esters (i) and ~ii) as described hereinabove, form the subject of another embodi-ment of this invention.
Another embodiment is middle distillate fuel compo-sitions which comprise a major proportion of a hydrocarbon-aceous middle distillate fuel and a minor wear-inhibiting amount of a combination of phosphate esters (i) and (ii) as described hereinabove.
In the various embodiments referred to above, most preferably each R is phenyl and Ar is m-phenylene. Like-wise, it is preferred that at least 50% by weight of the aryl polyphosphate correspond~ to the above formula of com-ponent (ii) wherein n is 1. Particularly preferred are (1) compositions wherein each R is phenyl and at least 50% by weight of the aryl polyphosphate is m-phenylenebis(diphenyl phosphate), and (2) compositions wherein at least 60~ by weight of the combination of phosphate esters is a combi-nation of m-phenylenebis(diphenyl phosphate) and triphenyl phosphate in a weight ratio of 1 to 35 parts o~ m-phenylene-bis(diphenyl phosphate) per each part by weight of triphenyl phosphate.
The above and other embodiments of this invention Case EI-6349~ 207~131 will be still further apparent from the ensuing description and appended claims.
In forming the combination of aryl phosphates, use can be made of phenol and/or one or more alkyl phenols which contain from 1 to 5 alkyl groups on the ring. Each such alkyl group can contain up to about 18 carbon atoms with the proviso that the alkyl substituent(s) should not sterically hinder the hydroxyl group to such an extent that the substi-tuted phenol is incapable of reacting with the phosphoryl trihalide. Examples of suitable alkyl phenols include o-, m~ and/or p-cresol; 2,3-, 2,4-, 2,5-, 2,6-, 3,4-, and/or 3,5-xylenol; o-, m-, and p-ethylphenol; p-tert-butylphenol;
p-tert-amylphenol; p-(1,1,3,3-tetramethylbutyl)phenol; p-nonylphenol; p-decylphenol; 2,4,5-trimethylphenol; 2,3,4,5-tetramethylphenol; pentamethylphenol, etc. Cycloalkylphe-nols such as p-cyclohexylphenol can also be used. Mixtures of two or more different phenols are also suitable.
The phosphoryl trihalide used in forming the phos-phate combinations is preferably phosphoryl trichloride, but other halides such as the tribromide can be used.
Resorcinol is the preferred dihydroxybenzene reac-tant used in forming the phosphate combinations. However alkyl-substituted resorcinols can be used again with the proviso that the compounds are not so sterically hindered as to be unable to undergo reaction on both hydroxyl groups with the intermediate formed from the reaction between the monohydric phenol and phosphoryl trihalide.
A few examples of alkyl-substituted resorcinols that can be used include 5-alkyl-1,3-dihydroxybenzenes where the alkyl group has 1 to about 18 carbon atoms; 2-methyl 1,3-di-hydroxylbenzene;4-methyl-1,3-dihydroxylbenzene;4,5-dimeth-yl-1,3-dihydroxybenzene; and the like.
The reactions of (a) and (b) above are usually con-ducted at temperatures in the range of absut 30C to about 200C. It is desirable and most economical to conduct these reactions without a solvent and in the presence of a ~ataly-tic amount of a Lewis acid. However, a suitable inert liq-uid solvent such as toluene, xylene, aromatic naphtha, or Case EI-6349-~ 2070131 the like can be used.
The amount of catalyst used is typically between 0.1 wt % and 10 wt % based upon the amount of phosphoryl triha-lide. More preferred is 0.5 wt % to 5.0 wt % and most pre-ferred is 0.75 wt % to 2.00 wt ~.
In place of the Lewis acid catalyst, an at least stoichiometric amount of a hydrogen halide acceptor can be used. Hydrogen halide acceptors which are preferably used in the reactions of (a) and (b) above are typified by tertiary amines such as pyridine, pyrimidine, pyrazine, triethylamine, tributylamine, and triphenylamine. Other known hydrogen halide acceptors are usable, however. It is most desirable to use an inert solvent for the reactions involving hydrogen halide acceptors in order to facilitate handling of the solid hydrohalide by~product. Suitable solvents are toluene, xylene, aromatic naphtha, or the like.

The following examples illustrate various phosphate combinations of this invention, and methods which can be used for their synthesis.

A 912.87 g (9.70 mole) portion of phenol (Aldrich, redistilled) and a 766.65 g (5.00 mole) portion of POC13 (Aldrich, 99%) were weighed into a dry, four-necked 5-L
flask in a glove box. The flask was then set up in a hood with a mechanical paddle stirrer, a thermometer, a glycol-cooled Friedrich condenser, an oil bath, and a rubber septum addition port. Exit gases from the condenser were passed through a trap and into an aqueous NaOH scrubber solution located on a balance. A slow nitrogen purge was maintained into the contents of the flask by a Teflon tube inserted through the rubber septum addition port.
The brownish-gold solution was warmed to 33C by the oil bath, and 15.42 g (2.01 wt % based on POCl3) of AlCl3 (Aldrich) catalyst was cautiously added. The solution was slowly heated to 116C over a seven hour period while 344.9 g of HC1 (97.5~ of theory) collected in the exit gas scrubber. The solution was then cooled to room temperature, Case EI-6349+ 2fJ70131 and a 291.79 g (2.65 mole) portion of resorcinol (Aldrich, recrystallized~ was added (in a ylove box). The reddish-purple mixture was then slowly heated to 170C over a five and one-half hour period while 172.1 g of HCl (89.1% of theory) collected in the scrubber.
The viscous golden-yellow crude product was dissolved in toluene t2544.5 g), and the solution was shaken with 10 wt % aqueous NaOH (2x1000 g) and then tap water (3x1000 g) to obtain 3840.4 g of cloudy colorless organic phase. The solution was then dried over 125 g of anhydrous MgS04. The liquid was decanted from the drying agent and passed through a bed (28 mm O.D. by 364 mm length) of 101.0 g activated silica gel (Aldrich, 70~230 mesh, 500 M2~g, wet packed using toluene). The eluate was then stripped on a 15 rotary evaporator (95C/0.1 torr) to obtain 1242.7 g (87.2~
yield) of a slightly hazy, pale yellow fluid. This liquid was pumped through a 10-micron Teflon membrane filter to obtain 1227.67 g of a clear pale yellow product, properties of which are summarized in Table I hereinafter.

A 77.24 g (0.5037 mol~) portion of POCl3 (Aldrich) and 148.6 g toluene were weighed into a 1-L four-necked flask in a glove box. The flask was set-up in a hood and equipped with a paddle stirrer, thermometer, 500-mL addition funnel, and a glycol-cooled Friedrich condenser attached to a nitrogen bubbler. The flask was cooled with an ice bath while a solution of 90.07 g (0.957 mole) phenol (Aldrich, redistilled), 99.64 g (0.986 mole) triethylamine (TEA, Aldrich), and 101.94 g toluene was added from the additional funnel in 2.5 hr at 3-15C. After stirring for 15 minutes at 7-15C, a hot (70-90C) clear blue solution of 30.51 g (0.277 mole) resorcinol (Aldrich, recrystallized~ in 118.19 g (1.170 mole) TEA was pressured into the reaction flask through a stainless steel transfer needle from a capped bottle in 13 minutes at 15-29C. The reaction mixture was stirred for 2.2 hr at 23-32C, and then 202.7 g of 5 wt ~
aqueous HCl was added follow d by 39.6 g concentrated hydrochloric acid. The mixture was transferred to a Case EI-6349~ 2070131 separatory funnel, and the lower hazy yellow aqueous layer (514.8 g, pH 1-2) was removed. After washing with water (3x225 g), the cloudy organic phase (513.6 g) was dried over 10.1 g anhydrous magnesium sulfate. Upon standing for 16 hr, the addition of 6.8 g of activated silica gel (Aldrich, 70-230 mesh, 500 m2/g) immediately reduced the color of the yellow liquid. The mixture was gravity filtered through paper, and the pale-yellow filtrate as stripped on a rotary evaporator (100C/1 torr) to obtain 131.3 g (92% yield) of hazy light-yellow fluid. A clear liquid was obtained after pumping the product through a 10-micron membrane filter.
Table I, presented hereinafter, summarizes the properties of this product.

This experiment was conducted as described in Exam-ple 1. A 184.46 g (1.960 mole) portion of phenol was com-bined with 153.33 g (1.000 mole) of POCl3 in a 500-mL four necked-flask. The pale-yellow solution was warmed to 38C, and 3.075 g (2.0 wt ~ based on POCl3) of MgCl2 was added, the pale-orange solution was then 510wly heated with an electric mantle for 8.0 hr to a final temperature of 150C. The cau-stic scrubber for the exit gases from the reaction increased ih weight by 65.1 g (91% theory for HCl). The reaction flask was transferred to a glove box where 57.26 g (0.520 mole) of white resorcinol (Aldrich, recrystalliz~d) was added. The mixture was then slowly heated over three and one-half hours to a final temperature of 140C with the subsequent incr~ase in the exit gas scrubber weight of 32.7 g (86.2% of theory for HCl). The dark brown viscous liquid (287.33 g) was dissolved in 557.29 g toluene and washed in a 2-L ssparatory funnel with 5.2 wt % aqueous NaOH (2x250 g~. The organic phase was then washed with tap water (3x275 g) until the recovered aqueous phase reached a pH of 7. The cloudy organic phase was dried over anhydrous magnesium sulfate (30.46 g). The mixture was then gravity filtered through paper, and the clear, nearly colorless filtrate was stripped of solvent on a rotary evaporator (0.1 torr/90~C) to obtain 202.2 g (70.8~ yield) of a slightly hazy pale-Case EI-6349+ - 8 - 2070131 yellow fluid. The liquid was pumped through a 10-micron Teflon membrane filter to obtain 193.36 g of a clear pale-yellow product. Properties of this sample are summarized in Table I below.

A 376.44 g (4.00 mole) portion of phenol is combined with 306.66 g (2.00 mole) of POCl3 in a l-L four necked flask in a glove box. The light-orange solution is warmed to 40OC
and 2.993 g (1.0 wt % based on POCl3) of pyridine (Baker) is added. The solution is heated with an electric mantle until gas evolution stops (llo0 hr/145C). The exit gas scrubber shows a weight increase of 139.8 g (95.9~ of theory for HCl).
A 114.51 g (1.04 mole) portion of resorcinol is added to the light-yellow reaction mixture in a glove box.
The solution is heated to 30~C and 3.062 g (1.0 wt % based on POCl3) of magnesium chloride is added. The rusty-brown solution is heated until gas evolution stops (7.0 hr/149C).
The subsequent increase in the exit gas scrubber is 64.0 g (84% of theory for HCl). The light-yellow viscous liquid is dissolved in 1070 g toluene. The solution is washed in a 4-L
separatory funnel with dilute (2.8 wt %) aqueous NaOH (2x290 g) and then water (3x400 g). The cloudy organic phase is gravity filtered through paper to obtain a clear colorless filtrate. The filtrate is stripped on the rotary evaporator (0.1 torr/95C) to obtain 484.8 g ~84.4~ yield) of pale yellow cloudy liquid~ The li~uid is pumped through a 10-micron Teflon membrane filter to obtain 472.5 g of clear product. Properties of this sample are given in Table I.

A 188.56 g (2.00 moles) portion of phenol (Aldrich, redistilled) was combined with 153.35 (1.00 mole) of POCl3 (Aldrich) in a 500-mL four-necked flask. The clear light-brown solution was warmed to 35C, and 3.039 g (1.98 wt %
based on POCl3) of aluminum chloride (Aldrich) was a~ded. A
small exotherm increased the temperature to 42C as HCl evolution began. The clear red solution was then slowly heated with an electric mantle for 5 hours to a final tem-Case EI-6349~ 2 ~ 7 ~
_ 9 perature of 109~C. The caustic scrubber for the exit gases from the reaction increased in weight by 70.4 g (96.5% of theory for HCl). The reaction flask was transferred to a glove box where 55.04 g (0.500 mole) of resorcinol (Aldrich, recrystallized) was added. The mixture was then slowly heated over 7 hours to a final temperature of 158C with the subsequent increase in the exit gas scrubber weight of 33.8 g (92.7% of theory for HCl). The light-orange viscous liguid (289.0 g) was dissolved in 467.8 g toluene and washed in a 2-L separatory funnel with 10 wt % aqueous NaOH (2x200 g). The cloudy organic phase was then washed with tap water (4x200g) until the recovered aqueous phase reached a pH of 6.5. The cloudy organic phase was dried over anhydrous mag-nesium sulfate (11.5 g). The mixture was then gravity fil-tered through paper, and the clear, nearly colorless fil-trate was stripped of solvent on a rotary evaporator (0.1 torr/90C) to obtain 252.7 g (87.9~ yield) of a slightly hazy pale-yellow fluid. The liquid was pumped through a 10-micron Teflon membrane filter to obtain 241.6 of clear pale-yellow product. The properties of this product aresummarized in Table I.

case EI-6349+ 2070131 T~BLE I

Properties ~ x. 1 IEX. 2 ¦EX. 3 ¦EX. 4 ¦EX. 5 . ~ I _ ¦Composition (HPLC wt%) .
l Triphenyl phospha-te 12.6 2.3 11.0 11.9 14.7 11 ¦ Diphosphate _ 57.278.1 66.0 65.8 63.~ Il IAPHA Color50-60 300150 60 60 1¦

¦Viscosity ae 25-C, cp 425_ 551 397 326 3~5 ¦ Density at 25'C, g/mL 1.293 1.297 1.292 1.288 1.288 ~¦
Acid Number, mg KOH/g 0 17 0.98 0.46 0.75 0 09 I _ o L Ionic Cl, ppm _~ _0 5 _12 _ 1.5 < 1.0 This experiment was carried out as described in Ex-ample 1. A 384.6 g ~1.75 mole) portion of nonylphenol wascombined with 137.94 g (0.8996 mole~ POCl3 in a 1-L four-necked flask. A 2.78 g (0.0208 mole) portion of AlCl3 was added to the mixture at 29 D C, and the mixture was heated to 118C over 3 hr. After cooling to room temperature, a 52.5 g (0.477 mole) portion of resorcinol was added to the reac-tion mixture. The reaction was completed by heating to 170C in 2.5 hr. After cooling to 45C, toluene (433.4 g) was added, and the solution was washed with 10 wt % aqueous NaOH (200 g) and twice with water. To obtain good phase separation for the last wash, the pH had to be adjusted to 10 with addition of aqueous NaOH. The organic phase was dried over anhydrous MgSO4 (25.7 g), gravity filtered through paper, and the filtrate stripped on a ro~ary evaporator (0.1 torr/100~C) to obtain 458.0 g (96.1% yield) of pale-yellow 0 oil. Properties are summarized in Table II below.

Example 6 was repeated replacing the nonylphenol with a mixture of phenol (91.30 g, 0.970 mole) and nonylphenol ~213.75 g, 0.970 mole). A 153.3~ g (1.00 mole) portion of POCl3, 58.36 g (0.530 mole) resorcinol and 3.130 g (0.023 mole) AlCl3 were used. The pale-yellow liquid Case EI-6349+ 2 0 7 01 31 product weighed 379.3 (93.1 % yield). Table II sets forth physical properties of this product.

A 55.1 g (0.50 mole) portion of resorcinol (MCB, recrystallized, 99.93 area % by GC) was weighed into a dry four-necked l-L flask in a glove box. The flask was then set-up in a hood with a mechanical paddle stirrer, a thermometer, a rubber septum addition port, and a Friedrich water condenser. Exit gases from the condenser were passed through a dry glass trap and into an aqueous NaOH scrubber solution located on a balance. A slow nitrogen flow was maintained on the exit gas line during the reaction to prevent back-up of the scrubber solution.
A 153.3 g (1.00 mole, 93 ml) portion of POC13 (Aldrich, 99~) was added to the flask by nitrogen pressure from a septum capped bottle using a stainless steel transfer needle. The easily stirred slurry was heated to 113C with less than 0.3 g of HCl being collected in the exit gas scrubber. After cooling to 40C, a 1.493 g (0.0112 mole) portion of anhydrous AlCl3 (Aldrich) catalyst was added to the purple-brown liquid. The sol~ltion was slowly heated to 110~C in 90 minutes while 37.5 g of HCl collected in the exit gas scrubber. The yellow-brown mixture was cooled to 63C and a 194.2 g (2.064 mole) portion of phenol (Aldrich, redistilled) was added in 15 min. The solution was heated to 155C in 2 hr while an additional 66.0 g (94.6% of theory for HCl~ of HCl was collected in the scrubber. Addition of another 0 93 g (0.0070 mole) AlCl3 at 120-129C did not cause release of additional HCl.
The viscous yellow-brown crude product (293.4 g) was dissolved in toluene (446.7 g), and the solution was washed with 5 wt % aqueous NaOH (3x200 g) and water (2x230 g).
The cloudy pale-yellow organic phase (722.2 g) was dried over 15.17 g of anhydrous magnesium sulfate. The mixture was gravity filtered through paper (What~an 2V), and the clear filtrate was stripped on a rotary ~vaporator (95C/0.1 torr) to obtain 260.1 g (90.5~ yield) of a slightly hazy, viscous, light-yellow liquid. The liquid was Case EI-6349+ 2070131 pumped through a 10 micron Teflon membrane filter to remove the hazy appearance. Properties of this product are summarized in Table II below.

Example 8 was repeated using the same reagents but with a higher level of resorcinol. Phosphoryl chloride (153.5 g, 1.001 mole) was added to resorcinol (66.15 g, 0.6008 mole) at 25C in 5 minutes. The temperature dropped to 20C, and there was no evidence of HCl evolution from the easily stirred slurry. A 1.561 g (0.0117 mole) portion of anhydrous AlC13 was added, and the mixture was warmed gently with an electric mantle. At 30C, HCl evolution began slowly and nearly all solids had dissolved in the red-brown liquid. Gas evolution continued at 60-80C for 1 hr. A
weight increase of 44.0 g was recorded for the exit gas scrubber, and the solution color changed to yellow-brown.
Liquid phenol (193.2 g, 2.053 mole) was then added 5 minutes at 70-77C. The mixture was held at 72-78C for 2.5 hr during which the scrubber weight increase rose to 99.0 g (90% of theory for HCl). The solution was then heated to 122C in 2 hr with the scrubber weight gain reaching a constant value of 103.5 g ~94.5% of theory). The clear orange liquid was sparged with nitrogen overnight at ambient temperature. A solution of the crude product (299.5 g) in toluene (449.4 g) was washed with 10 wt ~ aqueous NaO~
(4x200 g) and then deionized water (3x300 g) to obtain 697.9 g of a cloudy colorless organic phase. The solution was dried over 16.3 anhydrous MgSO4, gravity filtered through paper, and stripped on a rotary evaporator to obtain 238.1 g (84.8~ yield) of a slightly hazy, nearly colorless viscous liquid. The liquid was pumped through a 10 micron Teflon membrane filter to remove the hazy appearance.
Properties of the products formed in Examples 6-9 are summarized in Table II.

Case EI-6349+ 2~70~31 TABLE II

Propertles ¦ Ex. 6 j Ex. ' ¦ Ex. 8 ¦ Ex. 9 , _ __ ; . - ~r~-¦Composition (HPLC wt~) Triphenyl phosphate __ __ 1 17.4 9.2 Diphosphate __ __ 24.6 22.4 APHA Color __ __ 100 100-200 . . . _ .
Viscosity at 25-C, cp 111,40010,350 488 1270 Density at 25'C, g/mL 1.051 1.129 1.296 1.312 Acid Number, mg KOH/g O.10 O.07 O.41 O.07 Ionlc Cl, ppm ........ ~.1, 27~ 330< 40 ~ 97 The excellent thermal stability of the products of this invention was illustrated by a series of thermogravi-metric analyses in which weight loss of various phosphorus-containing materials was determined in the range of up to 600C. Subjected to this test were the phosphate combina-tion produced as in Example 1 and the phosphate combination produced as in Example 6. For comparative purposes TGA
analyses were also conducted on samples of tri~n-octyl phosphate (TOP), tricresyl phosphate (TCP~, tri-n-butoxy-ethyl phosphate (TBEP), and cresyl diphenyl phosphate (CDP).
The results of these determinations are summarized in the following table:

Case EI-6349~ 2 0 ~ O 131 TABLE III - TGA. % LOSS

TemPerature, C
Phosphorus Compound _ 100200 300 350400 500 600 Example 1 0.01.315.8 39.0 77.8 97.4 98.8 Example 6 0.00.6 4.8 8.420.281.5 --Example 7 0.00.6 4.3 -- 23.992.9 --TOP 0.0 3.398.3 -- 98.7 -- -~
TCP 0.0 1.276.3 -- 99.1 -- --TBEP 0.5 2.496.5 -- 97.1 -- --CDP 0.0 1.488.0 -- 99.5 99.6 --The antiwear properties of the phosphate combina-tions of this invention, are illustrated by the results obtained in a series of standard tests known as the ball on cylinder lubricity evaluation test. The test procedure is ASTM D 5001-90. In these tests scar diameter measurements are taken, and thus the smaller the scar diameter, the more e~fective the additive composition as regards wear inhi-bition. For convenience, the results are herein expressed in numerical values representing the scar diameter in milli-~eters multiplied by 100.
In a first series of tests the aryl phosphate combi-nation formed as in Example S was blended into a commer-cially-available jet fuel at a concentration of 25 pounds per thousand barrels (ptb). This blended fuel was stored at 77F under ambient liyht conditions for two months prior to conducting the lubricity test, to be sure that the fuel com-position had good storage stability. The clear base fuel in this test showed a scar diameter of 67 whereas the fuel con-taining the phosphate combination of this invention exhibit-ed a scar diameter of 44.
In another such test the base fuel had a scar dia-meter of 60 whereas the presence therein of 80 parts per million (ppm) of a combination formed as in Example 4 Case EI 6349+ 2070131 reduced the scar diameter to 40.
Another series of such lubricity tests were conduc-ted wherein the base fuel was a commercial JP-4 jet fuel.
This fuel as received gave a scar diameter of 60. The pre-sence in the fuel of an aryl phosphate combination producedas in Example 5 at the level of 25 ptb gave a scar diameter of 46. It is interesting to note that the presence in the same base fuel of comparable concentrations of tricresyl phosphate, trioctyl phosphate, and tributoxyethyl phosphate gave, respectively, scar diameters of 80, 80 and 83.
When the lubricity test was applied to a series of fuels based on a low sulfur grade of commercially-available diesel fuel, the following results were obtained:

Fuel composition Scar diameter 15 Base fuel 65 Base fuel + 25 ptb combination per Example 5 47 Base fuel + 25 ptb tricresyl phosphate 64 Base fuel + 25 ptb trioctyl phosphate 65 Base fuel + 25 ptb tributoxyethyl phosphate 66 Another series of lubricity tests was carried out using commercially-available jet fuel. The test results are tabulated below.

Fuel composition Scax diameter Base fuel 68 25 Base fuel ~ 25 ptb combination per Example 5 56 Base fuel ~ 25 ptb tricresyl phosphate 67 Base fuel + 25 ptb trioctyl pho~phate 68 Base fuel + 25 ptb tributoxyethyl phosphate 72 A group of tests were conducted in which two dif-ferent aryl phosphate combinations were blended into a com-mercially-available jet fuel at several different concen-tration levels. One such additive combination was produced as in Example 5 and thus, referring to the formulas given above, R was phenyl and Ar was m-phenylene. In the other Case EI-6349+ 2 0 7 01 31 such additive combination, R was nonylphenyl and Ar was m-phenylene. The results of these tests are presented below wherein "Combination A" refers to the combination wherein R
was phenyl, and "Combination B" refers to the combination wherein R was nonylphenyl:

Fuel composition Scar diameter Base fuel 73 Base fuel + 80 ppm Combination A 39 Base fuel ~ 40 ppm Combination A 56 10 Base fuel ~ 20 ppm Combination A67 Base fuel + 10 ppm Combination A 69 Base fuel + 80 ppm Combination B 68 Base fuel + 40 ppm Combination B 67 Base fuel + 20 ppm Combination B 68 15 Rase fuel + 10 ppm Combination B Ç8 The phosphate combinations of this invention can be used as antiwear agents in any middle distillate fuel suit-able for use in the operation of a jet engine, a gas turbine engine or a diesel engine. Such fuels are predominantly hy-drocarbonaceous in composition and are typically character-ized by boiling ~n the range of about 130C to about 400~C.
It is to be noted that the term "middle distillate fuel" is not intended to be restricted to straight-run distillate fractions. These middle distillate fuels or fuel oils can comprise straight run distillate fuel oils, catalytically or thermally cracked ~including hydrocracked) distillate fuel oils, or mixtures of straight run distillate fuel oils, naphthas and like stock6, with cracksd distillate stocks.
Moreover, such fuel oils can be treated in accordance with well known operations such as acid or caustic treatment, hydrogenation, solvent refining, clay treatment, and the like. The base fuels thus include diesel fuels, kerosenes, jet fuels, gas oils, cycle oils etc. While derived princi-pally from petroleum, the fuels can be derived at least in part from shale, tar sands, coal, lignite, biomass, and si-milar sources. The fuels can contain suitable oxygenated blending components, such as alcohols, ethers, etc, includ-Case EI-6349+ 207~3~

ing in situ produced oxygenates.
In general, the compositions of this invention are employed in the base fuel in an amount at least sufficient to inhibit wear between contacting metal surfaces.
Ordinarily, such amounts will fall within the range of from about 0.005 to about 5 percent by weight of the base fuel, and more typically within the range of from about 0.05 to about 2 percent by weight based on the weight of the base fuel.
Various additional additives may be used in the fuels of this invention. These include antioxidants, conductivity improvers (also known as static dissipator additives), metal deactivators, icing inhibitor additives, cetane improvers, combustion improvers (including smoke suppressants), detergent/dispersant additives, induction system cleanliness agents, corrosion inhibitors, demulsi-fying agents, top cylinder lubricants, dyes, and the like.
Of the antioxidants, use of phenolic antioxidants is preferred, although other fuel-soluble antioxidants are available and can be used. Other suitable types of anti-oxidants include amine antioxidants, phosphite esters, sulfur-containing antioxidants, and other similar sub-stances. Amounts of antioxidant in the range of about 1 to about 10 pound~ per thousand barrels are typical. However, greater or lesser amounts can be used whenever deemed necessary or desirable.
Various conductivity improvers suitable for use in the fuels of this invention are available in the market-place. These include ASA-3 marketed by Royal Lubricants Co., and Stadis 450 marketed by E. I. duPont de Nemours Co.
Typically, conductivity improvers are additives that can be dissolYed in the fuel in the amount necessary to increase the fuel conductivity to within a suitable range, such as between about 50 and about 600 pS/m as determined by ASTM D-2624. For further detail concerning conductivity improverswhich can be utilized, see U.S. Pat. Nos. 3,449,097; 3,455,-665; 3,578,421; 3,652,238; 3,676,647; 3,674,450; 3,784,362;
3,917,466; 4,029,480; 4,113,443; 4,252,542; 4,25~,087;

Case EI-6349+ 207~131 4,333,741; 4,356,002 and 4,416,668.
Metal deactivators which can be used in the fuels of this invention include N,N'-disalicylidene-1,2-propanedia-mine, N,N'-disalicylidene-1,2-cyclohexanediamille, N,N'-disalicylidene-1,2-ethanediamine, N,N"-disalicylidene-N'-methyl-dipropylenetriamine. 8-hydroxyquinoline, ethylene diaminetetracarboxylic acid, acetylacetone, octylacetoace-tate, and like substances. Thiadiazoles such as HITEC~ 314 additive (Ethyl Petroleum Additivas, Inc.; Ethyl Petroleum Additives, Ltd.; Ethyl Canada Ltd.; Ethyl S. A.) can also be used for this purposeO Amounts of up to about 2 pounds of metal deactivator per thousand barrels are ordinarily suffi-cient, but higher concentrations can be used whenever neces-sary or desirable.
Icing inhibitor additives that can be used include, for example, alcohols, glycols, monocarboxylic acid esters of polyoxyalkylene glycols, and nitroketonized amides.
Amounts of up to about 50 pounds per thousand barrels are usually sufficient.
Detergent/dispersant additives which are suitable for use in the fuels of this invention include amides and imides especially succinimides (e.g., U.S. Pat. Nos.
3,471,458; 3,655,351; 4,596,663; and 4,744,798); mono- and polycarboxylic acid esters especially succinic acid esters 25 (e.g., U.S. Pat~ Nos. 3,639,242; 3~708,522; and 4,596,663);
carbamates (e.g., U.S. Pat. No. 3,652,240); hydrocarbyl polyamines (e.g., U.S. Pak. Nos. 3,753,670 and 3,756,793);
and hydrocarbyl polyether polyamines (e.g., U.S. Pat. No.
4,778,481).
As used herein the term "fuel-soluble" means that the composition in the particular base fuel employed dis-solves at 25C to at least the minimum concentration herein specified.
The above phosphate combinations can be used as antiwear agents in any of a variety of oils of lubricating viscosity. Preferably they are used in a base oil composed by volume of at least 50% and up to and including 100% of one or more mineral oils, or at least 50% and up to and Case EI 6349~ 2070131 including 100% of one or more synthetic ester oils.
The concentrations of the phosphate combinations in the base oils are minor wear-inhibiting amounts. These amounts will of course vary depending upon such factors as the type of base oil employed, the type of service to be encountered, and the amount of wear protection desired. In general, however, amounts in the range of about 0.005 to about 10 weight percent based on the total weight of the finished lubricant will usually be sufficient. Preferred amounts are in the range of about 0.25 to about 5 weight percent again based on the total weight of the finished lubricant. The phosphate combinations can be included in additive concentrates of the type used in formulating fin-ished lubricants tsuch as crankcase motor oils for gasoline engines, crankcase motor oils for diesel engines, gear oils, tractor oils, etc.) and functional fluids (such as transmis-sion fluids, hydraulic fluids, cutting and machining oils, etc.).
Further embodiments of this invention are additive concentrates and lubricant or functional fluid compositions containing particular combinations of one or more additive components (hereinafter described) together with a phosphate combination employed pursuant to this invention. For con-venience, these. are referred to hereinbelow as Emhodiments A, B, C, D, and E.
Embodiment A
One such embodiment is an oil of lubricating visco-sity or an additive concentrate for use in oil of lubricat-ing viscosity containing at least the following components:
30 1) one or more oil-soluble zinc hydrocarbyl dithiophos-phates; and 2) an aryl phosphate ester combination composed of (i) at least one oil-soluble aryl phosphate of the formula (RO)3PO
wherein each R is, independently, phenyl or an alkyl-substi-tuted phenyl group or an alkenyl-substituted phenyl group;
and (ii) at least one oil-soluble aryl polyphosphate of the Case EI-6349+ 2070131 formula O O
Il 11 RO-[-P-O-Ar-O-]n~P(OR)2 OR
wherein each R is, indspendently, phenyl or an alkyl-substituted phenyl group or an alkenyl-substituted phenyl group, Ar is m-phenylene or an alkyl-substituted m-phenylene group, and n is a whole or fractional number from 1 to 4;
said combination containing from 2 to 30% by weight of com-ponent (i). The relative proportions of these components is preferably such that the weight ratio of phosphorus in 1) to total phosphorus in 2) is in the range of from about 0.001:1 to about 100:1. These combinations serve to inhibit wear;
to inhibit deposit, varnish and/or sludge formation and/or deposition; and to protect the lubricant or functional fluid composition from premature oxidative degradation, e~pecially at elevated temperatures. The quantity of these components 1) and 2) added to the base oil of lubricating viscosity is a minor wear-inhibiting amount, and is usually such that the total concentration of phosphorus provided by components 1) and 2) tproportioned as just described) falls in the range of about 0.005 to about S percent by weight of the total composition.
Embodiment B
Another embodiment of this invention is an oil of lu-bricating viscosity or an additive concentrate for use in oil of lubrisating viscosity containing at least the follow-ing components:
1) an aryl phosphate ester co~bination composed of (i) at least one oil-soluble aryl phosphate of the formula (RO)3po wherein each R is, independently, phenyl or an alkyl-substituted phenyl group or an alkenyl-substituted phenyl group; and (ii) at least one oil-soluble aryl polyphosphate of the formula Case EI-6349-t 2~7~3~

O O
Il 11 RO- [ -P-O-Ar -O- ] n~P ( OR ) 2 OR
wherein each R is, independently, phenyl or an alkyl-substituted phenyl ~roup or an alkenyl-substituted phenyl group, Ar is m-phenylene or an alkyl-substituted m-phenylene group, and n is a whole or fractional number from 1 to 4;
said combination containing from 2 to 30% by weight of com-ponent (i); and 2) one or more oil-soluble ashless dispersants containing basic nitrogen, preferably a succinimide sr succinic ester-amide.
The relative proportions of these components is preferably such that the weight ratio of component 1) to component 2) is in the range of from about 0.001:1 to about 100:1. These combinations serve to inhibit deposit, varnish and/or sludge formation and/or deposition; and to protect the lubricant or functional fluid composition from premature oxidative degra-dation, especially at elevated temperatures. The quantity of these components 1) and 2) added to the base oil of lu-bricating viscosity is a minor wear-inhibiting amount, and is usually such that the total concentration of components 2) and 3) (proportioned as just described) falls in the range of about 0.005 to about 20 percent by weight of the total composition.
Any of a variety of ashless dispersants can be utili~ed as component 3) of the compositions of this inven-tion. These include the ~ollowing types:
Type A - Carbox~lic Ashless Dispersants. These are reaction products of an acylating agent such as a monocar-boxylic acid, dicarboxylic acid, polycarboxylic acid, or derivatives thereof with compollnds which contain amine and/
or hydroxyl groups (and optionally, other groups such as mercapto groups, etc.). These products, herein referred to as carboxylic ashless dispersants, are described in many patents, including British patent specification No.
1,306,529 and the following ~. S. Patents: 3,163,603;

Case EI-634s+ 20701~1 3,184,474; 3,215,707; 3,219,666; 3,271,310; 3,272,746;
3,281,357; 3,306,908; 3,311,558; 3,316,177; 3,340,281;
3,341,542; 3,346,493; 3,381,022; 3,399,141; 3,415,750;
3,433,744; 3,444,170; 3,448,048; 3,448,049; 3,451,933;
3,454,607; 3,467,668; 3,522,179; 3,541,012; 3,542,678;
3,574,101; 3,576,743; 3,630,904; 3,632,510; 3,632,511;
3,697,428; 3,725,441; 3,868,330; 3,948,800; 4,234,435; and Re 26,433.
Type B - Hvdrocarbyl Polyamine Dispersants. This category of ashless dispersants which can be used as component 3) is likewise well known to those skill~d in the art and fully described in the literature. The hydrocarbyl polyamine dispersants are generally produced by reacting an aliphatic or alicyclic halide (or mixture thereof) contain-ing an average of at least about 40 carbon atoms with one ormore amines, preferably polyalkylene polyamines. Examples of such hydrocarbyl polyamine dispersants are described in U.S. Pat. Nos. 3,275,554; 3,438,757; 3,454,555; 3,565,804;
3,671,511; 3,821,302; 3,394,57~; and in European Patent Publication No. 382,405.
Type C - Mannich polyamine dispersants. This category of ashless dispersant which can be utilized is comprised of reaction products of an alkyl phenol, with one or more ali-phatic aldehydes containing from 1 to about 7 carbon atoms (especially formaldehyde and derivatives thereof), and poly-amines (especially polyalkylene polyamines of the type de-scribed hereinabove). Examples of these Mannich polyamine dispersants are described in the following U.S. Patents:
2,459,112; 2,962,442; 2,984,550; 3,036,003; 3,166,516;
3,236,770; 3,368,972; 3,413,347; 3,442,808; 3,~48,047;
3,454,497; 3,459,661; 3,493,520; 3,539,633; 3,558,743;
3,5~36,629; 3,591,598; 3,600,372; 3,634,515; 3,649,229;
3,697,574; 3,703,536; 3,704,308; 3,725,277; 3,725,480;
3,726,882; 3,73~,357; 3,751,365; 3,756,953; 3,793,202;
3,798,165; 3,798,247; 3,803,039; 3,872,019; 3,980,569; and 4,011,380.
Type D - Polymeric polyamine dispersants. Also suit-able for use of the compositions of this invention are poly-2~70~3~
Case EI-6349~ -mers containing basic amine groups and oil solubilizing groups (for exampl~, pendant alkyl groups having at least about 8 carbon atoms). Such polymeric dispersants are here-in referred to as polymeric polyamine dispersants. Such ma-terials include, but are not limited to, interpolymers ofdecyl methacrylate, vinyl decyl ether or a relatively high molecular weight olefin with aminoalkyl acrylates and ami-noalkyl acrylamides. Examples of polymeric polyamine dis-persants are set forth in the following patents: U.S. Pat.
lo Nos. 3,329,658; 3,449,250; 3,493,520i 3,519,565; 3,666,730;
3,687,849; 3,702,300.
Type E - Post-treated basic nitroaen-containinq and/or hydroxyl-containinq ashless dispersants. As is well known in the art, any of the ashless dispersants referred to above as types A-D can be subjected to post-treatment with one or more suitable reagents such as urea, thiourea, carbon disul-fide, aldehydes, ketones, carboxylic acids, anhydrides of low molecular weight dibasic acids, boron compounds, ni-triles, epoxides, phosphorus compounds, and the like. Such post-treated ashless dispersants can be used. Preferably, the post-treated dispersant contains residual basic nitro-gen. Examples of post-treatment procedures and post-treated ashless dispersants are set forth in the following U.S.
Patents: U.S. Pat. Nos. 3,036,003; 3,087,936; 3,200,107;
3,216,936; 3,254,025; 3,256,185; 3,278,550; 3,281,428;
3,282,955; 3,312,~19; 3,366,569; 3,367,943; 3,373,111;
3,403,102; 3,44~,808; 3,455,~31; 3,455,832; 3,493,520;
3,502,677; 3,513,093; 3,533,945; 3,539,633; 3,573,010;
3,579,450; 3,591,598; 3,600,372; 3,639,242; 3,6~9,~29;
3,649,659; 3,658,B36; 3,697,574; 3,702,757; 3,703,536;
3,704,308; 3,708,522; 4,025,445; 4,857,214; and 4~971,598.
Mannich-based derivatives of hydroxyaryl succinimides that have been post-treated with C5-C9 lactones such as ~-caprolactone and optionally with other post-treating agents as described for example in U.S. Pat. No. 4,971,711 can also be utilized in the practice of this invention. Preferably, such post-trea~ed Mannich based derivatives of hydroxyaryl succinimides contain basic nitrsgen. The disclosures of Case EI-6349+ 2 ~ 7 ~

U.S. Pat. No. 4,971,711, as well as related U.S. Pat. Nos.
4,820,432; 4,828,742; 4,866,135; 4,866,139; 4,866,140;
4,866,141; 4,866,142; 4,906,394; and 4,913,830 are refer to additional suitable basic nitrogen-containing ashless dis-persants which may be utilized.
One preferred category of post-treated ashless dis-persants is comprised of basic nitrogen-containing and/or hydroxyl group-containing ashless dispersants which have been heated with (i) a phosphorus compound such that they contain phosphorus, or (ii) a boron compound such that they contain boron, or preferably (iii) a phosphorus compound and a boron compound such that they contain boron and phospho-rus. Such post-treated ashless dispersants preferably con-tain residual basic nitrogen. Examples of such dispersants and methods for their production are described in U.S. Pat.
Nos. 3,087,936; 3,254,025; 3,184,411; 3,185,645; 3,235,497, 3,265,618; 3,281,428; 3,338,832; 3,2~2,955; 3,284,410;
3,324,032; 3,325,567; 3,403,102; 3,344,069; 3,502,677;
3,513,093; 3,511,780; 3,533,9~5; 3,623,985; 3,718,663;
3,865,740; 3,'~50,341; 3,991,056; 4,097,389; 4,234,435;
4,338,205; 4,428,849; 4,554,086; 4,615,826; ~,648,9~0;
4,7~7,971; 4,634,543; 4,857,214; and 4,873,004.
Embodiment C
Still another embodiment of this invention is an oil of lubricating viscosity or an additive concentrate for use in oil of lubricating viscosity containing at least the follow-ing components:
1) one or more oil-soluble zinc hydrocarbyl dithiophosphates;
2) an aryl phosphate ester combination of the type described hereinabove; and 3) one or more oil-soluble ashless dispersants containing basic nitrogen, preferably a succinimide or succinic ester-amide.
The relative proportions of these components is preferably such that the weight ratio of phosphorus in 1) to total phosphorus in 2) is in the range of from about 0.001:1 to about 100:1, and such that the weight ratio of component 2) 207~
Case EI-634s+

to component 3~ is in the range of from about 0.001:1 to about 100:1. These combinations serve to inhibit wear; to inhibit deposit, varnish and/or sludge formation and/or deposition; and to protect the lubricant or functional fluid composition from premature oxidative degradation, especially at elevated temperatures. The quantity of these components 1), 2) and 3) (proportioned as above) added to the base oil of lubricating viscosity is a minor wear-inhibiting amount, and is usually such that the total concentration of phosphorus provided by components 1) and 2) falls in the range of about 0.005 to about 5 percent by weight of the total composition.
Embodiment D
Yet another embodiment of this invention is an oil of lubricating viscosity or an additive concentrate for use in oil of lubricating viscosity containing at least the follow-ing components:
1) one or more oil-soluble sulfur-containing antiwear and/or extreme pressure agents; and 2) an aryl phosphate ester combination of the type described hereinabove; and 3) optionally, one or more oil-soluble ashless dispersants containing basic nitrogen, preferably a succinimide or succinic ester-a~ide; and 4) optionally, one or more oil~soluble zinc hydrocarbyl dithiophosphates.
It will be noted that in these compositions there are at least two required components, d~signated 1) and 2). This embodiment also includes two three-component mixtures, the first composed of the components designated as 1), 2) and 3) and the second composed o~ the components designated as l), 2) and 4). And additionally this e~bodiment comprises the f~ur-componen~ combinations composed of the components designated as l), 2), 3) and 4). In these various combina-tions the relative proportions of these components is pre-ferably such that the weight ratio of sulfur in l) to total phosphorus in 2) i5 in the range of from about 0.01:1 to about 100:1; such that when component 3) is employed, the Case EI-6343+ 2070131 weight ratio of component 2) to component 3) is in the range o' from about 0.001:1 to about 100:1; and such that when component 4) is employed, the weight ratio of total phos-phorus in component 2) to phosphorus in component 4) is in the range of from about 0.01:1 to about lOoO:l. These combinations serve to inhibit wear; to inhibit deposit, varnish and/or sludge formation and/or deposition; and to protect the lubricant or functional fluid composition from premature oxidative degradation, especially at elevated temperatures. The quantity of these components 1) and 2) added to the base oil of lubricating vis~osity is a minor wear-inhibiting amount, and preferably is such that the total concentration of sulfur and phosphorus provided by components 1) and 2) respectively, (proportioned as de-scribed above) falls in the range of about 0.005 to about 20percent by weight of the total composition. When component 3) is used --with or without component 4) -- the quantity of component 3) added to the base oil of lubricating viscosity is a minor dispersant amount, and is usually such as to maintain the proportions given above. Similarly, when com-ponent 4) -- with or without component 3) - is used, the quantity of component 4) added to the base oil of lubricat-ing viscosity is a minor wear-inhibiting amount, and is usually such as to mai~tain the proportions given abova.
Various types of sulfur-containing antiwear and/or ex-treme pressure agents can be used in the practice of Embodi-ment D.
When including component 3) in the practice of Embodi-ment D, use can be made of any of the ashless dispersants referred to hereinabove with reference to Embodiment B.
When including component 4) in the practice of ~mbodiment ~, u~e can be made of any of the zinc hydrocarbyl dithiophos-phates referred to hereinabove with refPrence to Embodiment A.
Embodiment E
A still further embodiment of this invention is an oil of lubricating viscosity or an additive concentrate for use in oil of lubricating viscosity containing at least the 2~7~
Case EI-6349~

following components:
1) at least one oil-soluble amine salt of at least one dihydrocarbyl ester of a thiophosphoric acid; and 2) an aryl phosphate ester combination of the type described hereinabove; and 3) optionally, one or more oil-soluble ashless dispersants containing basic nitrogen, preferably a succinimide or succinic ester-amide; and 4) optionally, one or more oil-soluble sulfur-containing antiwear and/or extreme pressure agents.
It will be noted that in these compositions there are at least two required components, designated 1) and 2). This embodin~ent also includes two three-component mixtures, the first composed of the components designated as 1), 2) and 3) and the second composed of the components designated as 1), 2) and 4). And additionally this embodiment comprises the four-component combinations composed of the components de-signated as 1), 2), 3) and 4). In these various combina-: 20 tions the relative proportions of these components is pre-ferably such that the weight ratio of phosphorus in 1) to total phosphorus in 2) is in the range of from about 0.001:1 to about 100:1; such that when component 3) is employed, the weight ratio of component 2) to component 3) is in the range o~ from about 0.001:1 ~o about ~00:1; and such that when component 4) is employed, the weight ratio of total phos-phorus in component 2) to sulfur in component 4) is in the range of from about 0.01:1 to abDut 100:1. These combina-tions serve to inhibit wear; to inhibit deposit, varnish and/or sludge formation and/or deposition; and to protect the lubricant or functional fluid composition from premature oxidative degradation, especially at elevated temperatures.
The quantity of these components 1) and 2) added to the base oil of lubricating viscosity should be such that the total concentration of phosphorus provided by components 1) and 2) (proportioned as described above) falls in the range of about 0.005 to about 5 percent by weight of the total com-position. When component 3) is used, the quantity thereof 2~0131 Case EI-6349~

added to the base oil of lubricating viscosity is a minor dispersant amount, and is usually within the proportions given above. Similarly, when component 4) is used, the quantity thereof added to the base oil of lubricating visco-sity is a minor wear-inhibiting amount, and is usually within the proportions given above.
The amine salts of dihydrocarbyl esters of thiophos-phoric acids employed as component designated 1) in Em-bodiment E are comprised of the oil-soluble amine salts (preferably the aliphatic monoamine salts) of one or more dihydrocarbyl esters of a thiophosphoric acid, which esters can be derived from a tetrathiophosphoric acid, a trithio-phosphoric acid, a dithiophosphoric acid, or a monothio-phosphoric acid, or a mixture of any two or more of the foregoing. The amine salts of dihydrocarbyl esters of a dithiophosphoric acid are preferred, and the amine salts of dihydrocarbyl esters of a monothiophosphoric acid are particularly preferred.
Methods for the synthesis of such amine salts are well known to those of skill in the art, and are reported in the literature. For example, see PCT Published International Application WO 87/07~38, published 17 December 1987.
When including compon~nt 3) in the practice of E~bodi-ment E, use can be made of any of the ashless dispersants referred to hereinabove with reference to Embodiment B.
When including component 4) in the practice of Embodiment E, use can be made of any of the sulfur-containing ~ntiwear and/or extreme pressure agents referred to hereinabove with reference to Embodiment D.
The effectiveness of the phosphate combinations of this invention in oils of lubricating viscosity was illustrated by means of ~-ball wear tests conducted using a mineral oil based hydraulic fluid containing 200-300 ppm of phosphorus as a phosphate combination of this invention. The tests 35 were conducted at 130F for 60 minutes while operating the 4 ball machine at 1800 rpm with a 40 kg load. In duplicate determinations a blend containing approximately 300 ppm of phosphorus as the phosphate co~bination gave wear scar dia-Case EI-6349~ ~07~131 meters of 0o58 and o.68 mm. Duplicate determinations with a blend containing approximately 200 ppm of phosphorus as the phosphate combination resulted in scars of 0.61 and 0.57 mm. The scars produced by the base oil were 0.90 and 0.95 mm in diameter.
The compositions of this invention are also useful as flame retardants for polymers such as polystyrene, poly-phenylene oxide, blends of poly(2,6-dimethylphenylene oxide) and rubber-modified polystyrene, polyethylene, polypropy-lene, and the like.
This invention is susceptible of considerable variation in its practice. Thus this invention is not intended to be limited by the specific exempli~ications set forth herein-above. Rather, what is intended to be covered is within the spirit and scope of the appended claims.

Claims (14)

1. A composition comprising (A) a major proportion of a hydrocarbonaceous middle distillate fuel or an oil of lubricating viscosity and (B) a minor wear-inhibiting amount of a wear inhibitor comprising a combination of (1) at least one hydrocarbon-soluble aryl phosphate of the formula (RO)3PO
wherein each R is, independently, phenyl or an alkyl-substituted phenyl group and (2) at least one hydrocarbon-soluble aryl polyphosphate of the formula:

wherein R is as defined above, Ar is m-phenylene or an alkyl-substituted m-phenylene group, and n is a whole or fractional number from 1 to 4; said combination containing
2 30% by weight of component (1).

2. The composition of claim 1 wherein R is phenyl and Ar is m-phenylene.
3. The composition of claim 1 wherein n is 1 in at least 50% by weight of the aryl polyphosphate.
4. The composition of claim 1 wherein each R is phenyl or nonylphenyl and at least 50% of the aryl polyphosphate is m-phenylenebis(diphenyl phosphate).
5. The composition of any of the preceding claims comprising a major proportion of a hydrocarbonaceous middle distillate fuel.
6. The composition of claim 5 also containing a minor effective amount of at least one fuel-soluble additive selected from antioxidants, conductivity improvers, metal deactivators, and icing inhibitors.

Case EI-6349+
7. The composition of any of claims 1-4 comprising a major proportion of an oil of lubricating viscosity.
8. The composition of claim 7 also containing a minor amount of (A) one or more oil-soluble zinc hydrocarbyl dithiophosphates, (B) one or more oil-soluble ashless dispersants containing basic nitrogen, or (C) a mixture of (A) and (B); or (D) one or more oil-soluble sulfur-containing antiwear and/or extreme pressure agents, or (E) a mixture of (D) with (A) and/or (B); or (F) at least one oil-soluble amine salt of at least one dihydrocarbyl ester of a thiophosphoric acid; or (G) a mixture of (F) with (B) and/or (D).
9. The composition of claim 7 wherein 50-100% by volume of said oil is a synthetic ester lubricating oil.
10. The composition of claim 9 also containing a minor amount of (A) one or more oil-soluble zinc hydrocarbyl dithiophosphates, (B) one or more oil-soluble ashless dispersants containing basic nitrogen, or (C) a mixture of (A) and (B); or (D) one or more oil-soluble sulfur-containing antiwear and/or extreme pressure agents, or (E) a mixture of (D) with (A) and/or (B); or (F) at least one oil-soluble amine salt of at least one dihydrocarbyl ester of a thiophosphoric acid; or (G) a mixture of (F) with (B) and/or (D).
11. A method of inhibiting wear of interacting metal surfaces which comprises providing as a lubricating for such interacting metal surfaces a lubricant composition of claim 7.
12. A method of inhibiting wear of interacting metal surfaces which comprises providing as a lubricating for such interacting metal surfaces a lubricant composition of claim 8.

case EI-6349+
13. A method of inhibiting wear of interacting metal surfaces which comprises providing as a lubricating for such interacting metal surfaces a lubricant composition of claim 9.
14. A method of inhibiting wear of interacting metal surfaces which comprises providing as a lubricating for such interacting metal surfaces a lubricant composition of claim 10 .
CA 2070131 1991-06-14 1992-06-01 Organic phosphates and their use as wear inhibitors Abandoned CA2070131A1 (en)

Applications Claiming Priority (4)

Application Number Priority Date Filing Date Title
US715,675 1985-03-25
US71567591A 1991-06-14 1991-06-14
US71567491A 1991-06-14 1991-06-14
US715,674 1991-06-14

Publications (1)

Publication Number Publication Date
CA2070131A1 true CA2070131A1 (en) 1992-12-15

Family

ID=27109400

Family Applications (1)

Application Number Title Priority Date Filing Date
CA 2070131 Abandoned CA2070131A1 (en) 1991-06-14 1992-06-01 Organic phosphates and their use as wear inhibitors

Country Status (1)

Country Link
CA (1) CA2070131A1 (en)

Similar Documents

Publication Publication Date Title
EP0521628B1 (en) Organic phosphates and their preparation
US3649659A (en) Coordinated complexes of mannich bases
US5344468A (en) Organic phosphates and their use as wear inhibitors
KR101125928B1 (en) Fuel and lubricant additive containing alkyl hydroxy carboxylic acid boron esters
US5312461A (en) Dihydrocarbyl substituted phenylenediamine-derived phenolic products as antioxidants
US20100041730A1 (en) Alkylated heterocyclic reaction products useful as antioxidants
US3969237A (en) Lubricant compositions containing benzotriazole derivatives as copper passivators
CA1038851A (en) Dispersant-detergent libricant and fuel additives
CA2021225A1 (en) Sulphur-bridged phenolic antioxidants
US2851417A (en) Complex alkoxy metal salts of organic acids and lubricating and fuel compositions thereof
US5407592A (en) Multifunctional additives
US4186102A (en) Lubricating oil composition
US3458495A (en) Reaction product of a phosphosulfurized hydrocarbon and an alkylene amino phenol and method for preparing
US5630852A (en) Organophosphorus additives for improved fuel lubricity
CA2070131A1 (en) Organic phosphates and their use as wear inhibitors
US5326487A (en) Mixed phosphorous- and sulfur- containing reaction products useful in power transmitting compositions
US3166509A (en) Antioxidant composition
CA2070123A1 (en) Organic phosphates and their preparation
US4353807A (en) Lubricants and fuels containing boroxarophenanthrene compounds
US3484375A (en) Lubricating oils and fuels containing organic phosphite reaction products
US5009802A (en) Phenolic antioxidant composition
US5681798A (en) Load-carrying additives based on organo-phosphites and amine phosphates
US4292047A (en) Benzoquinone and amine reaction product for fuels and mineral oils
US3449424A (en) Salicylaldimines
AU623670B2 (en) Mixed phosphorous- and sulfur-containing reaction products useful in power transmitting compositions

Legal Events

Date Code Title Description
FZDE Dead