The method is applied for decoration of household glass products. The decorated goods are of high artistic value and diverse decore nuances. After layering the glass dye until the formation of the preliminarily set model, the decoration is covered by one or more coloured fluxes, after which the good is baked at a temperature of between 500 to 520 degrees C.
BG090507A1989-11-301989-11-30Method for plastic and relief decoration of glass goods
BG49611A3
(en)
Processes for producing colored glass or glass-ceramic articles bearing a non-stick coating compositions for carrying out said processes and resultant colored articles
Process for decoration of manufactured, particularly metallic, products particularly for giving them pearled styles and manufactured products, particularly cups and trophies decorated by this process
Method for decorating a substrate involving replacing a part of the substrate with a decorated plastic film or applying the decorated plastic film onto the substrate, and products thereby obtained