BE866501A - IMPROVEMENTS FOR THE ELIMINATION OF EXCESS LIQUID COATING MATERIAL FROM A STRIP - Google Patents

IMPROVEMENTS FOR THE ELIMINATION OF EXCESS LIQUID COATING MATERIAL FROM A STRIP

Info

Publication number
BE866501A
BE866501A BE187219A BE187219A BE866501A BE 866501 A BE866501 A BE 866501A BE 187219 A BE187219 A BE 187219A BE 187219 A BE187219 A BE 187219A BE 866501 A BE866501 A BE 866501A
Authority
BE
Belgium
Prior art keywords
elimination
strip
coating material
liquid coating
excess liquid
Prior art date
Application number
BE187219A
Other languages
French (fr)
Original Assignee
British Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by British Steel Corp filed Critical British Steel Corp
Publication of BE866501A publication Critical patent/BE866501A/en

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C23COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
    • C23CCOATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
    • C23C2/00Hot-dipping or immersion processes for applying the coating material in the molten state without affecting the shape; Apparatus therefor
    • C23C2/14Removing excess of molten coatings; Controlling or regulating the coating thickness
    • C23C2/16Removing excess of molten coatings; Controlling or regulating the coating thickness using fluids under pressure, e.g. air knives
    • C23C2/18Removing excess of molten coatings from elongated material
    • C23C2/20Strips; Plates
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B05SPRAYING OR ATOMISING IN GENERAL; APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL
    • B05CAPPARATUS FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL
    • B05C11/00Component parts, details or accessories not specifically provided for in groups B05C1/00 - B05C9/00
    • B05C11/02Apparatus for spreading or distributing liquids or other fluent materials already applied to a surface ; Controlling means therefor; Control of the thickness of a coating by spreading or distributing liquids or other fluent materials already applied to the coated surface
    • B05C11/06Apparatus for spreading or distributing liquids or other fluent materials already applied to a surface ; Controlling means therefor; Control of the thickness of a coating by spreading or distributing liquids or other fluent materials already applied to the coated surface with a blast of gas or vapour

Landscapes

  • Chemical & Material Sciences (AREA)
  • Organic Chemistry (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Mechanical Engineering (AREA)
  • Metallurgy (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Coating Apparatus (AREA)
  • Coating With Molten Metal (AREA)
  • Cleaning In General (AREA)
  • Spray Control Apparatus (AREA)
  • Cleaning By Liquid Or Steam (AREA)
  • Cleaning And De-Greasing Of Metallic Materials By Chemical Methods (AREA)
BE187219A 1977-04-29 1978-04-27 IMPROVEMENTS FOR THE ELIMINATION OF EXCESS LIQUID COATING MATERIAL FROM A STRIP BE866501A (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
GB18013/77A GB1602731A (en) 1977-04-29 1977-04-29 Removal of excess liquid coatant from skip

Publications (1)

Publication Number Publication Date
BE866501A true BE866501A (en) 1978-08-14

Family

ID=10105144

Family Applications (1)

Application Number Title Priority Date Filing Date
BE187219A BE866501A (en) 1977-04-29 1978-04-27 IMPROVEMENTS FOR THE ELIMINATION OF EXCESS LIQUID COATING MATERIAL FROM A STRIP

Country Status (15)

Country Link
JP (1) JPS549122A (en)
BE (1) BE866501A (en)
BR (1) BR7802685A (en)
CA (1) CA1091994A (en)
DE (1) DE2818620A1 (en)
ES (2) ES469210A1 (en)
FI (1) FI781304A (en)
FR (1) FR2388605A1 (en)
GB (1) GB1602731A (en)
IT (1) IT7867976A0 (en)
LU (1) LU79566A1 (en)
NL (1) NL7804630A (en)
NO (1) NO781500L (en)
SE (1) SE7804918L (en)
ZA (1) ZA782226B (en)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61207790A (en) * 1985-03-13 1986-09-16 清水建設株式会社 Excavation of geothermal production well
DE19834759C2 (en) * 1998-08-01 2002-02-21 Salzgitter Ag Method and device for removing dendrites
WO2010130884A1 (en) * 2009-05-14 2010-11-18 Arcelormittal Investigacion Y Desarrollo Sl Method for producing a coated metal band having an improved appearance

Family Cites Families (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
IT1005507B (en) * 1972-11-27 1976-09-30 Italsider Spa PERFECTED DEVICE FOR CONTINUOUS REGULATION OF THE ZINC COATING OF A STEEL SHEET OR SIMILAR
IT1023842B (en) * 1974-08-08 1978-05-30 Italsider Spa PERFECTED DEVICE FOR BLOWING A BLADE OF AIR AGAINST A TAPE COATED WITH A LAYER OF LIQUID MATERIAL, IN PARTICULAR AGAINST A METALLIC TAPE COVERED WITH A LAYER OF MELTED ZICO

Also Published As

Publication number Publication date
ES469210A1 (en) 1979-10-01
CA1091994A (en) 1980-12-23
ZA782226B (en) 1979-04-25
ES475992A1 (en) 1979-07-16
FI781304A (en) 1978-10-30
IT7867976A0 (en) 1978-04-28
BR7802685A (en) 1978-11-14
NL7804630A (en) 1978-10-31
FR2388605A1 (en) 1978-11-24
DE2818620A1 (en) 1978-11-02
LU79566A1 (en) 1978-11-03
GB1602731A (en) 1981-11-18
JPS549122A (en) 1979-01-23
SE7804918L (en) 1978-10-30
NO781500L (en) 1978-10-31

Similar Documents

Publication Publication Date Title
FR2428473B1 (en) DEVICE FOR THE CONTINUOUS APPLICATION OF A COATING ON A STRIP OF MATERIAL
LU79148A1 (en) AEROSOL DISPENSER
BE842647A (en) IMPROVED PROCESS FOR COATING A LIQUID COMPOSITION ON A SUPPORT
JPS5311838A (en) Metal flameemetallization material for obtaining coating having good machinability
BE878006A (en) BRAZING MATERIAL
GB2031036B (en) Liquid trestment of metal strip
DE2960458D1 (en) Process for the synthesis of 2-(perfluoroalkyl)-ethanols
FR2432463B1 (en) TAPE FOR THE TAPE PROCESS
FR2297799A1 (en) DEVICE FOR THE ACCUMULATION OF STRIP MATERIALS
JPS53141339A (en) Liquid coating material containing no or little solvent
FR2340784A1 (en) APPARATUS FOR THE DISTRIBUTION OF A COATING MATERIAL
RO72810A (en) MACHINE FOR THE CONTINUOUS EXTRUSION OF METALLIC MATERIALS
BE866501A (en) IMPROVEMENTS FOR THE ELIMINATION OF EXCESS LIQUID COATING MATERIAL FROM A STRIP
RO72397A (en) MATERIAL FOR COATING OF FER-SILICON ALLOY SEMI-PRODUCTS
BE871281A (en) DRY IMAGE FORMING MATERIAL
SE415177B (en) PROCEDURE FOR THE RECYCLING OF ANTIMONSULPHIDE FROM A WATER SOLUTION
FR2344342A1 (en) MENISQUE APPARATUS FOR THE APPLICATION OF A COATING ON A TAPE OF METAL OR OTHER
IT1102473B (en) APPARATUS FOR MEASURING THE AREA OF STRETCHED TAPE MATERIALS
GB2021459B (en) Apparatus for the electrorotative casting of liquid metal
CH611021A5 (en) Apparatus for the metering of a liquid
BE869872A (en) IMPROVEMENT OF WATERPROOFING COATINGS FOR WORKS OF ART
BE868844A (en) STICK FOR THE APPLICATION OF ADHESIVE MATERIAL
RO71136A (en) MATERIAL FOR COATING OF FER-SILICON ALLOY SEMI-PRODUCTS
PH16159A (en) Stripping excess coating liquid from moving strip materials
JPS5351226A (en) Material for coatng wall

Legal Events

Date Code Title Description
RE Patent lapsed

Owner name: BRITISH STEEL CORP.

Effective date: 19850427