AU2017100354A4 - Method for manufacturing an embossing cylinder configured for producing microstructure image effects - Google Patents

Method for manufacturing an embossing cylinder configured for producing microstructure image effects Download PDF

Info

Publication number
AU2017100354A4
AU2017100354A4 AU2017100354A AU2017100354A AU2017100354A4 AU 2017100354 A4 AU2017100354 A4 AU 2017100354A4 AU 2017100354 A AU2017100354 A AU 2017100354A AU 2017100354 A AU2017100354 A AU 2017100354A AU 2017100354 A4 AU2017100354 A4 AU 2017100354A4
Authority
AU
Australia
Prior art keywords
cylinder
embossing
relief structures
security
microstructure
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Ceased
Application number
AU2017100354A
Other versions
AU2017100354B4 (en
Inventor
Karlo Ivan Jolic
Gary Fairless Power
Patrick Swift
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CCL Security Pty Ltd
Original Assignee
Innovia Secutiry Pty Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Innovia Secutiry Pty Ltd filed Critical Innovia Secutiry Pty Ltd
Priority to AU2017100354A priority Critical patent/AU2017100354B4/en
Publication of AU2017100354A4 publication Critical patent/AU2017100354A4/en
Assigned to CCL SECURE PTY LTD reassignment CCL SECURE PTY LTD Request to Amend Deed and Register Assignors: INNOVIA SECURITY PTY LTD
Application granted granted Critical
Publication of AU2017100354B4 publication Critical patent/AU2017100354B4/en
Priority to FR1852578A priority patent/FR3064210A1/en
Priority to PCT/AU2018/050285 priority patent/WO2018176090A1/en
Ceased legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

Abstract A method for manufacturing an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect in one or more security devices applied to a security document is provided. The method includes the steps of providing a blank embossing cylinder having a surface; and forming surface relief structures corresponding to the at least one microstructure image effect directly on the surface of the cylinder.

Description

2017100354 27 Mar 2017 1
METHOD FOR MANUFACTURING AN EMBOSSING CYLINDER CONFIGURED FOR PRODUCING MICROSTRUCTURE IMAGE EFFECTS
Technical Field [0001] The invention relates generally to embossing rollers for producing security devices used as an anti-counterfeiting measure in security devices, and in particular to the manufacture of such an embossing roller.
Background of Invention [0002] A variety of security devices are applied to security documents and tokens to deter counterfeiters. For example, bank notes may have a relief structure, such as a diffraction grating or hologram incorporated into a layer of radiation curable ink. One method of incorporating a relief structure into a security document is an embossing process which embosses the desired diffractive relief structure into a radiation curable ink applied to the substrate and irradiating the same whilst the embossing tool is in contact with the radiation curable ink to permanently fix the embossed relief structure.
[0003] While various embossing tools are available, in the past, only “shims” have been found suitable for the production of the finer relief structures required for micro-optical effect imagery than can be produced using an embossing roller. A shim consists of a transfer foil of metallic material bearing the negative of the desired micro-scale or nano-scale diffractive relief structures which is then wrapped around a blank roller.
[0004] It is a disadvantage of the use of such shims, that a protracted set-up time is required to mount the shim on an embossing roller using adhesive tape, taking care to avoid, as much as practicable, malalignment of the shim. The shim must be mounted squarely on the embossing roller using alignment crosses. In some cases, the mounting process will fail due to malalignment, resulting in the shim needing to be discarded and the mounting process recommenced with a fresh shim. Moreover, “seams” tend to form, where the edge of a shim is joined with another edge of the shim or otherwise attached to the roller. In addition, personal injury can occur when handling shims due to their sharp, exposed edges. 2017100354 27 Mar 2017 2 [0005] The use of an embossing roller bearing micro-optical effect image structures has the potential to overcome these problems. Moreover, an embossing cylinder can be removed from the press for cleaning and reuse. This is not possible with a shim which typically sustains irreparable damage on removal from the roller.
[0006] It is therefore desirable to provide a method for manufacturing an embossing roller configured for production of the finer relief structures required for micro-optical effect imagery and an embossing roller manufactured by such a method.
Definitions
Security Document or Token [0007] As used herein the term security document includes all types of documents and tokens of value and identification documents including, but not limited to the following: items of currency such as banknotes and coins, credit cards, cheques, passports, identity cards, securities and share certificates, driver's licenses, deeds of title, travel documents such as airline and train tickets, entrance cards and tickets, birth, death and marriage certificates, and academic transcripts.
[0008] The invention is particularly, but not exclusively, applicable to security documents such as banknotes or identification documents such as identity cards or passports formed from a substrate to which one or more layers of printing are applied. The diffraction gratings and optically variable devices described herein may also have application in other products, such as packaging.
Substrate [0009] As used herein, the term substrate refers to the base material from which the security document or token is formed. The base material may be paper or other fibrous material such as cellulose; a plastic or polymeric material including but not limited to polypropylene (PP), polyethylene (PE), polycarbonate (PC), polyvinyl chloride (PVC), polyethylene terephthalate (PET); or a composite material of two or more materials, such as a laminate of paper and at least one plastic material, or of two or more polymeric materials. 3 2017100354 27 Mar 2017 [0010] The use of plastic or polymeric materials in the manufacture of security documents pioneered in Australia has been very successful because polymeric banknotes are more durable than their paper counterparts and can also incorporate new security devices and features. One particularly successful security feature in polymeric banknotes produced for Australia and other countries has been a transparent area or “window”.
Transparent Windows and Half Windows [0011 ] As used herein the term window refers to a transparent or translucent area in the security document compared to the substantially opaque region to which printing is applied. The window may be fully transparent so that it allows the transmission of light substantially unaffected, or it may be partly transparent or translucent partially allowing the transmission of light but without allowing objects to be seen clearly through the window area.
[0012] A window area may be formed in a polymeric security document which has at least one layer of transparent polymeric material and one or more opacifying layers applied to at least one side of a transparent polymeric substrate, by omitting least one opacifying layer in the region forming the window area. If opacifying layers are applied to both sides of a transparent substrate a fully transparent window may be formed by omitting the opacifying layers on both sides of the transparent substrate in the window area.
[0013] A partly transparent or translucent area, hereinafter referred to as a “halfwindow,” may be formed in a polymeric security document which has opacifying layers on both sides by omitting the opacifying layers on one side only of the security document in the window area so that the “half-window” is not fully transparent, but allows some light to pass through without allowing objects to be viewed clearly through the half-window.
[0014] Alternatively, it is possible for the substrates to be formed from an substantially opaque material, such as paper or fibrous material, with an insert of transparent plastics material inserted into a cut-out, or recess in the paper or fibrous substrate to form a transparent window or a translucent half-window area. 4 2017100354 27 Mar 2017
Opacifying Layers [0015] One or more opacifying layers may be applied to a transparent substrate to increase the opacity of the security document. An opacifying layer is such that LT<L0 where L0 is the amount of light incident on the document, and LT is the amount of light transmitted through the document. An opacifying layer may comprise any one or more of a variety of opacifying coatings. For example, the opacifying coatings may comprise a pigment, such as titanium dioxide, dispersed within a binder or carrier of heat-activated cross-linkable polymeric material. Alternatively, a substrate of transparent plastic material could be sandwiched between opacifying layers of paper or other partially or substantially opaque material to which indicia may be subsequently printed or otherwise applied.
Security Device or Feature [0016] As used herein the term security device or feature includes any one of a large number of security devices, elements or features intended to protect the security document or token from counterfeiting, copying, alteration or tampering. Security devices or features may be provided in or on the substrate of the security document or in or on one or more layers applied to the base substrate, and may take a wide variety of forms, such as security threads embedded in layers of the security document; security inks such as fluorescent, luminescent and phosphorescent inks, metallic inks, iridescent inks, photochromic, thermochromic, hydrochromic or piezochromic inks; printed and embossed features, including relief structures; interference layers; liquid crystal devices; lenses and lenticular structures; optically variable devices (OVDs) such as diffractive devices including diffraction gratings, holograms and diffractive optical elements (DOEs).
Embossable Radiation Curable Ink [0017] The term embossable radiation curable ink used herein refers to any ink, lacquer or other coating which may be applied to the substrate in a printing process, and which can be embossed while soft to form a relief structure and cured by radiation to fix the embossed relief structure. The curing process does not take place before the radiation curable ink is embossed, but it is possible for the curing process to take place either after embossing or at substantially the same time as the 2017100354 27 Mar 2017 5 embossing step. The radiation curable ink is preferably curable by ultraviolet (UV) radiation. Alternatively, the radiation curable ink maybe cured by other forms of radiation, such as electron beams or X-rays.
[0018] The radiation curable ink is preferably a transparent or translucent ink formed from a clear resin material. Such a transparent or translucent ink is particularly suitable for printing light-transmissive security elements such as sub-wavelength gratings, transmissive diffractive gratings and lens structures.
[0019] In one particularly preferred embodiment, the transparent or translucent ink preferably comprises an acrylic based UV curable clear embossable lacquer or coating, [0020] Such UV curable lacquers can be obtained from various manufacturers, including Kingfisher Ink Limited, product ultraviolet type UVF-203 or similar. Alternatively, the radiation curable embossable coatings maybe based on other compounds, e.g. nitro-cellulose.
[0021] The radiation curable inks and lacquers used herein have been found to be particularly suitable for embossing microstructures, including diffractive structures such as diffraction gratings and holograms, and microlenses and lens arrays. However, they may also be embossed with larger relief structures, such as non-diffractive optically variable devices.
[0022] The ink is preferably embossed and cured by ultraviolet (UV) radiation at substantially the same time. In a particularly preferred embodiment, the radiation curable ink is applied and embossed at substantially the same time in a Gravure printing process.
[0023] Preferably, in order to be suitable for Gravure printing, the radiation curable ink has a viscosity falling substantially in the range from about 20 to about 175 centipoise, and more preferably from about 30 to about 150 centipoise. The viscosity may be determined by measuring the time to drain the lacquer from a Zahn Cup #2. A sample which drains in 20 seconds has a viscosity of 30 centipoise, and a sample which drains in 63 seconds has a viscosity of 150 centipoise. 2017100354 27 Mar 2017 6 [0024] With some polymeric substrates, it may be necessary to apply an intermediate layer to the substrate before the radiation curable ink is applied to improve the adhesion of the embossed structure formed by the ink to the substrate. The intermediate layer preferably comprises a primer layer, and more preferably the primer layer includes a polyethylene imine. The primer layer may also include a crosslinker, for example a multi-functional isocyanate. Examples of other primers suitable for use in the invention include: hydroxyl terminated polymers; hydroxyl terminated polyester based co-polymers; cross-linked or uncross-linked hydroxylated acrylates; polyurethanes; and UV curing anionic or cationic acrylates. Examples of suitable cross-linkers include: isocyanates; polyaziridines; zirconium complexes; aluminium acetyl acetone; melamines; and carbodi-imides.
Summary of Invention [0025] According to an aspect of the present invention, there is provided a method for manufacturing an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect in one or more security devices applied to a security document, the method including the following steps: providing a blank embossing cylinder having a surface; and forming surface relief structures corresponding to the at least one microstructure image effect directly on the surface of the cylinder.
[0026] What constitutes a microstructure with regard to dimensions will vary depending on the particular type of optical effect. That is, the dimensions of microstructures that can be formed using the method of the present invention is limited by the minimum feature size that can be achieved using various techniques suitable for manufacturing embossing cylinders having surface relief structures configured for producing microstructure images.
[0027] According to an embodiment, the step of forming one or more surface relief structures directly on the surface of the cylinder involves laser ablation.
[0028] For example, in one particular form of the invention, the laser is configured to produce a laser beam width of substantially 5 microns or less. 2017100354 27 Mar 2017 7 [0029] The laser may be configured to produce a laser pulse duration sufficient to vaporise the surface of the cylinder. In one exemplary embodiment the laser is configured to produce a laser pulse duration in the range of femtoseconds to nanoseconds. Moreover, selection of a suitable laser will be dependent on the cylinder material to be ablated.
[0030] A laser beam shaping optical element may be applied in an optical path formed between the laser and the surface of the cylinder in order to achieve the requisite uniformity of the laser beam.
[0031 ] According to another embodiment, the step of forming surface relief structures directly on the surface of the cylinder is carried out by electro-mechanical engraving means using for example, an oscillating stylus formed from a suitable material such as diamond. The electro-mechanical engraving tool may be configured to engrave microstructures of substantially 35 microns or less, or of substantially 5 microns or less.
[0032] According to yet another embodiment, the step of forming surface relief structures directly on the surface of the cylinder is carried out by chemical etching. The step of forming surface relief structures directly on the surface of the cylinder by chemical etching may be preceded by one of the following steps: coating the surface the cylinder with a mask material and laser ablating a pattern of proposed surface relief structures into the mask material to expose the pattern on the surface of the cylinder to thereby form an etching mask; coating the surface of the cylinder with a resist, UV exposing the resist through a film containing a pattern of proposed surface relief structures and developing the UV-exposed resist to expose the pattern on the surface of the cylinder; or coating the surface of the cylinder with a resist, scanning a focussed beam of light onto the resist to expose a pattern of proposed surface relief structures in the resist that is subsequently developed to expose the pattern on the surface of the cylinder.
[0033] According to still another embodiment, the method for manufacturing an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect in one or more security devices applied to a security 8 2017100354 27 Mar 2017 document further includes the step of electroforming a layer of material over the surface relief structures to reduce a size of the microstructure.
[0034] Preferably, the electroformed layer of material is a metal.
[0035] The electroformed layer of material may be deposited in a uniform layer.
[0036] According to yet another embodiment of the present invention, there is provided a computer program product storing instructions for manufacturing an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect in at least one security device applied to a security document, the computer program product storing instructions for controlling a processor to control a device to form surface relief structures corresponding to the at least one microstructure image effect directly on a surface of the cylinder.
[0037] According to a further embodiment of the present invention, there is provided an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect in at least one security device applied to a security document, the surface relief structures corresponding to the at least one microstructure image effects being formed directly on a surface of the cylinder.
[0038] The surface relief structures may comprise microstructures having dimensions of substantially 35 microns or less, or of substantially 5 microns or less.
Brief Description of Drawings [0039] Embodiments of the invention will now be described with reference to the accompanying drawings. It is to be understood that the embodiments are given by way of illustration only and the invention is not limited by this illustration. In the drawings: [0040] Figure 1 shows and exemplary apparatus for manufacturing a security document.
[0041 ] Figure 2 shows an exemplary microstructure that can be formed on an embossing cylinder by the method of the present invention. 9 2017100354 27 Mar 2017 [0042] Figure 3 shows an exemplary laser ablation system which is used in one embodiment of the present invention.
[0043] Figure 4 shows an exemplary micro-mechanical engraving system which is used in another embodiment of the present invention.
[0044] Figure 5 show an optical microscope photograph of an array of micro images of the letter “A” formed by mask ablation according to an embodiment of the present invention.
[0045] Figures 6A and 6B show an image structure that has been electroplated to reduce the size of the image structure in a post processing step according to one embodiment of the present invention.
Detailed Description [0046] Referring firstly to Figure 1 there is shown an exemplary apparatus for manufacturing a security document. A radiation curable ink, such as a UV curable ink, is applied to a security element area where a surface relief structure configured for producing at least one image effect in a security device applied to a security document is to be positioned. The security element area may take the form of a stripe, a discrete patch in the form of a simple geometric shape, or in the form of a more complex graphical design.
[0047] While the radiation curable ink remains at least partially liquid, it is processed at a processing station 100 including an embossing roller 110 for embossing the security element structure into the radiation curable ink. The cylindrical surface 120 of the embossing roller 110 may have a repeating pattern of surface relief formations or the relief structures may be localized to individual shapes corresponding to the shape of the security elements area on the substrate.
[0048] The radiation curable ink on the substrate is brought into contact with the cylindrical embossing surface 120 of the embossing roller 110 by a nip roller 130 at the processing station 100, such that the liquid radiation curable ink flows into the surface relief structures of the embossing surface 120. At this stage, the radiation curable ink is exposed to UV radiation to permanently fix the embossed structures. 10 2017100354 27 Mar 2017 [0049] The present invention is directed to the manufacture of an embossing roller 110 suitable for forming microstructure image effects in security devices in security documents. Such micro-optical effect imagery is at least in part defined by dimension and includes security features such as micro-text, lens based optical effects such as image flips, contrast switches, animations, morphing effects, three dimensional floating and/or receding images, moire magnification effects and combinations thereof.
[0050] What constitutes a microstructure with regard to dimensions will vary depending on the particular type of optical effect. For example, in the case of holograms and diffractive optically variable devices (DOVDs), the smallest dimension of a microstructure is a couple of microns or less. Using current technology, these would be difficult to directly mechanically engrave. In the case of lens based effects, the smallest dimensions will depend on the size of the lenses used and the particular optical effect. For example, moire magnification effects employ microstructures having the smallest dimensions. For refractive lenses, configured to magnify imagery deployed on the other side of a typical polymer substrate, the smallest dimension is around 2 to 10 microns. The actual size is dependent on the complexity of the moire magnified image, i.e., the more complex the image, the smaller is the minimum feature size within the microstructure. Particular challenges are encountered in forming microstructures of sufficient resolution and integrity in a roller to produce high fidelity and high complexity micro-optical effects. These are addressed by the method of the present invention.
[0051] Referring now to Figure 2, there is shown an exemplary microstructure formed by the method of the present invention. That is the microstructure is ablated, engraved or otherwise formed directly in the surface 120 of a blank embossing cylinder 110 (see Figure 1). In the illustrated example, the microstructure 200 consists of an array of the numeral “5” 220 arranged in a hexagonal grid with 55 microns pitch. The numerals 220 are formed by recessing approximately 4 microns deep into the surface 120 of the embossing cylinder 110. The smallest feature size of the numerals 220 is the feature width on the cylinder surface 120, at substantially 5 microns. An embossing cylinder 110 having such a microstructure 210 formed in its surface by the method of the present invention could be used to emboss microstructures, for example, moire effect security features on bank notes that utilise hexagonally packed 11 2017100354 27 Mar 2017 micro lenses having a similar, but different pitch to that of the correspondingly embossed microstructures, e.g. 56 microns pitch lenses could be employed.
[0052] The embossing roller 110 may be manufactured by forming the microstructures 210 that correspond to the microstructure image effects to be created in one or more security devices by direct laser ablation, chemical etching, mask ablation, or by micro-mechanical engraving means or other suitable techniques.
[0053] Now described with reference to Figure 3 is one embodiment of a system 300 for manufacturing an embossing roller 110 having surface relief structures configured for producing at least one microstructure image effect. In this case the surface relief structures are formed on the embossing roller by laser ablation, wherein the laser 310 is selected and/or configured to produce a beam width of 5 microns or less. The laser ablation system 300 includes a laser 310, e.g. a picosecond laser, a laser beam 320, an objective lens 330 and a blank embossing cylinder 340. The laser beam 320 width and uniformity is configured to enable homogeneous ablation of the cylinder surface on exposure to the laser beam. To achieve the requisite beam uniformity, optical elements 350 including lenses and/or mirrors and/or beam shapers are placed in the optical pathway between the laser 310 and the cylinder 340 surface.
[0054] The pulse duration and pulse energy of the laser 310 is controlled so as to vaporise the surface of the cylinder 340 to form a cell. The shape of the cell is defined by the material to be ablated, the intensity profile and pulse duration of the laser beam, the number of applied pulses, and the position of each pulse on the cylinder surface. Suitable laser pulse durations are in the femtosecond to nanosecond range, and preferably in the picosecond range. Depending on the material of which the cylinder 340 to be laser ablated is comprised, a single laser pulse typically vaporises around 1 micron or less of the material in depth.
[0055] The embossing cylinders can be formed from a range of materials since the radiation cured embossing process itself causes minimal wear. For example, the blank embossing cylinder may take the form of a hollow steel cylinder that is copper, nickel or zinc plated. Other materials such as chromium or polymers are also envisaged. It will be understood that selection of a suitable laser will be dependent on the cylinder material to be ablated. For example, for materials with high vaporisation 12 2017100354 27 Mar 2017 temperatures, such as metals, a Q switched YAG laser may be suitable choice. For example, a Q-switched Nd:YAG multimode laser, with 400W at 1064nm with a repetition rate of 35 KHz. However, for materials requiring a not so high vaporisation temperature, such as polymeric materials, an excimer laser may be a suitable choice.
[0056] A mask or beam shaping optic 350 such as a diffractive optical element may be used to shape the profile of the cross section of the smallest spot size to optimise the process, for example by facilitating efficient expulsion of materials from the ablated profile. Moreover, the laser beam 320 can be otherwise controlled, for example, by dynamically controlling the beam width to increase the beam focus where an area of increased depth ablation is required and conversely, to decrease the beam focus where an area of decreased depth ablation is required.
[0057] The laser ablation process can be configured as a step and repeat process using a mask modulated beam. Alternatively, the laser can be controlled by a suitably designed control system that can write a bitmap file or similar, directly on a blank cylinder, wherein the bitmap file represents a simple ON/OFF laser pulse. In another embodiment, the laser is capable of direct writing a greyscale file to the cylinder, wherein each greyscale value corresponds to the ablation depth in the cylinder at the position concerned.
[0058] The micro images may be at least partially hidden by integrating them into a larger or macro image. For example, portions of a 2D array of micro images, that form part of a moire magnification device, could be placed in non-image areas within the macro image. Alternatively, the density of the array of micro image elements could be varied, for example, by reducing the number of array elements in the array, to simulate grey levels in the macro image.
[0059] Referring now to Figure 4, the microstructures could similarly be formed on a blank embossing roller using a direct micro-mechanical engraving system 400 having an oscillating stylus, typically diamond, which cuts cells directly into the surface of the embossing cylinder, assuming that the selected system provides a suitable engraving resolution. One example of a micro-mechanical engraving machine that can achieve high resolution engraving is the Hell Extreme engraving System having an engraving resolution of substantially 5 microns. Another is the MicroStar™ 13 2017100354 27 Mar 2017
MicroEngraving System offered by Daetwyler R&amp;D Corp. The MicroStar™ system 400 is schematically depicted in Figure 4 and is suitable for engraving a blank embossing cylinder at a resolution of 5 microns and less and could accordingly, be employed to engrave functional micro-optical effect imagery micro structures for lenses on security documents such as bank notes. An appropriately selected cutting tool 420 is controlled via interface 430 which enables importing and uploading of microstructure design files.
[0060] Alternative methods suitable for manufacturing an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect, include chemical etching which involves copying the proposed surface relief structures by direct contact exposing from film to the metal surface of the embossing cylinder. After exposure, developing steps and chemical etching are performed to produce recessed structures in the embossing cylinder which will subsequently contain UV-curable ink for producing the microstructure image effects in security devices. The exposure step is performed by passing UV light through the film, to expose the underlying resist-coated surface of the cylinder. As an alternative method, which does not involve the use of films/contact exposure, the resist-coated cylinder surface may be directly UV exposed with a focused beam of UV light or UV laser light. Mask ablation methods involve coating the cylinder with a mask using immersion or spray coating techniques. The mask is then removed from areas to be chemically etched by thermal ablation, following this the cylinder is chemically etched to produce recessed microstructures. Referring now to Figure 5 there is shown an optical microscope photograph 500 of an array of micro images of the letter “A” 510 with a pitch of 50 microns produced using mask ablation followed by chrome plating. The engraving resolution used was 10,160 dots per inch. The engraving artwork was provided in the form of a 10,160 dpi monochromatic TIF file containing a binary image of the letter “A” array.
[0061] The dimensions of microstructures that can be formed using the method of the present invention is limited by the minimum feature size that can be achieved using various techniques suitable for manufacturing embossing cylinders having surface relief structures configured for producing microstructure images. As previously noted such techniques include film contact exposure, focused beam 2017100354 27 Mar 2017 14 exposure, mask ablation, chemical etching, micro-electromechanical engraving techniques, and direct laser ablation.
[0062] The minimum feature size will correspondingly impact the minimum image feature size that will be projected by lenses in the case where the microstructure is overlaid with an array of micro lenses. That minimum size is accepted to be substantially 5 microns. However, if the security feature design dictates that smaller microstructures are required to produce the desired image effects, then this may be achieved by electroforming a layer of material, e.g. metal over the surface relief structures in a layer of uniform thickness.
[0063] Referring now to Figures 6A and 6B there is shown schematically how electroforming a layer of material over the microstructure can effectively reduce the size of the surface relief structures. That is, Figure 6A shows the originally formed microstructure having a dimension of 5 microns. Figure 6B shows the same structure 610 after a layer of chrome 620 that is 1 micron thick is electroformed over the surface relief structure. This has the effect of decreasing the dimensions of the microstructure 630 to 3 microns. The decreased dimensions allow a smaller minimum feature size to be achieved. A further advantage of the addition of the chrome layer is that it may assist in extending the embossing lifetime of the tool.
[0064] Accordingly, design of suitable microstructures for electroplating may entail firstly developing the design so that the portions of the design representing the recessed microstructure have dimensions equal to the target dimensions of the recessed structure after electroplating. Secondly, the design must be adjusted to compensate for the electroplating by enlarging the portion of the design representing the recessed area so that its perimeter moves away from the recessed area (i.e. perimeter moves perpendicular to its local tangent), by a predetermined distance, so that the recessed feature area will be increased. If the design is represented as a raster image, this enlargement compensation step could be achieved by applying “Minimum” or “Maximum” filter functions to the image in Photoshop (depending on whether the recessed areas are represented by black or white pixels). The “Erode” or “Dilate” functions known in image processing theory could also be used. 15 2017100354 27 Mar 2017 [0065] It is an advantage of the present invention that reducing the reliance on shims having a limited useful life simplifies and reduces the costs of generating micro imagery for security devices. An embossing cylinder having integrated surface relief structures configured for producing at least one microstructure image effect can simply be removed from the processing station for cleaning as required, whilst shims are too fragile to endure the shim removal process that is required in order to clean them. Moreover, the problems encountered when using conventional shims, including alignment issues and the presence of joins/seams, are avoided using an embossing cylinder with integral surface relief structures configured for producing at least one microstructure image effect. Moreover, the angular alignment of the micro imagery to lenses is also improved such that image effects due to lens-to-image skew are reduced, since alignment error due to shim mounting is avoided. This enables larger images implementing multi frame optical effects such as flips, contrast switches, animations and three dimensional designs including interlaced, integral and moire effects, to be created.
[0066] The embossing process is simplified and made more efficient by reducing set-up time and opportunities for errors. Moreover, the risk of personnel injury inherent in handling metal shims due to sharp edges is avoided.
[0067] Where the terms "comprise", "comprises", "comprised" or "comprising" are used in this specification (including the claims) they are to be interpreted as specifying the presence of the stated features, integers, steps or components, but not precluding the presence of one or more other features, integers, steps or components, or group thereof.
[0068] While the invention has been described in conjunction with a limited number of embodiments, it will be appreciated by those skilled in the art that many alternatives, modifications and variations in light of the foregoing description are possible. Accordingly, the present invention is intended to embrace all such alternatives, modifications and variations as may fall within the spirit and scope of the invention as disclosed.
[0069] The present application may be used as a basis or priority in respect of one or more future applications and the claims of any such future application may be 2017100354 27 Mar 2017 16 directed to any one feature or combination of features that are described in the present application. Any such future application may include one or more of the following claims, which are given by way of example and are non-limiting in regard to what may be claimed in any future application.

Claims (5)

  1. The claims defining the invention are as follows
    1. A method for manufacturing an embossing cylinder having surface relief structures configured for producing at least one microstructure image effect in one or more security devices applied to a security document, the method including the following steps: providing a blank embossing cylinder having a surface; and forming surface relief structures corresponding to the at least one microstructure image effect directly on the surface of the cylinder.
  2. 2. A method according to claim 1, wherein the step of forming one or more surface relief structures directly on the surface of the cylinder is carried out by at least one of the following means: (a) laser ablation; (b) electro-mechanical engraving; or (c) chemical etching.
  3. 3. A method according to any one of the preceding claims, further including the step of electroforming a layer of material over the surface relief structures to reduce a size of the microstructure.
  4. 4. A method according to claim 3, wherein the electroformed layer of material is a metal.
  5. 5. A method according to claim 3 or 4, wherein the electroformed layer of material is deposited in a uniform layer.
AU2017100354A 2017-03-27 2017-03-27 Method for manufacturing an embossing cylinder configured for producing microstructure image effects Ceased AU2017100354B4 (en)