KR102471020B1 - Protection film for display device, display device and manufacturing method thereof - Google Patents

Protection film for display device, display device and manufacturing method thereof Download PDF

Info

Publication number
KR102471020B1
KR102471020B1 KR1020160030513A KR20160030513A KR102471020B1 KR 102471020 B1 KR102471020 B1 KR 102471020B1 KR 1020160030513 A KR1020160030513 A KR 1020160030513A KR 20160030513 A KR20160030513 A KR 20160030513A KR 102471020 B1 KR102471020 B1 KR 102471020B1
Authority
KR
South Korea
Prior art keywords
film
section
display device
folding axis
strength
Prior art date
Application number
KR1020160030513A
Other languages
Korean (ko)
Other versions
KR20170107141A (en
Inventor
최원우
권승욱
윤승호
이상봉
황채룡
Original Assignee
삼성디스플레이 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 삼성디스플레이 주식회사 filed Critical 삼성디스플레이 주식회사
Priority to KR1020160030513A priority Critical patent/KR102471020B1/en
Publication of KR20170107141A publication Critical patent/KR20170107141A/en
Application granted granted Critical
Publication of KR102471020B1 publication Critical patent/KR102471020B1/en

Abstract

본 발명의 일 실시예에 따른 표시 장치는 제1 구간 및 제 2 구간을 포함하는 표시 패널 및 상기 표시 패널의 일면에 위치하는 강점 필름을 포함하며, 상기 표시 패널은 폴딩 축을 축으로 상기 강점 필름이 바깥 면에 오도록 접힐 수 있고, 상기 폴딩 축은 상기 제1 구간을 지나고 상기 제2 구간은 지나지 않으며, 상기 강점 필름은 상기 제2 구간에 대응하여 위치하며, 상기 제1 구간에는 위치하지 않는다.A display device according to an embodiment of the present invention includes a display panel including a first section and a second section and a strength film positioned on one side of the display panel, wherein the display panel has the strength film around a folding axis. It may be folded to face the outer surface, the folding axis passes through the first section and does not pass through the second section, and the strength film is located corresponding to the second section and not located in the first section.

Description

표시 장치용 보호 필름, 표시 장치 및 이의 제조 방법{PROTECTION FILM FOR DISPLAY DEVICE, DISPLAY DEVICE AND MANUFACTURING METHOD THEREOF}Protective film for display device, display device and manufacturing method thereof

본 개시는 표시 장치용 보호 필름, 표시 장치 및 이의 제조 방법에 관한 것으로서, 보다 구체적으로 가요성 표시 장치에 관한 것이다.The present disclosure relates to a protective film for a display device, a display device, and a manufacturing method thereof, and more particularly, to a flexible display device.

현재 알려져 있는 표시 장치에는 액정 표시 장치(liquid crystal display: LCD), 플라즈마 표시 장치(plasma display panel: PDP), 유기 발광 표시 장치(organic light emitting diode device: OLED device), 전계 발광 표시 장치(field emission display: FED), 전기 영동 표시 장치(electrophoretic display device) 등이 있다.Currently known display devices include a liquid crystal display (LCD), a plasma display panel (PDP), an organic light emitting diode device (OLED device), and a field emission display. display: FED), electrophoretic display device, and the like.

이러한 표시 장치는 일반적으로 박막 트랜지스터, 발광층을 포함하는 표시 패널과 표시 패널 상에 편광 필름, 터치 스크린 패널(TSP; touch screen panel) 등의 층들이 적층된다. 표시 장치의 최외곽부에는 외부로부터의 수분 및 산소 침투를 막기 위하여, 투명 윈도우를 이용하여 표시 패널 및 편광 필름, 터치 스크린 패널 등의 층들을 봉지(encapsulation)하게 된다.Such a display device generally includes a display panel including a thin film transistor and a light emitting layer, and layers such as a polarizing film and a touch screen panel (TSP) are stacked on the display panel. Layers such as a display panel, a polarizing film, and a touch screen panel are encapsulated by using a transparent window in order to prevent permeation of moisture and oxygen from the outside to the outermost portion of the display device.

특히, 폴더블 표시 장치의 경우, 가요성 표시 패널을 이용하며, 각 층들을 감압 접착제(PSA; Pressure Sensitive Adhesive) 등으로 부착시키는데, 표시 장치를 폴딩할 때 층간 점착력이 가장 약한 층이 떨어져서 버클링(buckling), 박리와 같은 불량이 발생하게 된다.In particular, in the case of a foldable display, a flexible display panel is used, and each layer is attached with a pressure sensitive adhesive (PSA) or the like. Defects such as buckling and peeling occur.

실시예들은 보호 필름의 변형을 방지할 수 있는 표시 장치용 보호 필름 제공 및 이를 통해 가요성이 향상된 표시 장치를 제공하기 위한 것이다.Embodiments are intended to provide a protective film for a display device capable of preventing deformation of the protective film and a display device having improved flexibility through the protective film.

본 발명의 일 실시예에 따른 표시 장치는 제1 구간 및 제 2 구간을 포함하는 표시 패널 및 상기 표시 패널의 일면에 위치하는 강점 필름을 포함하며, 상기 표시 패널은 폴딩 축을 축으로 상기 강점 필름이 바깥 면에 오도록 접힐 수 있고, 상기 폴딩 축은 상기 제1 구간을 지나고 상기 제2 구간은 지나지 않으며, 상기 강점 필름은 상기 제2 구간에 대응하여 위치하며, 상기 제1 구간에는 위치하지 않는다.A display device according to an embodiment of the present invention includes a display panel including a first section and a second section and a strength film positioned on one side of the display panel, wherein the display panel has the strength film around a folding axis. It may be folded to face the outer surface, the folding axis passes through the first section and does not pass through the second section, and the strength film is located corresponding to the second section and not located in the first section.

상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 구부러지는 부분이며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 구부러지지 않고 편평한 부분일 수 있다.The first section may be a portion that is bent when the display device is folded around the folding axis, and the second section may be a flat portion that is not bent when the display device is folded around the folding axis.

상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 곡률을 갖는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 곡률을 갖지 않는 부분일 수 있다.The first section may be a portion having a curvature when the display device is folded around the folding axis, and the second section may be a portion having no curvature when the display device is folded around the folding axis.

상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 외력을 받는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 외력을 받지 않는 부분일 수 있다.The first section may be a portion that receives an external force when the display device is folded around the folding axis, and the second section may be a portion that does not receive an external force when the display device is folded around the folding axis.

상기 제1 구간은 상기 표시 장치가 많이 접힐수록 폭이 넓을 수 있다.The first section may have a wider width as the display device is folded more.

상기 강점 필름은 폴레에틸렌 테레프탈레이트(PET; polyethylene terephthalate), 폴리에틸렌 나프탈레이트(PEN; polyethylene naphthalate), 폴리에틸렌 설파이드(PES; polyethylene sulfide) 및 폴리에틸렌(PE; polyethylene) 중 적어도 어느 하나를 포함할 수 있다.The strength film may include at least one of polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyethylene sulfide (PES), and polyethylene (PE).

본 발명의 일 실시예에 따른 표시 장치의 제조 방법은 제1 구간 및 상기 제1 구간에 의해 구분되는 제2 구간을 포함하는 약점 필름 일면에 상기 제2 구간에는 대응하여 위치하여 상기 제1 구간에 대응하여는 공간을 갖도록 강점 필름을 부착하는 단계, 상기 공간에 액상 점착제층을 형성하는 단계, 상기 감정 필름 및 상기 액상 점착제층을 사이에 두고 상기 약점 필름과 마주보도록 이형 필름을 부착하는 단계 및 상기 액상 점착제층을 경화하는 단계를 포함하는 하부 보호 필름 형성 단계를 포함하며, 상기 하부 보호 필름 형성 단계를 거쳐 형성된 하부 보호 필름에서 상기 이형 필름을 제거하여 마더 글라스에 부착하는 단계, 상기 약점 필름과 함께 상기 액상 점착제층을 제거하는 단계를 포함한다.A method of manufacturing a display device according to an embodiment of the present invention is provided on one side of a weak film including a first section and a second section divided by the first section and positioned corresponding to the second section to form the first section. Correspondingly, the step of attaching a strength film to have a space, the step of forming a liquid adhesive layer in the space, the step of attaching a release film to face the weak film with the emotion film and the liquid pressure-sensitive adhesive layer interposed therebetween, and A step of forming a lower protective film including curing the liquid adhesive layer, and removing the release film from the lower protective film formed through the step of forming the lower protective film and attaching the release film to the mother glass, together with the weak film and removing the liquid pressure-sensitive adhesive layer.

점착력은 상기 액상 점착제층에 비하여 상기 약점 필름이 클 수 있으며, 상기 약점 필름에 비하여 상기 강점 필름이 클 수 있다.The adhesive strength of the weak film may be greater than that of the liquid pressure-sensitive adhesive layer, and the strength film may be greater than that of the weak film.

상기 표시 장치는 폴딩 축을 축으로 상기 강점 필름이 바깥 면에 오도록 접힐 수 있으며. 상기 제1 구간은 상기 폴딩 축을 포함하여 상기 폴딩 축의 주변에 설정될 수 있다.The display device may be folded around a folding axis so that the strength film faces an outer surface. The first section may be set around the folding axis including the folding axis.

상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 구부러지는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 구부러지지 않고 편평한 부분일 수 있다.The first section may be a portion that is bent when the display device is folded around the folding axis, and the second section may be a flat portion that is not bent when the display device is folded around the folding axis.

상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 곡률을 갖는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 곡률을 갖지 않는 부분일 수 있다.The first section may be a portion having a curvature when the display device is folded around the folding axis, and the second section may be a portion having no curvature when the display device is folded around the folding axis.

상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 외력을 받는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 외력을 받지 않는 부분일 수 있다.The first section may be a portion that receives an external force when the display device is folded around the folding axis, and the second section may be a portion that does not receive an external force when the display device is folded around the folding axis.

상기 하부 보호 필름은 상기 마더 글라스에 패널 단위로 부착할 수 있다.The lower protective film may be attached to the mother glass in a panel unit.

본 발명의 일 실시예에 따른 표시 장치용 보호 필름은 제1 구간 및 상기 제1 구간에 의해 구분되는 제2 구간을 포함하는 약점 필름, 상기 약점 필름 일면에 위치하며 상기 제2 구간에 대응하여 위치하는 강점 필름, 상기 강점 필름 사이의 상기 제1 구간에 대응하는 부분에 위치하는 액상 점착제층 및 상기 액상 점착제층 및 상기 강점 필름을 사이에 두고 상기 약점 필름과 마주보는 이형 필름을 포함하며, 점착력은 상기 액상 점착제층에 비하여 상기 약점 필름이 크며, 상기 약점 필름에 비하여 상기 강점 필름이 크다.A protective film for a display device according to an embodiment of the present invention is a weak film including a first section and a second section divided by the first section, located on one surface of the weak film and positioned corresponding to the second section. A strength film, a liquid pressure-sensitive adhesive layer positioned in a portion corresponding to the first section between the strength film, and a release film facing the weak point film with the liquid pressure-sensitive adhesive layer and the strength film interposed therebetween, wherein the adhesive strength is The weak film is larger than the liquid pressure-sensitive adhesive layer, and the strong film is larger than the weak film.

상기 제1 구간은 상기 표시 장치용 보호 필름이 폴딩 축을 축으로 접힐 때 구부러지는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치용 보호 필름이 상기 폴딩 축을 축으로 접힐 때 구부러지지 않고 편평한 부분일 수 있다.The first section may be a portion that is bent when the protective film for a display device is folded around a folding axis, and the second section may be a flat portion that is not bent when the protective film for a display device is folded around the folding axis. can

상기 제1 구간은 상기 표시 장치용 보호 필름이 폴딩 축을 축으로 접힐 때 곡률을 갖는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치용 보호 필름이 상기 폴딩 축을 축으로 접힐 때 곡률을 갖지 않는 부분일 수 있다.The first section may be a portion having curvature when the protective film for a display device is folded around a folding axis, and the second section may be a portion having no curvature when the protective film for a display device is folded around the folding axis. can be

상기 제1 구간은 상기 표시 장치용 보호 필름이 폴딩 축을 축으로 접힐 때 외력을 받는 부분일 수 있으며, 상기 제2 구간은 상기 표시 장치용 보호 필름이 상기 폴딩 축을 축으로 접힐 때 외력을 받지 않는 부분일 수 있다.The first section may be a portion that receives an external force when the protective film for a display device is folded around the folding axis, and the second section is a portion that does not receive an external force when the protective film for a display device is folded around the folding axis. can be

실시예들에 따르면, 보호 필름의 변형을 방지할 수 있는 표시 장치용 보호 필름을 제공할 수 있고 이를 통해 가요성이 향상된 표시 장치를 제조할 수 있다.According to embodiments, a protective film for a display device capable of preventing deformation of the protective film may be provided, and a display device having improved flexibility may be manufactured through the protective film.

도 1은 본 발명의 일 실시예에 따른 표시 장치의 단면도이다.
도 2는 도 1의 표시 장치를 구부리는 과정을 도시한 단면도이다.
도 3은 본 발명의 일 실시예에 따른 표시 장치를 구부린 형태를 전체적으로 나타낸 개략도이다.
도 4는 비교예에 따른 표시 장치의 단면도이다.
도 5는 도 4의 비교예에 따른 표시 장치를 구부린 단면도이다.
도 6은 도 5의 비교예에 따른 표시 장치를 구부렸다 다시 핀 단면도이다.
도 7 내지 도 14는 본 발명의 일 실시예에 따른 표시 장치의 제조 방법을 순차적으로 나타낸 도면이다.
도 15는 본 발명의 일 실시예에 따른 표시 장치의 단면도이다.
도 16은 본 발명의 일 실시예에 따른 표시 장치를 구부린 형태를 전체적으로 나타낸 개략도이다.
1 is a cross-sectional view of a display device according to an exemplary embodiment of the present invention.
FIG. 2 is a cross-sectional view illustrating a process of bending the display device of FIG. 1 .
3 is a schematic diagram showing a bent shape of a display device according to an exemplary embodiment of the present invention as a whole.
4 is a cross-sectional view of a display device according to a comparative example.
5 is a cross-sectional view in which the display device according to the comparative example of FIG. 4 is bent.
FIG. 6 is a cross-sectional view of a pin of the display device according to the comparative example of FIG. 5 after being bent.
7 to 14 are diagrams sequentially illustrating a method of manufacturing a display device according to an exemplary embodiment of the present invention.
15 is a cross-sectional view of a display device according to an exemplary embodiment.
16 is a schematic diagram showing a bent shape of a display device according to an exemplary embodiment of the present invention as a whole.

이하, 첨부한 도면을 참고로 하여 본 발명의 여러 실시예들에 대하여 본 발명이 속하는 기술 분야에서 통상의 지식을 가진 자가 용이하게 실시할 수 있도록 상세히 설명한다. 본 발명은 여러 가지 상이한 형태로 구현될 수 있으며 여기에서 설명하는 실시예들에 한정되지 않는다.Hereinafter, various embodiments of the present invention will be described in detail with reference to the accompanying drawings so that those skilled in the art can easily carry out the present invention. This invention may be embodied in many different forms and is not limited to the embodiments set forth herein.

본 발명을 명확하게 설명하기 위해서 설명과 관계없는 부분은 생략하였으며, 명세서 전체를 통하여 동일 또는 유사한 구성요소에 대해서는 동일한 참조 부호를 붙이도록 한다.In order to clearly describe the present invention, parts irrelevant to the description are omitted, and the same reference numerals are assigned to the same or similar components throughout the specification.

또한, 도면에서 나타난 각 구성의 크기 및 두께는 설명의 편의를 위해 임의로 나타내었으므로, 본 발명이 반드시 도시된 바에 한정되지 않는다. 도면에서 여러 층 및 영역을 명확하게 표현하기 위하여 두께를 확대하여 나타내었다. 그리고 도면에서, 설명의 편의를 위해, 일부 층 및 영역의 두께를 과장되게 나타내었다.In addition, since the size and thickness of each component shown in the drawings are arbitrarily shown for convenience of explanation, the present invention is not necessarily limited to the shown bar. In the drawings, the thickness is shown enlarged to clearly express the various layers and regions. And in the drawings, for convenience of explanation, the thicknesses of some layers and regions are exaggerated.

또한, 층, 막, 영역, 판 등의 부분이 다른 부분 "위에" 또는 "상에" 있다고 할 때, 이는 다른 부분 "바로 위에" 있는 경우뿐 아니라 그 중간에 또 다른 부분이 있는 경우도 포함한다. 반대로 어떤 부분이 다른 부분 "바로 위에" 있다고 할 때에는 중간에 다른 부분이 없는 것을 뜻한다. 또한, 기준이 되는 부분 "위에" 또는 "상에" 있다고 하는 것은 기준이 되는 부분의 위 또는 아래에 위치하는 것이고, 반드시 중력 반대 방향 쪽으로 "위에" 또는 "상에" 위치하는 것을 의미하는 것은 아니다.In addition, when a part such as a layer, film, region, plate, etc. is said to be "on" or "on" another part, this includes not only the case where it is "directly on" the other part, but also the case where another part is in the middle. . Conversely, when a part is said to be "directly on" another part, it means that there is no other part in between. In addition, being "above" or "on" a reference part means being located above or below the reference part, and does not necessarily mean being located "above" or "on" in the opposite direction of gravity. .

또한, 명세서 전체에서, 어떤 부분이 어떤 구성요소를 "포함" 한다고 할 때, 이는 특별히 반대되는 기재가 없는 한 다른 구성요소를 제외하는 것이 아니라 다른 구성요소를 더 포함할 수 있는 것을 의미한다.In addition, throughout the specification, when a certain component is said to "include", it means that it may further include other components without excluding other components unless otherwise stated.

또한, 명세서 전체에서, "평면상"이라 할 때, 이는 대상 부분을 위에서 보았을 때를 의미하며, "단면상"이라 할 때, 이는 대상 부분을 수직으로 자른 단면을 옆에서 보았을 때를 의미한다.In addition, throughout the specification, when it is referred to as "planar image", it means when the target part is viewed from above, and when it is referred to as "cross-sectional image", it means when a cross section of the target part cut vertically is viewed from the side.

이하에서, 도 1 내지 도 3을 참조하여 본 발명의 일 실시예에 따른 표시 장치를 설명한다. 도 1은 본 발명의 일 실시예에 따른 표시 장치의 단면도이다. 도 2는 도 1의 표시 장치를 구부리는 과정을 도시한 단면도이다. 도 3은 본 발명의 일 실시예에 따른 표시 장치를 구부린 형태를 전체적으로 나타낸 개략도이다.Hereinafter, a display device according to an exemplary embodiment of the present invention will be described with reference to FIGS. 1 to 3 . 1 is a cross-sectional view of a display device according to an exemplary embodiment of the present invention. FIG. 2 is a cross-sectional view illustrating a process of bending the display device of FIG. 1 . 3 is a schematic diagram showing a bent shape of a display device according to an exemplary embodiment of the present invention as a whole.

표시 장치(1000)는 화상을 표시하는 표시 패널(100), 표시 패널(100)의 제1 면에 위치하는 상부 보호 필름(5) 및 표시 패널(100)의 제2 면에 위치하는 강점 필름(2)을 포함한다.The display device 1000 includes a display panel 100 displaying an image, an upper protective film 5 positioned on a first surface of the display panel 100, and a strength film positioned on a second surface of the display panel 100 ( 2) include.

표시 장치(1000)는 폴딩 축(도 1 및 2의 점선 라인 참조, 이라 편의상 F라 칭한다)을 축으로 하여 접힐 수 있다. 표시 장치(1000)는 표시 장치(1000)를 도 1 및 도 2에서와 같이 3분하는 두 개의 지점에서 두 개의 폴딩 축(F)을 축으로 하여 접힐 수 있다. 표시 장치(1000)는 도 2 및 도 3에 도시한 바와 같이 상부 보호 필름(5)이 위치하는 면이 안쪽으로 가고 강점 필름(2)이 위치한 면이 바깥 면이 되도록 접힌다. 도 1 및 도 2에서는 표시 장치(1000)가 표시 장치(1000)를 3분하는 두 개의 폴딩 축(F)을 축으로 하여 접힐 수 있는 것으로 도시하였으나, 실시예에 따라서 표시 장치(1000)는 한 개 이상의 폴딩 축(F)을 포함할 수 있으며, 폴딩 축(F)의 위치는 본 도면에 한정되지 않고 필요에 따라 자유로이 위치할 수 있다. 표시 장치(1000)는 폴딩 축(F)을 축으로 하여 반복적으로 접었다 피는 것이 가능하다.The display device 1000 may be folded using a folding axis (refer to the dotted line in FIGS. 1 and 2 , and referred to as F for convenience) as an axis. The display device 1000 may be folded using two folding axes F as axes at two points dividing the display device 1000 into thirds as shown in FIGS. 1 and 2 . As shown in FIGS. 2 and 3 , the display device 1000 is folded so that the side on which the upper protective film 5 is located is inward and the side on which the strength film 2 is located is on the outside. 1 and 2 show that the display device 1000 can be folded around two folding axes F that divide the display device 1000 into three parts, but according to embodiments, the display device 1000 can It may include one or more folding axes F, and the position of the folding axis F is not limited to this drawing and may be freely positioned as needed. The display device 1000 can be repeatedly folded and unfolded around the folding axis F as an axis.

도 2 및 도 3을 참고하면, 제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 접혀 구부러지는 부분이고, 제2 구간(B)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 접히지 않고 편평한 부분이다. 폴딩 축(F)은 제1 구간(A)을 지난다. 도 3과 같이, 제1 구간(A)은 표시 장치(1000)가 접히는 부분을 따라 표시 장치(1000)를 가로질러 뻗어있다. 제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 곡률을 갖는 부분일 수 있으며, 제2 구간(B)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 곡률을 갖지 않는 부분일 수 있다. 또는, 제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 제2 구간(B)에 비해 곡률이 큰 부분일 수 있다. 제2 구간(B)은 제1 구간(A)보다 폭이 클 수 있다. 제1 구간(A)의 폭은 표시 장치(1000)가 접히는 각도에 따라 달라질 수 있다.Referring to FIGS. 2 and 3 , the first section A is a portion that is bent when the display device 1000 is folded around the folding axis F, and the second section B is the portion of the display device 1000 is a flat portion that is not folded when folded around the folding axis F. The folding axis (F) passes through the first section (A). As shown in FIG. 3 , the first section A extends across the display device 1000 along a folded portion of the display device 1000 . The first section A may have a curvature when the display device 1000 is folded around the folding axis F, and the second section B may have a curvature when the display device 1000 is folded around the folding axis F. It may be a part that does not have curvature when folded axially. Alternatively, the first section A may have a greater curvature than the second section B when the display device 1000 is folded along the folding axis F. The second section (B) may have a wider width than the first section (A). The width of the first section A may vary according to the angle at which the display device 1000 is folded.

도 1 및 도 2에서는 제1 구간(A)의 폭은 폴딩 축(F)을 중심으로 좌우가 대칭이며, 두 개의 제1 구간(A)의 폭이 같은 것으로 도시하였으나, 실시예에 따라서는 제1 구간(A)의 폭이 폴딩 축(F)을 중심으로 좌우가 대칭이 아닐 수 있으며, 두 개의 제1 구간(A)의 폭도 서로 다를 수 있다. 제1 구간(A) 및 제2 구간(B)은 표시 장치(1000)가 접히는 모양에 따라 다양하게 설정될 수 있다.In FIGS. 1 and 2, the width of the first section A is symmetrical on the left and right around the folding axis F, and the widths of the two first sections A are the same, but depending on the embodiment, The width of one section (A) may not be symmetrical on the left and right around the folding axis (F), and the widths of the two first sections (A) may also be different from each other. The first section (A) and the second section (B) may be set in various ways according to the folding shape of the display device 1000 .

강점 필름(2)은 표시 패널(100) 제2 면에 위치하며, 표시 패널(100)과 강점 필름(2) 사이에는 점착제층(미도시)이 위치할 수 있다.The strength film 2 is positioned on the second surface of the display panel 100, and an adhesive layer (not shown) may be positioned between the display panel 100 and the strength film 2.

강점 필름(2)은 제2 구간(B)에 대응하는 부분에 위치한다. 강점 필름(2)은 제1 구간(A)에 대응하는 부분에는 위치하지 않는다. 즉, 강점 필름(2)은 표시 장치(1000)가 접히는 부분에는 위치하지 않는다. 강점 필름(2)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 접히지 않고 편평한 부분인 제2 구간(B)과 대응하는 부분에 위치하고, 구부러지는 부분인 제1 구간(A)과 대응하는 부분에서는 위치하지 않는다. 즉, 강점 필름(2)은 표시 장치(1000)가 접히는 부분에 해당하는 제1 구간(A)에 의해 복수의 영역(2a, 2b, 2c)으로 구분된다. 강점 필름(2)은 표시 장치(1000)를 가로 질러 뻗어있는 제1 구간(A)에 의해 구분되는 복수의 영역(2a, 2b, 2c), 즉, 제1 영역(2a), 제2 영역(2b) 및 제3 영역(2c)을 포함한다. 강점 필름(2)은 폴딩 축(F)을 중심으로 좌우로 같은 폭만큼 이격되어 위치할 수 있다. 즉, 제1 영역(2a) 및 제2 영역(2b)은 폴딩 축(F)을 중심으로 좌우로 대칭인 위치에 위치할 수 있으며, 제2 영역(2b) 및 제3 영역(2c)도 폴딩 축(F)을 중심으로 좌우로 대칭인 위치에 위치할 수 있다. 폴딩 축(F)은 강점 필름(2)을 지나지 않는다. 강점 필름(2)은 표시 장치(1000)가 접히는 모양에 따라 다양한 형태의 복수의 영역을 포함할 수 있다.The strong film 2 is located in a portion corresponding to the second section B. The strength film 2 is not located in a portion corresponding to the first section A. That is, the strength film 2 is not positioned at a portion where the display device 1000 is folded. Strength The film 2 is located in a portion corresponding to the second section B, which is a flat portion that is not folded when the display device 1000 is folded around the folding axis F, and the first section A, which is a bent portion. It is not located in the part corresponding to That is, the strength film 2 is divided into a plurality of areas 2a, 2b, and 2c by the first section A corresponding to the folded portion of the display device 1000 . The strength film 2 includes a plurality of regions 2a, 2b, and 2c divided by the first section A extending across the display device 1000, that is, the first region 2a and the second region ( 2b) and a third area 2c. The strength film 2 may be spaced apart from each other by the same width from side to side around the folding axis F. That is, the first region 2a and the second region 2b may be positioned symmetrically left and right about the folding axis F, and the second region 2b and the third region 2c may also be folded. It may be located in a symmetrical position left and right about the axis (F). The folding axis (F) does not pass through the strength film (2). The strength film 2 may include a plurality of regions of various shapes according to a shape in which the display device 1000 is folded.

강점 필름(2)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 곡률을 갖지 않는 부분에 위치할 수 있고, 곡률을 갖는 부분에는 위치하지 않을 수 있다. 또는, 강점 필름(2)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 제2 구간(B)에 비해 곡률이 큰 부분에 위치할 수 있다.When the display device 1000 is folded along the folding axis F, the strength film 2 may be located on a portion having no curvature, and may not be located on a portion having a curvature. Alternatively, when the display device 1000 is folded along the folding axis F, the strength film 2 may be positioned at a portion with greater curvature than the second section B.

강점 필름(2)은 폴레에틸렌 테레프탈레이트(Polyethylene Terephthalate, PET), 폴리에틸렌 나프탈레이트(Polyethylene Naphthalate, PEN), 폴리에틸렌 설파이드(Polyethylene Sulfide, PES), 폴리에틸렌(Polyethylene PE) 중 적어도 어느 하나의 물질을 포함할 수 있다.The strength film (2) may contain at least one of polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polyethylene sulfide (PES), and polyethylene (PE). can

강점 필름(2)은 25 마이크로미터(㎛) 내지 300 마이크로미터(㎛)의 두께를 가질 수 있다. 강점 필름(2)은 100 마이크로미터(㎛)의 두께를 가질 수 있다.The strong film 2 may have a thickness of 25 micrometers (μm) to 300 micrometers (μm). The strength film 2 may have a thickness of 100 micrometers (μm).

강점 필름(2)은 표시 패널(100)의 외부와의 직접적인 물리적 접촉을 방지하여 표시 패널(100)의 물리적 손상을 방지할 수 있다.The strength film 2 may prevent physical damage to the display panel 100 by preventing direct physical contact with the outside of the display panel 100 .

한 실시예에 따르면, 표시 패널(100)은 TFT 기판(110), 박막 봉지층(210) 및 TFT 기판(110)과 박막 봉지층(210) 사이에 위치하는 유기 발광 소자(300)을 포함할 수 있다.According to an embodiment, the display panel 100 may include a TFT substrate 110, a thin film encapsulation layer 210, and an organic light emitting device 300 positioned between the TFT substrate 110 and the thin film encapsulation layer 210. can

TFT 기판(110)은 투명한 기판으로 고분자 필름과 같은 가요성(flexible) 기판일 수 있고, 게이트 신호를 전달하는 게이트선, 데이터 신호를 전달하는 데이터선, 구동 전압을 전달하는 구동 전압선 등을 포함하는 복수의 신호선 및 스위칭 트랜지스터, 구동 트랜지스터 등을 포함하는 복수의 박막 트랜지스터(TFT)를 포함할 수 있다.The TFT substrate 110 is a transparent substrate and may be a flexible substrate such as a polymer film, and includes a gate line for transmitting a gate signal, a data line for transmitting a data signal, a driving voltage line for transmitting a driving voltage, and the like. It may include a plurality of thin film transistors (TFTs) including a plurality of signal lines and switching transistors and driving transistors.

스위칭 트랜지스터의 제어 단자는 게이트선에 연결되어 있고, 입력 단자는 데이터선에 연결되어 있으며, 출력 단자는 구동 트랜지스터에 연결되어 있다. 스위칭 트랜지스터는 게이트선으로 부터 받은 게이트 신호에 응답하여 데이터선으로부터 받은 데이터 신호를 구동 트랜지스터에 전달한다.The control terminal of the switching transistor is connected to the gate line, the input terminal is connected to the data line, and the output terminal is connected to the driving transistor. The switching transistor transfers the data signal received from the data line to the driving transistor in response to the gate signal received from the gate line.

구동 트랜지스터의 제어 단자는 스위칭 트랜지스터에 연결되어 있고, 입력 단자는 구동 전압선에 연결되어 있으며, 출력 단자는 유기 발광 소자에 연결되어 있다. 구동 트랜지스터는 제어 단자와 출력 단자 사이에 걸리는 전압에 따라 그 크기가 달라지는 출력 전류를 흘린다.A control terminal of the driving transistor is connected to the switching transistor, an input terminal is connected to the driving voltage line, and an output terminal is connected to the organic light emitting element. The driving transistor flows an output current whose size varies according to the voltage applied between the control terminal and the output terminal.

유기 발광 소자(300)는 예를 들면 유기 발광 다이오드(organic light emitting diode, OLED)로서, 구동 트랜지스터의 출력 단자에 연결되어 있는 애노드(anode)와 공통 전압에 연결되어 있는 캐소드(cathode)를 포함한다. 유기 발광 소자(300)는 구동 트랜지스터의 출력 전류에 따라 세기를 달리하여 발광함으로써 영상을 표시한다. 유기 발광 소자(300)는 적색, 녹색, 청색의 삼원색 등 기본색 중 어느 하나 또는 하나 이상의 빛을 고유하게 내는 유기 물질을 포함할 수 있으며, 유기 발광 표시 장치는 이들 색의 공간적인 합으로 원하는 영상을 표시한다.The organic light emitting device 300 is, for example, an organic light emitting diode (OLED), and includes an anode connected to the output terminal of the driving transistor and a cathode connected to a common voltage. . The organic light emitting diode 300 displays an image by emitting light with different intensity according to the output current of the driving transistor. The organic light emitting diode 300 may include any one of the three primary colors of red, green, and blue, or an organic material that uniquely emits one or more lights. display

박막 봉지층(210)은 TFT 기판(110)과 대향하며, 외부로부터 산소 및 수분이 유입되는 것을 방지하여 유기 발광 소자(300)을 보호할 수 있다.The thin film encapsulation layer 210 faces the TFT substrate 110 and can protect the organic light emitting device 300 by preventing oxygen and moisture from entering from the outside.

앞서 설명한 바와 같이, 표시 패널(100)의 제1 면에는 상부 보호 필름(5)이 위치한다. 상부 보호 필름(5)은 박막 봉지층(210)의 손상을 방지할 수 있다. 상부 보호 필름(5)은 편광 필름과 같은 기능성 필름일 수 있다. 편광 필름은 편광 필름이 갖는 편광축과 동일한 축방향의 빛은 통과시키고 다른 빛은 흡수한다. 즉, 편광 필름을 통과한 빛은 선편광된다. 편광 필름으로는 다양한 종류의 편광 필름이 사용될 수 있다. 상부 보호 필름(5)은 약점 필름을 포함할 수 있다. 약점 필름은 강점 필름(2)보다 점착력이 약할 수 있다.As described above, the upper protective film 5 is positioned on the first surface of the display panel 100 . The upper protective film 5 can prevent damage to the thin film encapsulation layer 210 . The upper protective film 5 may be a functional film such as a polarizing film. The polarizing film transmits light in the same axial direction as the polarization axis of the polarizing film and absorbs other light. That is, light passing through the polarizing film is linearly polarized. As the polarizing film, various types of polarizing films may be used. The upper protective film 5 may include a weak point film. The weak film may have weaker adhesion than the strong film (2).

다른 한 실시예에 따르면, 표시 패널은 유기 발광 표시 패널 외에 액정 표시 패널 등일 수 있으며, 액정 표시 패널인 경우 표시 패널은 TFT기판, 액정 분자를 포함하는 액정층, 상부 기판을 포함할 수 있다. TFT기판은 제어 단자가 게이트선에 연결되어 있고 입력 단자가 데이터선에 연결되어 있으며 출력 단자가 화소 전극에 연결되어 있는 스위칭 트랜지스터를 포함할 수 있으며, 액정 표시 패널은 데이터 전압을 인가 받은 화소 전극과 공통 전압을 인가 받은 공통 전극 사이에 형성되는 전계에 의하여 액정 분자의 기울기를 조절하여 다양한 영상을 표시할 수 있다.According to another embodiment, the display panel may be a liquid crystal display panel other than an organic light emitting display panel. In case of a liquid crystal display panel, the display panel may include a TFT substrate, a liquid crystal layer including liquid crystal molecules, and an upper substrate. The TFT substrate may include a switching transistor having a control terminal connected to a gate line, an input terminal connected to a data line, and an output terminal connected to a pixel electrode. Various images can be displayed by adjusting the gradient of liquid crystal molecules by an electric field formed between common electrodes to which a common voltage is applied.

이하에서, 도 1 및 도 2와 함께 도 4 내지 도 6을 참조하여 본 발명의 일 실시예에 따른 표시 장치용 보호 필름을 설명한다. 앞서 설명한 실시예와 동일한 구성에 대한 설명은 생략한다. 도 4는 비교예에 따른 표시 장치의 단면도이다. 도 5는 도 4의 비교예에 따른 표시 장치를 구부린 단면도이다. 도 6은 도 5의 비교예에 따른 표시 장치를 구부렸다 다시 핀 단면도이다.Hereinafter, a protective film for a display device according to an exemplary embodiment of the present invention will be described with reference to FIGS. 4 to 6 along with FIGS. 1 and 2 . A description of the same configuration as that of the previously described embodiment will be omitted. 4 is a cross-sectional view of a display device according to a comparative example. 5 is a cross-sectional view in which the display device according to the comparative example of FIG. 4 is bent. FIG. 6 is a cross-sectional view of a pin of the display device according to the comparative example of FIG. 5 after being bent.

비교예에 따른 표시 장치(1001)는 표시 패널(101)의 제2 면 전면에 위치하는 강점 필름(22)을 포함한다. 표시 장치(1001)는 강점 필름(22), TFT 기판(111), 유기 발광 소자(301), 박막 봉지층(211), 상부 보호 필름(55)이 차례로 위치한다. 강점 필름(22)과 TFT 기판(111) 사이에는 점착제층(미도시)이 위치할 수 있다.The display device 1001 according to the comparative example includes a strength film 22 positioned on the entire surface of the second surface of the display panel 101 . In the display device 1001, a strength film 22, a TFT substrate 111, an organic light emitting element 301, a thin film encapsulation layer 211, and an upper protective film 55 are sequentially positioned. An adhesive layer (not shown) may be positioned between the strength film 22 and the TFT substrate 111 .

표시 장치(1001)는 폴딩 축(F)을 축으로 하여 접힐 수 있다. 제1 구간(A)은 표시 장치(1001)가 폴딩 축(F)을 축으로 접힐 때 접혀 구부러지는 부분이며, 제2 구간(B)은 표시 장치(1001)가 폴딩 축(F)을 축으로 접힐 때 접히지 않고 편평한 부분이다. 도 4의 표시 장치(1001)를 화살표 방향을 따라 폴딩 축(F)을 중심으로 접으면 도 5와 같은 형태가 된다.The display device 1001 may be folded around the folding axis F as an axis. The first section (A) is a portion that is bent when the display device 1001 is folded around the folding axis (F), and the second section (B) is the portion where the display device 1001 is folded around the folding axis (F). It is a flat part that does not fold when folded. When the display device 1001 of FIG. 4 is folded around the folding axis F in the direction of the arrow, the shape shown in FIG. 5 is obtained.

표시 장치(1001)가 폴딩 축(F)을 축으로 화살표 방향으로 접힐 때, 강점 필름(22)이 접히는 부분에서 누르는 힘과 양 쪽으로 당기는 힘이 작용한다. 도 4 및 도 5을 보면, 외력이 작용하는 부분의 예시로써 강점 필름(22) 위에 점을 표시하였다. 폴딩 축(F) 위에 위치하는 강점 필름(22)의 점에는 화살표 방향과 같은 힘이 작용한다. 표시 장치(1001)가 접히면서 표시 패널(101)에 의해 강점 필름(22)이 폴딩 축(F)을 중심으로 눌려 강점 필름(22)위 점에는 누르는 힘이 작용한다. 또한, 표시 장치(1001)가 접히면서 표시 장치(1001)가 폴딩 축(F)을 기준으로 양 옆으로 늘어나기 때문에 강점 필름(22)의 점에는 폴딩 축(F)을 중심으로 양 쪽으로 당기는 힘이 작용한다.When the display device 1001 is folded along the folding axis F in the direction of the arrow, a pressing force at the folded portion of the strength film 22 and a pulling force in both directions act. Referring to FIGS. 4 and 5 , dots are marked on the strength film 22 as an example of a portion where an external force acts. A force in the direction of the arrow acts on a point of the strong film 22 positioned on the folding axis F. While the display device 1001 is folded, the display panel 101 presses the strength film 22 about the folding axis F, and a pressing force acts on a point on the strength film 22. In addition, as the display device 1001 is folded, the display device 1001 is stretched on both sides with respect to the folding axis F, so the point of the strength film 22 is the pulling force to both sides around the folding axis F. this works

도 5의 표시 장치(1001)를 다시 피면 도 6과 같은 형태가 된다. 강점 필름(22)에 누르는 힘과 당기는 힘이 작용하는 상태로 유지되었다가 외력이 없어지는 경우, 누르는 힘과 당기는 힘에 의해 강점 필름(22)이 변형을 일으킬 수 있다. 강점 필름(22)이 외력을 받는 동안 늘어나서 외력이 없어진 후에는 원래보다 얇아지고 점착상태가 해소되어 떨어지게 된다. 그 결과 강점 필름(22)은 도 6과 같이 주름이 발생할 수 있다. 또한, 강점 필름(22)과 TFT 기판(111)사이의 점착제층(미도시) 역시, 누르는 힘에 의해 양쪽으로 빠져나가려 하게 되고, 외력이 없어진 후 원래 보다 얇아지고 점착력이 약해져 강점 필름(22)이 떨어지는데 원인이 될 수 있다.When the display device 1001 of FIG. 5 is opened again, it becomes the same form as that of FIG. 6 . When the pressing force and the pulling force are maintained on the strength film 22 and the external force disappears, the strength film 22 may be deformed by the pressing force and the pulling force. The strength film 22 is stretched while receiving an external force, and after the external force is removed, it becomes thinner than the original and the adhesive state is resolved and falls off. As a result, the strength film 22 may have wrinkles as shown in FIG. 6 . In addition, the adhesive layer (not shown) between the strength film 22 and the TFT substrate 111 also tends to escape to both sides by the pressing force, and after the external force is removed, it becomes thinner than the original and the adhesive force is weakened, resulting in the strength film 22 This may cause it to fall.

그러나, 도 1 및 도 2를 참고하면, 실시예에 따른 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때, 외력이 작용하여 문제가 될 수 있는 제1 구간(A)에서는 강점 필름(2)이 제거되어 있다. 강점 필름(2)은 표시 장치(1000)가 접히는 부분인 제1 구간(A)에 위치하지 않으므로 외력에 의한 강점 필름(2)의 변형을 방지할 수 있다. 또한, 표시 장치(1000)가 접히는 부분인 제1 구간(A)에서 강점 필름(2)이 제거됨으로써, 표시 장치(1000)의 전체 두께가 얇아진다. 따라서, 보호 필름의 두께로 인해 표시 장치(1000)를 더 작은 곡률 반경을 가지도록 구부릴 수 있다.However, referring to FIGS. 1 and 2 , when the display device 1000 according to the embodiment is folded along the folding axis F, the strength film is applied in the first section A, which may cause problems due to an external force. (2) is removed. Since the strength film 2 is not located in the first section A, which is a foldable portion of the display device 1000, deformation of the strength film 2 due to external force may be prevented. In addition, since the strength film 2 is removed from the first section A, which is a foldable portion of the display device 1000, the overall thickness of the display device 1000 is reduced. Accordingly, the display device 1000 may be bent to have a smaller radius of curvature due to the thickness of the protective film.

제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 외력을 받는 부분일 수 있으며, 제2 구간(B)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 외력을 받지 않는 부분일 수 있다. 또는, 제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 제2 구간(B)에 비해 상대적으로 외력을 더 많이 받는 부분일 수 있다. 즉, 강점 필름(2)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 외력을 받는 부분에는 위치하지 않을 수 있다.The first section (A) may be a portion that receives an external force when the display device 1000 is folded around the folding axis (F), and the second section (B) may be a portion where the display device 1000 is folded along the folding axis (F). It may be a part that does not receive an external force when folded into an axis. Alternatively, the first section A may be a portion that receives relatively more external force than the second section B when the display device 1000 is folded along the folding axis F. That is, the strength film 2 may not be positioned at a portion that receives an external force when the display device 1000 is folded along the folding axis F.

이하에서, 도 1 및 도 7 내지 도 14를 참조하여 본 발명의 일 실시예에 따른 표시 장치를 설명한다. 앞서 설명한 실시예와 동일한 구성에 대한 설명은 생략한다. 도 7 내지 도 14는 본 발명의 일 실시예에 따른 표시 장치의 제조 방법을 순차적으로 나타낸 도면이다.Hereinafter, a display device according to an exemplary embodiment of the present invention will be described with reference to FIGS. 1 and 7 to 14 . A description of the same configuration as that of the previously described embodiment will be omitted. 7 to 14 are diagrams sequentially illustrating a method of manufacturing a display device according to an exemplary embodiment of the present invention.

우선, 도 7과 같이 약점 필름(1)을 준비한다. 약점 필름(1)은 아크릴(Acryl) 계열에 치환기가 붙은 약점착 필름일 수 있으며, 점착력은 1 gf/inch 이상에서 5 gf/inch 이하일 수 있다.First, as shown in FIG. 7, a weak film 1 is prepared. The weak film 1 may be a weak adhesive film having an acrylic substituent attached thereto, and may have an adhesive strength of 1 gf/inch or more to 5 gf/inch or less.

약점 필름(1) 일면에 강점 필름(2)를 부착한다. 강점 필름(2)은 추후 완성될 표시 장치의 접히는 부분을 고려하여 접히는 부분에 대응되는 부분에는 부착하지 않는다. 즉, 추후 완성될 표시 장치가 폴딩 축(F)을 축으로 접힐 때 접히지 않고 편평한 부분인 제2 구간(B)과 대응하는 곳에만 강점 필름(2)을 부착하고, 구부러지는 부분인 제1 구간(A)과 대응하는 곳에서는 강점 필름(2)을 부착하지 않고 공간을 만든다.A strong film (2) is attached to one side of the weak film (1). The strong film 2 is not attached to a portion corresponding to the folded portion in consideration of the folded portion of the display device to be completed later. That is, when the display device to be completed later is folded around the folding axis F, the strength film 2 is attached only to a portion corresponding to the second section B, which is a flat portion that is not folded, and the first section, which is a bent portion ( In a place corresponding to A), a space is created without attaching the strength film (2).

다음으로 도 8과 같이 액상 점착제층(3)을 강점 필름(2)의 공간에 형성한다. 점착제층(3)은 잉크젯(Inkjet) 공정으로 형성될 수 있다. 주입기(50)를 강점 필름(2)의 공간 부분에 맞게 정렬하고, 액상 점착제를 주입기(50)를 통해 공간에 주입하여 형성할 수 있다. 본 실시예에서는 잉크젯(Inkjet) 공정을 예로 들어 설명하였으나, 그 밖에 슬릿 코팅(Slit Coating) 방법 등이 사용될 수 있으며, 액체를 주입할 수 있는 방법이라면 모두 사용될 수 있다. 점착력은 점착제층(3)에 비하여 약점 필름(1)이 크며, 약점 필름(1)에 비하여 강점 필름(2)이 크다.Next, as shown in FIG. 8, a liquid adhesive layer 3 is formed in the space of the strength film 2. The pressure-sensitive adhesive layer 3 may be formed by an inkjet process. It may be formed by aligning the injector 50 to fit the space portion of the strength film 2 and injecting the liquid adhesive into the space through the injector 50 . In this embodiment, an inkjet process has been described as an example, but other methods such as slit coating may be used, and any method capable of injecting a liquid may be used. The adhesive strength is greater in the weak film (1) than in the pressure-sensitive adhesive layer (3), and greater in the strength film (2) than in the weak film (1).

다음, 도 9와 같이 강점 필름(2) 및 점착제층(3)를 사이에 두고 약점 필름(1)과 마주보도록 이형 필름(4)을 부착한다. 이형 필름(4)은 점착제층(3) 및 강점 필름(2)의 오염 및 외부 접촉을 방지하기 위한 보호지로서, 하부 보호 필름(10)이 표시 패널(100)의 아래에 부착되기 전에 제거되어 점착제층(3) 및 강점 필름(2)이 TFT기판(110) 아래에 용이하게 부착되게 한다. 이형 필름(4)의 내측면에 실리콘을 0.1㎛ 내지 2㎛의 두께로 그라비아(Gravure) 코팅 방법을 이용하여 코팅하여 이형 필름(4)의 탈거 공정을 용이하게 할 수 있다. 이형 필름(4) 부착 후 UV 또는 열을 이용하여 도포된 점착제층(3)을 경화시킨다.Next, as shown in FIG. 9 , the release film 4 is attached so as to face the weak film 1 with the strength film 2 and the pressure-sensitive adhesive layer 3 interposed therebetween. The release film 4 is a protective paper for preventing contamination and external contact of the adhesive layer 3 and the strength film 2, and is removed before the lower protective film 10 is attached to the lower portion of the display panel 100 to prevent the adhesive Layer (3) and strong film (2) are easily deposited under the TFT substrate (110). A process of removing the release film 4 may be facilitated by coating silicon on the inner surface of the release film 4 to a thickness of 0.1 μm to 2 μm using a gravure coating method. After the release film 4 is attached, the applied pressure-sensitive adhesive layer 3 is cured using UV or heat.

다음으로, 도 10과 같이 약점 필름(1), TFT기판(110), 유기 발광 소자(300), 박막 봉지층(210) 및 상부 보호 필름(5) 차례대로 적층한 마더 글라스(M)를 준비한다. 마더 글라스(M)는 복수의 패널(P) 단위를 포함한다. 약점 필름(1)은 아크릴(Acryl) 계열에 치환기가 붙은 약점착 필름일 수 있으며, 점착력은 1 gf/inch 이상에서 5 gf/inch 이하일 수 있다.Next, as shown in FIG. 10, a mother glass (M) in which a weak film (1), a TFT substrate (110), an organic light emitting element (300), a thin film encapsulation layer (210), and an upper protective film (5) are sequentially laminated is prepared. do. The mother glass M includes a plurality of panel P units. The weak film 1 may be a weak adhesive film having an acrylic substituent attached thereto, and may have an adhesive strength of 1 gf/inch or more to 5 gf/inch or less.

다음, 도 11과 같이 하나의 패널(P) 단위로 약점 필름(1)을 제거하고, 도 9의 하부 보호 필름(10)에서 이형 필름(4)를 탈거한 후 도 11의 약점 필름(1)을 제거한 자리에 부착한다. 이때, 이형 필름(4)를 탈거한 하부 보호 필름의 폴딩 축(F)과 도 11의 패널(P)의 폴딩 축(F) 거의 일치하도록 도 12와 같이 부착한다. TFT기판(110) 하부에 강점 필름(2) 및 점착제층(3)이 오고, 그 하부에 약점 필름(1)이 오도록 부착한다. 약점 필름(1) 제거와 하부 보호 필름(10)의 부착을 패널(P)단위로 하는 이유는 패널(P)과 하부 보호 필름(10)의 폴딩 축(F)의 얼라인을 용이하게 하기 위함이다. 그러나, 패널(P) 단위가 아닌 마더 글라스(M)단위로 공정을 진행하여도 가능하다.Next, as shown in FIG. 11, the weak point film 1 is removed in units of one panel (P), and after removing the release film 4 from the lower protective film 10 of FIG. 9, the weak point film 1 of FIG. 11 is attached to the place where it was removed. At this time, it is attached as shown in FIG. 12 so that the folding axis (F) of the lower protective film from which the release film 4 is removed and the folding axis (F) of the panel (P) of FIG. 11 are substantially coincident. It is attached so that the strength film 2 and the pressure-sensitive adhesive layer 3 come to the bottom of the TFT substrate 110 and the weak point film 1 comes to the bottom. The reason why the weak film 1 is removed and the lower protective film 10 is attached on a panel P basis is to facilitate alignment of the folding axis F of the panel P and the lower protective film 10. to be. However, it is possible to perform the process in units of mother glass (M) instead of unit of panel (P).

다음으로 도 13과 같이 강점 필름(2) 하부의 약점 필름(1)을 제거 한다. 점착제층(3)의 점착력은 약점 필름(1)보다 약하므로, 약점 필름(1)을 제거할 때 같이 제거된다. 상술한 바와 같이 점착제층이 강점 필름(2)의 공간 사이에 위치하다 제거되는 경우 공정 중에 강점 필름(2)의 공간에 기포가 발생하는 것을 방지할 수 있다.Next, as shown in FIG. 13, the weak film 1 under the strong film 2 is removed. Since the adhesive force of the pressure-sensitive adhesive layer 3 is weaker than that of the weak film 1, it is removed when the weak film 1 is removed. As described above, when the pressure-sensitive adhesive layer is located between the spaces of the strength film 2 and removed, it is possible to prevent bubbles from being generated in the space of the strength film 2 during the process.

도 14는 약점 필름(1)과 강점 필름(2) 사이에 있던 점착제층(3)이 함께 제거된 모습이다. 약점 필름(1)과 점착제층(3)을 제거 후 마더 글라스(M)를 패널(P)단위로 자르면 도 1과 같은 표시 장치(1000)가 완성된다.14 shows the adhesive layer 3 between the weak film 1 and the strong film 2 removed together. After removing the weak point film 1 and the adhesive layer 3, the display device 1000 as shown in FIG. 1 is completed by cutting the mother glass M into panels P units.

이하에서, 도 9를 참조하여 본 발명의 일 실시예에 따른 표시 장치용 보호 필름에 대하여 설명한다. 앞서 설명한 실시예와 동일한 구성에 대한 설명은 생략한다. 도 9는 본 발명의 일 실시예에 따른 표시 장치용 보호 필름의 단면도이다.Hereinafter, a protective film for a display device according to an exemplary embodiment of the present invention will be described with reference to FIG. 9 . A description of the same configuration as that of the previously described embodiment will be omitted. 9 is a cross-sectional view of a protective film for a display device according to an exemplary embodiment.

표시 장치용 하부 보호 필름(10)은 약점 필름(1), 강점 필름(2), 점착제층(3) 및 이형 필름(4)을 포함한다.The lower protective film 10 for a display device includes a weak film 1 , a strong film 2 , an adhesive layer 3 and a release film 4 .

약점 필름(1)은 아크릴(Acryl) 계열에 치환기가 붙은 약점착 필름일 수 있으며, 점착력은 1 gf/inch 이상에서 5 gf/inch 이하일 수 있다.The weak film 1 may be a weak adhesive film having an acrylic substituent attached thereto, and may have an adhesive strength of 1 gf/inch or more to 5 gf/inch or less.

약점 필름(1) 일면에는 강점 필름(2)이 위치한다. 강점 필름(2)은 추후 하부 보호 필름(10)을 부착할 표시 장치가 접히는 부분에는 위치하지 않는다. 강점 필름(2)은 제2 구간(B)에 대응하여 위치하며 제1 구간(A)에서는 위치하지 않는다. 즉, 강점 필름(2)은 추후 하부 보호 필름(10)을 부착할 표시 장치가 폴딩 축(F)을 축으로 접힐 때 접히지 않고 편평한 부분인 제2 구간(B)과 대응하는 곳에 위치하고, 구부러지는 부분인 제1 구간(A)과 대응하는 곳에서는 위치하지 않는다. 강점 필름(2)은 추후 표시 장치가 접히는 부분에 해당하는 제1 구간(A)에 의해 복수의 영역(2a, 2b, 2c)으로 구분된다. 강점 필름(2)은 폴딩 축(F)을 중심으로 좌우로 같은 폭만큼 이격되어 위치할 수 있다. 즉, 제1 영역(2a) 및 제2 영역(2b)은 폴딩 축(F)을 중심으로 좌우로 대칭인 위치에 위치할 수 있으며, 제2 영역(2b) 및 제3 영역(2c)도 폴딩 축(F)을 중심으로 좌우로 대칭인 위치에 위치할 수 있다. 폴딩 축(F)은 강점 필름(2)을 지나지 않는다. 강점 필름(2)은 표시 장치(1000)가 접히는 모양에 따라 다양한 형태의 복수의 영역을 포함할 수 있다.On one side of the weak film 1, the strong film 2 is located. The strong film 2 is not located at a folded portion of the display device to which the lower protective film 10 will be attached later. The strength film 2 is positioned corresponding to the second section (B) and is not positioned in the first section (A). That is, the strength film 2 is located in a position corresponding to the second section B, which is a flat portion that is not folded when the display device to which the lower protective film 10 will be attached later is folded along the folding axis F, and is not bent. It is not located in a place corresponding to the first section (A), which is a part. The strength film 2 is divided into a plurality of areas 2a, 2b, and 2c by a first section A corresponding to a portion where the display device is later folded. The strength film 2 may be spaced apart from each other by the same width from side to side around the folding axis F. That is, the first region 2a and the second region 2b may be positioned symmetrically left and right about the folding axis F, and the second region 2b and the third region 2c may also be folded. It may be located in a symmetrical position left and right about the axis (F). The folding axis (F) does not pass through the strength film (2). The strength film 2 may include a plurality of regions of various shapes according to the shape in which the display device 1000 is folded.

점착제층(3)이 강점 필름(2)의 공간에 위치한다. 점착력은 점착제층(3)에 비하여 약점 필름(1)이 크며, 약점 필름(1)에 비하여 강점 필름(2)이 크다.An adhesive layer (3) is located in the space of the strength film (2). The adhesive strength is greater in the weak film (1) than in the pressure-sensitive adhesive layer (3), and greater in the strength film (2) than in the weak film (1).

강점 필름(2) 및 점착제층(3)을 사이에 두고 약점 필름(1)과 마주보도록 이형 필름(4)이 위치한다. 이형 필름(4)의 내측 면에는 실리콘이 0.1㎛ 내지 2㎛의 두께로 코팅되어 있을 수 있다.The release film 4 is positioned to face the weak film 1 with the strong film 2 and the pressure-sensitive adhesive layer 3 interposed therebetween. The inner surface of the release film 4 may be coated with silicon to a thickness of 0.1 μm to 2 μm.

상기와 같은 하부 보호 필름(10)은 표시 장치에 부착되어 표시 장치의 외부와의 직접적인 물리적 접촉을 방지하고 표시 장치의 물리적 손상을 방지할 수 있다.The lower protective film 10 as described above may be attached to the display device to prevent direct physical contact with the outside of the display device and physical damage to the display device.

이하에서, 도 15 및 도 16을 참조하여 본 발명의 일 실시예에 따른 표시 장치용 보호 필름을 설명한다. 앞서 설명한 실시예와 동일한 구성에 대한 설명은 생략한다. 도 15는 본 발명의 일 실시예에 따른 표시 장치의 단면도이다. 도 16은 본 발명의 일 실시예에 따른 표시 장치를 구부린 형태를 전체적으로 나타낸 개략도이다.Hereinafter, a protective film for a display device according to an exemplary embodiment of the present invention will be described with reference to FIGS. 15 and 16 . A description of the same configuration as that of the previously described embodiment will be omitted. 15 is a cross-sectional view of a display device according to an exemplary embodiment. 16 is a schematic diagram showing a bent shape of a display device according to an exemplary embodiment of the present invention as a whole.

표시 장치(1000)는 폴딩 축(F)을 축으로 하여 접힐 수 있다. 표시 장치(1000)는 표시 장치(1000)를 도 15 및 도 16에서와 같이 2분하는 두 개의 지점에서 두 개의 폴딩 축(F)을 축으로 하여 접힐 수 있다. 표시 장치(1000)를 도 12의 폴딩 축(F)을 기준으로 접으면 도 16과 같은 형태가 된다.The display device 1000 may be folded around the folding axis F as an axis. The display device 1000 may be folded using two folding axes F as axes at two points dividing the display device 1000 into two parts as shown in FIGS. 15 and 16 . When the display device 1000 is folded based on the folding axis F of FIG. 12 , the shape shown in FIG. 16 is obtained.

제1 구간(A')은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 접혀 구부러지는 부분이며, 도 16과 같이 표시 장치(1000)가 접히는 부분을 따라 표시 장치(1000)를 가로질러 뻗어있다. 제2 구간(B)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 접히지 않고 편평한 부분이다. 제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 곡률을 갖는 부분일 수 있으며, 제2 구간(B)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 곡률을 갖지 않는 부분일 수 있다. 또는, 제1 구간(A)은 표시 장치(1000)가 폴딩 축(F)을 축으로 접힐 때 제2 구간(B)에 비해 곡률이 큰 부분일 수 있다. 제1 구간(A)의 폭은 표시 장치(1000)가 접히는 각도에 따라 달라질 수 있다. 표시 장치(1000)가 더 많이 접힐수록 제1 구간(A)의 폭이 더 넓게 형성될 수 있다. 표시 장치(1000)가 더 많이 접힐수록 표시 패널(100)이 표시 패널(100) 하부의 필름을 누르는 힘이 더 커지고 힘을 받는 영역이 더 넓어지기 때문이다. 따라서 표시 장치(1000)가 더 많이 접힐수록 제1 구간(A)의 폭을 더 넓게 형성하여 필름의 탈락 및 변형을 더 효과적으로 방지할 수 있다. 도 16 보다 표시 장치(1000)가 더 많이 접히는 도 3의 실시예와 비교할 경우, 도 3의 실시예에서 제1 구간의 폭이 더 넓다.The first section A' is a portion that is bent when the display device 1000 is folded around the folding axis F, and the display device 1000 is formed along the folded portion as shown in FIG. 16 . stretched across The second section B is a flat portion that is not folded when the display device 1000 is folded along the folding axis F. The first section A may have a curvature when the display device 1000 is folded around the folding axis F, and the second section B may have a curvature when the display device 1000 is folded around the folding axis F. It may be a part that does not have curvature when folded axially. Alternatively, the first section A may have a greater curvature than the second section B when the display device 1000 is folded along the folding axis F. The width of the first section A may vary according to the angle at which the display device 1000 is folded. As the display device 1000 is more folded, the first section A may have a wider width. This is because the more the display device 1000 is folded, the greater the force exerted by the display panel 100 pressing the film under the display panel 100 and the wider the region receiving the force. Therefore, the more the display device 1000 is folded, the wider the width of the first section A may be, thereby preventing the film from falling off and being deformed more effectively. Compared to the embodiment of FIG. 3 in which the display device 1000 is folded more than that of FIG. 16 , the width of the first section is wider in the embodiment of FIG. 3 .

강점 필름(2)은 표시 패널(100) 아래에 부착되어 있으며, 강점 필름(2)은 제2 구간(B)에 대응하여 위치하며 제1 구간(A)에서는 위치하지 않는다. 강점 필름(2)은 표시 장치(1000)가 접히는 부분에 해당하는 제1 구간(A)에 의해 복수의 영역(2a, 2b)으로 구분된다. 강점 필름(2) 역시 표시 장치(1000)가 더 많이 접힐수록 강점 필름(2)의 복수의 영역(2a, 2b) 간의 폭이 더 넓게 형성될 수 있다. 표시 장치(1000)가 더 많이 접힐수록 표시 패널(100)이 표시 패널(100) 하부의 필름을 누르는 힘이 더 커지고 힘을 받는 영역이 더 넓어지므로 강점 필름(2)의 공간의 폭을 더 넓게 형성하여 필름의 탈락 및 변형을 더 효과적으로 방지할 수 있다.The strength film 2 is attached below the display panel 100 , and the strength film 2 is located in the second section B and not in the first section A. The strength film 2 is divided into a plurality of regions 2a and 2b by a first section A corresponding to a portion where the display device 1000 is folded. In the strength film 2, as the display device 1000 is folded more, the width between the plurality of areas 2a and 2b of the strength film 2 may be wider. The more the display device 1000 is folded, the greater the force that the display panel 100 presses on the film below the display panel 100 and the wider the area receiving the force, so the width of the space of the strength film 2 becomes wider. Formation can more effectively prevent the film from falling off and deformation.

이상에서 본 발명의 실시예에 대하여 상세하게 설명하였지만 본 발명의 권리범위는 이에 한정되는 것은 아니고 다음의 청구범위에서 정의하고 있는 본 발명의 기본 개념을 이용한 당업자의 여러 변형 및 개량 형태 또한 본 발명의 권리범위에 속하는 것이다.Although the embodiments of the present invention have been described in detail above, the scope of the present invention is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concept of the present invention defined in the following claims are also included in the scope of the present invention. that fall within the scope of the right.

A: 제1 구간
B: 제2 구간
F: 폴딩 축
1: 약점 필름
2: 강점 필름
3: 점착제층
4: 이형 필름
5: 상부 보호 필름
100: 표시 패널
1000: 표시 장치
A: 1st section
B: Second section
F: folding axis
1: weak point film
2: strength film
3: adhesive layer
4: release film
5: upper protective film
100: display panel
1000: display device

Claims (17)

삭제delete 삭제delete 삭제delete 삭제delete 삭제delete 삭제delete 제1 구간 및 상기 제1 구간에 의해 구분되는 제2 구간을 포함하는 약점 필름 일면에 상기 제2 구간에는 대응하여 위치하여 상기 제1 구간에 대응하여는 공간을 갖도록 강점 필름을 부착하는 단계,
상기 공간에 액상 점착제층을 형성하는 단계,
상기 강점 필름 및 상기 액상 점착제층을 사이에 두고 상기 약점 필름과 마주보도록 이형 필름을 부착하는 단계 및
상기 액상 점착제층을 경화하는 단계를 포함하는 하부 보호 필름 형성 단계를 포함하며,
상기 하부 보호 필름 형성 단계를 거쳐 형성된 하부 보호 필름에서 상기 이형 필름을 제거하여 마더 글라스에 부착하는 단계,
상기 약점 필름과 함께 상기 액상 점착제층을 제거하는 단계를 포함하는 표시 장치의 제조 방법.
Attaching a strong film to one surface of a weak film including a first section and a second section divided by the first section to have a space corresponding to the first section by being positioned corresponding to the second section;
Forming a liquid adhesive layer in the space;
attaching a release film facing the weak point film with the strength film and the liquid adhesive layer interposed therebetween; and
And a lower protective film forming step comprising curing the liquid pressure-sensitive adhesive layer,
Removing the release film from the lower protective film formed through the lower protective film forming step and attaching it to the mother glass;
and removing the liquid adhesive layer together with the weak film.
제7항에서,
점착력은 상기 액상 점착제층에 비하여 상기 약점 필름이 크며, 상기 약점 필름에 비하여 상기 강점 필름이 큰, 표시 장치의 제조 방법.
In paragraph 7,
The adhesive strength of the weak film is greater than that of the liquid pressure-sensitive adhesive layer, and the strength film is greater than the weak film.
제8항에서,
상기 표시 장치는 폴딩 축을 축으로 상기 강점 필름이 바깥 면에 오도록 접힐 수 있게 형성되며,
상기 제1 구간은 상기 폴딩 축을 포함하여 상기 폴딩 축의 주변에 설정되는 표시 장치의 제조 방법.
In paragraph 8,
The display device is formed to be foldable around a folding axis so that the strength film faces an outer surface,
The first section includes the folding axis and is set around the folding axis.
제9항에서,
상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 구부러지는 부분이며, 상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 구부러지지 않고 편평한 부분인 표시 장치의 제조 방법.
In paragraph 9,
The first section is a portion that is bent when the display device is folded around the folding axis, and the second section is a flat portion that is not bent when the display device is folded around the folding axis.
제9항에서,
상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 곡률을 갖는 부분이며,
상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 곡률을 갖지 않는 부분인 표시 장치의 제조 방법.
In paragraph 9,
The first section is a portion having a curvature when the display device is folded around the folding axis;
The second section is a portion having no curvature when the display device is folded around the folding axis.
제9항에서,
상기 제1 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 외력을 받는 부분이며,
상기 제2 구간은 상기 표시 장치가 상기 폴딩 축을 축으로 접힐 때 외력을 받지 않는 부분인 표시 장치의 제조 방법.
In paragraph 9,
The first section is a portion that receives an external force when the display device is folded around the folding shaft;
The second section is a portion that does not receive an external force when the display device is folded around the folding shaft.
제10항에서,
상기 하부 보호 필름은 상기 마더 글라스에 패널 단위로 부착하는 표시 장치의 제조 방법.
In paragraph 10,
The method of manufacturing a display device in which the lower protective film is attached to the mother glass in a panel unit.
제1 구간 및 상기 제1 구간에 의해 구분되는 제2 구간을 포함하는 약점 필름,
상기 약점 필름 일면에 위치하며 상기 제2 구간에 대응하여 위치하는 강점 필름,
상기 강점 필름 사이의 상기 제1 구간에 대응하는 부분에 위치하는 액상 점착제층 및
상기 액상 점착제층 및 상기 강점 필름을 사이에 두고 상기 약점 필름과 마주보는 이형 필름을 포함하며,
점착력은 상기 액상 점착제층에 비하여 상기 약점 필름이 크며, 상기 약점 필름에 비하여 상기 강점 필름이 큰, 표시 장치용 보호 필름.
A weak film comprising a first section and a second section divided by the first section,
A strong film located on one side of the weak film and located in correspondence with the second section;
A liquid adhesive layer located in a portion corresponding to the first section between the strength films, and
A release film facing the weak point film with the liquid adhesive layer and the strength film interposed therebetween,
The adhesive strength of the weak film is greater than that of the liquid pressure-sensitive adhesive layer, and the strong film is greater than the weak film.
제14항에서,
상기 제1 구간은 상기 표시 장치용 보호 필름이 폴딩 축을 축으로 접힐 때 구부러지는 부분이며, 상기 제2 구간은 상기 표시 장치용 보호 필름이 상기 폴딩 축을 축으로 접힐 때 구부러지지 않고 편평한 부분인 표시 장치용 보호 필름.
In paragraph 14,
The first section is a portion that is bent when the protective film for the display device is folded around the folding axis, and the second section is a flat portion that is not bent when the protective film for the display device is folded around the folding axis. protective film.
제14항에서,
상기 제1 구간은 상기 표시 장치용 보호 필름이 폴딩 축을 축으로 접힐 때 곡률을 갖는 부분이며,
상기 제2 구간은 상기 표시 장치용 보호 필름이 상기 폴딩 축을 축으로 접힐 때 곡률을 갖지 않는 부분인 표시 장치용 보호 필름.
In paragraph 14,
The first section is a portion having a curvature when the protective film for the display device is folded around a folding axis,
The second section is a portion having no curvature when the protective film for a display device is folded around the folding axis.
제14항에서,
상기 제1 구간은 상기 표시 장치용 보호 필름이 폴딩 축을 축으로 접힐 때 외력을 받는 부분이며,
상기 제2 구간은 상기 표시 장치용 보호 필름이 상기 폴딩 축을 축으로 접힐 때 외력을 받지 않는 부분인 표시 장치용 보호 필름.

In paragraph 14,
The first section is a portion that receives an external force when the protective film for the display device is folded around a folding axis,
The second section is a portion that does not receive an external force when the protective film for a display device is folded around the folding axis.

KR1020160030513A 2016-03-14 2016-03-14 Protection film for display device, display device and manufacturing method thereof KR102471020B1 (en)