JPS5795405A - Bending method for surface-hardened synthetic resin sheet - Google Patents

Bending method for surface-hardened synthetic resin sheet

Info

Publication number
JPS5795405A
JPS5795405A JP17089180A JP17089180A JPS5795405A JP S5795405 A JPS5795405 A JP S5795405A JP 17089180 A JP17089180 A JP 17089180A JP 17089180 A JP17089180 A JP 17089180A JP S5795405 A JPS5795405 A JP S5795405A
Authority
JP
Japan
Prior art keywords
synthetic resin
resin sheet
hardened
bending method
hardened synthetic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP17089180A
Other languages
Japanese (ja)
Other versions
JPS5858210B2 (en
Inventor
Tsugio Hirota
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHINSHI KOGYO KK
Original Assignee
SHINSHI KOGYO KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHINSHI KOGYO KK filed Critical SHINSHI KOGYO KK
Priority to JP17089180A priority Critical patent/JPS5858210B2/en
Publication of JPS5795405A publication Critical patent/JPS5795405A/en
Publication of JPS5858210B2 publication Critical patent/JPS5858210B2/en
Expired legal-status Critical Current

Abstract

PURPOSE: To bend a surface-hardened synthetic resin sheet without formation of breakage or cracks in a hardened layer, by shaving off the surface-hardened layer from a part to be bent, and then bending the sheet.
CONSTITUTION: A proper shaving-off means is applied to the part 3, to be bent, of a surface-hardened synthetic resin sheet A prepared by forming surface-hardened layers 2 on the two surfaces of a synthetic resin sheet 1, to expose the surface 1a of the synthetic resin sheet. The surface 1a is heated and softened by a heater 4, and then the sheet is bent.
COPYRIGHT: (C)1982,JPO&Japio
JP17089180A 1980-12-05 1980-12-05 Bending method for surface-hardened synthetic resin plates Expired JPS5858210B2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP17089180A JPS5858210B2 (en) 1980-12-05 1980-12-05 Bending method for surface-hardened synthetic resin plates

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP17089180A JPS5858210B2 (en) 1980-12-05 1980-12-05 Bending method for surface-hardened synthetic resin plates

Publications (2)

Publication Number Publication Date
JPS5795405A true JPS5795405A (en) 1982-06-14
JPS5858210B2 JPS5858210B2 (en) 1983-12-23

Family

ID=15913229

Family Applications (1)

Application Number Title Priority Date Filing Date
JP17089180A Expired JPS5858210B2 (en) 1980-12-05 1980-12-05 Bending method for surface-hardened synthetic resin plates

Country Status (1)

Country Link
JP (1) JPS5858210B2 (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2021053854A (en) * 2019-09-27 2021-04-08 株式会社丸三金属 Molding method of adherend film

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS60181518U (en) * 1984-05-10 1985-12-02 バブコツク日立株式会社 Fluidized bed combustion equipment

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2021053854A (en) * 2019-09-27 2021-04-08 株式会社丸三金属 Molding method of adherend film

Also Published As

Publication number Publication date
JPS5858210B2 (en) 1983-12-23

Similar Documents

Publication Publication Date Title
IT7926596A0 (en) PROCESS FOR THE PRODUCTION OF ADHESIVE-REPELLENT COATINGS ON FLAT MATERIAL, IN SHEET OR TAPE FORM.
DE3163367D1 (en) Laminating process
DE3381609D1 (en) SURFACE WAVE FILTER, AND METHOD FOR PRODUCING A DAMPING LAYER FOR SURFACE WAVE FILTER.
DE3165542D1 (en) Laminating process
DE69006870D1 (en) Device for covering a flat surface with a layer of uniform thickness.
JPS5795405A (en) Bending method for surface-hardened synthetic resin sheet
PH15917A (en) Resinous polymer sheet materials having selective,surface decorative effects and method of making the same
IT7922042A0 (en) METHOD FOR FORMING UNIVERSAL THIN LAYER RESISTORS.
CA2219588A1 (en) Method and apparatus for applying a decoration to an article using heat
JPS5567549A (en) Production of curved laminated glass with joined surface printed
JPS5286429A (en) Method of application of water-dispersed resin coating
JPS56129121A (en) Manufacture of decorative material
JPS5746848A (en) Coating method
JPS5269270A (en) Coating method of photoresist
JPS5376747A (en) Forming method of insulation film
JPS5418275A (en) Forming method of ohmic contact
JPS5551523A (en) Preparation of dressed material
ATE5238T1 (en) PROCESS FOR MANUFACTURE OF HEAT EXCHANGE ELEMENTS AND DEVICE FOR CARRYING OUT THE PROCESS.
ATA210481A (en) METHOD FOR CONTINUOUSLY ONE-SIDED COATING A BLANK METAL STRIP WITH MOLTEN METAL, AND DEVICE FOR CARRYING OUT THE METHOD
JPS5327099A (en) Automated ticket
JPS5691871A (en) Working of coated part of steel pipe coated with plastic layer
JPS5424284A (en) Improving method for film with ion exchangeability
JPS57144724A (en) Manufacture of corrugated sheet or flat sheet
JPS5432549A (en) Method of smoothing coated film