GB2394479B - Process for applying a coating to a surface - Google Patents
Process for applying a coating to a surfaceInfo
- Publication number
- GB2394479B GB2394479B GB0324367A GB0324367A GB2394479B GB 2394479 B GB2394479 B GB 2394479B GB 0324367 A GB0324367 A GB 0324367A GB 0324367 A GB0324367 A GB 0324367A GB 2394479 B GB2394479 B GB 2394479B
- Authority
- GB
- United Kingdom
- Prior art keywords
- coating
- applying
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C24/00—Coating starting from inorganic powder
- C23C24/02—Coating starting from inorganic powder by application of pressure only
- C23C24/04—Impact or kinetic deposition of particles
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
- Application Of Or Painting With Fluid Materials (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US41940302P | 2002-10-18 | 2002-10-18 | |
US67168303A | 2003-09-29 | 2003-09-29 |
Publications (3)
Publication Number | Publication Date |
---|---|
GB0324367D0 GB0324367D0 (en) | 2003-11-19 |
GB2394479A GB2394479A (en) | 2004-04-28 |
GB2394479B true GB2394479B (en) | 2005-05-25 |
Family
ID=29587223
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
GB0324367A Expired - Fee Related GB2394479B (en) | 2002-10-18 | 2003-10-17 | Process for applying a coating to a surface |
Country Status (6)
Country | Link |
---|---|
JP (1) | JP2004137602A (en) |
CA (1) | CA2444917A1 (en) |
DE (1) | DE10346836C5 (en) |
FR (1) | FR2845937B1 (en) |
GB (1) | GB2394479B (en) |
RU (1) | RU2266978C2 (en) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US8113413B2 (en) | 2006-12-13 | 2012-02-14 | H.C. Starck, Inc. | Protective metal-clad structures |
US8491959B2 (en) | 2007-05-04 | 2013-07-23 | H.C. Starck Inc. | Methods of rejuvenating sputtering targets |
US8514664B2 (en) | 2010-04-16 | 2013-08-20 | Pgs Geophysical As | System and method for gathering marine geophysical data |
US9116253B2 (en) | 2011-01-11 | 2015-08-25 | Pgs Geophysical As | System and method for using biocide coating to prevent marine growth on geophysical equipment |
US9244185B2 (en) | 2009-05-01 | 2016-01-26 | Pgs Geophysical As | System and method for towed marine geophysical equipment |
US9465127B2 (en) | 2013-05-07 | 2016-10-11 | Pgs Geophysical As | Disposable antifouling covers for geophysical survey equipment |
Families Citing this family (30)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101052746B (en) * | 2004-09-25 | 2010-04-14 | Abb技术股份公司 | Corresponding shield parts for manufacturing fire-proof and anti-corrosion coating and for vacuum switch-box |
US7632592B2 (en) * | 2004-11-01 | 2009-12-15 | Gm Global Technology Operations, Inc. | Method of fabricating corrosion-resistant bipolar plate |
US7553385B2 (en) * | 2004-11-23 | 2009-06-30 | United Technologies Corporation | Cold gas dynamic spraying of high strength copper |
US20060121183A1 (en) * | 2004-12-03 | 2006-06-08 | United Technologies Corporation | Superalloy repair using cold spray |
US20060134320A1 (en) * | 2004-12-21 | 2006-06-22 | United Technologies Corporation | Structural repair using cold sprayed aluminum materials |
US20060134321A1 (en) * | 2004-12-22 | 2006-06-22 | United Technologies Corporation | Blade platform restoration using cold spray |
US20060216428A1 (en) * | 2005-03-23 | 2006-09-28 | United Technologies Corporation | Applying bond coat to engine components using cold spray |
RU2418886C2 (en) | 2005-05-05 | 2011-05-20 | Х.К. Штарк Гмбх | Procedure for application of coating for fabrication or restoration of sputtering targets and anodes of x-ray tubes |
BRPI0611539B1 (en) | 2005-05-05 | 2017-04-04 | Starck H C Gmbh | method of applying a coating to a surface, cold spray coat and coated object |
US20080078268A1 (en) | 2006-10-03 | 2008-04-03 | H.C. Starck Inc. | Process for preparing metal powders having low oxygen content, powders so-produced and uses thereof |
US8192792B2 (en) * | 2006-10-27 | 2012-06-05 | United Technologies Corporation | Cold sprayed porous metal seals |
US20080099538A1 (en) | 2006-10-27 | 2008-05-01 | United Technologies Corporation & Pratt & Whitney Canada Corp. | Braze pre-placement using cold spray deposition |
JP2008127676A (en) * | 2006-11-24 | 2008-06-05 | Toyohashi Univ Of Technology | Formation method of metallic film |
US7820238B2 (en) * | 2006-12-20 | 2010-10-26 | United Technologies Corporation | Cold sprayed metal matrix composites |
FR2920440B1 (en) * | 2007-08-31 | 2010-11-05 | Commissariat Energie Atomique | METHOD OF TREATING ANTI-CORROSION OF A PIECE BY DEPOSITION OF A ZIRCONIUM LAYER AND / OR ZIRCONIUM ALLOY |
JP5228149B2 (en) * | 2007-11-15 | 2013-07-03 | 国立大学法人豊橋技術科学大学 | Nozzle for film formation, film formation method, and film formation member |
JP2010047825A (en) * | 2008-08-25 | 2010-03-04 | Mitsubishi Heavy Ind Ltd | Metal film forming method and aerospace structural member |
US8246903B2 (en) | 2008-09-09 | 2012-08-21 | H.C. Starck Inc. | Dynamic dehydriding of refractory metal powders |
US8043655B2 (en) | 2008-10-06 | 2011-10-25 | H.C. Starck, Inc. | Low-energy method of manufacturing bulk metallic structures with submicron grain sizes |
US20110174207A1 (en) * | 2010-01-21 | 2011-07-21 | Pgs Geophysical As | System and method for using copper coating to prevent marine growth on towed geophysical equipment |
FR2957937B1 (en) * | 2010-03-29 | 2012-04-27 | Air Liquide | PROCESS FOR PRODUCING A STAINLESS STEEL COATING ON A COPPER MATRIX |
US9120183B2 (en) | 2011-09-29 | 2015-09-01 | H.C. Starck Inc. | Methods of manufacturing large-area sputtering targets |
US8448839B1 (en) | 2012-03-23 | 2013-05-28 | General Electric Company | Brazing method using BCuP and BAg braze alloys |
DE102012023210A1 (en) | 2012-11-28 | 2014-05-28 | Wieland-Werke Ag | Copper strip for the production of printed circuit boards |
CZ306441B6 (en) * | 2014-12-05 | 2017-01-25 | Safina, A.S. | A method of manufacturing a metal body with a homogeneous, fine-grained structure using the cold spray technology; the metal body thus produced; and a method of repairing the dedusted metal bodies used |
WO2016093403A1 (en) * | 2014-12-11 | 2016-06-16 | 주식회사 탑피온 | Screw pneumatic copper powder application apparatus |
CN109701854A (en) * | 2019-01-29 | 2019-05-03 | 晟光科技股份有限公司 | One kind being used for the cold spray painting copper coating technique in aluminium alloy mobile phone shell surface |
CN110129613A (en) * | 2019-05-30 | 2019-08-16 | 深圳市金中瑞通讯技术有限公司 | A kind of compound copper powder and preparation method thereof, spraying method and purposes |
CN110093052A (en) * | 2019-05-30 | 2019-08-06 | 深圳市金中瑞通讯技术有限公司 | A kind of compound aluminium powder and preparation method thereof, spraying method and purposes |
CN110093051A (en) * | 2019-05-30 | 2019-08-06 | 深圳市金中瑞通讯技术有限公司 | A kind of compound zinc powder and preparation method thereof, spraying method and purposes |
Citations (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01263281A (en) * | 1988-04-15 | 1989-10-19 | Sumitomo Metal Ind Ltd | Formation of coating film of superplastic alloy |
US5302414A (en) * | 1990-05-19 | 1994-04-12 | Anatoly Nikiforovich Papyrin | Gas-dynamic spraying method for applying a coating |
GB2367073A (en) * | 2000-07-25 | 2002-03-27 | Ford Global Tech Inc | Free-form tooling; rapid prototyping |
WO2002034967A1 (en) * | 2000-10-27 | 2002-05-02 | Siemens Westinghouse Power Corporation | Abradable coating applied with cold spray technique |
WO2002061177A2 (en) * | 2001-01-30 | 2002-08-08 | Siemens Westinghouse Power Corporation | Thermal barrier coating applied with cold spray technique |
US6464933B1 (en) * | 2000-06-29 | 2002-10-15 | Ford Global Technologies, Inc. | Forming metal foam structures |
WO2003056064A1 (en) * | 2001-12-21 | 2003-07-10 | Rosti A/S | Applying metallic coatings to plastics materials |
EP1383610A1 (en) * | 2001-04-24 | 2004-01-28 | Innovative Technology, Inc. | An apparatus and process for solid-state deposition and consolidation of high velocity powder particles using thermal plastic deformation |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6134785A (en) * | 1992-05-18 | 2000-10-24 | The Boeing Company | Method of fabricating an article of manufacture such as a heat exchanger |
DE19915082C1 (en) * | 1999-04-01 | 2000-07-13 | Daimler Chrysler Ag | Regeneratively cooled rocket motor nozzle comprizes spiraled coolant-flowed tubing subsequently sprayed with loadbearing and fixing layers once exterior mandrel former is stripped off. |
US20020073982A1 (en) * | 2000-12-16 | 2002-06-20 | Shaikh Furqan Zafar | Gas-dynamic cold spray lining for aluminum engine block cylinders |
-
2003
- 2003-10-15 CA CA 2444917 patent/CA2444917A1/en not_active Abandoned
- 2003-10-17 GB GB0324367A patent/GB2394479B/en not_active Expired - Fee Related
- 2003-10-17 FR FR0312173A patent/FR2845937B1/en not_active Expired - Fee Related
- 2003-10-17 DE DE2003146836 patent/DE10346836C5/en not_active Expired - Fee Related
- 2003-10-20 RU RU2003130773/02A patent/RU2266978C2/en not_active IP Right Cessation
- 2003-10-20 JP JP2003359667A patent/JP2004137602A/en not_active Ceased
Patent Citations (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH01263281A (en) * | 1988-04-15 | 1989-10-19 | Sumitomo Metal Ind Ltd | Formation of coating film of superplastic alloy |
US5302414A (en) * | 1990-05-19 | 1994-04-12 | Anatoly Nikiforovich Papyrin | Gas-dynamic spraying method for applying a coating |
US5302414B1 (en) * | 1990-05-19 | 1997-02-25 | Anatoly N Papyrin | Gas-dynamic spraying method for applying a coating |
US6464933B1 (en) * | 2000-06-29 | 2002-10-15 | Ford Global Technologies, Inc. | Forming metal foam structures |
GB2367073A (en) * | 2000-07-25 | 2002-03-27 | Ford Global Tech Inc | Free-form tooling; rapid prototyping |
WO2002034967A1 (en) * | 2000-10-27 | 2002-05-02 | Siemens Westinghouse Power Corporation | Abradable coating applied with cold spray technique |
WO2002061177A2 (en) * | 2001-01-30 | 2002-08-08 | Siemens Westinghouse Power Corporation | Thermal barrier coating applied with cold spray technique |
EP1383610A1 (en) * | 2001-04-24 | 2004-01-28 | Innovative Technology, Inc. | An apparatus and process for solid-state deposition and consolidation of high velocity powder particles using thermal plastic deformation |
WO2003056064A1 (en) * | 2001-12-21 | 2003-07-10 | Rosti A/S | Applying metallic coatings to plastics materials |
Cited By (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US8113413B2 (en) | 2006-12-13 | 2012-02-14 | H.C. Starck, Inc. | Protective metal-clad structures |
US8448840B2 (en) | 2006-12-13 | 2013-05-28 | H.C. Starck Inc. | Methods of joining metallic protective layers |
US8777090B2 (en) | 2006-12-13 | 2014-07-15 | H.C. Starck Inc. | Methods of joining metallic protective layers |
US9095932B2 (en) | 2006-12-13 | 2015-08-04 | H.C. Starck Inc. | Methods of joining metallic protective layers |
US8491959B2 (en) | 2007-05-04 | 2013-07-23 | H.C. Starck Inc. | Methods of rejuvenating sputtering targets |
US8883250B2 (en) | 2007-05-04 | 2014-11-11 | H.C. Starck Inc. | Methods of rejuvenating sputtering targets |
US9244185B2 (en) | 2009-05-01 | 2016-01-26 | Pgs Geophysical As | System and method for towed marine geophysical equipment |
US8514664B2 (en) | 2010-04-16 | 2013-08-20 | Pgs Geophysical As | System and method for gathering marine geophysical data |
US9116253B2 (en) | 2011-01-11 | 2015-08-25 | Pgs Geophysical As | System and method for using biocide coating to prevent marine growth on geophysical equipment |
US9465127B2 (en) | 2013-05-07 | 2016-10-11 | Pgs Geophysical As | Disposable antifouling covers for geophysical survey equipment |
Also Published As
Publication number | Publication date |
---|---|
FR2845937B1 (en) | 2006-12-22 |
CA2444917A1 (en) | 2004-04-18 |
RU2266978C2 (en) | 2005-12-27 |
JP2004137602A (en) | 2004-05-13 |
GB2394479A (en) | 2004-04-28 |
DE10346836B4 (en) | 2007-06-06 |
DE10346836A1 (en) | 2004-05-06 |
GB0324367D0 (en) | 2003-11-19 |
RU2003130773A (en) | 2005-04-10 |
DE10346836C5 (en) | 2009-12-10 |
FR2845937A1 (en) | 2004-04-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB2394479B (en) | Process for applying a coating to a surface | |
AU2003286547A8 (en) | Method and apparatus for applying designs to a substrate | |
AU2003247709A8 (en) | Process for coating to obtain special surface effects | |
AU2001246414A1 (en) | Process for coating a surface | |
GB0423685D0 (en) | Improved method for coating a substrate | |
AU2003284940A8 (en) | Laminate and method used for applying a design to a substrate | |
AU2003213025A1 (en) | Methods of applying a coating to an optical surface | |
AU2003291811A8 (en) | Robotic paint/surface coating removal apparatus | |
EP1687135A4 (en) | Anti-reflective coating for a substrate | |
GB2379896B (en) | Process for coating a substrate | |
AU2002303706A1 (en) | Process for preparing chrome surface for coating | |
AU2002354987A1 (en) | Method for applying a self-cleaning coating to textile materials | |
AU2003218727A8 (en) | Method for applying a substance to a substrate | |
GB0002613D0 (en) | A method of applying a coating to a can | |
AU2003214495A8 (en) | Process for transferring a decorative cosmetic product on a basic cosmetic product | |
GB0219911D0 (en) | Process for the application of a bituminous coating | |
GB0212818D0 (en) | Apparatus for applying a finish to a texturable decorative coating | |
PL1685078T3 (en) | Method for applying a coating mass | |
AU2002328250A1 (en) | Method for application of a coating to a bread surface on a piece of bread | |
GB0227446D0 (en) | Improvements relating to a deposition process | |
GB2388846B (en) | Coating process | |
GB0326833D0 (en) | A method for applying a pattern to a glass panel | |
GB0330020D0 (en) | Method for coating a surface | |
GB2356376B (en) | Apparatus for applying a finish to a texturable decorative coating | |
AU2002350459A1 (en) | A process for treating a surface |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PCNP | Patent ceased through non-payment of renewal fee |
Effective date: 20161017 |