CN201234412Y - Plastic rubber case and mobile phone adopting the plastic rubber case - Google Patents

Plastic rubber case and mobile phone adopting the plastic rubber case Download PDF

Info

Publication number
CN201234412Y
CN201234412Y CNU200820095680XU CN200820095680U CN201234412Y CN 201234412 Y CN201234412 Y CN 201234412Y CN U200820095680X U CNU200820095680X U CN U200820095680XU CN 200820095680 U CN200820095680 U CN 200820095680U CN 201234412 Y CN201234412 Y CN 201234412Y
Authority
CN
China
Prior art keywords
plastic casing
film layer
adhesive layer
thickness
transparent film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CNU200820095680XU
Other languages
Chinese (zh)
Inventor
卜来来
付军
方焱
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BYD Co Ltd
Original Assignee
BYD Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BYD Co Ltd filed Critical BYD Co Ltd
Priority to CNU200820095680XU priority Critical patent/CN201234412Y/en
Application granted granted Critical
Publication of CN201234412Y publication Critical patent/CN201234412Y/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model provides a plastic casing and a mobile telephone adopting the plastic casing. The plastic casing comprises a substrate, and a transparent film layer positioned on the surface of the substrate. The plastic casing is characterized in that the plastic casing also comprises a metallic film layer, and the metallic film layer is positioned between the surface of the substrate and the transparent film layer. The metallic film layer is arranged on the surface of the substrate of the product adopting the structure, and the transparent film layer is arranged outside the metallic film layer for protection, so as to enable the product to be more wearable and the quality to be more reliable while processing the metallic tactile sensation and the metallic luster with high brightness, and improve the quality and the grade of the product.

Description

A kind of plastic casing and adopt the mobile phone of this plastic casing
Technical field
The utility model relates to a kind of plastic casing and adopts the mobile phone of this plastic casing.
Background technology
The housing of present electronic product normally adopts plastic cement products to make as mobile phone, computer, mp3 etc.In order to make shell obtain the appearance of high-quality pattern or color, normal in-mode inserts injection moulding (IML) technology that adopts is processed electronic product casing in the industry, this technology be by be printed with printing ink thin slice put into mould and carry out injection moulding, in injection moulding process, the plastic pellet of thin slice and fusing combines becomes finished product.The product characteristics that its technology makes is: the product substrate surface is coated with the transparent membrane of one deck sclerosis; the transparent membrane inner surface is printed with ink design layer; like this because printing ink has the film protection; can make and prevent that printing ink from being scratched; make the wear-resisting wiping of product, and the distinctness that can keep color for a long time fugitive color not.
Though the IML product quality is really up to the mark, form is attractive in appearance.But its pattern only limits to the color and luster of printing ink itself, and the loss of process transparent base, and the ink colors that transmits can not be vivid as primary colors.Aspect embodiment metallic luster, both the use metal ink can not embody vivid metal-like.
The utility model content
The purpose of this utility model is to overcome the relatively poor defective of plastic casing glossiness of the prior art, provide a kind of decorative effect more perfect plastic casing.
The utility model provides a kind of plastic casing, and this plastic casing comprises base material and the transparent film layer that is positioned on the described substrate surface, and this plastic casing also comprises metallic diaphragm, and this metallic diaphragm is between substrate surface and transparent film layer.
Further, this plastic casing also comprises the ink lay that is arranged between described transparent film layer and the metallic diaphragm.
Further, this plastic casing also comprises the adhesive layer that is arranged between metallic diaphragm and the substrate surface.
The utility model also provides a kind of phone housing, and this phone housing is made by above-mentioned plastic casing.
Plastic casing according to the utility model provides is provided with metallic diaphragm at substrate surface, and metallic diaphragm is provided with transparent film layer outward, makes this housing in the metallic luster with very strong metal-like and high light, more wear-resisting wiping, and quality is more reliable.Make the product that adopts this plastic casing promote the quality and the class of product.
Description of drawings
Fig. 1 is the schematic diagram of the utility model embodiment plastic casing.
Embodiment
The plastic casing that the utility model provides comprises base material and the transparent film layer that is positioned on the described housing substrate surface, and wherein, this housing also comprises metallic diaphragm, and this metallic diaphragm is between substrate surface and transparent film layer.
As shown in Figure 1, the plastic casing that provides according to present embodiment comprises housing base material 1, is positioned at the transparent film layer 6 on base material 1 surface, and the metallic diaphragm 4 between base material 1 surface and transparent film layer 6.
Between metallic diaphragm 4 and transparent film layer 6, ink lay 5 is set, in order to embody the pattern color of product.Protect metallic diaphragm 4 simultaneously for the adhesion that increases between metallic diaphragm 4 and the base material 1, between metallic diaphragm 4 and base material 1, be provided with adhesive layer.The present embodiment adhesive layer is preferably two-layer, comprises first adhesive layer 2 and second adhesive layer 3 that is positioned on first adhesive layer 2 on base material 1 surface, and described first adhesive layer is an adhesive phase, and second adhesive layer is the gloss oil layer.
Described housing base material can be various plastic rubber substrates, the for example common plastic material that electronic product adopted is as polyester, polycarbonate, acrylonitrile-butadiene-styrene (ABS) ABS, polymetylmethacrylate or at least two kinds composite material among them
Described transparent film layer 6 materials have many kinds, as polycarbonate, and polyethylene terephtalate, polymetylmethacrylate etc.This example is selected the sheet material of PC material for use, and the moulding of PC sheet material and processing are all better, and surface gloss, anti-wear performance are also better.The PC sheet material that this example is used is the DMX light facesheet of GE company.
Before transparent film layer 6 moulding, need earlier on the PC sheet material moulding printing ink layer 5, metallic diaphragm 4, second adhesive layer 3, first adhesive layer 2 successively.
Described printing ink layer 5 is selected printing ink high temperature resistant, that adhesive force good, flexibility good and softening point is high for use.What present embodiment used is the N2K series ink of company of German Baolong: printing ink is the semi-transparent yellow green printing ink of N2K series, and diluent is selected N2K097-003 for use, and addition is 15%; Curing agent is selected N2K005 for use, and addition is 3%; Used printing process is a screen painting: select 150~300 orders/cm coloured polyester silk screen for use, solvent-resisting light sensitive layer, printing machine are conventional presses, and printing process is known for those skilled in the art, no longer too much describe herein.The PC sheet material that has printed printing ink is put in the baking box with 80 ℃ of bakings 30 minutes, made the solvent evaporates in the printing ink complete, finish-drying.
Described metal level 4 can be the various metal levels that can be plated on the described housing base material, and for example nickel, chromium, tin, indium, indium stannum alloy, aluminium or stainless steel make housing of the present utility model have the texture of metal.The utility model embodiment states metal level 4 and is preferably tin, the formation method of this metal level can adopt the whole bag of tricks, the preferred method that adopts physical vapor deposition (PVD) in the utility model, the method of physical vapor deposition (PVD) comprises sputter coating, ion film plating, evaporation coating, preferably adopts the method for evaporation coating.The method of evaporation coating adopts conventional method to carry out, and for example uses to rise and wins stove formula evaporation equipment, and vacuum degree is 1-8 * 10-2Pa, and pre-thermal power is 10%-30% (accounting for the percentage of gross power), warm-up time 10-20s; Fritting power 25%-35% (accounting for the percentage of gross power), fritting time 15-25s; Plated film power 30%-60% (accounting for the percentage of gross power), the plated film time is 15-25s.Sputter coating also is a conventional method, for example makes the horizontal coating machine of UFSOFT's prestige, cleans vacuum degree 1-5 * 10 -2Pa cleans power 600W, scavenging period 20s, plated film vacuum degree 2-5 * 10 -3Pa, plated film power 3KW, plated film time 2S, coating times is once.The rete of sputter coating is than the densification of evaporation, and is also thinner, and adhesive force is better than evaporation
Described second adhesive layer 3 adopts the transparent gloss oil of N2K093 of company of German Baolong, can pass through the typography moulding, to be attached with the cleaning of the PC sheet material of metallic diaphragm 4 before the printing, otherwise the dirty meeting on metallic diaphragm 4 surfaces causes that the aberration of printing and bubble etc. are bad.Printing equipment is identical with above-mentioned printing ink layer 2 with printing process.
Described first adhesive layer 2 adopts aqueous binder, and printing equipment is identical with above-mentioned printing second adhesive 3 with printing process.When having bubble to produce when causing printing because of adhesive meter is glutinous, can add some defoamer head it offs, general additional proportion is no more than 0.5%, in order to cooperate whole technology, present embodiment has printed adhesive three times, carry out again after every printing all will be dried for one time next all over the printing, and each all over the printing all to ensure the quality of products, prevent bad appearance such as aberration, impurity, bubble.
The PC sheet material that will finish above-mentioned operation cuts into the size that needs, and then the PC material is carried out compression molding, is the shape that cooperates with base material 1 outer surface with smooth PC sheet forming.Compression molding has strict requirement to Mould design and manufacturing.The die cavity that must be noted that shaping mould and injection mould cooperatively interacts, and the shape of the two, scale error should have very high machining accuracy.Avoid occurring the turnover of acute angle, the arc transition mode all should be adopted in every corner.Present embodiment is a high-pressure molding, promptly with the temperature more than 150 ℃ to the PC sheet material that carried out preheating on metal die with the air pressurized moulding.Forming process should be noted that and mix up forming temperature, and configuration pressure size and dwell time, this routine use equipment is LFORM100-A type high-pressure forming machine, 380 ℃ of forming temperatures, stoving time 7s, high pressure pressurization 41Kg, pressurize 6s, low pressure pressurization 7Kg then, pressurize 5s.Last exhaust 12s.
After the part that does not need on the PC sheet material to cooperate with base material 1 cut, be fixed to transparent film layer 6.Before base material 1 injection moulding began, the transparent film layer 6 of setting was bumped into the injection mold from the back in advance.This injection mold comprises die and shaping mould (punch), the degree of depth in recessed membranous type chamber should be than the height of shaping mould the thickness of a big transparent film layer 6, after transparent film layer 6 is put into die, the injection molding material of base material 1 is injected at the inner surface of transparent film layer 6, makes injection molding material and transparent film layer 6 be bonded into the one curing molding.Present embodiment uses injection molding material to be PC7300, injection temperature 260-275 ℃.The method of described injection mo(u)lding has been conventionally known to one of skill in the art, for example can carry out injection mo(u)lding by using sea day 100 tonnes of injection moulding machines.
The plastic casing that provides according to the utility model embodiment, the thickness of formed first adhesive layer 2 is 20~70 microns, is preferably 50 microns, the thickness of formed second adhesive layer is 15~25 microns, is preferably 20 microns, the thickness of formed metallic diaphragm is 20~40 nanometers, be preferably 30 nanometers, the thickness of formed ink lay is 15~25 microns, is preferably 20 microns that the thickness of formed transparent film layer is 0.1~0.2 millimeter, is preferably 0.175 millimeter.
The plastic casing that provides according to the utility model, can on the housing base material, realize high-quality metal high brightness, effect lucuriant in design and have the pattern of fineness, exquisite texture, make the decorative effect of housing more improve a step, and wear-resistant, quality is higher.
The plastic casing that provides according to the utility model, the various performances of housing for example adhesive force, anti-scratch performance, vibration resistance polishing machine still can keep good effect, can reach 0 grade as adhesive force hundred lattice experimental tests and (have 0,1,2,3,4 and 5 grade, 0 grade best), anti-zoned trace can reach 2N, vibration abrasion can reach 2H (H for hour, generally require more than 1.5 hours).

Claims (8)

1, a kind of plastic casing, this plastic casing comprise base material and the transparent film layer that is positioned on the described substrate surface, it is characterized in that this plastic casing also comprises metallic diaphragm, and this metallic diaphragm is between substrate surface and transparent film layer.
2, plastic casing according to claim 1 is characterized in that, this plastic casing also comprises the ink lay that can be arranged between described transparent film layer and the metallic diaphragm.
3, plastic casing according to claim 1 and 2 is characterized in that, this plastic casing also comprises the adhesive layer that is arranged between metallic diaphragm and the substrate surface.
4, plastic casing according to claim 3 is characterized in that, described adhesive layer comprises first adhesive layer and second adhesive layer that is positioned on first adhesive layer on the substrate surface.
5, plastic casing according to claim 4 is characterized in that, described first adhesive layer is an adhesive phase, and second adhesive layer is the gloss oil layer.
6, plastic casing according to claim 4, wherein, the thickness of described first adhesive layer is 15~100 microns, the thickness of described second adhesive layer is 15~40 microns, the thickness of described metallic diaphragm is 20~50 nanometers, described thickness transparent or that be printed on the ink lay of pattern color is 20~40 microns, and the thickness of described transparent film layer is 0.1~0.3 millimeter.
7, plastic casing according to claim 6, wherein, the thickness of described first adhesive layer is 20~70 microns, the thickness of described second adhesive layer is 15~25 microns, the thickness of described metallic diaphragm is 30~40 nanometers, described thickness transparent or that be printed on the ink lay of pattern color is 25~35 microns, and the thickness of described transparent film layer is 0.1~0.2 millimeter.
8, a kind of mobile phone is characterized in that, described phone housing requires 1 to 8 each described plastic casing to make by aforesaid right.
CNU200820095680XU 2008-07-15 2008-07-15 Plastic rubber case and mobile phone adopting the plastic rubber case Expired - Lifetime CN201234412Y (en)