CN107911964A - Method for producing shell, housing and electronic equipment - Google Patents

Method for producing shell, housing and electronic equipment Download PDF

Info

Publication number
CN107911964A
CN107911964A CN201711052520.7A CN201711052520A CN107911964A CN 107911964 A CN107911964 A CN 107911964A CN 201711052520 A CN201711052520 A CN 201711052520A CN 107911964 A CN107911964 A CN 107911964A
Authority
CN
China
Prior art keywords
layer
paint
skin
sandblasting
housing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201711052520.7A
Other languages
Chinese (zh)
Other versions
CN107911964B (en
Inventor
杨光明
张涛
孙文峰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Oppo Mobile Telecommunications Corp Ltd
Original Assignee
Guangdong Oppo Mobile Telecommunications Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangdong Oppo Mobile Telecommunications Corp Ltd filed Critical Guangdong Oppo Mobile Telecommunications Corp Ltd
Priority to CN201711052520.7A priority Critical patent/CN107911964B/en
Publication of CN107911964A publication Critical patent/CN107911964A/en
Application granted granted Critical
Publication of CN107911964B publication Critical patent/CN107911964B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The embodiment of the present application discloses a kind of method for producing shell, housing and electronic equipment, wherein, method for producing shell includes:One casing substrate is provided, the outer surface of casing substrate is processed by shot blasting;Blasting treatment is carried out to the casing substrate outer surface after polishing treatment, in blasting treatment excessively, specifically to close to first while or/and pre-blast area when the 3rd carry out blasting treatment, to form the sandblasting floor of coarse structure in pre-blast area;Then oxidation processes are carried out to the casing substrate outer surface after blasting treatment, to form oxide layer on casing substrate outer surface and sandblasting layer;Spray painting at least once is carried out to the casing substrate outer surface after oxidation processes to handle, and at least one layer of skin of paint is formed in oxide layer.The embodiment of the present application skin of paint is located at the outermost layer of housing outer surface, can make it that surface of shell is smooth, fingerprint not easy to stick, housing outer surface can be kept clean and tidy.

Description

Method for producing shell, housing and electronic equipment
Technical field
This application involves technical field of electronic equipment, and in particular to a kind of method for producing shell, housing and electronic equipment.
Background technology
At present, electronic equipment, the raw material that for example mobile phone, the housing of tablet computer prepare processing is usually aluminium, and business The aluminium being commercially available then due to its rigidity the problems such as can not directly use.Need to carry out multiple working process to raw material aluminium Shell structure needed for formation.However, after housing processing of the prior art, housing outer surface easily glues fingerprint.
The content of the invention
The embodiment of the present application provides a kind of method for producing shell, housing and electronic equipment, it is possible to reduce housing outer surface Viscous fingerprint.
In a first aspect, the embodiment of the present application provides a kind of method for producing shell, the housing is applied in electronic equipment, institute Stating method for producing shell includes:
One casing substrate is provided, the casing substrate include end to end first while, second while, the 3rd side and the 4th Side, the casing substrate further include close to described first while or/and pre-blast area when the 3rd;
The outer surface of the casing substrate is processed by shot blasting;
Blasting treatment is carried out to the casing substrate outer surface after the polishing treatment, and the position of the blasting treatment is in institute Pre-blast area is stated, the sandblasting floor with coarse structure is formed in the pre-blast area;
Oxidation processes are carried out to the casing substrate outer surface after the blasting treatment, in the casing substrate outer surface and institute State and form oxide layer on sandblasting layer;
Spray painting at least once is carried out to the casing substrate outer surface after the oxidation processes to handle, the shape in the oxide layer Into at least one layer of skin of paint.
Second aspect, the embodiment of the present application also provide a kind of housing, and the housing uses housing making side as described above Method is formed.
The third aspect, the embodiment of the present application additionally provide a kind of housing, and applied in electronic equipment, the housing includes head Tail be connected first while, second while, the 3rd while and when the 4th, the housing includes the inner surface and the outer surface being oppositely arranged, institute State housing further include close to described first while or/and pre-blast area when the 3rd, the sandblasting area be located at the housing outer surface, The housing further includes sandblasting layer, oxide layer and skin of paint, and the sandblasting layer has coarse structure, and the sandblasting layer is formed in institute State in pre-blast area, the oxide layer is formed in the housing outer surface and the sandblasting layer, and the skin of paint is formed in institute State in oxide layer.
Fourth aspect, the embodiment of the present application additionally provide a kind of electronic equipment, including housing, and the housing is as described above Housing.
Method for producing shell provided by the embodiments of the present application, first, there is provided a casing substrate, and to the appearance of casing substrate Face is processed by shot blasting;Blasting treatment is carried out to the casing substrate outer surface after polishing treatment, in blasting treatment excessively, is specifically To close to first while or/and pre-blast area when the 3rd carry out blasting treatment, to form the sandblasting of coarse structure in pre-blast area Layer;Then oxidation processes are carried out to the casing substrate outer surface after blasting treatment, with casing substrate outer surface and sandblasting layer Form oxide layer;To after oxidation processes casing substrate outer surface carry out at least once spray painting handle, formed in oxide layer to Few one layer of skin of paint, to form overall housing structure.User is taken with hand and holds electronic equipment, is often taken and is held casting of electronic device Side margins, the application housing first while or/and position forms the sandblasting layer of coarse structure when the 3rd, friction can be increased Power, increases antiskid effect.And skin of paint is located at the outermost layer of housing outer surface, it can make it that surface of shell is smooth, no Fingerprint easy to stick, can keep housing outer surface clean and tidy.
Brief description of the drawings
In order to illustrate more clearly of the technical solution in the embodiment of the present application, make required in being described below to embodiment Attached drawing is briefly described, it should be apparent that, drawings in the following description are only some embodiments of the present application, for For those skilled in the art, without creative efforts, it can also be obtained according to these attached drawings other attached Figure.
Fig. 1 is the structure diagram of electronic equipment provided by the embodiments of the present application.
Fig. 2 is the structure diagram of housing provided by the embodiments of the present application.
Fig. 3 is the structure diagram of rear cover provided by the embodiments of the present application.
Fig. 4 is profiles of the Fig. 3 in A-A directions.
Fig. 5 is another profiles of the Fig. 3 in A-A directions.
Fig. 6 is another profiles of the Fig. 3 in A-A directions.
Fig. 7 is another profiles of the Fig. 3 in A-A directions.
Fig. 8 is another profiles of the Fig. 3 in A-A directions.
Fig. 9 is another profiles of the Fig. 3 in A-A directions.
Figure 10 is another profiles of the Fig. 3 in A-A directions.
Figure 11 is another profiles of the Fig. 3 in A-A directions.
Figure 12 is another structure diagram of rear cover provided by the embodiments of the present application.
Figure 13 is profiles of the Figure 12 in B-B directions.
Figure 14 is another profiles of the Figure 12 in B-B directions.
Figure 15 is another profiles of the Figure 12 in B-B directions.
Figure 16 is the structure diagram that rear exterior surface provided by the embodiments of the present application carries out blasting treatment.
Figure 17 is another structure diagram of rear cover provided by the embodiments of the present application.
Figure 18 is profiles of the Figure 17 in C-C directions.
Figure 19 is another structure diagram of housing provided by the embodiments of the present application.
Figure 20 is another structure diagram of rear cover provided by the embodiments of the present application.
Figure 21 is another structure diagram of electronic equipment provided by the embodiments of the present application.
Figure 22 is the flow diagram of rear cover production method provided by the embodiments of the present application.
Figure 23 is the flow diagram of spray painting processing provided by the embodiments of the present application.
Embodiment
Below in conjunction with the attached drawing in the embodiment of the present application, the technical solution in the embodiment of the present application is carried out clear, complete Site preparation describes.Obviously, described embodiments are only a part of embodiments of the present application, instead of all the embodiments.It is based on Embodiment in the application, the every other implementation that those skilled in the art are obtained without creative efforts Example, shall fall in the protection scope of this application.
In the description of the present application, it is to be understood that term " " center ", " longitudinal direction ", " transverse direction ", " length ", " width ", " thickness ", " on ", " under ", "front", "rear", "left", "right", " vertical ", " level ", " top ", " bottom ", " interior ", " outer ", " up time The orientation or position relationship of the instruction such as pin ", " counterclockwise " are based on orientation shown in the drawings or position relationship, are for only for ease of Describe the application and simplify to describe, rather than indicate or imply that signified device or element must have specific orientation, Yi Te Fixed azimuth configuration and operation, therefore it is not intended that limitation to the application.In addition, term " first ", " second " are only used for Purpose is described, and it is not intended that instruction or hint relative importance or the implicit quantity for indicating indicated technical characteristic. Thus, " first " is defined, the feature of " second " can be expressed or implicitly includes one or more feature. In the description of the present application, " multiple " are meant that two or more, unless otherwise specifically defined.
, it is necessary to illustrate in the description of the present application, unless otherwise clearly defined and limited, term " installation ", " phase Even ", " connection " should be interpreted broadly, for example, it may be being fixedly connected or being detachably connected, or be integrally connected;Can To be mechanical connection or electrical connection or can mutually communicate;It can be directly connected, can also be by between intermediary Connect connected, can be the interaction relationship of connection inside two elements or two elements.For the ordinary skill of this area For personnel, the concrete meaning of above-mentioned term in this application can be understood as the case may be.
In this application, unless otherwise clearly defined and limited, fisrt feature second feature it " on " or it " under " Can directly it be contacted including the first and second features, it is not directly to contact but pass through it that can also include the first and second features Between other characterisation contact.Moreover, fisrt feature second feature " on ", " top " and " above " to include first special Sign is directly over second feature and oblique upper, or is merely representative of fisrt feature level height and is higher than second feature.Fisrt feature exists Second feature " under ", " lower section " and " following " fisrt feature that includes are immediately below second feature and obliquely downward, or be merely representative of Fisrt feature level height is less than second feature.
Following disclosure provides many different embodiments or example is used for realizing the different structure of the application.In order to Simplify disclosure herein, hereinafter the component and setting of specific examples are described.Certainly, they are merely examples, and And purpose does not lie in limitation the application.In addition, the application can in different examples repeat reference numerals and/or reference letter, This repetition is for purposes of simplicity and clarity, between itself not indicating discussed various embodiments and/or setting Relation.In addition, this application provides various specific techniques and material examples, but those of ordinary skill in the art can be with Recognize the application of other techniques and/or the use of other materials.
The embodiment of the present application provides a kind of method for producing shell, housing and electronic equipment.It will carry out respectively below detailed Explanation.
In the present embodiment, will be described from the angle of rear cover production method, which can form shell Body, the housing can be set in the electronic device, such as mobile phone, tablet computer, palm PC (Personal Digital Assistant, PDA) etc..
Refer to the structure diagram that 1, Fig. 1 is electronic equipment provided by the embodiments of the present application.The electronic equipment 1 includes shell Body 10, display screen 20, printed circuit board 30, battery 40.
Referring to Fig. 2, Fig. 2 is the structure diagram of housing provided by the embodiments of the present application.Wherein, which can wrap Cover board 11, center 12 and rear cover 13 are included, cover board 11, center 12 and rear cover 13 are mutually combined to form the housing 10, which has There is the confined space formed by cover board 11, center 12 and rear cover 13, to accommodate display screen 20, printed circuit board 30, battery 40 Deng device.In certain embodiments, the lid of cover board 11 is set on center 12, and the lid of rear cover 13 is set on center 12, cover board 11 and rear cover 13 are located at the opposite face of center 12, and cover board 11 and rear cover 13 are oppositely arranged, and the confined space of housing 10 is located at cover board 11 and rear cover Between 13.
Wherein, cover board 11 can be transparent glass cover plate.In some embodiments, cover board 11 can be with such as blue precious Glass cover-plate made of the materials such as stone.Wherein, center 12 can be metal shell, such as aluminium alloy center 12.Need what is illustrated It is that the material of the embodiment of the present application center 12 is not limited to this, other manner can also be used, such as:Center 12 can ceramics Center, glass center.For another example:Center 12 can be plastic cement center.Also such as:Center 12 can be metal and plastic cement phase interworking The structure of conjunction, can form plastic portions and being molded on sheet metal.Wherein, rear cover 13 can be with metal back cover, such as aluminium Alloy rear cover.
Also referring to Fig. 3, Fig. 3 is the structure diagram of rear cover provided by the embodiments of the present application.The rear cover 13 can wrap The inner surface 131 being oppositely arranged and outer surface 132 are included, the inner surface 131 of the rear cover 13 forms shell close to center 12 and cover board 11 The inner surface of body 10, the outer surface 132 of the rear cover 13 is away from center 12 and cover board 11, the outer surface of formation housing 10.The rear cover 13 can also include perforate 133, which can install camera.
In certain embodiments, rear cover 13 include end to end first at 111, second the 112, the 3rd side 113 and the Four sides 114, wherein, first is 113 opposite at 111 and the 3rd, and second is 114 opposite at 112 and the 4th.In some embodiments In, the second side 112 can be located at the bottom of electronic equipment 1, and the 4th side 114 can be located at the top of electronic equipment 1, the first side 111 and the 3rd side 113 can be located at electronic equipment 1 both sides.Wherein, perforate 133 can be located at 114 position of the 4th side.
Also referring to Fig. 4, Fig. 4 is profiles of the Fig. 3 in A-A directions.Rear cover 13a can include rear cover substrate 137, Oxide layer 134 and skin of paint 136.
Wherein, rear cover substrate 137 can use aluminium, such as aluminium alloy.The rear cover substrate 137 includes 131 He of inner surface Outer surface 132, the inner surface of the rear cover substrate 137 can be understood as the inner surface of rear cover 13, and the rear cover substrate 137 is outer Surface can be understood as the outer surface before the non-oxidation processes of rear cover, spray painting processing etc..137 rear cover 13a tools of the rear cover substrate Have same first at 111, second the 112, the 3rd in 113 and the 4th while 114.
Wherein, oxide layer 134 is formed on the outer surface 132 of rear cover substrate 137.The oxide layer 134 can be by once Oxidation forms layer of oxide layer 134.Such as:Monochrome oxidation forms the oxide layer 134, specifically can be by being carried out after oxidation technology Coloring is formed.It should be noted that in some embodiments, it is also possible to formed using oxidation twice or oxidation more than twice Multilayer oxide layer.
Such as:Referring to Fig. 5, Fig. 5 is another profiles of the Fig. 3 in A-A directions.Fig. 5 and Fig. 4 difference lies in:Rear cover The oxide layer 134 of 13b includes two layers, i.e. the first oxide layer 1341 and the second oxide layer 1342.First oxide layer 1341 is formed in On the outer surface 132 of rear cover substrate 137, the second oxide layer 1342 is formed in the first oxide layer 1341, in certain embodiments, Second oxide layer can only cover the part in the first oxide layer.First oxide layer 1341 and the second oxide layer 1342 can With increase and the combination power of skin of paint 136.Wherein, the sandwich construction on oxide layer, no longer illustrates one by one herein.One In a little embodiments, which can be colored oxide layer, and the second oxide layer can also be colored oxide layer.First oxygen The color for changing layer can be different from the color of the second oxide layer, can also be identical.
Wherein, skin of paint 136 is formed in oxide layer 134, oxide layer 134 be located at skin of paint 136 and rear cover substrate 137 it Between.In certain embodiments, one layer of paint can be sprayed in oxide layer 134 and forms the skin of paint 136.The skin of paint 136 is located at The outermost layer of 13 outer surface of rear cover, its surface is smooth, and fingerprint not easy to stick, exterior surface cleaning is smooth after can keeping.
It should be noted that in some embodiments, it is also possible to two layers of paint or more than two layers are sprayed in oxide layer 134 Paint, to form two layers of skin of paint or multilayer skin of paint.Such as:Referring to Fig. 6, Fig. 6 is another sections of the Fig. 3 in A-A directions Figure.Fig. 6 and Fig. 4 difference lies in:The skin of paint 136 of rear cover 13c includes the first skin of paint 1361 and the second skin of paint 1362.Should First skin of paint 1361 is formed in oxide layer 134, which is formed on the first skin of paint 1361.At some In embodiment, the thickness of the second skin of paint 1362 is more than the thickness of the first skin of paint 1361, further, the second skin of paint 1362 Thickness be twice of thickness of the first skin of paint 1361, for example the thickness of the second skin of paint 1362 is 10um, the first skin of paint 1361 thickness is 5um.It should also be noted that, the second skin of paint 1362 and the first skin of paint 1361 in process of production may There are certain error amount, for example error amount is 0.5um.The setting of second skin of paint and the first paint layer thickness can be to rear cover Outer surface provides preferably protection, and so that is bonded between two layers of skin of paint even closer.
For another example:Referring to Fig. 7, Fig. 7 is another profiles of the Fig. 3 in A-A directions.Fig. 7 and Fig. 4 difference lies in:Afterwards The skin of paint 136 of lid 13d includes the first skin of paint 1361, the second skin of paint 1362 and the 3rd skin of paint 1363.First paint Layer 1361 is formed in oxide layer 134, which is formed on the first skin of paint 1361, the 3rd skin of paint 1363 are formed on the second skin of paint 1362.Formed in oxide layer 134 two layers or three layers of skin of paint can increase oxide layer and The combination power of skin of paint, to the protecting effect of rear cover more preferably.In certain embodiments, the thickness of the 3rd skin of paint 1363 is more than the Two skin of paints 1362, the thickness of the second skin of paint 1362 are more than the thickness of the first skin of paint 1361.Further, the 3rd skin of paint 1363 thickness is twice of the thickness of the second skin of paint 1362, and the thickness of the second skin of paint 1362 is the first skin of paint 1361 Twice of thickness, for example the thickness of the 3rd skin of paint 1363 is 8um, the thickness of the second skin of paint 1362 are 4um, the first skin of paint 1361 thickness is 2um.
In certain embodiments, the thickness of the 3rd skin of paint 1363, the second skin of paint 1362 and the first skin of paint 1361 according to Secondary equal thickness is reduced, for example the thickness of the 3rd skin of paint 1363 is 9um, and the thickness of the second skin of paint 1362 is 6um, and first paints The thickness of layer 1361 is 3um.The setting of 3rd skin of paint, the second skin of paint and the first paint layer thickness can be to rear exterior surface Preferably protection is provided, and so that is bonded between three layers of skin of paint even closer.
In certain embodiments, which transparent can be set.It should be noted that when skin of paint is at least two layers When, wherein at least one layer of skin of paint transparent can be set.Further, the transparent setting of all skin of paints.Aoxidized with rear cover Layer is the appearance face color of rear cover.
In order to increase the combination power between skin of paint 136 and oxide layer 134, in certain embodiments, referring to Fig. 8, Fig. 8 For another profiles of the Fig. 3 in A-A directions.Fig. 8 and Fig. 4 difference lies in:Rear cover 13e can also include binder course 135.The knot Close layer 135 to be formed in oxide layer 134, skin of paint 136 is formed on binder course 135.In certain embodiments, the binder course 135 can be formed in oxide layer 134 using the mode of PVD (Physical Vapor Deposition, physical vapour deposition (PVD)) On.The binder course 135 can increase between oxide layer 134 and skin of paint 136 between oxide layer 134 and skin of paint 136 With reference to power.It should be noted that the embodiment of the present application can also other manner oxide layer formed binder course, to increase oxide layer With the combination power of skin of paint.
In certain embodiments, referring to Fig. 9, Fig. 9 for Fig. 3 in another profile in A-A directions, the difference of Fig. 9 and Fig. 4 It is:The outer surface of rear cover 13f rear covers substrate 137 forms the sandblasting layer 1371 with coarse structure, on the sandblasting layer 1371 Coarse structure can be formed by way of sand-blasting machine uses sandblasting so that and 137 outer surface of rear cover substrate is cleaned, is coarse, and then The combination power being formed on the sandblasting layer 1371 between oxide layer 134 and skin of paint 136 can be increased.In certain embodiments, The sandblasting layer 1371 is covered on the whole outer surface of rear cover substrate 137.
In certain embodiments, which can be concaveconvex structure, which can be the structure of rule, i.e., Concaveconvex structure is uniformly arranged on the outer surface of rear cover substrate 137;Can also be irregular structure, the i.e. different row of spacing Cloth is on the outer surface of rear cover substrate 137.It should be noted that the coarse structure of the embodiment of the present application is not limited to this, also may be used To be only projective structure, such as:Figure 10 can be referred to, Figure 10 is the area of another profiles of the Fig. 3 in A-A directions, Figure 10 and Fig. 9 It is not:Coarse structure in Figure 10 is projective structure, can be uniformly distributed salient point or the salient point of uneven arrangement. Also such as:Can refer to Figure 11, Figure 11 be another profiles of the Fig. 3 in A-A directions, Figure 11 and Fig. 9 difference lies in:In Figure 11 Coarse structure be sunk structure, can be uniformly distributed concave point or the concave point of uneven arrangement.
In certain embodiments, another structural representation that 2, Figure 12 is rear cover provided by the embodiments of the present application is please referred to Fig.1 Figure.The outer surface of rear cover 13g includes pre-blast area 115, should be two with pre-blast area 115, and 115 phase of Liang Ge pre-blasts area Mutually it is arranged at intervals.Specifically, Liang Ge pre-blasts area 115 respectively close to first at 111 and the 3rd 113.That is a pre-blast area 115 are disposed adjacent close to the first side 111, in other words 115 and first side 111 of a pre-blast area;Another pre-blast area 115 is leaned on Nearly 3rd side 113, in other words 115 and the 3rd side 113 of a pre-blast area be disposed adjacent.
In certain embodiments, can pre-blast area 115 sand-blasting machine use sandblasting by way of handled, with Pre-blast area 115 forms coarse structure.Specifically, please referring to Fig.1 3, Figure 13 is profiles of the Figure 12 in B-B directions.Spraying in advance Sand area 115 forms the sandblasting floor 1373 with coarse structure, which has two parts, i.e. 1371 He of the first sandblasting layer Second sandblasting layer 1372.Wherein, in a 1371 pre-blast area 115 formed therein of the first sandblasting floor, the first sandblasting layer 1371 It is adjacent with the first side 111.Wherein, the second sandblasting floor 1372 is formed in another pre-blast area 115,1372 He of the second sandblasting layer 3rd side 113 is adjacent.First sandblasting layer 1371 and the second sandblasting layer 1372 are spaced.
In certain embodiments, which can be concaveconvex structure, which can be the structure of rule, i.e., Concaveconvex structure is uniformly arranged on the outer surface of rear cover substrate 137;Can also be irregular structure, the i.e. different row of spacing Cloth is on the outer surface of rear cover substrate 137.It should be noted that the coarse structure of the embodiment of the present application is not limited to this, also may be used To be only projective structure, such as:Figure 14 can be referred to, Figure 14 is another profiles of the Figure 12 in B-B directions, Figure 14 and Figure 13's Difference lies in:Coarse structure in Figure 14 is projective structure, can be the convex of uniformly distributed salient point or uneven arrangement Point.Also such as:Can refer to Figure 15, Figure 15 be another profiles of the Figure 12 in B-B directions, Figure 15 and Figure 13 difference lies in: Coarse structure in Figure 15 is sunk structure, can be uniformly distributed concave point or the concave point of uneven arrangement.
In certain embodiments, please refer to Fig.1 6, Figure 16 and carry out sandblasting for rear exterior surface provided by the embodiments of the present application The structure diagram of processing.Wherein, second at 112 and the 4th 114 distance be H1, sandblasting layer 1373 close to the second side 112, Sandblasting layer 1373 second while 112 to the 4th while 113 directions height be H2, wherein, 2/5H1 < H2 < 4/5H1.Need to illustrate , in some other embodiment, the height of sandblasting layer 1373 can be configured according to the actual requirements.
Wherein, sandblasting layer 1373 first while 111 to the 3rd while 113 directions width be W, wherein, 1cm < W < 2cm. It should be noted that the width of sandblasting layer 1373 can be configured according to the actual requirements.
In certain embodiments, sandblasting layer 1373 can be arcuate structure, the bending direction of the arcuate structure can be from First at 111 to the 3rd 113 directions.
It should be noted that user, during by electronic equipment 1 is held, it is electronic equipment 1 that duration, which takes the region held, Housing outer surface, particularly user is by the rear cover both sides of the edge position for holding housing.More specifically, user takes and holds rear cover appearance The palm of the hand takes the width held to take the width held in 1-2cm in 1-2cm, and finger in the direction of the width in face.In addition, user is taken with hand The height duration for holding electronic equipment 1 is to take more than half for arriving 1 height of electronic equipment.Therefore, the embodiment of the present application according to Family carries out blasting treatment by custom, region of electronic equipment 1 etc. is held in the both sides of the edge position of rear cover, can be formed with coarse The sandblasting layer of structure, so as to increase frictional force, can increase antiskid effect.
It should be noted that the pre-blast area 115 of the embodiment of the present application is not limited to this, can be one.Specifically, please Refering to Figure 17 and Figure 18, Figure 17 is another structure diagram of rear cover provided by the embodiments of the present application, and Figure 18 is Figure 17 in C-C side To profile.Figure 17, Figure 18 and the Figure 12, Figure 13 difference lies in:Pre-blast area 115 is one, which leans on Nearly first side 111,115 and first side 111 of pre-blast area is adjacent in other words.
It should be noted that when pre-blast area 115 is one, can also be by a pre-blast area 115 close to the 3rd side 113 are set.It should also be noted that, the coarse structure of Figure 17 and Figure 18 can include concaveconvex structure, projective structure or depression knot Structure, can specifically refer to above content, details are not described herein.
It should be noted that skin of paint can be formed in the whole outer surface of rear cover, can also be formed on sandblasting layer.When When skin of paint is formed on sandblasting layer, skin of paint can be overlapping with sandblasting layer., can will wherein when two layers of skin of paint or multilayer One layer of skin of paint is arranged on sandblasting layer, and wherein one or more layers skin of paint can also be arranged on to the whole outer surface of rear cover On.
It should be noted that the structure of the rear cover is not limited to this, such as:Rear cover can include two layers or multilayer aoxidizes Layer, two layers or multilayer skin of paint.For another example:Rear cover can include two layers or multilayer oxide layer, two layers or multilayer skin of paint and Binder course.For another example:Rear cover can include two layers or multilayer oxide layer, two layers or multilayer skin of paint and sandblasting layer.Need Bright, the number of plies between oxide layer, sandblasting layer, binder course and skin of paint changes in the protection domain of the embodiment of the present application Within, no longer illustrate one by one herein.
It should be noted that the structure of the embodiment of the present application housing is not limited to this, such as, please refer to Fig.1 9, Tu19Wei Another structure diagram of housing provided by the embodiments of the present application.Wherein, the housing 10a shown in Figure 19 includes cover board 16 and rear cover 17.In certain embodiments, the directly lid of cover board 16 is set on rear cover 17, and cover board 16 and rear cover 17 are mutually combined to form the housing 10a, housing 10a have the confined space formed by cover board 16 and rear cover 17, to accommodate display screen 20, printed circuit board 30th, the device such as battery 40.Compared to the housing 10 shown in Fig. 2, housing 10a does not include center, or perhaps by the center in Fig. 2 12 and rear cover 13 be integrally formed to form 17 structure of a rear cover (certainly, middle frame structure can also be named as herein).Specifically, it please join Figure 20 is read, Figure 20 is another structure diagram of rear cover provided by the embodiments of the present application.In certain embodiments, rear cover 17 includes Inner surface 171 and outer surface 172, inner surface 171 and outer surface 172 are oppositely arranged, and form the whole surface of rear cover 17.The rear cover 17 each Rotating fields can refer to rear cover 13, and details are not described herein.
Wherein, which installs in the housing 10, which can be the master of electronic equipment 1 Plate, can be integrated with antenna, motor, microphone, camera, light sensor, receiver and processing on printed circuit board 30 The functional units such as device.In certain embodiments, which is fixed in housing 10.Specifically, the printed circuit board 30 can be screwed on center 12 by screw, card can also be fitted on by the way of buckle on center 12.It should be noted that The mode that the embodiment of the present application printed circuit board 30 is specifically fixed on center 12 is not limited to this, can with other manner, than Such as by way of being buckled and screw is fixed jointly.
Wherein, which installs in the housing 10, and battery 40 is electrically connected with the printed circuit board 30, with to electronics Equipment 1 provides power supply.Housing 10 can be as the battery cover of battery 40.Housing 10 covers battery 40 to protect battery 40, specifically Be that rear cover 13 covers battery 40 to protect battery 40, reduce battery 40 due to electronic equipment 1 collision, fall etc. and be subject to Damage.
Wherein, which installs in the housing 10, meanwhile, which is electrically connected on printed circuit board 30, To form the display surface of electronic equipment 1.The display screen 20 includes display area 14 and non-display area 15.The display area 14 can With for showing the picture of electronic equipment 1 or carry out touching manipulation etc. for user.The top area of the non-display area 15 is opened If for the perforate of sound and light conduction, the functions such as fingerprint module, touch controlled key can be set on 15 bottom of non-display area Component.Wherein the cover board 11 is installed on display screen 20, to cover display screen 20, forms the display area identical with display screen 20 And non-display area, display area that specifically can be refering to display screen 20 and non-display area.
It should be noted that the structure of the display screen 20 is not limited to this.For example the display screen can be comprehensive screen or different Property screen, specifically, refer to Figure 21, Figure 21 is another structure diagram of electronic equipment provided by the embodiments of the present application.Figure 21 In electronic equipment and Fig. 1 in electronic equipment difference lies in:Non-display area 15a is formed directly on display screen 20a, For example it is arranged to transparent configuration in the non-display area 15a of display screen 20a, so that optical signal passes through, or directly in display screen The non-display area of 20a is opened up for structures such as the perforate of light conduction or notches, can be by front camera, photoelectric sensor etc. Non-display area position is arranged at, so that front camera is taken pictures, photoelectric sensor detects.Display area 14a is paved with electronics Equipment 1a whole surfaces.It should be noted that the device such as housing 10, printed circuit board 30 and battery 40 in electronic equipment 1a Above content can be referred to, details are not described herein.
It should also be noted that, display screen can also be displayed in full screen, and it is not provided with non-display area.
In order to further describe the shell structure of the embodiment of the present application, carried out specifically by taking method for producing shell as an example below It is bright.It should be noted that method for producing shell can specifically include rear cover production method, center production method.Housing system below Make method to illustrate by taking rear cover production method as an example, it is to be understood that the embodiment of the present application method for producing shell is simultaneously unlimited In rear cover.
Also referring to Figure 22, Figure 22 is the flow diagram of rear cover production method provided by the embodiments of the present application.After this Lid production method comprises the following steps:
In a step 101, there is provided a rear cover substrate.The rear cover substrate can be metal material, such as aluminium, further , such as aluminium alloy.It should be noted that the rear cover substrate can be directly commercially available, sheet fabrication can also be obtained, than Such as aluminum alloy plate materials are forged and pressed, timeliness process obtains.It should also be noted that, rear cover substrate can specifically refer to Above content, details are not described herein.
Wherein, which can include the inner surface and the outer surface for being oppositely arranged, the rear cover substrate and its inner surface, Outer surface can refer to above content, and details are not described herein.The rear cover substrate can also include end to end first side, second While, the 3rd while and the 4th side, the rear cover substrate first while, second while, the 3rd while and the 4th while can be understood as the of rear cover On one side, second while, the 3rd while and the 4th side, can specifically refer to above content, details are not described herein.
In certain embodiments, the outer surface of the rear cover substrate can include pre-blast area, which can be two It is a, and the spaced setting in Liang Ge pre-blasts area.Specifically, Liang Ge pre-blasts area is respectively close to the first side of rear cover substrate and Three sides.That is a pre-blast area is disposed adjacent close to the first side, in other words a pre-blast area and the first side;Another pre-blast Area is disposed adjacent close to the 3rd side, in other words a pre-blast area and the 3rd side.
It should be noted that the pre-blast area can also be one, can be close to the first side when pre-blast area is one Set, can also be set close to the 3rd side.
In a step 102, the outer surface of rear cover substrate is processed by shot blasting.So that rear cover outer surface of substrate is smooth.
In certain embodiments, can be by the way of machinery, chemistry, electrochemistry or ultrasonic wave etc. to rear cover substrate appearance Realize polishing in face.So that rear cover base plate surface roughness reduces, to obtain bright, flat surface rear cover outer surface of substrate. Wherein, chemical polishing mode is to carry out regular dissolving to rear cover outer surface of substrate to reach smooth.Wherein, electrochemical polish It using rear exterior surface as anode, insoluble petal is cathode that mode, which is, and the two poles of the earth are immersed in electrolytic cell at the same time, logical direct current and produce Raw selective anodic dissolution, so that the increase of rear cover outer surface of substrate brightness is big.The mode wherein mechanically polished is By cutting rear cover outer surface of substrate so that rear cover outer surface of substrate plastic deformation removes the convex portion after polishing and obtains even surface. The mode of wherein ultrasonic polishing is that rear cover substrate is put into abrasive suspension and is placed in together in ultrasound field, by ultrasound The oscillation action of ripple, makes abrasive material in workpiece surface grinding-polishing.
In certain embodiments, can be first to rear cover substrate before being processed by shot blasting to the outer surface of rear cover substrate Outer surface carries out grinding process, and then the rear cover outer surface of substrate after grinding process is processed by shot blasting again, makes polishing treatment It is better so that rear cover outer surface of substrate is more smooth.Here, it should be noted that the grinding process can be understood as pair Roughing before polishing treatment.I.e., it is possible to first carry out once thick polishing to rear cover outer surface of substrate, then once carefully polished, Complete polishing treatment.
In step 103, blasting treatment, the position of the blasting treatment are carried out to the rear cover outer surface of substrate after polishing treatment In pre-blast area, the sandblasting floor with coarse structure is formed in pre-blast area.
The sandblasting layer with coarse structure can increase the combination power between oxide layer and skin of paint.
In certain embodiments, with reference to Figure 12 to Figure 18, the side of sandblasting can be used by sand-blasting machine in pre-blast area 115 Formula is handled, and to form the sandblasting floor 1373 with coarse structure in pre-blast area 115, which can have two Part, i.e. the first sandblasting layer 1371 and the second sandblasting layer 1372.Wherein, 1371 pre-blast formed therein of the first sandblasting layer In area 115, the first sandblasting layer 1371 and the first side 111 are adjacent.Wherein, the second sandblasting floor 1372 is formed in another pre-blast area On 115, the second sandblasting layer 1372 and the 3rd side 113 are adjacent.First sandblasting layer 1371 and the second sandblasting layer 1372 are spaced.
In certain embodiments, 6 are please referred to Fig.1, wherein, second at 112 and the 4th 114 distance be H1, sandblasting layer 1373 close to the second side 112, sandblasting layer 1373 second while 112 to the 4th while 113 directions height be H2, wherein, 2/5H1 < H2 < 4/5H1.It should be noted that in some other embodiment, the height of sandblasting layer 1373 can according to the actual requirements into Row is set.
Wherein, sandblasting layer 1373 first while 111 to the 3rd while 113 directions width be W, wherein, 1cm < W < 2cm. It should be noted that the width of sandblasting layer 1373 can be configured according to the actual requirements.
In certain embodiments, sandblasting layer 1373 can be arcuate structure, the bending direction of the arcuate structure can be from First at 111 to the 3rd 113 directions.Wherein, the coarse structure of the sandblasting layer 1373 can include concaveconvex structure, projective structure Or sunk structure, above content can be specifically referred to, details are not described herein.
It should be noted that user, during by electronic equipment 1 is held, it is electronic equipment 1 that duration, which takes the region held, Housing outer surface, particularly user is by the rear cover both sides of the edge position for holding housing.More specifically, user takes and holds rear cover appearance The palm of the hand takes the width held to take the width held in 1-2cm in 1-2cm, and finger in the direction of the width in face.In addition, user is taken with hand The height duration for holding electronic equipment 1 is to take more than half for arriving 1 height of electronic equipment.Therefore, the embodiment of the present application according to Family carries out blasting treatment by custom, region of electronic equipment 1 etc. is held in the both sides of the edge position of rear cover, can be formed with coarse The sandblasting layer of structure, so as to increase frictional force, can increase antiskid effect.
It should be noted that the sandblasting layer can also be one, such as the first sandblasting layer 1371.It should be noted that should Sandblasting layer can also be the second sandblasting layer.Figure 17, Figure 18 and above content can be specifically combined, details are not described herein.
In certain embodiments, the combination between oxide layer and skin of paint can should be increased with the sandblasting layer of coarse structure Area, and then the combination power between oxide layer and skin of paint can be increased.
At step 104, oxidation processes are carried out to the rear cover outer surface of substrate after blasting treatment.
In certain embodiments, oxidation processes at least once can be carried out to the rear cover outer surface of substrate after blasting treatment, To form oxide layer, or perhaps oxide-film.Oxidation every time can be coloured in oxidizing process, so it is outer needed for formation See color.Such as:Can to after blasting treatment rear exterior surface carry out once oxidation processing, formed layer of oxide layer, and Coloring treatment is carried out after the oxidation, forms required color, such as red, blueness etc..
It should be noted that in some embodiments, it is also possible to two are carried out to the rear cover outer surface of substrate after blasting treatment Secondary or oxidation processes more than twice, to form at least two layers of oxide layer, and carry out coloring treatment in oxidizing process, and then shape Into required appearance color.By oxidation processes two or more times not only to the protecting effect of rear exterior surface more preferably, and two At least two layers formed after secondary or more time oxidation and the combination power of skin of paint it is more preferable.
In certain embodiments, which is covered in the outer surface of rear cover substrate, which is specifically formed in sandblasting On layer and rear cover outer surface of substrate.
In step 105, carry out spray painting at least once to the rear cover outer surface of substrate after oxidation processes to handle, in rear cover base Plate outer surface forms at least one layer of skin of paint, to form complete rear cover structure.At least one layer skin of paint is formed in oxide layer On.At least one layer skin of paint is located at the outermost layer of rear cover outer surface of substrate, its surface is smooth, fingerprint not easy to stick, can be with Exterior surface cleaning is smooth after holding.
In certain embodiments, once spray painting processing can be carried out in oxide layer, forms one layer of skin of paint, can also be The processing of spray painting two or more times is carried out in oxide layer, forms two layers or more than two layers of skin of paint.It should be noted that work as oxygen When change layer only has one or two layers or multilayer, once spray painting can be directly carried out in oxide layer and handled, form one layer of skin of paint, The processing of spray painting two or more times can also be carried out in oxide layer, forms two layers or more than two layers of skin of paint.
In certain embodiments, after rear cover outer surface of substrate after the oxidising treat-ment carries out the processing of spray painting at least once, Rear cover outer surface of substrate can be toasted at least once, high-temperature baking can be used, rear cover substrate appearance will be sprayed on The paint drying in face forms skin of paint.For example rear exterior surface is dried when baking temperature is 80 degree, baking time is 1 small It is roasting.It should be noted that once baking processing can be carried out after the processing of spray painting each time.Below by taking processing of painting twice as an example Illustrate, refer to Figure 23, Figure 23 is the flow diagram of spray painting processing provided by the embodiments of the present application.Spray painting processing Technical process includes:
In step 1051, first time spray painting processing is carried out to the rear cover outer surface of substrate after oxidation processes.At oxidation Rear cover outer surface of substrate after reason carries out first time spray painting, spraying layer of transparent paint.
In certain embodiments, first time spray painting processing can carry out on the whole outer surface of rear cover, you can with right The whole outer surface of rear cover substrate carries out first time spray painting processing.
It should be noted that in some other embodiment, can also only be carried out in sandblasting layer position at first time spray painting Reason.In spray painting processing procedure for the first time is carried out to sandblasting layer position, remaining position of rear cover outer surface of substrate can be blocked Firmly, first time spray painting processing is carried out.The region of the spray painting processing for the first time can be overlapping with sandblasting layer, can also be slightly less than or omit More than sandblasting layer.It is understood that in processing procedure of actually painting, there are certain error.
In step 1052, the rear cover outer surface of substrate after handling first time spray painting carries out first time baking processing, Rear cover outer surface of substrate forms the first skin of paint.Spray painting processing for the first time and baking processing can increase oxide layer and first time The combination power of spray paint.
In certain embodiments, which can cover the whole outer surface of rear cover substrate.In some other reality Apply in example, which can cover a part of region of rear cover outer surface of substrate, and particularly the first skin of paint covers Cover on sandblasting layer, and sandblasting layer is overlapping.
In step 1053, the rear cover outer surface of substrate after handling first time baking carries out second of spray painting processing. Rear cover outer surface of substrate after first time baking processing carries out second of spray painting processing, sprays celluloid paint.
In certain embodiments, second of spray painting processing can be carried out in the whole outer surface of rear cover substrate, can also Second of spray painting processing is carried out in the subregion of rear cover outer surface of substrate, for example is carried out in sandblasting layer position at second of spray painting Reason.
It should be noted that in first time spray painting processing and second of spray painting processing procedure, at least once at spray painting Reason is to cover the whole outer surface of rear cover substrate.Paint processing procedure, can once be sprayed in sandblasting layer position twice Paint processing, once carries out spray painting processing in the whole outer surface of rear cover.Can also it be carried out twice in the whole outer surface of rear cover substrate Spray painting is handled.
In step 1054, the rear cover outer surface of substrate after handling second of spray painting carries out second of baking processing, after Lid outer surface of substrate forms the second skin of paint.
Wherein, which can be formed on the first skin of paint.Second skin of paint can also be formed in oxidation On layer and the first skin of paint.In certain embodiments, at least one layer of first skin of paint and the second skin of paint cover rear cover The whole outer surface of substrate.
In certain embodiments, first skin of paint and the second skin of paint are that celluloid paint is formed.Need what is illustrated Be have in the first skin of paint and the second skin of paint one layer for clean oil enamelled coating it is also possible.
It should be noted that can also be painted three times processing and baking processing three times, details are not described herein.Wherein, Thickness relationship between each skin of paint can refer to above content, and details are not described herein.It should also be noted that, can also carry out Spray painting processing and baking processing above three times more than three times.
In certain embodiments, first the rear cover outer surface of substrate after oxidation processes can be carried out between spray painting processing Physical vapour deposition (PVD) process, binder course is formed in rear cover outer surface of substrate.Then the rear cover after physical vapour deposition (PVD) process again Outer surface of substrate carries out spray painting processing.
Specifically, after the oxidising treat-ment, in order to increase the combination power between skin of paint and oxide layer, physics gas can be used Mutually the mode of deposition forms one layer of binder course in oxide layer, spray painting processing is then carried out on binder course again, on binder course Form skin of paint.Binder course can increase oxide layer and the combination power of skin of paint, to the protecting effect of rear exterior surface more preferably.
In summary, rear cover production method provided by the embodiments of the present application, can sequentially form in rear exterior surface and be located at Afterwards exterior surface specific region and the sandblasting layer with coarse structure, at least one layer of oxide layer, one or two layers or multilayer oil Enamelled coating, sandblasting layer can increase user and take the frictional force for holding electronics portion, and skin of paint is formed in the outermost of rear exterior surface Layer, it is its highlight surface, penetrating so that its surface is smooth, fingerprint not easy to stick, and exterior surface is clean and tidy after can keeping.
It will be understood by those skilled in the art that the structure of the electronic equipment 1 shown in Fig. 1 is not formed to electronic equipment 1 Restriction.Electronic equipment 1 can be included than illustrating more or fewer components, either combine some components or different portions Part is arranged.Electronic equipment 1 can also include memory, bluetooth module etc., and details are not described herein.
Method for producing shell provided by the embodiments of the present application, housing and electronic equipment are described in detail above, this Specific case is applied in text to be set forth the principle and embodiment of the application, the explanation of above example is only intended to Help understands the application.Meanwhile for those skilled in the art, according to the thought of the application, in embodiment and answer With there will be changes in scope, in conclusion this specification content should not be construed as the limitation to the application.

Claims (20)

1. a kind of method for producing shell, the housing is applied in electronic equipment, it is characterised in that the method for producing shell bag Include:
One casing substrate is provided, the casing substrate include end to end first while, second while, the 3rd while and when the 4th, institute State casing substrate further include close to described first while or/and pre-blast area when the 3rd;
The outer surface of the casing substrate is processed by shot blasting;
Blasting treatment is carried out to the casing substrate outer surface after the polishing treatment, and the position of the blasting treatment is described pre- Sandblasting area, the sandblasting floor with coarse structure is formed in the pre-blast area;
Oxidation processes are carried out to the casing substrate outer surface after the blasting treatment, in the casing substrate outer surface and the spray Oxide layer is formed on layer of sand;
To after the oxidation processes casing substrate outer surface carry out at least once spray painting handle, formed in the oxide layer to Few one layer of skin of paint.
2. method for producing shell according to claim 1, it is characterised in that the sandblasting layer is arcuate structure.
3. method for producing shell according to claim 1, it is characterised in that the sandblasting layer includes the positioned at same layer One sandblasting layer and the second sandblasting layer, the first sandblasting layer and the second sandblasting layer are spaced and be arranged in parallel, and described One sandblasting layer is close to first side, and the second sandblasting layer is close to the 3rd side.
4. method for producing shell according to claim 1, it is characterised in that described second while and it is described 4th while distance For H1, the sandblasting layer is in the height of second side to the 4th edge direction close to second side, the sandblasting layer H2, wherein, 2/5H1 < H2 < 4/5H1.
5. method for producing shell according to claim 4, it is characterised in that the sandblasting layer is on first side to described The width of 3rd edge direction is W, wherein, 1cm < W < 2cm.
6. method for producing shell according to any one of claim 1 to 5, it is characterised in that it is described to the oxidation at Casing substrate outer surface after reason carries out the step of spray painting processing at least once, including:
Once spray painting is carried out to the casing substrate outer surface after the oxidation processes to handle, and one layer of oil is formed in the oxide layer Enamelled coating.
7. method for producing shell according to claim 6, it is characterised in that the housing base to after the oxidation processes Plate outer surface carries out the step of once spray painting processing, including:
Once spray painting is carried out to the casing substrate outer surface after the oxidation processes to handle;
Casing substrate outer surface after handling the once spray painting carries out once baking and handles, and one is formed in the oxide layer Layer skin of paint.
8. method for producing shell according to any one of claim 1 to 5, it is characterised in that it is described to the oxidation at Casing substrate outer surface after reason carries out the step of spray painting processing at least once, including:
The processing of spray painting twice is carried out to the casing substrate outer surface after the oxidation processes, two layers of oil is formed in the oxide layer Enamelled coating.
9. method for producing shell according to claim 8, it is characterised in that the housing base to after the oxidation processes Plate outer surface carries out the step of spray painting processing twice, including:
First time spray painting processing is carried out to the casing substrate outer surface after the oxidation processes;
Casing substrate outer surface after handling the first time spray painting carries out first time baking processing, the shape in the oxide layer Into the first skin of paint;
Casing substrate outer surface after handling the first time baking carries out second of spray painting processing;
Casing substrate outer surface after handling second of spray painting carries out second of baking processing, the shape on the first skin of paint Into the second skin of paint.
10. method for producing shell according to claim 9, it is characterised in that the thickness of second skin of paint is more than institute State the thickness of the first skin of paint.
11. method for producing shell according to claim 9, it is characterised in that the housing to after the oxidation processes Outer substrate surface carries out the step of spray painting processing for the first time, including:
To the casing substrate outer surface spraying layer of transparent paint after the oxidation processes;
Casing substrate outer surface after the processing to the first time baking carries out the step of second of spray painting is handled, including:
Casing substrate outer surface spraying layer of transparent paint after handling the first time baking.
12. a kind of housing, applied in electronic equipment, it is characterised in that the housing is used as any in claim 1 to 11 The item method for producing shell is formed.
13. a kind of housing, applied in electronic equipment, it is characterised in that the housing includes end to end first side, second While, the 3rd while and the 4th side, the housing include the inner surface and the outer surface for being oppositely arranged, the housing is further included close to described First while or/and pre-blast area when the 3rd, the sandblasting area be located at the housing outer surface, the housing further includes sandblasting Layer, oxide layer and skin of paint, the sandblasting layer have coarse structure, and the sandblasting floor is formed in the pre-blast area, described Oxide layer is formed in the housing outer surface and the sandblasting layer, and the skin of paint is formed in the oxide layer.
14. housing according to claim 13, it is characterised in that the sandblasting layer is arcuate structure.
15. housing according to claim 13, it is characterised in that the sandblasting layer includes the first sandblasting positioned at same layer Layer and the second sandblasting layer, the first sandblasting layer and the second sandblasting layer are spaced and be arranged in parallel, first sandblasting Layer is close to first side, and the second sandblasting layer is close to the 3rd side.
16. housing according to claim 13, it is characterised in that described second while and it is described 4th while distance be H1, The sandblasting layer is H2 in the height of second side to the 4th edge direction close to second side, the sandblasting layer, its In, 2/5H1 < H2 < 4/5H1.
17. housing according to claim 16, it is characterised in that the sandblasting layer is described first while to the described 3rd The width in direction is W, wherein, 1cm < W < 2cm.
18. the housing according to any one of claim 13 to 17, it is characterised in that the skin of paint includes the first paint Layer and the second skin of paint, second paint are formed on first skin of paint, and first skin of paint is formed in the oxygen Change on layer, first skin of paint is between the oxide layer and second skin of paint, the thickness of second skin of paint More than the thickness of first skin of paint.
19. housing according to claim 18, it is characterised in that in first skin of paint and the second skin of paint at least Layer of transparent is set.
20. a kind of electronic equipment, it is characterised in that including housing, the housing is such as any one of claim 12 to 19 institute The housing stated.
CN201711052520.7A 2017-10-30 2017-10-30 Shell manufacturing method, shell and electronic equipment Expired - Fee Related CN107911964B (en)