WO2006034980A1 - Method for replenishing or introducing light stabilizers - Google Patents
Method for replenishing or introducing light stabilizers Download PDFInfo
- Publication number
- WO2006034980A1 WO2006034980A1 PCT/EP2005/054716 EP2005054716W WO2006034980A1 WO 2006034980 A1 WO2006034980 A1 WO 2006034980A1 EP 2005054716 W EP2005054716 W EP 2005054716W WO 2006034980 A1 WO2006034980 A1 WO 2006034980A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- hydroxy
- coating
- bis
- benzotriazole
- butyl
- Prior art date
Abstract
Description
Claims